CN107088581A - 一种检查清理热轧机组机架上锈蚀物的方法 - Google Patents
一种检查清理热轧机组机架上锈蚀物的方法 Download PDFInfo
- Publication number
- CN107088581A CN107088581A CN201710433646.2A CN201710433646A CN107088581A CN 107088581 A CN107088581 A CN 107088581A CN 201710433646 A CN201710433646 A CN 201710433646A CN 107088581 A CN107088581 A CN 107088581A
- Authority
- CN
- China
- Prior art keywords
- clear
- high pressure
- spades
- check
- twisted
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明属于热轧设备维护技术领域,公开了一种检查清理热轧机组机架上锈蚀物的方法,通过按机架间、机架上、衬板内外等空间定位方法,结合机械清理和高压水冲洗,使机组在检修恢复后保持在洁净状态,进而减少锈蚀物掉落。该方法可使热轧机组在长时间停机恢复生产后锈蚀物掉落大大减少,同时保证带钢表面质量满足客户需求并减少了金属损失,提高了经济效益。
Description
技术领域
本发明涉及热轧设备维护技术领域,特别涉及一种检查清理热轧机组机架上锈蚀物的方法。
背景技术
热轧机组机架上以及机架之间的设备部分因常年经干湿、冷热交替影响,结构部件会不断锈蚀、腐蚀,当热轧轧制带钢穿带过程中轧机产生震动,导致锈蚀物掉落到带钢表面产生异物压入缺陷甚至后道工序孔洞缺陷,为保证产品交货质量不得不切除缺陷部分,造成成材率损失,进而导致大量经济损失。
发明内容
本发明提供一种检查清理热轧机组机架上锈蚀物的方法,解决现有技术中热轧机组锈蚀物掉落影响带钢表面质量的技术问题。
为解决上述技术问题,本发明提供了一种检查清理热轧机组机架上锈蚀物的方法,包括:
检查并清理F2-F7精轧机入口侧导板侧面衬板、内侧上面以及水平面和立面之间的缝隙里的锈蚀及粘钢,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F2~F7精轧机入口护板立面和下平面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F6精轧机出口上导卫下表面锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机入口刮板护板夹缝锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间冷却集水管及护板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理
检查并清理F2~F7精轧机入口刮板气缸固定梁锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水护板收集槽锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理;
检查并清理F1~F6精轧机出口机架护板,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机进出口扁担梁侧面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理,包括上面的螺栓。
本申请实施例中提供的一个或多个技术方案,至少具有如下技术效果或优点:
本申请实施例中提供的检查清理热轧机组机架上锈蚀物的方法,通过按机架间、机架上、衬板内外的空间定位方法,结合机械清理和高压水冲洗,使机组在检修恢复后保持在洁净状态,进而减少锈蚀物掉落。该方法可使热轧机组在长时间停机恢复生产后锈蚀物掉落大大减少,同时保证带钢表面质量满足客户需求并减少了金属损失,提高了经济效益。
具体实施方式
本申请实施例通过提供一种检查清理热轧机组机架上锈蚀物的方法,解决现有技术中热轧机组锈蚀物掉落影响带钢表面质量的技术问题。
为了更好的理解上述技术方案,下面将结合说明书及具体的实施方式对上述技术方案进行详细说明,应当理解本发明实施例以及实施例中的具体特征是对本申请技术方案的详细的说明,而不是对本申请技术方案的限定,在不冲突的情况下,本申请实施例以及实施例中的技术特征可以相互组合。
一种检查清理热轧机组机架上锈蚀物的方法,包括:
检查并清理F2-F7精轧机入口侧导板侧面衬板、内侧上面以及水平面和立面之间的缝隙里的锈蚀及粘钢,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F2~F7精轧机入口护板立面和下平面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F6精轧机出口上导卫下表面锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机入口刮板护板夹缝锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间冷却集水管及护板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理
检查并清理F2~F7精轧机入口刮板气缸固定梁锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水护板收集槽锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理;
检查并清理F1~F6精轧机出口机架护板,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机进出口扁担梁侧面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理,包括上面的螺栓。
全面、清晰掌握常规热轧机组机架上以及机架间设备部件上锈蚀物检查、清理方法,减少机架上锈蚀物、铁皮灰等异物的掉落,通过按机架间、机架上、衬板内外等空间定位方法,结合机械清理和高压水冲洗,使机组在检修恢复后保持在洁净状态,进而减少锈蚀物掉落。
本申请实施例中提供的一个或多个技术方案,至少具有如下技术效果或优点:
本申请实施例中提供的检查清理热轧机组机架上锈蚀物的方法,通过按机架间、机架上、衬板内外的空间定位方法,结合机械清理和高压水冲洗,使机组在检修恢复后保持在洁净状态,进而减少锈蚀物掉落。该方法可使热轧机组在长时间停机恢复生产后锈蚀物掉落大大减少,同时保证带钢表面质量满足客户需求并减少了金属损失,提高了经济效益。
最后所应说明的是,以上具体实施方式仅用以说明本发明的技术方案而非限制,尽管参照实例对本发明进行了详细说明,本领域的普通技术人员应当理解,可以对本发明的技术方案进行修改或者等同替换,而不脱离本发明技术方案的精神和范围,其均应涵盖在本发明的权利要求范围当中。
Claims (1)
1.一种检查清理热轧机组机架上锈蚀物的方法,其特征在于,包括:
检查并清理F2-F7精轧机入口侧导板侧面衬板、内侧上面以及水平面和立面之间的缝隙里的锈蚀及粘钢,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F2~F7精轧机入口护板立面和下平面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F6精轧机出口上导卫下表面锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机入口刮板护板夹缝锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间冷却集水管及护板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理
检查并清理F2~F7精轧机入口刮板气缸固定梁锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水护板收集槽锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理机架间挡水板锈蚀物,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理;
检查并清理F1~F6精轧机出口机架护板,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗;
检查并清理F1-F7精轧机进出口扁担梁侧面,先用铁铲、钢刷或绞磨机等清理工具敲击、清铲或打磨,最后用高压水冲洗,内外侧都要清理,包括上面的螺栓。