CN106835481A - The preparation method of noctilucence flannel fabric lining - Google Patents
The preparation method of noctilucence flannel fabric lining Download PDFInfo
- Publication number
- CN106835481A CN106835481A CN201611225967.5A CN201611225967A CN106835481A CN 106835481 A CN106835481 A CN 106835481A CN 201611225967 A CN201611225967 A CN 201611225967A CN 106835481 A CN106835481 A CN 106835481A
- Authority
- CN
- China
- Prior art keywords
- fabric
- noctilucence
- preparation
- silk organization
- organization
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses the preparation method of noctilucence flannel fabric lining, including following preparation processes:The selection of raw material, selects one kind or mixing twisting silk in the dacron thread or cellulose fibre of different fineness as bottom silk organization and surface silk organization, and the quality of bottom silk organization accounts for the 30 ~ 45% of fabric gross mass, and the quality of surface silk organization accounts for the 70 ~ 55% of fabric gross mass;Warping, weaving, cuts open width, thermal finalization, stamp, and stamp is carried out using luminescent coating and dispersion paints to sizing fabric, respectively obtains calico, Final finishing, including drying, fluffing, soft treatment, shape again, hot light and cropping.Through the above way, the present invention can be prepared and be presented that excellent, flexibility is high, good hand touch noctilucence flannel fabric lining with permanent luminous effect, noctilucence sunset glow time long, noctilucence flower pattern and color, have the advantages that process procedure is few, technical factor is not harsh.
Description
Technical field
The present invention relates to functional textile field, more particularly to a kind of preparation side of noctilucence flannel fabric lining
Method.
Background technology
With economy and the development of people's consumption demand diversification, luminous fiber functional textile is also more and more, such as
Can be lighted work clothes, wind coat, vest, underwear etc., therefore exploitation noctilucence textile will also turn into following development trend.
The fabric of the use noctilucence silk production for occurring in the market, this kind of fabric is usually plain color, all by noctilucence silk
Make, such production cost is high, price, outward appearance is relatively simple.Printed flannels fabric product currently on the market is a lot, but
It is that in addition to flower pattern difference, other parts are quite similar to the sense organ of client, have no special feature.
The content of the invention
The present invention solves the technical problem of a kind of preparation method of noctilucence flannel fabric lining is provided, can make
It is standby to obtain being presented with permanent luminous effect, noctilucence sunset glow time long, noctilucence flower pattern and color that excellent, flexibility is high, good hand touch
Noctilucence flannel fabric lining.
In order to solve the above technical problems, one aspect of the present invention is:
A kind of preparation method of noctilucence flannel fabric lining, including following preparation processes are provided:
1)The selection of raw material, selects the one kind in the dacron thread of 50D ~ 150D or the cellulose fibre of 100D ~ 150D or mixing to add
Twisted filament chooses the one kind in the dacron thread of 100D ~ 150D or the cellulose fibre of 80D ~ 100D or mixing adds as bottom silk organization
Twisted filament is surface silk organization, wherein the quality of the bottom silk organization accounts for the 30 ~ 45% of fabric gross mass, the quality of the surface silk organization
Account for the 70 ~ 55% of fabric gross mass;
2)Warping, to step 1)The selected bottom silk organization and the raw material of the surface silk organization carry out warping respectively;
3)Weaving, to step 2)It is middle woven by tricot machine by the bottom silk organization of warping and the raw material of the surface silk organization
Make, obtain fabric;
4)Width is cutd open, to step 3)The fabric for obtaining carries out cuing open width;
5)Thermal finalization, by step 4)The fabric cutd open after width for obtaining introduces forming machine and carries out thermal finalization, controls the temperature of thermal finalization
And the time, obtain fabric of shaping;
6)Stamp, to step 5)The sizing fabric for obtaining carries out stamp using luminescent coating and dispersion paints, respectively obtains stamp
Cloth;
7)Final finishing, to step 6)The stained clot-h or calico for obtaining carry out Final finishing, including drying, fluffing, soft treatment, again
Sizing, hot light and cropping.
In a preferred embodiment of the present invention, in step 5)In, the temperature control of the thermal finalization at 160 ~ 180 DEG C,
The time control of thermal finalization is in 35 ~ 45S.
