CN107385671A - One kind is without net bat preparation method - Google Patents
One kind is without net bat preparation method Download PDFInfo
- Publication number
- CN107385671A CN107385671A CN201710787182.5A CN201710787182A CN107385671A CN 107385671 A CN107385671 A CN 107385671A CN 201710787182 A CN201710787182 A CN 201710787182A CN 107385671 A CN107385671 A CN 107385671A
- Authority
- CN
- China
- Prior art keywords
- cotton
- bat
- mill
- net bat
- net
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
Include the invention discloses one kind without net bat preparation method, methods described:By cotton by shredding, removal of impurities, combing, thin thin cotton piece is formed, lays the thin thin cotton piece is overlapping and is rolled into lap;The lap is cut apart with a knife or scissors from side, forms tampon blank, and manually pull and pave;The tampon blank is put on the even paper of mill and carries out first time grinding, sizing, is formed initially without net bat;Described be initially put into without net bat on the even cloth of mill is subjected to second of grinding, forms no net bat finished product;The even cloth of mill is specially the cloth that flatness error is no more than 0.02mm.In above-mentioned technical proposal, in second of process of lapping, traditional insulating paper is instead of with the even cloth of mill voluntarily developed, it is more smooth compared to insulating paper surface to grind even cloth, the bat come is ground, particle is finer and closely woven uniformly, and aesthetics, tensile strength are all more preferable.In addition, by 2 coiled, tampon blank uniform stresseds, make that bat fixed effect is more preferable, is unlikely to deform.Product more soft comfortable is durable in use.
Description
Technical field
The present invention relates to textile preparing technical field, and more particularly to one kind is without net bat preparation method.
Background technology
Traditional bat typically takes gined cotton to be fabricated to through cleaning, bullet pine, combing, shaping lapping yarn, grinding using plantation, has
There is the characteristics of hygroscopicity is strong, warming, healthy.
But in traditional bat preparation process be ground using traditional insulating paper at present, conventional insulator paper table
Face is not smooth high, causes the particle that the bat come is ground not fine and closely woven uniform enough, tensile strength deficiency.
Therefore, have that the bat particle that traditional bat manufacture craft makes is not uniformly fine and closely woven enough, and bat resists in the prior art
The technical problem of tensile strength deficiency.
The content of the invention
The invention provides one kind without net bat preparation method, made for solving traditional cotton tire present in prior art
The bat particle that technique makes is not uniformly fine and closely woven enough, the technical problem of bat tensile strength deficiency.
In order to solve the above-mentioned technical problem, technical scheme provided by the invention is as follows:
One kind is without net bat preparation method, it is characterised in that methods described includes:
By cotton by shredding, removal of impurities, combing, thin thin cotton piece is formed, lays the thin thin cotton piece is overlapping and is rolled into cotton
Volume;
The lap is cut apart with a knife or scissors from side, forms tampon blank, and manually pull and pave;
The tampon blank is put on the even paper of mill and carries out first time grinding, sizing, is formed initially without net bat;
Described be initially put into without net bat on the even cloth of mill is subjected to second of grinding, forms no net bat finished product;The mill
Even cloth is specially the cloth that flatness error is no more than 0.02mm.
Preferably, the shredding is specially:By the cotton block that the cotton shredding is 1g-2g.
Preferably, the removal of impurities is preliminary removal of impurities, is specifically included:Remove the obvious impurity in the cotton block and obvious short fibre
The gross weight of dimension, the obvious impurity and the obvious chopped fiber accounts for the 1% of cotton gross weight.
Preferably, after the removal of impurities, methods described also includes:
Cotton block after the removal of impurities is rolled into initial lap.
Preferably, the combing use carding machine, and the initial lap is combed, rejecting fine impurity and trickle short
Fiber, and form the thin thin cotton piece;Wherein, the gross weight of the fine impurity and the trickle chopped fiber accounts for cotton gross weight
7%.
Preferably, it is described by the tampon blank is put into progress first time grinding on the even paper of mill, shaping specifically includes:
The tampon blank is put on the even paper of mill and ground 2-4 minutes, it is ground to melt cotton fiber as one up and down
Body, makes that the upper and lower surface of cotton piece overlapping in the tampon blank forms the reticulate pattern that is interleaved with each other and the upper and lower surface of each layer cotton piece is formed
Fine particle;One side is ground and has carried out manual bound edge afterwards, then the other one side of grinding.
Preferably, it is described that described be initially put into without net bat on the even cloth of mill is subjected to second of grinding, form no net bat
Finished product, specifically include:
Described be initially put into without net bat on the even cloth of mill is ground into 14-20 minutes, made described initially without on net bat
Fine particle on per square inch reaches more than 140, average diameter of particles 1mm.
