CN106835718A - A kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying - Google Patents

A kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying Download PDF

Info

Publication number
CN106835718A
CN106835718A CN201710013398.6A CN201710013398A CN106835718A CN 106835718 A CN106835718 A CN 106835718A CN 201710013398 A CN201710013398 A CN 201710013398A CN 106835718 A CN106835718 A CN 106835718A
Authority
CN
China
Prior art keywords
pure cotton
cotton fabric
drying
sorting
moisture absorbing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201710013398.6A
Other languages
Chinese (zh)
Other versions
CN106835718B (en
Inventor
吴懋盛
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Foshan Dahe Weaving Co ltd
Foshan Guangjia Textile Technology Co ltd
Original Assignee
Foshan Jiaxing Textile Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Foshan Jiaxing Textile Technology Co Ltd filed Critical Foshan Jiaxing Textile Technology Co Ltd
Priority to CN201710013398.6A priority Critical patent/CN106835718B/en
Publication of CN106835718A publication Critical patent/CN106835718A/en
Application granted granted Critical
Publication of CN106835718B publication Critical patent/CN106835718B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention discloses a kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying, comprises the following steps:It is concise:Wetting agent is added in concise operation;Dyeing;Fixation;Washing;Dispersant treatment:Dispersant is added to be processed;It is excessively soft in bath:Processed using hydrophilic softener;Dehydration;Drying.The method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying of the invention, make textile cotton yarn at the same have moisture absorption, perspire, the function of quick-drying, with good penetrability and gas permeability, allow the very quick inspiration of sweat to pure cotton fiber the inside and quickly spread apart makes the pure cotton textile dry and comfortable comfortable so as to reach moisture absorbing and sweat releasing quick-drying function.

Description

A kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying
Technical field
The present invention relates to pure cotton fabric finishing field, a kind of method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying is related generally to And pure cotton fabric.
Background technology
With the improvement of people ' s living standards with the development of textile industry, consumer is to the comfortableness of clothes, outward appearance and function Property pursue more and more higher.Therefore, the development trend that material that is not only comfortable but also having certain function is textile from now on is produced.
Natural fiber, particularly pure cotton material, its comfortableness and the feature of environmental protection are very popular with consumers.Pure cotton has The features such as warming, heat-resisting, alkaline-resisting, health does not stimulate skin, there is certain hygroscopicity, but will be next to the skin after moisture absorption, makes to disappear Expense person feels uncomfortable.Exploitation is with quickly absorb water, perspire pure cotton functional material and product gesture rapid, that perspire quick-drying function Must go, and product should also have comfortable and easy to wear, dry and comfortable, good hand touch, have good appearance and washing fastness.Each world brand exists Just always in the pure cotton material of the ceaselessly moisture absorbing and sweat releasing quick-drying of exploitation pure cotton after into Chinese market, but all do not succeed always The fast dry substance of pure cotton moisture absorbing and sweat releasing for meeting national standard and international standard is developed, such as NIKE, ADIDAS brand is 2004 The team for just having specialty year develops.It to do the chemical fiber material of moisture absorbing and sweat releasing quick drying technology is skill that Under Armour brands are The art strong point wins one of consumer typical brand, even so, also successfully the moisture absorbing and sweat releasing of exploitation pure cotton is not fast Dry material and production technology.
Therefore, prior art has yet to be improved and developed.
The content of the invention
In view of above-mentioned the deficiencies in the prior art, it is an object of the invention to provide a kind of pure cotton fabric moisture absorbing and sweat releasing quick-drying Method for sorting and pure cotton fabric, it is intended to solve the problems, such as that existing pure-cotton fabric cannot be while accomplish the function of moisture absorbing and sweat releasing quick-drying.
