CN107214060A - One kind is by decorations body surface coating process - Google Patents
One kind is by decorations body surface coating process Download PDFInfo
- Publication number
- CN107214060A CN107214060A CN201710645075.9A CN201710645075A CN107214060A CN 107214060 A CN107214060 A CN 107214060A CN 201710645075 A CN201710645075 A CN 201710645075A CN 107214060 A CN107214060 A CN 107214060A
- Authority
- CN
- China
- Prior art keywords
- body surface
- facial mask
- hypoglyph
- decorations
- spraying
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses one kind by decorations body surface coating process, comprise the following steps, handled by decorations body surface, upper counterdie, upper facial mask is dried;The present invention by decorations body surface coating process, simple to operate, what the film with color and luster or color can be tightly is attached to by decorations body surface, is not in fade or decolouring phenomenon.
Description
Technical field
The invention belongs to body surface furnishing fields, more particular to one kind is by decorations body surface coating process.
Background technology
In order to enrich the life of people, people often spray various colors in body surface or spray various colors, color and luster
Film so that object seems rich and varied.
The content of the invention
It is simple to operate it is an object of the invention to provide one kind by decorations body surface coating process, with color and luster or color
Film can be tightly be attached to by decorations body surface, be not in fade or decolouring phenomenon.
Technical solution of the present invention one kind is comprised the following steps by decorations body surface coating process,
The first step, is handled by decorations body surface
(1)Ash is greasy:Will be flat or grey smooth by decorations body surface ash with putty;
(2)Sand is beaten:With sand paper polish ash it is greasy after by decorations body surface;
(3)Look for greasy:Carried out looking for greasy by decorations body surface to unsmooth or aperture class so that the decorations smooth smoothness of body surface, nothing
Slit;
(4)Carefully beat:It will be tied with fine sandpaper by decorations body surface or smooth;
(5)Remove:It will be cleaned out by the dust of decorations body surface, particulate matter;
Second step, upper counterdie
(1)Spray the first hypoglyph:The first hypoglyph is uniformly sprayed to by decorations body surface, and the first hypoglyph is by counterdie, solid
Agent and diluent are mixed, and wherein the proportioning of counterdie, curing agent and diluent is 1:0.5:1;
(2)Sand is beaten:After the first hypoglyph is sprayed two hours, the first hypoglyph is polished with fine sandpaper, makes first layer bottom
The smooth smoothness of film;
(3)Spray the second hypoglyph and third layer counterdie:Successively to first the second hypoglyph of hypoglyph surface spraying and third layer
Counterdie, and the counterdie just sprayed is polished with fine sandpaper after every hypoglyph is sprayed two hours;
3rd step, upper facial mask
(1)Early-stage preparations:Dust granule material on removing counterdie, the facial mask of the different color and lusters of preparation, facial mask color and luster at least four,
There are heavy color, light color, light phase advancing coloud nearside and contrastive colours respectively, and account for 10%, 60%, 20% and the 10% of facial mask total amount, face difference successively
The facial mask of color and luster is mixed by facial mask, curing agent and diluent, and the proportioning of facial mask, curing agent and diluent is 1:0.5:
1.2, each group color and luster facial mask stands 5 to 10 minutes after stirring, and prepares spray gun 4;
(2)Upper facial mask:First with spray gun in the light facial mask of body surface to be onstructed spraying twice,
Then with spray gun in body surface to be onstructed spraying together light phase advancing coloud nearside facial mask,
Again afterwards with spray gun in body surface to be onstructed spraying weight color facial mask, during spraying, by spray gun air pressure adjustment to minimum value, weight color
Facial mask coating thickness is thin, and spraying profile is simple, and track should not be excessively and overlapping;
Finally with spray gun body surface to be onstructed it is irregular spraying contrastive colours facial mask, during spraying, by spray gun air pressure adjustment extremely
Normal value, during spraying, finger control spray gun air pressure size interval shape spraying;
4th step, is dried, and will spray being placed in by jewelry body in dustless space after facial mask, and standing is got product for 72 hours.