Compared with prior art, the present invention has the following technical effect that or advantage:
It is even with the mill voluntarily developed in second of process of lapping due to no net bat preparation method provided by the invention
Cloth instead of traditional insulating paper, grind the bat that even cloth is more smooth compared to insulating paper surface, is ground, particle is more
Refinement is close uniformly, and aesthetics, tensile strength are all more preferable.
It is coiled by 2 times due to no net bat preparation method provided by the invention, tampon blank uniform stressed, bat is shaped
Effect is more preferable, is unlikely to deform.Product more soft comfortable is durable in use.
Brief description of the drawings
Fig. 1 is a kind of method flow diagram of no net bat preparation method of the embodiment of the present invention.
Embodiment
The embodiments of the invention provide one kind without net bat preparation method, to solve traditional cotton present in prior art
The bat particle that tire manufacture craft makes is not uniformly fine and closely woven enough, the technical problem of bat tensile strength deficiency.
To make the purpose, technical scheme and advantage of the embodiment of the present invention clearer, below in conjunction with the embodiment of the present invention
In accompanying drawing, the technical scheme in the embodiment of the present invention is clearly and completely described, it is clear that described embodiment is
Part of the embodiment of the present invention, rather than whole embodiments.Based on the embodiment in the present invention, those of ordinary skill in the art
The every other embodiment obtained under the premise of creative work is not made, belongs to the scope of protection of the invention.
First, the background technology of the embodiment of the present invention is introduced.
Traditional bat typically takes gined cotton to be fabricated to through cleaning, bullet pine, combing, shaping lapping yarn, grinding using plantation, has
There is the characteristics of hygroscopicity is strong, warming, healthy.
But in traditional bat preparation process be ground using traditional insulating paper at present, conventional insulator paper table
Face is not smooth high, causes the particle that the bat come is ground not fine and closely woven uniform enough, tensile strength deficiency.
Therefore, have that the bat particle that traditional bat manufacture craft makes is not uniformly fine and closely woven enough, and bat resists in the prior art
The technical problem of tensile strength deficiency.
The embodiment of the present invention is described in detail below in conjunction with the accompanying drawings.
Fig. 1 is referred to, includes following step without net bat preparation method, methods described the embodiments of the invention provide one kind
Suddenly:
Step S101:By cotton by shredding, removal of impurities, combing, thin thin cotton piece is formed, will the overlapping lay of the carefully thin cotton piece
And it is rolled into lap.
In specific implementation process, cotton selects high quality cotton, such as 129A level cottons, and after choosing cotton, shredding cotton will
The mode of cotton shredding has, naturally it is also possible to shredding is carried out using machinery, in shredding
When, by the cotton block that cotton shredding is 1g-2g.
Further, after shredding cotton, exactly cotton is cleaned, the removal of impurities is preliminary removal of impurities, is exactly gone
Except the obvious impurity in the cotton block and obvious chopped fiber, it is total that the weight of the obvious impurity and the obvious chopped fiber accounts for cotton
The 1% of weight.
After preliminary removal of impurities, the cotton block after removal of impurities is rolled into initial lap.
After being rolled into initial lap, combed, the combing uses carding machine, and the initial lap is combed, picked
Except the fine impurity in the initial lap and trickle chopped fiber, and form the thin thin cotton piece;Wherein, the fine impurity and
The weight of the trickle chopped fiber accounts for the 7% of cotton gross weight.
In specific implementation process, the thin thin cotton piece is more thin more Bao Yuehao, after the thin thin cotton piece is formed, by institute
The overlapping lay of thin thin cotton piece is stated, and is rolled into lap.In lay that the thin thin cotton piece is overlapping, according to different weight standards,
The cotton piece number of plies is different, e.g., 3 kilograms without net bat, the paving cotton number of plies need to reach 1000 layers or so.
After completing step S101, step S102 is performed:The lap is cut apart with a knife or scissors from side, forms tampon blank, and manually pull
Pave.
In specific implementation process, according to the demand of user, tampon blank is pullled into corresponding size.
After completing step S102, step S103 is performed:The tampon blank is put on the even paper of mill and carries out first time grinding, is determined
Type, formed initially without net bat.