Technical scheme is as follows:
A kind of method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, comprise the following steps:
It is concise:Wetting agent is added in concise operation;
Dyeing;
Fixation:
Washing;
Dispersant treatment:Dispersant is added to be processed;
It is excessively soft in bath:Processed using hydrophilic softener;
Dehydration;
Drying.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the wetting agent is by hydrophilic group and oleophylic The surfactant of base composition;The wetting agent is silanol class nonionic surfactant.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the time of concise operation is 10 ~ 60 minutes, Treatment temperature is 30 ~ 80 DEG C, and the consumption of the wetting agent is 15-30g/L.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the wetting agent is polyether-modified poly- organic Silicone compounds.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the dispersant is polyethylene glycol 200 or poly- Ethylene glycol 400.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the process time of dispersant treatment process is 15-80 minutes, treatment temperature was 40 ~ 60 DEG C, and the consumption of the dispersant is 1-20g/L.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the hydrophilic softening agent be fatty amine and its Derivative species, organic silicon and their complex;The silicone softening agent for using is polyether-modified oxirane, epoxy The organic silicon softening agent of propane polymerization.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the process time of excessively soft operation is in bath 10-30 minutes, treatment temperature was 30-50 DEG C, and the consumption of hydrophilic softening agent is 1-10g/ L.
The method for sorting of described pure cotton fabric moisture absorbing and sweat releasing quick-drying, wherein, the process time of washing operation is 5 ~ 60 points Clock, treatment temperature is 50 ~ 60 DEG C, and the consumption of detergent is 0.5-3g/L;
The process time of laking procedure is 15 ~ 65 minutes, and treatment temperature is 30 ~ 90 DEG C, and the consumption of color fixing agent is 1-5g/L;
The treatment temperature of baking operation is 100 ~ 130 DEG C.
A kind of pure cotton fabric, wherein, the pure cotton fabric is whole using pure cotton fabric moisture absorbing and sweat releasing quick-drying as described above Reason method is processed.
Beneficial effect:The method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying of the invention, makes textile cotton yarn while having suction It is wet, perspire, the function of quick-drying, with good penetrability and gas permeability, allow the very quick inspiration of sweat to pure cotton fiber The inside and quickly spread apart makes the pure cotton textile dry and comfortable comfortable so as to reach moisture absorbing and sweat releasing quick-drying function.Using described The method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying carries out processing the textile cotton yarn for obtaining has advantages below:
1st, by the evaluation of national standard GB/T 21655.1-2008 textile absorbing fast-dryings, its measure wicking height can reach More than 150mm, water absorption rate can reach more than 230%, and the moisture diffusion time is as short as within 1.4s, and moisture evaporation speed reaches To more than 0.23g/h, each side index is much higher by professional standard.Can effectively absorb and discharge body surface sweat, especially Suitable for dress and personal adornment such as tights, shirt, easy dress, gym suit, socks, underwears;Sultry and viscous body of perspiring can be solved to ask Topic, can also improve the comfortableness of tights, improve value-added content of product.
2nd, using 100% pure-cotton fabric, there is good feel by hydrophilic soft finish, with excellent wearing comfort.
3rd, with fabulous washing fastness, according to AATCC143 washing methods can with resistance to more than 10 times home washings, Can keep good performance, and colour fading after washing is also little.
Specific embodiment
The present invention provides a kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying, to make mesh of the invention , technical scheme and effect it is clearer, clear and definite, the present invention is described in more detail below.It should be appreciated that described herein Specific embodiment be only used to explain the present invention, be not intended to limit the present invention.
A kind of method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying provided by the present invention, is the finisher to textile cotton yarn Skill carries out the pretreatment of difference in functionality, make textile cotton yarn and meanwhile have moisture absorption, perspire, the function of quick-drying.
Specifically, the method for sorting of the pure cotton fabric moisture absorbing and sweat releasing quick-drying, comprises the following steps:
It is concise:Wetting agent is added in concise operation, the time of concise operation is 10 ~ 60 minutes, and treatment temperature is 30 ~ 80 DEG C, The consumption of the wetting agent is 15-30g/L;
Dyeing;With conventional disperse dyestuff normal procedure and technique;
Fixation:With conventional color fixing agent normal procedure and technique;
Washing:The process time of washing operation is 5 ~ 60 minutes, and treatment temperature is 50 ~ 60 DEG C, and the consumption of detergent is 0.5-3g/ L;
Dispersant treatment:Dispersant is added after washing, the process time of dispersant treatment process is 15-80 minutes, treatment temperature It is 40 ~ 60 DEG C to spend, and the consumption of the dispersant is 1-20g/L;
It is excessively soft in bath:Using hydrophilic softener, process time is 10-30 minutes, and treatment temperature is 30-50 DEG C;Consumption is 1-10g/ L。
Dehydration;Normal procedure and technique
Drying:The temperature of drying is 100 ~ 130 DEG C.