It is preferred that, described can be that plane can also be concave-convex curved surface by decorations body surface.
It is preferred that, the first step(2)Middle sand paper is 600# sand paper, the first step(4)Medium-fine sand paper is 1000# sand paper, the
Two steps(2)Medium-fine sand paper is 1000# sand paper, second step(3)Medium-fine sand paper is 1000# sand paper.
It is preferred that, spray gun model W71 used in the 3rd step.
It is preferred that, mulch film is PE counterdies or PU counterdies in the second step.
The technology of the present invention beneficial effect:
Technical solution of the present invention one kind passes through coating process by decorations body surface coating process so that the coloured film of tool can
Firm attachment is body surface, is not in decolourize or the phenomenon that fades, can produce the film of various shapes and color so that
Enriched by decorations color of object surface, pattern variation.
Embodiment
For ease of skilled artisan understands that technical solution of the present invention, in conjunction with specific embodiment or embodiment to this
Inventive technique scheme is described further.
One kind is comprised the following steps by decorations body surface coating process,
The first step, is handled by decorations body surface
(1)Ash is greasy:Will be flat or grey smooth by decorations body surface ash with putty, can be that plane can also be recessed by decorations body surface
Convex uneven Irregular Boundary Surface;
(2)Sand is beaten:With 600# sand paper polish ash it is greasy after by decorations body surface;
(3)Look for greasy:Carried out looking for greasy by decorations body surface to unsmooth or aperture class so that the decorations smooth smoothness of body surface, nothing
Slit;
(4)Carefully beat:It will be tied with 1000# fine sandpapers by decorations body surface or smooth;
(5)Remove:It will be cleaned out by the dust of decorations body surface, particulate matter;
Second step, upper counterdie
(1)Spray the first hypoglyph:Uniformly spray the first hypoglyph to by decorations body surface, the first hypoglyph by PE counterdies or
PU counterdies, curing agent and diluent are mixed, and wherein the proportioning of counterdie, curing agent and diluent is 1:0.5:1;
(2)Sand is beaten:After the first hypoglyph is sprayed two hours, the first hypoglyph is polished with 1000# fine sandpapers, makes first
The smooth smoothness of hypoglyph;
(3)Spray the second hypoglyph and third layer counterdie:Successively to first the second hypoglyph of hypoglyph surface spraying and third layer
Counterdie, and the counterdie just sprayed is polished with 1000# fine sandpapers after every hypoglyph is sprayed two hours;
3rd step, upper facial mask
(1)Early-stage preparations:Dust granule material on removing counterdie, the facial mask of the different color and lusters of preparation, facial mask color and luster at least four,
There are heavy color, light color, light phase advancing coloud nearside and contrastive colours respectively, and account for 10%, 60%, 20% and the 10% of facial mask total amount, face difference successively
The facial mask of color and luster is mixed by facial mask, curing agent and diluent, and the proportioning of facial mask, curing agent and diluent is 1:0.5:
1.2, each group color and luster facial mask stands 5 to 10 minutes after stirring, and prepares 4 W71 spray guns;
(2)Upper facial mask:First with spray gun in the light facial mask of body surface to be onstructed spraying twice,
Then with spray gun in body surface to be onstructed spraying together light phase advancing coloud nearside facial mask,
Again afterwards with spray gun in body surface to be onstructed spraying weight color facial mask, during spraying, by spray gun air pressure adjustment to minimum value, weight color
Facial mask coating thickness is thin, and spraying profile is simple, and track should not be excessively and overlapping;
Finally with spray gun body surface to be onstructed it is irregular spraying contrastive colours facial mask, during spraying, by spray gun air pressure adjustment extremely
Normal value, during spraying, finger control spray gun air pressure size interval shape spraying;
4th step, is dried, and will spray being placed in by jewelry body in dustless space after facial mask, and standing is got product for 72 hours.