In a preferred embodiment of the present invention, in step 6)In, the component of the luminescent coating of use is fabric weight
The 0.1 ~ 0.3% of amount.
In a preferred embodiment of the present invention, in step 6)In, during stamp, the luminescent coating is equipped with and helps
Agent, is printed and is attached on flannel fabric;When half tone is made, the colored position of luminescent coating does not weigh with the colored position of disperse dyes
It is folded.
In a preferred embodiment of the present invention, in step 7)In, hydrophilic softener, the parent are added during soft treatment
Aqueous softening agent is the 0.3 ~ 0.5% of fabric weight.
In a preferred embodiment of the present invention, the luminescent coating be by luminescent powder, fluorescent material, dispersant, anti-settling agent,
Levelling agent, resin binder and aqueous solvent are prepared from.
In a preferred embodiment of the present invention, the cellulose fibre of the dacron thread of selection 80D ~ 120D and 100D ~ 120D
Mixing twisting silk as bottom silk organization, twisting quantity ratio is 1:1~2;Choose the dacron thread of 120D ~ 130D and the fibre of 85D ~ 95D
Cellulose fiber twisting silk is surface silk organization, and twisting quantity ratio is 1:1~3.
In a preferred embodiment of the present invention, the cellulose fibre mixing twisting of the dacron thread of selection 120D and 100D is made
It is bottom silk organization, twisting quantity ratio is 1:1;The cellulose fibre mixing twisting for choosing the dacron thread and 90D of 120D is face silk group
Knit, twisting quantity ratio is 1:1.5.
In a preferred embodiment of the present invention, the quality of the bottom silk organization accounts for the 40% of fabric gross mass, the face silk
The quality of tissue accounts for the 60% of fabric gross mass.
The beneficial effects of the invention are as follows:The preparation method of noctilucence flannel fabric lining of the present invention, can prepare tool
Excellent, flexibility is high, good hand touch noctilucence method to have permanent luminous effect, noctilucence sunset glow time long, noctilucence flower pattern and color to present
Blue Down Fiber fabric, has the advantages that process procedure is few, technical factor is not harsh.
Specific embodiment
Presently preferred embodiments of the present invention is described in detail below so that advantages and features of the invention can be easier to by
It will be appreciated by those skilled in the art that apparent clearly being defined so as to be made to protection scope of the present invention.
Embodiment 1:A kind of preparation method of noctilucence flannel fabric lining, including following preparation processes:
1)The selection of raw material, selects the cellulose fibre mixing twisting of dacron thread and 100D of 120D as bottom silk organization, twisting
Quantity ratio is 1:1;The cellulose fibre mixing twisting for choosing the dacron thread and 90D of 120D is surface silk organization, and twisting quantity ratio is
1:1.5;
The quality of wherein described bottom silk organization accounts for the 40% of fabric gross mass, and the quality of the surface silk organization accounts for fabric gross mass
60%;
2)Warping, to step 1)The selected bottom silk organization and the raw material of the surface silk organization carry out warping respectively;
3)Weaving, to step 2)It is middle woven by tricot machine by the bottom silk organization of warping and the raw material of the surface silk organization
Make, obtain fabric;
4)Width is cutd open, to step 3)The fabric for obtaining carries out cuing open width;
5)Thermal finalization, by step 4)The fabric cutd open after width for obtaining introduces forming machine and carries out thermal finalization, controls the temperature of thermal finalization
At 160 ~ 180 DEG C, the time control of thermal finalization obtains fabric of shaping in 35 ~ 45S;
6)Stamp, to step 5)The sizing fabric for obtaining carries out stamp using luminescent coating and dispersion paints, respectively obtains stamp
Cloth;During stamp, the luminescent coating is equipped with by auxiliary agent using printing machine, is printed and be attached on flannel fabric,
The component of the luminescent coating of use is the 0.2% of fabric weight;The aperture in the half tone hole of printing machine is 50 ~ 90 mesh, is making half tone
When, the colored position of luminescent coating is not overlap with the colored position of disperse dyes, and two colored positions need air switch;
7)Final finishing, to step 6)The stained clot-h or calico for obtaining carry out Final finishing, including drying, fluffing, soft treatment, again
Sizing, hot light and cropping;Add hydrophilic softener during soft treatment, the hydrophilic softener be fabric weight 0.3 ~
0.5%。