Wherein, kiering, dyeing, fixation, washing etc. is processed by normal plant process, and wetting is simply added in scouring process Agent, makes textile cotton yarn have the function of quick water suction;Increase dispersant treatment process after washing operation, there is textile cotton yarn The water that inspiration is gone(Sweat)The effect come can be quickly spread apart, the function of fast row's quick-drying is reached.
The surfactant that the wetting agent is made up of hydrophilic group and lipophilic group, the species of the wetting agent can be silanol Class nonionic surfactant, feature:Molecular weight is low, and many hydrophobic groups are in umbrella shape symmetrical structure, compared with traditional activated dose, profit Wet, infiltration sex expression is extremely excellent, efficient, is revolutionary surfactant of new generation.Dynamic and static surface tension is extremely low, contains Double hydroxyls, response type activating agent, chemical property is inertia, is typically not involved in the chemical reaction of system, and resistance to acids and bases is good, chemically Matter stabilization.Preferably, the wetting agent can be polyether-modified polyorganosiloxane compounds.When being contacted with the surface of solids, Lipophilic group is attached to the surface of solids, during hydrophilic group is outwards towards liquid, liquid is formed continuous phase in the surface of solids, here it is profit The general principle of wet effect is that can be aligned on the surface of solution, and can make the material that surface tension is remarkably decreased, so as to reach To the function of quick water suction.In technical solution of the present invention, the consumption of the wetting agent is 15-30g/L.
Processed according to common process using conventional color fixing agent in the laking procedure.During the treatment of laking procedure Between can be:The fixation time is 15 ~ 65 minutes, and treatment temperature is 30 ~ 90 DEG C, and the consumption of color fixing agent is 1-5g/L.
It is to be processed using common detergent in the washing operation, consumption is 0.5-3g/L.
The species of the dispersant is polyethylene glycol 200 or PEG400(Molecular weight about 190-420), it is water-soluble Fine dispersion agent/solubilizer/wetting agent/the solvent of dispersion.Polyethylene glycol 200 400 is oleophylic, can be very good with The dispersion for having relatively low hydrophilic lipophilic balance (HLB value) forms the dispersion of stabilization.Substantially the original of dispersant effect Reason:Diffusion area in laws of diffusion, i.e. same time, diffusingsurface is bigger, and volatilization is bigger, so will do soon.Make pure cotton The water that cotton yarn can go inspiration(Sweat)Rapidly spread apart and, so as to reach the function of fast row's quick-drying.In technical solution of the present invention In, the consumption of the dispersant is 10-20g/L.
In the bath in excessively soft operation, use hydrophilic softener, hydrophilic softener can for fatty amine and its Derivative species, organic silicon and their complex.The silicone softening agent for using is polyether-modified oxirane, epoxy The organic silicon softening agent of propane polymerization, wherein consumption are 1-10g/ L.The benefit processed using hydrophilic softener is product Crossing after softness will not hinder the water imbibition and diffusivity of pure cotton material, and the softening agent of general category silicone oil is draining, so will From water imbibition softening agent.
At present, general textile cotton yarn can only accomplish the function of moisture absorption or quick-drying, because generally in the art by cotton Yarn carries out hydrophilic treated, makes it have moisture absorbing, but cotton yarn is hydrophilic, is difficult quick-drying, will be next to the skin after cotton yarn moisture absorption, makes to disappear Expense person feels uncomfortable;And hydrophobic treatment is carried out to cotton yarn, quick-drying function is made it have, but cotton yarn is hydrophobic, is difficult moisture absorption, disappears Its skin surface then feels not dry and comfortable, sultry, glutinous greasy after expense person perspires.Therefore, before the application day, the moisture absorption of textile cotton yarn With quick-drying be two cannot simultaneous function.
And the present invention is by using the handling process different from prior art, there is provided a kind of new pure cotton fabric moisture absorption row The method for sorting of sweat quick-drying, make textile cotton yarn and meanwhile have moisture absorption, perspire, the function of quick-drying, with good penetrability and thoroughly Gas, allows the very quick inspiration of sweat to pure cotton fiber the inside and quickly spreads apart come so as to reach moisture absorbing and sweat releasing quick-drying Function and make pure cotton textile dry and comfortable comfortable, health does not stimulate skin, reduces and produces peculiar smell.