Invention is exemplarily described above in conjunction with embodiment for technical solution of the present invention, it is clear that the present invention is specific real
Now it is not subject to the restrictions described above, as long as employing the various unsubstantialities of inventive concept and technical scheme of the present invention progress
Improve, or it is not improved the design of invention and technical scheme are directly applied into other occasions, the equal protection models in the present invention
Within enclosing.
Claims (5)
1. one kind is by decorations body surface coating process, it is characterised in that comprise the following steps,
The first step, is handled by decorations body surface
(1)Ash is greasy:Will be flat or grey smooth by decorations body surface ash with putty;
(2)Sand is beaten:With sand paper polish ash it is greasy after by decorations body surface;
(3)Look for greasy:Carried out looking for greasy by decorations body surface to unsmooth or aperture class so that the decorations smooth smoothness of body surface, nothing
Slit;
(4)Carefully beat:It will be tied with fine sandpaper by decorations body surface or smooth;
(5)Remove:It will be cleaned out by the dust of decorations body surface, particulate matter;
Second step, upper counterdie
(1)Spray the first hypoglyph:The first hypoglyph is uniformly sprayed to by decorations body surface, and the first hypoglyph is by counterdie, solid
Agent and diluent are mixed, and wherein the proportioning of counterdie, curing agent and diluent is 1:0.5:1;
(2)Sand is beaten:After the first hypoglyph is sprayed two hours, the first hypoglyph is polished with fine sandpaper, makes first layer bottom
The smooth smoothness of film;
(3)Spray the second hypoglyph and third layer counterdie:Successively to first the second hypoglyph of hypoglyph surface spraying and third layer
Counterdie, and the counterdie just sprayed is polished with fine sandpaper after every hypoglyph is sprayed two hours;
3rd step, upper facial mask
(1)Early-stage preparations:Dust granule material on removing counterdie, the facial mask of the different color and lusters of preparation, facial mask color and luster at least four,
There are heavy color, light color, light phase advancing coloud nearside and contrastive colours respectively, and account for 10%, 60%, 20% and the 10% of facial mask total amount, face difference successively
The facial mask of color and luster is mixed by facial mask, curing agent and diluent, and the proportioning of facial mask, curing agent and diluent is 1:0.5:
1.2, each group color and luster facial mask stands 5 to 10 minutes after stirring, and prepares spray gun 4;
(2)Upper facial mask:First with spray gun in the light facial mask of body surface to be onstructed spraying twice,
Then with spray gun in body surface to be onstructed spraying together light phase advancing coloud nearside facial mask,
Again afterwards with spray gun in body surface to be onstructed spraying weight color facial mask, during spraying, by spray gun air pressure adjustment to minimum value, weight color
Facial mask coating thickness is thin, and spraying profile is simple, and track should not be excessively and overlapping;
Finally with spray gun body surface to be onstructed it is irregular spraying contrastive colours facial mask, during spraying, by spray gun air pressure adjustment extremely
Normal value, during spraying, finger control spray gun air pressure size interval shape spraying;
4th step, is dried, and will spray being placed in by jewelry body in dustless space after facial mask, and standing is got product for 72 hours.
2. one kind according to claim 1 is by decorations body surface coating process, it is characterised in that described by decorations body surface
Can be that plane can also be concave-convex curved surface.
3. one kind according to claim 1 is by decorations body surface coating process, it is characterised in that the first step(2)In
Sand paper is 600# sand paper, the first step(4)Medium-fine sand paper is 1000# sand paper, second step(2)Medium-fine sand paper is 1000# sand paper, second
Step(3)Medium-fine sand paper is 1000# sand paper.
4. one kind according to claim 1 is by decorations body surface coating process, it is characterised in that used in the 3rd step
Spray gun model W71.
5. one kind according to claim 1 is by decorations body surface coating process, it is characterised in that mulch film in the second step
For PE counterdies or PU counterdies.