Embodiment 2:A kind of preparation method of noctilucence flannel fabric lining, including following preparation processes:
1)The selection of raw material, selects the mixing of the cellulose fibre of the dacron thread and 120D of 100D to twist silk as bottom silk organization,
Twisting quantity ratio is 1:2;It is surface silk organization to choose the dacron thread of 120D and the cellulose fibre twisting silk of 95D, twists quantity ratio
It is 1: 3;
The quality of wherein described bottom silk organization accounts for the 35% of fabric gross mass, and the quality of the surface silk organization accounts for fabric gross mass
65%;
2)Warping, to step 1)The selected bottom silk organization and the raw material of the surface silk organization carry out warping respectively;
3)Weaving, to step 2)It is middle woven by tricot machine by the bottom silk organization of warping and the raw material of the surface silk organization
Make, obtain fabric;
4)Width is cutd open, to step 3)The fabric for obtaining carries out cuing open width;
5)Thermal finalization, by step 4)The fabric cutd open after width for obtaining introduces forming machine and carries out thermal finalization, controls the temperature of thermal finalization
At 160 ~ 180 DEG C, the time control of thermal finalization obtains fabric of shaping in 35 ~ 45S;
6)Stamp, to step 5)The sizing fabric for obtaining carries out stamp using luminescent coating and dispersion paints, respectively obtains stamp
Cloth;During stamp, the luminescent coating is equipped with by auxiliary agent using printing machine, is printed and be attached on flannel fabric,
The component of the luminescent coating of use is the 0.3% of fabric weight;The aperture in the half tone hole of printing machine is 50 ~ 90 mesh, is making half tone
When, the colored position of luminescent coating is not overlap with the colored position of disperse dyes, and two colored positions need air switch;
7)Final finishing, to step 6)The stained clot-h or calico for obtaining carry out Final finishing, including drying, fluffing, soft treatment, again
Sizing, hot light and cropping;Add hydrophilic softener during soft treatment, the hydrophilic softener be fabric weight 0.3 ~
0.5%。
Embodiment 3:A kind of preparation method of noctilucence flannel fabric lining, including following preparation processes:
1)The selection of raw material, selects the mixing of the cellulose fibre of the dacron thread and 110D of 80D to twist silk as bottom silk organization, plus
Twisting count amount ratio is 1:1.5;It is surface silk organization to choose the dacron thread of 130D and the cellulose fibre twisting silk of 85D ~ 95D, twists number
Amount is than being 1:2;
The quality of wherein described bottom silk organization accounts for the 30% of fabric gross mass, and the quality of the surface silk organization accounts for fabric gross mass
70%;
2)Warping, to step 1)The selected bottom silk organization and the raw material of the surface silk organization carry out warping respectively;
3)Weaving, to step 2)It is middle woven by tricot machine by the bottom silk organization of warping and the raw material of the surface silk organization
Make, obtain fabric;
4)Width is cutd open, to step 3)The fabric for obtaining carries out cuing open width;
5)Thermal finalization, by step 4)The fabric cutd open after width for obtaining introduces forming machine and carries out thermal finalization, controls the temperature of thermal finalization
At 160 ~ 180 DEG C, the time control of thermal finalization obtains fabric of shaping in 35 ~ 45S;
6)Stamp, to step 5)The sizing fabric for obtaining carries out stamp using luminescent coating and dispersion paints, respectively obtains stamp
Cloth;During stamp, the luminescent coating is equipped with by auxiliary agent using printing machine, is printed and be attached on flannel fabric,
The component of the luminescent coating of use is the 0.15% of fabric weight;The aperture in the half tone hole of printing machine is 50 ~ 90 mesh, is making net
During version, the colored position of luminescent coating is not overlap with the colored position of disperse dyes, and two colored positions need air switch;
7)Final finishing, to step 6)The stained clot-h or calico for obtaining carry out Final finishing, including drying, fluffing, soft treatment, again
Sizing, hot light and cropping;Add hydrophilic softener during soft treatment, the hydrophilic softener be fabric weight 0.3 ~
0.5%。
Luminescent coating in any of the above-described embodiment is by luminescent powder, fluorescent material, dispersant, anti-settling agent, levelling agent, resin
Binder and aqueous solvent are mixed with and form, with noctilucence sunset glow is long, luminous effect is good, the characteristics of economic and environment-friendly.
