CN107498896A - The internal stress minimizing technology and method for paint spraying of plastic product - Google Patents

The internal stress minimizing technology and method for paint spraying of plastic product Download PDF

Info

Publication number
CN107498896A
CN107498896A CN201710695341.9A CN201710695341A CN107498896A CN 107498896 A CN107498896 A CN 107498896A CN 201710695341 A CN201710695341 A CN 201710695341A CN 107498896 A CN107498896 A CN 107498896A
Authority
CN
China
Prior art keywords
plastic product
diluent
internal stress
ethyl acetate
spraying
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201710695341.9A
Other languages
Chinese (zh)
Inventor
范红波
梁俊松
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhuhai Chunsheng Hardware Industrial Co Ltd
Original Assignee
Zhuhai Chunsheng Hardware Industrial Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhuhai Chunsheng Hardware Industrial Co Ltd filed Critical Zhuhai Chunsheng Hardware Industrial Co Ltd
Priority to CN201710695341.9A priority Critical patent/CN107498896A/en
Publication of CN107498896A publication Critical patent/CN107498896A/en
Pending legal-status Critical Current

Abstract

The present invention provides a kind of the internal stress minimizing technology and method for paint spraying of plastic product, and internal stress minimizing technology includes:In the surface spraying diluent of plastic product, diluent is derived from the diluent of solvent-based paints, the boiling point of diluent be 115.9 DEG C to 188 DEG C between, flash-point be 15.6 DEG C, burning-point is 448 DEG C, vapor pressure 2000Pa, density 0.815kg/m3;Processing is dried in the plastic product for spraying diluent.Method for paint spraying includes:The above method of learning from else's experience removes the plastic product of internal stress, is wiped, dust removal process, plastic product is painted using the solvent-based paints of above-mentioned dilution dilution agent, processing is dried to the plastic product after spray painting.The present invention can promote the internal stresses release of plastic product to come out by diluent, and the painted surface of plastic product is not cracked after spray painting.

Description

The internal stress minimizing technology and method for paint spraying of plastic product
Technical field
The present invention relates to the processing technique field of plastic product, more particularly to the internal stress minimizing technology of plastic product and spray Paint method.
Background technology
Plastic product is influenceed in melt-processed shaping by factors such as the orientation of macromolecular chain and cooling meats, Internal stress is produced in plastic product, in use, internal stress can slowly discharge plastic product, not interfere with plastics typically The outward appearance and performance of product.Plastic product is painting(Particularly solvent-based paints)During, the diluent in solvent-based paints The release of the internal stress of plastic product can be accelerated, crackle is formed on the surface of the paint of plastic product, influence the outer of plastic product See.
By adjusting the condition of injection molding, the effect for eliminating internal stress can be reached, but this method is more complicated, And its internal stress can not also be completely eliminated for complex-shaped plastic product, adjustment injection molding condition.Also have and pass through ultrasound The method that ripple cleaning machine eliminates the internal stress of plastic product occurs, but the equipment cost of supersonic wave cleaning machine is high, adds life Produce cost.
The content of the invention
The main object of the present invention is to provide that a kind of cost is low, the internal stress minimizing technology of the simple plastic product of method.
It is a further object of the present invention to provide a kind of method for paint spraying of plastic product.
In order to realize above-mentioned main purpose, the internal stress minimizing technology of plastic product provided by the invention includes, in plastics The surface spraying diluent of product, diluent are derived from the diluent of solvent-based paints, and the boiling point of diluent is 115.9 DEG C to 188 DEG C, flash-point be 15.6 DEG C, burning-point is 448 DEG C, vapor pressure 2000Pa, density 0.815kg/m3;Diluent will be sprayed Processing is dried in plastic product.
As seen from the above technical solution, the internal stresses release that can promote plastic product by diluent comes out, so as to go Except the internal stress of plastic product, the cost of diluent is low, and the internal stresses release method of plastic product is simple.
Further scheme is that drying process is natural air drying or drying.
Further scheme is, diluent be toluene, ethyl acetate, dimethylbenzene, hexone, ethyl acetate and The mixed solution of ethylbenzene.
Further scheme is, in percentage by weight, diluent include 35% to 40% toluene, 5% to 10% Ethyl acetate, 1% to 5% dimethylbenzene, 15% to 20% hexone, 25% to 30% ethyl acetate and 0.1% to 1% Ethylbenzene.
It can be seen that above-mentioned diluent is the diluent that common solvent-based paints use.
In order to realize above-mentioned another object, the method for paint spraying of plastic product provided by the invention includes, in plastic product Surface spraying diluent, diluent are derived from the diluent of solvent-based paints, and the boiling point of diluent is 115.9 DEG C to 188 DEG C, flash-point It it is 448 DEG C for 15.6 DEG C, burning-point, vapor pressure 2000Pa, density 0.815kg/m3;The plastic product of diluent will be sprayed Processing is dried;Plastic product is wiped, dust removal process;Using the solvent-based paints of dilution dilution agent to plastic product Painted;Processing is dried to the plastic product after spray painting.
As seen from the above technical solution, spray painting processing is carried out again after the internal stress of plastic product is discharged by diluent, can Effectively to prevent that plastic product discharges internal stress in painting process, therefore, will not go out after the paint drying on the surface of plastic product Existing crackle.
Further scheme is, diluent be toluene, ethyl acetate, dimethylbenzene, hexone, ethyl acetate and The mixed solution of ethylbenzene.
Further scheme is that in percentage by weight, diluent includes 35% to 40% toluene, 5% to 10% second Acetoacetic ester, 1% to 5% dimethylbenzene, 15% to 20% hexone, 25% to 30% ethyl acetate and 0.1% to 1% Ethylbenzene.
The invention has the advantages that by diluent by the internal stresses release of plastic product, prevent after spray painting in plastics The painted surface of product is cracked, influences the outward appearance of product.Discharge the dilution of the diluent and paint of plastic product internal stress Agent is same diluent, and both will not chemically react, and secondary stress will not be caused to discharge.
Embodiment
The internal stress minimizing technology embodiment of plastic product
The good plastic product of injection molding is taken, carries out dust removal process, then in the surface spraying diluent of plastic product, finally will Processing is dried in the plastic product of spraying diluent, can pass through natural air drying or drying.Internal stress is carried out to plastic product Check, plastic product internal stress free, reason is that diluent promotes the internal stresses release of plastic product to come out.
Diluent is derived from the diluent of solvent-based paints, the boiling point of diluent be 115.9 DEG C to 188 DEG C before, flash-point be 15.6 DEG C, burning-point be 448 DEG C, vapor pressure 2000Pa, density 0.815kg/m3, in percentage by weight, diluent Including 35% to 40% toluene, 5% to 10% ethyl acetate, 1% to 5% dimethylbenzene, 15% to 20% hexone, 25% to 30% ethyl acetate and 0.1% to 1% ethylbenzene.
The method for paint spraying embodiment of plastic product
The above method of learning from else's experience removes the plastic product of internal stress, is wiped, dust removal process, uses above-mentioned dilution dilution agent Solvent-based paints paint to plastic product, and processing is dried to the plastic product after spray painting, can pass through natural air drying Or drying.The plastic product after spray painting is checked, it is not cracked on the surface of paint.Diluent and removal due to spray painting The diluent of internal stress is identical, and chemical reaction is not present in same diluent, will not cause the release of secondary stress.
Certainly, above-described embodiment is only the preferable embodiment of the present invention, can also have more changes during practical application, Within the spirit and principles of the invention, any modification, equivalent substitution and improvements done etc., it should be included in power of the present invention In the protection domain that profit requires.