In specific implementation process, first, even paper (insulating paper) will be ground and be fixed on the case platform of grinder, then by institute
State tampon blank and be put into grinding 2-4 minutes on the even paper of mill, it is ground that cotton fiber combines together up and down, make the tampon blank
In the upper and lower surface of overlapping cotton piece form the reticulate pattern being interleaved with each other and the upper and lower surface of each layer cotton piece forms fine particle;Grind
Manual bound edge is carried out after simultaneously, then the other one side of grinding.
After completing step S104, step S104 is performed:Described be initially put into without net bat on the even cloth of mill is carried out second
Grinding, forms no net bat finished product;The even cloth of mill is specially the cloth that flatness error is no more than 0.02mm.
It is to make to grind even cloth first, by latex, paste with 1 in specific implementation process:5 proportioning is blent,
Purified cotton cloth is put into wherein, is soaked 5 minutes, taking-up is dried;After soaking, drying repeatedly for three times, choose flatness error and be no more than
0.02mm cloth is as the even cloth of mill for grinding use for the second time.Then the even cloth of mill is fixed on grinder, then
Described be initially put into without net bat on the even cloth of mill is ground into 14-20 minutes, made described initially without every square of English on net bat
Fine particle on very little reaches more than 140, average diameter of particles 1mm.
Said one or multiple technical schemes in the embodiment of the present invention, at least there is following one or more technology effects
Fruit:
In the embodiment of the present invention, due in second of process of lapping, instead of with the even cloth of mill voluntarily developed traditional
Insulating paper, the bat that even cloth is more smooth compared to insulating paper surface, is ground is ground, particle is finer and closely woven uniformly, beautiful
Sight degree, tensile strength are all more preferable.
Further, due in invention embodiment, by 2 times in rolls, tampon blank uniform stressed, making bat shape
Effect is more preferable, is unlikely to deform.Product more soft comfortable is durable in use.
The general principle and principal character and advantages of the present invention of the present invention has been shown and described above.The technology of the industry
Personnel are not departing from spirit and scope of the invention it should be appreciated that merely illustrating the principles of the invention described in this specification
Under the premise of, various changes and modifications of the present invention are possible, and these changes and improvements all fall within the protetion scope of the claimed invention,
The scope of the present invention is defined by the appended claims and its equivalents.
Claims (7)
1. one kind is without net bat preparation method, it is characterised in that methods described includes:
By cotton by shredding, removal of impurities, combing, thin thin cotton piece is formed, lays the thin thin cotton piece is overlapping and is rolled into lap;
The lap is cut apart with a knife or scissors from side, forms tampon blank, and manually pull and pave;
The tampon blank is put on the even paper of mill and carries out first time grinding, sizing, is formed initially without net bat;
Described be initially put into without net bat on the even cloth of mill is subjected to second of grinding, forms no net bat finished product;The even cloth of mill
Specially flatness error is no more than 0.02mm cloth.
2. as claimed in claim 1 without net bat preparation method, it is characterised in that the shredding is specially:By the cotton
Shredding is 1g-2g cotton block.
3. as claimed in claim 2 without net bat preparation method, it is characterised in that the removal of impurities is preliminary removal of impurities, specifically bag
Include:Remove the gross weight of the obvious impurity in the cotton block and obvious chopped fiber, the obvious impurity and the obvious chopped fiber
Account for the 1% of cotton gross weight.
4. as claimed in claim 3 without net bat preparation method, it is characterised in that after the removal of impurities, methods described is also
Including:
Cotton block after the removal of impurities is rolled into initial lap.
5. as claimed in claim 4 without net bat preparation method, it is characterised in that the combing uses carding machine, to described
Initial lap is combed, and rejects fine impurity and trickle chopped fiber, forms the thin thin cotton piece;Wherein, the fine impurity
The 7% of cotton gross weight is accounted for the gross weight of the trickle chopped fiber.
6. as claimed in claim 1 without net bat preparation method, it is characterised in that described that the tampon blank is put on the even paper of mill
Carry out first time grinding, sizing specifically includes:
The tampon blank is put on the even paper of mill and ground 2-4 minutes, it is ground that cotton fiber combines together up and down, make
The reticulate pattern and the upper and lower surface of each layer cotton piece that the upper and lower surface formation of overlapping cotton piece is interleaved with each other in the tampon blank form trickle
Particle;One side is ground and has carried out manual bound edge afterwards, then the other one side of grinding.
7. as claimed in claim 1 without net bat preparation method, it is characterised in that described to be initially put into described without net bat
Grind and second of grinding is carried out on even cloth, form no net bat finished product, specifically include:
Described be initially put into without net bat on the even cloth of the mill is ground into 14-20 minutes, made described initially without often being put down on net bat
Fine particle on square inch reaches more than 140, average diameter of particles 1mm.