CN106639301A - 一种铝模板混凝土墙底烂根防护结构 - Google Patents
一种铝模板混凝土墙底烂根防护结构 Download PDFInfo
- Publication number
- CN106639301A CN106639301A CN201710088399.7A CN201710088399A CN106639301A CN 106639301 A CN106639301 A CN 106639301A CN 201710088399 A CN201710088399 A CN 201710088399A CN 106639301 A CN106639301 A CN 106639301A
- Authority
- CN
- China
- Prior art keywords
- aluminum alloy
- pattern plate
- alloy pattern
- snapping
- hole
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种铝模板混凝土墙底烂根防护结构。本发明包括固定在铝模板下缘的扣接片,以及与扣接片活动连接的泥浆挡板;所述扣接片为“L”型,且在扣接片与铝模板相连的一端设有通孔,另一端设有长条形孔;所述泥浆挡板通过连接螺栓与扣接片相连;所述连接螺栓一端与泥浆挡板的一侧连接,另一端穿过长条形孔且通过螺纹连接在连接螺栓上的两个螺帽与扣接片相连,两个螺帽分别位于长条形通孔的两侧。本发明利用了铝模板本身结构进行有效的连接,连接方式简单、可靠、牢固;本发明通过泥浆挡板对缝隙封闭严实,防治墙柱根部漏浆效果极佳;本发明能够根据现场情况调整泥浆挡板的高度,提高了其适用性。
Description
技术领域
本发明涉及一种铝模板混凝土墙底烂根防护结构。
背景技术
建筑铝合金模板作为一种新型材料,因其众多优点在世界范围广为使用,目前铝合金模板在我国也拥有了广阔的发展空间。铝膜是组装模板,模板尺寸定型精确,但楼面混凝土的平整度直接影响到铝模板的安装,铝模与已浇筑混凝土面之间缝隙的大小,容易出现墙柱根部漏浆,形成烂根,对其防止措施一般为控制楼面平整度,模板下口缝隙塞木条、海绵条或抹砂浆评层等方式,但是上述效果不理想。
发明内容
为了改善上述问题,本发明的目的在于提供一种铝模板混凝土墙底烂根防护结构。
为了实现上述目的,本发明采用的技术方案如下:
一种铝模板混凝土墙底烂根防护结构,包括固定在铝模板下缘的扣接片,以及与扣接片活动连接的泥浆挡板;所述扣接片为“L”型,且在扣接片与铝模板相连的一端设有通孔,另一端设有长条形孔;所述泥浆挡板通过连接螺栓与扣接片相连;所述连接螺栓一端与泥浆挡板的一侧连接,另一端穿过长条形孔且通过螺纹连接在连接螺栓上的两个螺帽与扣接片相连,两个螺帽分别位于长条形通孔的两侧。
进一步地,所述连接螺栓的直径小于长条形孔的宽度。
再进一步地,所述泥浆挡板通过两个以上的扣接片固定于铝模板下缘下方。
更进一步地,所述扣接片上的通孔大小与铝模板下缘的销钉孔眼大小相同。
另外,所述连接螺栓长度为40~55㎜。
另外,所述长条形孔长度为30~35㎜。
进一步地,所述泥浆挡板的宽度为30~35㎜。
再进一步地,所述扣接片上通孔的内沿设有能够插入铝模板下缘的销钉孔眼内的凸圈。
更进一步地,所述扣接片另一端还设有与长条形孔连通的横向通孔。
本发明与现有技术相比,具有以下优点及有益效果:
本发明利用了铝模板本身结构进行有效的连接,连接方式简单、可靠、牢固;本发明通过泥浆挡板对缝隙封闭严实,防治墙柱根部漏浆效果极佳;本发明能够根据现场情况调整泥浆挡板的高度,提高了其适用性;本发明与铝模板结合紧密,浇筑后根本诚信好,效率高,不需后续施工处理。
附图说明
图1为本发明的结构示意图。
其中,附图中标记对应的零部件名称为:1-扣接片,2-泥浆挡板,3-通孔,4-长条形孔,5-连接螺栓,6-螺帽,7-铝模角铝,8-铝模墙板,9-销钉孔眼。
具体实施方式
下面结合附图和实施例对本发明作进一步说明,本发明的实施方式包括但不限于下列实施例。
实施例