Embodiments of the invention are the foregoing is only, the scope of the claims of the invention is not thereby limited, it is every to utilize this hair
Equivalent structure or equivalent flow conversion that bright description is made, or directly or indirectly it is used in other related technology necks
Domain, is included within the scope of the present invention.
Claims (9)
1. a kind of preparation method of noctilucence flannel fabric lining, it is characterised in that including following preparation processes:
1)The selection of raw material, selects the one kind in the dacron thread of 50D ~ 150D or the cellulose fibre of 100D ~ 150D or mixing to add
Twisted filament chooses the one kind in the dacron thread of 100D ~ 150D or the cellulose fibre of 80D ~ 100D or mixing adds as bottom silk organization
Twisted filament is surface silk organization, wherein the quality of the bottom silk organization accounts for the 30 ~ 45% of fabric gross mass, the quality of the surface silk organization
Account for the 70 ~ 55% of fabric gross mass;
2)Warping, to step 1)The selected bottom silk organization and the raw material of the surface silk organization carry out warping respectively;
3)Weaving, to step 2)It is middle woven by tricot machine by the bottom silk organization of warping and the raw material of the surface silk organization
Make, obtain fabric;
4)Width is cutd open, to step 3)The fabric for obtaining carries out cuing open width;
5)Thermal finalization, by step 4)The fabric cutd open after width for obtaining introduces forming machine and carries out thermal finalization, controls the temperature of thermal finalization
And the time, obtain fabric of shaping;
6)Stamp, to step 5)The sizing fabric for obtaining carries out stamp using luminescent coating and dispersion paints, respectively obtains stamp
Cloth;
7)Final finishing, to step 6)The stained clot-h or calico for obtaining carry out Final finishing, including drying, fluffing, soft treatment, again
Sizing, hot light and cropping.
2. the preparation method of noctilucence flannel fabric lining according to claim 1, it is characterised in that in step 5)In,
, at 160 ~ 180 DEG C, the time control of thermal finalization is in 35 ~ 45S for the temperature control of the thermal finalization.
3. the preparation method of noctilucence flannel fabric lining according to claim 1, it is characterised in that in step 6)In,
The component of the luminescent coating for using is the 0.1 ~ 0.3% of fabric weight.
4. the preparation method of the noctilucence flannel fabric lining according to claim 1 or 3, it is characterised in that in step 6)
In, during stamp, the luminescent coating is equipped with auxiliary agent, is printed and is attached on flannel fabric;When half tone is made,
The colored position of luminescent coating is not overlap with the colored position of disperse dyes.
5. the preparation method of noctilucence flannel fabric lining according to claim 1, it is characterised in that in step 7)In,
Hydrophilic softener is added during soft treatment, the hydrophilic softener is the 0.3 ~ 0.5% of fabric weight.
6. the preparation method of noctilucence flannel fabric lining according to claim 1, it is characterised in that the luminescent coating
It is to be prepared from by luminescent powder, fluorescent material, dispersant, anti-settling agent, levelling agent, resin binder and aqueous solvent.
7. according to the preparation method of the described noctilucence flannel fabric lining of one of claim 1 ~ 6, it is characterised in that selection
Used as bottom silk organization, twist quantity ratio is the mixing twisting silk of the dacron thread of 80D ~ 120D and the cellulose fibre of 100D ~ 120D
1:1~2;It is surface silk organization to choose the dacron thread of 120D ~ 130D and the cellulose fibre twisting silk of 85D ~ 95D, and twisting quantity ratio is
1:1~3。
8. the preparation method of noctilucence flannel fabric lining according to claim 7, it is characterised in that characterized in that,
Select the cellulose fibre mixing twisting of dacron thread and 100D of 120D as bottom silk organization, twisting quantity ratio is 1:1;Choose
The cellulose fibre mixing twisting of the dacron thread and 90D of 120D is surface silk organization, and twisting quantity ratio is 1:1.5.
9. according to the preparation method of the described noctilucence flannel fabric lining of one of claim 1 ~ 6, it is characterised in that the bottom
The quality of silk tissue accounts for the 40% of fabric gross mass, and the quality of the surface silk organization accounts for the 60% of fabric gross mass.