CN107791526A - 一种高效塑料焊接方法 - Google Patents
一种高效塑料焊接方法 Download PDFInfo
- Publication number
- CN107791526A CN107791526A CN201711084905.1A CN201711084905A CN107791526A CN 107791526 A CN107791526 A CN 107791526A CN 201711084905 A CN201711084905 A CN 201711084905A CN 107791526 A CN107791526 A CN 107791526A
- Authority
- CN
- China
- Prior art keywords
- welding
- plastics
- soldering tip
- plastic
- efficient plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Withdrawn
Abstract
一种高效塑料焊接方法,其特征在于包括以下步骤:首先把所需焊接的一个塑料用夹具固定;对焊头进行加热;然后把另一个塑料放置到所需焊接的塑料上,接着利用焊头对其进行接触,使两块塑料熔化后连接在一起;最后对其焊接的部位进行风吹冷却直到使其固化。本发明的高效塑料焊接方法,在塑料利用焊头进行热熔熔化后,再马上对焊接的部位进行风吹冷却使得固化,这样使得塑料焊接的部位焊接强度高,焊接效率也高,满足了生产的正常需求。
Description
技术领域
本发明涉及一种焊接方法,尤其涉及一种用于塑料的焊接方法。
背景技术
塑料制品的焊接方法有很多种,其中热焊接是一种普遍应用的塑料焊接。但是这种焊接方法在操作中存在着一些不足,塑料制品在采用热焊接的时候,一般都是直接采用焊头对塑料制品进行焊接,这样容易出现拉丝现象,导致焊接不成功,焊接质量差,焊接效率低下,影响了正常的生产。
发明内容
针对上述存在的技术问题,本发明的目的是:提出了一种焊接质量和焊接效率高的高效塑料焊接方法。
本发明的技术解决方案是这样实现的:一种高效塑料焊接方法,包括以下步骤:
一、首先把所需焊接的一块塑料用夹具固定起来;
二、对焊头进行加热;
三、然后把另一块塑料放置到所需焊接的塑料附近,接着利用焊头对其进行接触,使两块塑料熔化后连接在一起;
四、最后对其焊接的部位进行风吹冷却直到使其固化。
由于上述技术方案的运用,本发明与现有技术相比具有下列优点:本发明的高效塑料焊接方法,在塑料利用焊头进行热熔熔化后,再马上对焊接的部位进行风吹冷却使得固化,这样使得塑料焊接的部位焊接强度高,焊接效率也高,满足了生产的正常需求。
具体实施方式
本发明所述的一种高效塑料焊接方法,包括以下步骤:一、首先把所需焊接的一块塑料用夹具固定起来;二、对焊头进行加热;三、然后把另一块塑料放置到所需焊接的塑料附近,接着利用焊头对其进行接触,使两块塑料熔化后连接在一起;四、最后对其焊接的部位进行风吹冷却直到使其固化。
本发明的高效塑料焊接方法,在塑料利用焊头进行热熔熔化后,再马上对焊接的部位进行风吹冷却使得固化,这样使得塑料焊接的部位焊接强度高,焊接效率也高,满足了生产的正常需求。
上述实施例只为说明本发明的技术构思及特点,其目的在于让熟悉此项技术的人士能够了解本发明的内容并加以实施,并不能以此限制本发明的保护范围,凡根据本发明精神实质所作的等效变化或修饰,都应涵盖在本发明的保护范围内。
Claims (1)
1.一种高效塑料焊接方法,其特征在于:包括以下步骤:
首先把所需焊接的一个塑料用夹具固定;对焊头进行加热;然后把另一个塑料放置到所需焊接的塑料上,接着利用焊头对其进行接触,使两块塑料熔化后连接在一起;最后对其焊接的部位进行风吹冷却直到使其固化。