如图1所示,一种铝模板混凝土墙底烂根防护结构,包括固定在铝模板下缘(具体是在铝模角铝7与铝模墙板8相连处)的扣接片1,以及与扣接片活动连接的泥浆挡板2;所述扣接片为“L”型,且在扣接片与铝模板相连的一端设有通孔3,另一端设有长条形孔4;所述泥浆挡板通过连接螺栓5与扣接片相连;所述连接螺栓一端与泥浆挡板的一侧连接,另一端穿过长条形孔且通过螺纹连接在连接螺栓上的两个螺帽6与扣接片相连,两个螺帽分别位于长条形通孔的两侧。
通过采用上述装置,能够利用现有的铝模板本身结构进行连接固定,具体是利用销钉穿过扣接片上的通孔和铝模板上的销钉孔眼将扣接片固定到铝模板下缘;安装极其方便,而且稳定性强。而泥浆挡板则是位于铝模角铝下方通过连接螺栓与扣接片连接;具体是根据铝模与已浇筑混凝土面之间缝隙的大小调整泥浆挡板的位置,然后通过两个螺母将连接螺栓固定在扣接片上,从而对泥浆挡板进行固定。由于连接螺栓是贯穿长条形孔的,且能够在其内上下移动,故而能够带动泥浆挡板上下移动,从而实现调整泥浆挡板的位置,更好实现防治墙柱根部漏浆的问题。
具体地,所述连接螺栓的直径小于长条形孔的宽度。由于连接螺栓的直径小于长条形孔的宽度,这样便于连接螺栓在长条形孔中移动,避免移动时受阻。
具体地,所述泥浆挡板通过两个以上的扣接片固定于铝模板下缘下方。通过多个扣接片进行固定,固定的更加稳固,避免了泥浆挡板倾斜,能够使泥浆挡板始终保持水平。
具体地,所述扣接片上的通孔大小与铝模板下缘的销钉孔眼9大小相同。通过上述设置,便于销钉穿过进行固定,使得安装更加容易。作为另一种方式,所述扣接片上通孔的内沿设有能够插入铝模板下缘的销钉孔眼9内的凸圈。通过设置凸圈,能够将扣接片通孔处卡在销钉孔眼内,这样能够起到一定的固定作用,更加方便后续插入销钉时,扣接片跑位,提高了施工效率。
作为一种优选,所述连接螺栓长度为40~55㎜;所述长条形孔长度为30~35㎜;所述泥浆挡板的宽度为30~35㎜。通过上述限定能够避免材料过长或过短影响正常的安装和挡泥效果。
作为一种优选,所述扣接片另一端还设有与长条形孔连通的横向通孔。在扣接片上设置横向通孔,能够使连接螺栓横向移动,这样就能够使连接螺栓竖向和横向均能移动,也就意味着泥浆挡板也能够上下左右移动,从而更好的实现挡泥效果。
按照上述实施例,便可很好地实现本发明。值得说明的是,基于上述结构设计的前提下,为解决同样的技术问题,即使在本发明上做出的一些无实质性的改动或润色,所采用的技术方案的实质仍然与本发明一样,故其也应当在本发明的保护范围内。
Claims (9)
1.一种铝模板混凝土墙底烂根防护结构,其特征在于,包括固定在铝模板下缘的扣接片(1),以及与扣接片活动连接的泥浆挡板(2);所述扣接片为“L”型,且在扣接片与铝模板相连的一端设有通孔(3),另一端设有长条形孔(4);所述泥浆挡板通过连接螺栓(5)与扣接片相连;所述连接螺栓一端与泥浆挡板的一侧连接,另一端穿过长条形孔且通过螺纹连接在连接螺栓上的两个螺帽(6)与扣接片相连,两个螺帽分别位于长条形通孔的两侧。
2.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述连接螺栓的直径小于长条形孔的宽度。
3.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述泥浆挡板通过两个以上的扣接片固定于铝模板下缘下方。
4.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述扣接片上的通孔大小与铝模板下缘的销钉孔眼大小相同。
5.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述连接螺栓长度为40~55㎜。
6.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述长条形孔长度为30~35㎜。
7.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述泥浆挡板的宽度为30~35㎜。
8.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述扣接片上通孔的内沿设有能够插入铝模板下缘的销钉孔眼内的凸圈。
9.根据权利要求1所述的一种铝模板混凝土墙底烂根防护结构,其特征在于,所述扣接片另一端还设有与长条形孔连通的横向通孔。