Further, a kind of pure cotton fabric is also provided in the present invention, the pure cotton fabric is knitted using pure cotton as described above The method for sorting of thing moisture absorbing and sweat releasing quick-drying is processed.The pure cotton fabric has advantages below:
1st, by the evaluation of national standard GB/T 21655.1-2008 textile absorbing fast-dryings, its measure wicking height can reach More than 150mm, water absorption rate can reach more than 230%, and the moisture diffusion time is as short as within 1.4s, and moisture evaporation speed reaches To more than 0.23g/h, each side index is much higher by professional standard.Can effectively absorb and discharge body surface sweat, especially Suitable for dress and personal adornment such as tights, shirt, easy dress, gym suit, socks, underwears;Sultry and viscous body of perspiring can be solved to ask Topic, can also improve the comfortableness of tights, improve value-added content of product.
2nd, using 100% pure-cotton fabric, there is good feel by hydrophilic soft finish, with excellent wearing comfort.
3rd, with fabulous washing fastness, according to AATCC143 washing methods can with resistance to more than 10 times home washings, Can keep good performance, and colour fading after washing is also little.
Below by way of specific embodiment, the invention will be further described.
Embodiment 1
The method for sorting of the pure cotton fabric moisture absorbing and sweat releasing quick-drying, comprises the following steps:
It is concise:Polyether-modified polyorganosiloxane compounds are added in concise operation, the time of concise operation is 10 minutes, place Reason temperature is 80 DEG C, and the consumption of the wetting agent is 15g/ L;
Dyeing:Processed according to normal plant process;
Fixation:Processed using common color fixing agent, the fixation time is 15 minutes, treatment temperature is 90 DEG C, consumption is 1g/ L;
Washing:The process time of washing operation is 5 minutes, and treatment temperature is 60 DEG C, and detergent uses common detergent, detergent Consumption be 3g/L;
Dispersant treatment:Polyethylene glycol 200 dispersant is added after washing, the process time of dispersant treatment process is 80 points Clock, treatment temperature is 40 DEG C, and the consumption of dispersant is 20g/L;
It is excessively soft in bath:Using hydrophilic polyether modified organic silicon softening agent, process time is 30 minutes, and treatment temperature is 30 DEG C, the consumption of hydrophilic softener is 10g/ L;
Dehydration;
Drying:The temperature of drying is 100 ~ 130 DEG C.
To the textile cotton yarn processed by above-mentioned method for sorting, inhaled by national standard GB/T 21655.1-2008 textiles The evaluation of wet rapid-drying properties, its measure wicking height can reach 155mm, and water absorption rate can reach 235%, and the moisture diffusion time is short To 1.2s, moisture evaporation speed reaches 0.24g/h.
Embodiment 2
The method for sorting of the pure cotton fabric moisture absorbing and sweat releasing quick-drying, comprises the following steps:
It is concise:Polyether-modified polyorganosiloxane compounds are added in concise operation, the time of concise operation is 55 minutes, place Reason temperature is 30 DEG C, and the consumption of wetting agent is 20g/L;
Dyeing:Processed according to normal plant process;
Fixation:Processed using common color fixing agent, the fixation time is 40 minutes, treatment temperature is 50 DEG C, consumption is 3g/ L;
Washing:The process time of washing operation is 30 minutes, and treatment temperature is 50 DEG C, and detergent uses common detergent, washing The consumption of agent is 1.5g/L;
Dispersant treatment:Dispersant polyethylene glycol 200 is added after washing, the process time of dispersant treatment process is 15 points Clock, treatment temperature is 60 DEG C, and the consumption of dispersant is 2g/L;
It is excessively soft in bath:Using hydrophilic polyether modified organic silicon softening agent, process time is 20 minutes, and treatment temperature is 40 DEG C, the consumption of hydrophilic softener is 5g/ L;
Dehydration;
Drying:The temperature of drying is 100 ~ 130 DEG C.
To the textile cotton yarn processed by above-mentioned method for sorting, inhaled by national standard GB/T 21655.1-2008 textiles The evaluation of wet rapid-drying properties, its measure wicking height can reach 153mm, and water absorption rate can reach 241%, and the moisture diffusion time is short To 1.3s, moisture evaporation speed reaches 0.25g/h.