Claims (7)

1. the internal stress minimizing technology of plastic product, it is characterised in that:
In the surface spraying diluent of the plastic product, the diluent is derived from the diluent of solvent-based paints, the dilution The boiling point of agent be 115.9 DEG C to 188 DEG C between, flash-point be 15.6 DEG C, burning-point is 448 DEG C, vapor pressure 2000Pa, density are 0.815kg/m3
Processing is dried in the plastic product for spraying the diluent.
2. the internal stress minimizing technology of plastic product according to claim 1, it is characterised in that:
The drying process is natural air drying or drying.
3. the internal stress minimizing technology of plastic product according to claim 1, it is characterised in that:
The diluent is the mixed solution of toluene, ethyl acetate, dimethylbenzene, hexone, ethyl acetate and ethylbenzene.
4. the internal stress minimizing technology of plastic product according to claim 3, it is characterised in that:
In percentage by weight, the diluent include 35% to 40% toluene, 5% to 10% ethyl acetate, 1% to 5% Dimethylbenzene, 15% to 20% hexone, 25% to 30% ethyl acetate and 0.1% to 1% ethylbenzene.
5. the method for paint spraying of plastic product, it is characterised in that:
In the surface spraying diluent of the plastic product, the diluent is derived from the diluent of solvent-based paints, the dilution The boiling point of agent be 115.9 DEG C to 188 DEG C between, flash-point be 15.6 DEG C, burning-point is 448 DEG C, vapor pressure 2000Pa, density are 0.815kg/m3
Processing is dried in the plastic product for spraying the diluent;
The plastic product is wiped, dust removal process;
The plastic product is painted using the solvent-based paints of the dilution dilution agent;
Processing is dried to the plastic product after spray painting.
6. the method for paint spraying of plastic product according to claim 5, it is characterised in that:
The diluent is the mixed solution of toluene, ethyl acetate, dimethylbenzene, hexone, ethyl acetate and ethylbenzene.
7. the method for paint spraying of plastic product according to claim 6, it is characterised in that:
In percentage by weight, the diluent include 35% to 40% toluene, 5% to 10% ethyl acetate, 1% to 5% Dimethylbenzene, 15% to 20% hexone, 25% to 30% ethyl acetate and 0.1% to 1% ethylbenzene.
CN201710695341.9A 2017-08-15 2017-08-15 The internal stress minimizing technology and method for paint spraying of plastic product Pending CN107498896A (en)