CN106565190A - Environment-friendly brick and production method thereof - Google Patents

Environment-friendly brick and production method thereof Download PDF

Info

Publication number
CN106565190A
CN106565190A CN201610996102.2A CN201610996102A CN106565190A CN 106565190 A CN106565190 A CN 106565190A CN 201610996102 A CN201610996102 A CN 201610996102A CN 106565190 A CN106565190 A CN 106565190A
Authority
CN
China
Prior art keywords
environmental protection
protection brick
raw material
environment
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Withdrawn
Application number
CN201610996102.2A
Other languages
Chinese (zh)
Inventor
不公告发明人
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Wenzhou Environmental Protection Technology Co Ltd Hungnam
Original Assignee
Wenzhou Environmental Protection Technology Co Ltd Hungnam
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Wenzhou Environmental Protection Technology Co Ltd Hungnam filed Critical Wenzhou Environmental Protection Technology Co Ltd Hungnam
Priority to CN201610996102.2A priority Critical patent/CN106565190A/en
Publication of CN106565190A publication Critical patent/CN106565190A/en
Withdrawn legal-status Critical Current

Abstract

The invention discloses an environment-friendly brick and a production method thereof. The environment-friendly brick is characterized by being prepared from the following raw materials: flyash, quick lime, straws, river sand and water. The environment-friendly brick is strong in compression resistance, simple in process, low in cost and free of pollution to environment; the resources are comprehensively utilized; the gradation of the raw materials is improved.

Description

A kind of environmental protection brick and preparation method thereof
Technical field
The present invention relates to a kind of environmental protection brick and preparation method thereof, belongs to garbage reutilization technology field.
Background technology
Still based on clay brick, its main component is clay to current bearing bricks for building, and Jing bases, roasting are formed.It is raw Producing this brick not only needs to expend a large amount of arable lands, and a large amount of harmful gass, such as carbon monoxide, dioxy can be discharged in sintering procedure Change carbon, hydrogen sulfide etc., to environment, be detrimental to health.Traditional fluvial sand brickmaking is because aggregate is single or thus raw material Level causes product strength not high with the requirement such as complex process.
The content of the invention
(One)The technical problem to be solved
To solve the above problems, the present invention proposes a kind of environmental protection brick pressure resistance of offer, and process is simple fully utilizes money Source, improves raw material level and matches somebody with somebody, low cost, environmental protection brick of environmentally safe and preparation method thereof.
(Two)Technical scheme
A kind of environmental protection brick of the present invention and preparation method thereof, it is characterised in that:The raw material of the environmental protection brick is prepared by flyash, life Calx, straw, fluvial sand and water composition.
Further, each raw material accounts for the percentage ratio of raw material gross weight and is respectively:Flyash 30~50%, quick lime 5~10%, The percentage by weight sum of straw 10~15%, fluvial sand 10~20%, water 3~5%, and all raw materials is 100%.
Further, the method is specially:Digestion is sufficiently stirred for after each raw material is mixed 3~8 hours, be then pressed into Type, finally the steam press maintenance under the conditions of 200~220 DEG C, 1~1.2MPa, obtains environmental protection brick.
Further, the described steam press maintenance time is 8~12 hours.
(Three)Beneficial effect
Compared with prior art, it has the advantages that the present invention:The environmental protection brick pressure resistance that the present invention is provided, technique letter It is single, resource is fully utilized, improve raw material level and match somebody with somebody, low cost, environmentally safe.
Specific embodiment
Embodiment 1
Take and be sufficiently stirred for digestion 3 hours after 30kg flyash, 5kg quick lime, 10kg straws, 10kg fluvial sand, the mixing of 3kg water, so It is compressing afterwards, obtain adobe, finally by adobe send into still kettle in, temperature be 200 DEG C, pressure be 1Mpa under the conditions of steam pressure Maintenance 8 hours, obtains environmental protection brick.Crushing resistance is carried out to environmental protection brick manufactured in the present embodiment according to GB11945-1999 standards and is resisted Folding endurance is tested, and comprcssive strength is 12.5MPa, and rupture strength is 3.8Mpa.
Embodiment 2
Take and be sufficiently stirred for digestion 8 hours after 50kg flyash, 10kg quick lime, 15kg straws, 20kg fluvial sand, the mixing of 5kg water, so It is compressing afterwards, obtain adobe, finally by adobe send into still kettle in, temperature be 200 DEG C, pressure be 1Mpa under the conditions of steam pressure Maintenance 12 hours, obtains environmental protection brick.According to GB11945-1999 standards environmental protection brick manufactured in the present embodiment is carried out crushing resistance and Fold resistance is tested, and comprcssive strength is 16.5MPa, and rupture strength is 4.5Mpa.
Embodiment 3
Take and be sufficiently stirred for digestion 5 hours after 40kg flyash, 8kg quick lime, 12kg straws, 15kg fluvial sand, the mixing of 4kg water, so It is compressing afterwards, obtain adobe, finally by adobe send into still kettle in, temperature be 200 DEG C, pressure be 1Mpa under the conditions of steam pressure Maintenance 10 hours, obtains environmental protection brick.According to GB11945-1999 standards environmental protection brick manufactured in the present embodiment is carried out crushing resistance and Fold resistance is tested, and comprcssive strength is 13.5MPa, and rupture strength is 4Mpa.
The environmental protection brick pressure resistance that the present invention is provided, process is simple fully utilizes resource, improves raw material level and match somebody with somebody, cost It is low, environmentally safe.
Embodiment described above is only that the preferred embodiment of the present invention is described, not to the structure of the present invention Think and model point encloses and is defined.On the premise of without departing from design concept of the present invention, skill of this area ordinary person to the present invention Various modifications and improvement that art scheme is made, all should drop into protection scope of the present invention, in the technology that the present invention is claimed Hold, all recorded in detail in the claims.

Claims (4)

1. a kind of environmental protection brick and preparation method thereof, it is characterised in that:Prepare the raw material of the environmental protection brick by flyash, quick lime, Straw, fluvial sand and water composition.
2. a kind of environmental protection brick and preparation method thereof, it is characterised in that:Each raw material accounts for the percentage ratio of raw material gross weight and is respectively:Fine coal Ash 30~50%, quick lime 5~10%, straw 10~15%, fluvial sand 10~20%, water 3~5%, and the weight percent of all raw materials It is 100% than sum.
3. a kind of environmental protection brick according to claim 1 and preparation method thereof, it is characterised in that:The method is specially:Will be each Digestion is sufficiently stirred for after raw material mixing 3~8 hours, type is then pressed into, finally under the conditions of 200~220 DEG C, 1~1.2MPa Steam press maintenance, obtains environmental protection brick.
4. a kind of environmental protection brick according to claim 2 and preparation method thereof, it is characterised in that:The described steam press maintenance time For 8~12 hours.
CN201610996102.2A 2016-11-12 2016-11-12 Environment-friendly brick and production method thereof Withdrawn CN106565190A (en)