Embodiment 3
The method for sorting of the pure cotton fabric moisture absorbing and sweat releasing quick-drying, comprises the following steps:
It is concise:The polyether-modified polyorganosiloxane compounds of wetting agent are added in concise operation, the time of concise operation is 30 Minute, treatment temperature is 50 DEG C, and the consumption of wetting agent is 30g/L;
Dyeing:Processed according to normal plant process;
Fixation:Processed using common color fixing agent, the fixation time is 65 minutes, treatment temperature is 30 DEG C, consumption is 5g/ L;
Washing:The process time of washing operation is 60 minutes, and treatment temperature is 55 DEG C, and detergent uses common detergent, washing The consumption of agent is 0.5g/L;
Dispersant treatment:Dispersant PEG400 is added after washing, the process time of dispersant treatment process is 40 points Clock, treatment temperature is 50 DEG C, and the consumption of dispersant is 10g/L;
It is excessively soft in bath:Using hydrophilic polyether modified organic silicon softening agent, process time is 10 minutes, and treatment temperature is 50 DEG C, the consumption of hydrophilic softener is 3g/ L;
Dehydration;
Drying:The temperature of drying is 100 ~ 130 DEG C.
To the textile cotton yarn processed by above-mentioned method for sorting, inhaled by national standard GB/T 21655.1-2008 textiles The evaluation of wet rapid-drying properties, its measure wicking height can reach 150mm, and water absorption rate can reach 240%, and the moisture diffusion time is short To 1.4s, moisture evaporation speed reaches 0.23g/h.
It should be appreciated that application of the invention is not limited to above-mentioned citing, and for those of ordinary skills, can To be improved according to the above description or converted, all these modifications and variations should all belong to the guarantor of appended claims of the present invention Shield scope.

Claims (10)

1. a kind of method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying, it is characterised in that comprise the following steps:
It is concise:Wetting agent is added in concise operation;
Dyeing;
Fixation:
Washing;
Dispersant treatment:Dispersant is added to be processed;
It is excessively soft in bath:Processed using hydrophilic softener;
Dehydration;
Drying.
2. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 1, it is characterised in that the wetting agent It is the surfactant being made up of hydrophilic group and lipophilic group;The wetting agent is silanol class nonionic surfactant.
3. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 2, it is characterised in that concise operation Time is 10 ~ 60 minutes, and treatment temperature is 30 ~ 80 DEG C, and the consumption of the wetting agent is 15-30g/L.
4. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 3, it is characterised in that the wetting agent It is polyether-modified polyorganosiloxane compounds.
5. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 1, it is characterised in that the dispersant It is polyethylene glycol 200 or PEG400.
6. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 5, it is characterised in that dispersant treatment The process time of operation is 15-80 minutes, and treatment temperature is 40 ~ 60 DEG C, and the consumption of the dispersant is 1-20g/L.
7. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 1, it is characterised in that described hydrophilic soft Soft dose is fatty amine and its derivative species, organic silicon and their complex;The silicone softening agent for using changes for polyethers Oxirane, the organic silicon softening agent of Polymerization of Propylene Oxide of property.
8. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 7, it is characterised in that excessively soft work in bath The process time of sequence is 10-30 minutes, and treatment temperature is 30-50 DEG C, and the consumption of hydrophilic softening agent is 1-10g/ L.
9. the method for sorting of pure cotton fabric moisture absorbing and sweat releasing quick-drying according to claim 1, it is characterised in that washing operation Process time is 5 ~ 60 minutes, and treatment temperature is 50 ~ 60 DEG C, and the consumption of detergent is 0.5-3g/L;
The process time of laking procedure is 15 ~ 65 minutes, and treatment temperature is 30 ~ 90 DEG C, and the consumption of color fixing agent is 1-5g/L;
The treatment temperature of baking operation is 100 ~ 130 DEG C.
10. a kind of pure cotton fabric, it is characterised in that the pure cotton fabric is knitted using the pure cotton as described in claim 1 ~ 9 is any The method for sorting of thing moisture absorbing and sweat releasing quick-drying is processed.
CN201710013398.6A 2017-01-09 2017-01-09 A kind of method for sorting and pure cotton fabric of pure cotton fabric moisture absorbing and sweat releasing quick-drying Expired - Fee Related CN106835718B (en)