CN106370063A - Manufacturing method for colorful firecrackers - Google Patents
Manufacturing method for colorful firecrackers Download PDFInfo
- Publication number
- CN106370063A CN106370063A CN201610755149.XA CN201610755149A CN106370063A CN 106370063 A CN106370063 A CN 106370063A CN 201610755149 A CN201610755149 A CN 201610755149A CN 106370063 A CN106370063 A CN 106370063A
- Authority
- CN
- China
- Prior art keywords
- parts
- component
- potassium
- manufacture method
- chlorinated rubber
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention discloses a manufacturing method for colorful firecrackers. The manufacturing method comprises the steps that firstly, a component A and a component B are used for preparing a chemical, the component A comprises, by weight, 40-45 parts of potassium perchlorate, 7-10 parts of aluminum powder, 7-10 parts of barium nitrate, 2-2.5 parts of antimonous oxide and 0.8-3 parts of chlorinated rubber, the component B comprises, by weight, 40-45 parts of potassium perchlorate, 7-10 parts of aluminum powder, 7-10 parts of nitrate of potash, 1-4 parts of chlorinated rubber, 7-9 parts of starch and 8-9 parts of phenolic resin, the component B is evenly divided into several parts each accounting for 3 g-4 g, the component A is evenly divided into several parts each accounting for 0.5 g-1 g, and chemical particles with each part of the component A as a core and each part of the component B as a coating are manufactured; and secondly, a paper drum is filled with the chemical. The colorful firecrackers are more environment-friendly and safer, and colors are more abundant during setting off.
Description
Technical field
The present invention relates to a kind of five colours firecracker manufacture method.
Background technology
Firecracker is one of celebrating article that people commonly use, and either celebrates a festival or marriage marriage, enters to learn and be transferred and promoted and big
Summer completion, shop opening, firecracker is seted off to show congratulation by metropolis.The oxidant that traditional medicament is adopted is potassium nitrate, modern age
Then potassium nitrate is replaced as oxidant by potassium chlorate, because the heat stability of both oxidants is all very poor, easily cause safety
Accident, and No. 52 files of the General Office of the State Council in 2002 are even more and specify: fireworks and firecrackers industry production is forbidden to use potassium chlorate;Simultaneously
Sulfur is used as reducing agent in a large number, and sulfur itself is a kind of very active combustible of chemical property, more reduces
The stability of medicament, and poisonous and hazardous sulfur dioxide gas can be produced after setting off, affect environment, native land man makes to this restriction
With.Accordingly, it would be desirable to a kind of more environmentally friendly and safe firecrackers.
Content of the invention
For the problems referred to above, the present invention has designed and developed a kind of more environmentally friendly, safer, coloury five colours firecracker making
Method.
The technical scheme that the present invention provides is:
A kind of five colours firecracker manufacture method, comprising:
Step (1) prepares medicament using component a and component b;Described component a is by the following components group of meter by weight
Become: 40~45 parts of potassium hyperchlorate, 7~10 parts of aluminium powder, 7~10 parts of barium nitrate, 2~2.5 parts of antimony oxide, chlorinated rubber 0.8
~3 parts;Described component b is made up of the following components of meter by weight: 40~45 parts of potassium hyperchlorate, 7~10 parts of aluminium powder, nitric acid
7~10 parts of potassium, 1~4 part of chlorinated rubber, 7~9 parts of starch, 8~9 parts of phenolic resin;Component b is divided into several pieces, every part 3
~4g, and every part of component b kneading is become cake skin shape;Component a is divided into several pieces, every part of 0.5~1g;Every part of component a is put
In every part of component b, make with every part of component a as core, the pharmacy particle with every part of component b as skin;
Step (2) loads described medicament in paper web.
Preferably, in described multicolored firecracker manufacture method, described component a is by the following components group of meter by weight
Become: 45 parts of potassium hyperchlorate, 10 parts of aluminium powder, 10 parts of barium nitrate, 2.5 parts of antimony oxide, 3 parts of chlorinated rubber.
Preferably, in described multicolored firecracker manufacture method, described component b is by the following components group of meter by weight
Become: 40 parts of potassium hyperchlorate, 7 parts of aluminium powder, 7 parts of potassium nitrate, 1 part of chlorinated rubber, 7 parts of starch, 8 parts of phenolic resin.
Preferably, in described multicolored firecracker manufacture method, component b is divided into several pieces, every part of 4g;By component a
It is divided into several pieces, every part of 1g.
Preferably, in described multicolored firecracker manufacture method, the particle diameter of described pharmacy particle is 0.8~1mm.
Five colours firecracker manufacture method of the present invention does not adopt potassium chlorate, sulfide, more environmentally friendly, safer, Er Qieben
Two kinds of components are made pharmacy particle by invention, and when setting off, color is more rich.
Specific embodiment
The present invention is described in further detail below, with make those skilled in the art with reference to specification word being capable of evidence
To implement.
The present invention provides a kind of five colours firecracker manufacture method, comprising: step (1) prepares medicament using component a and component b;
Described component a is made up of the following components of meter by weight: 40~45 parts of potassium hyperchlorate, 7~10 parts of aluminium powder, and barium nitrate 7~
10 parts, 2~2.5 parts of antimony oxide, 0.8~3 part of chlorinated rubber;Described component b is by the following components group of meter by weight
Become: 40~45 parts of potassium hyperchlorate, 7~10 parts of aluminium powder, 7~10 parts of potassium nitrate, 1~4 part of chlorinated rubber, 7~9 parts of starch, phenolic aldehyde
8~9 parts of resin;Component b is divided into several pieces, every part of 3~4g, and every part of component b kneading is become cake skin shape;Component a is equal
It is divided into several pieces, every part of 0.5~1g;Every part of component a is placed in every part of component b, makes with every part of component a as core, with every part
Component b is the pharmacy particle of skin;Step (2) loads described medicament in paper web.
The present invention selects component a and component b, contains barium nitrate, contain potassium nitrate, barium nitrate and nitre in component b in component a
Sour potassium can bring the smog of different colours.Phenolic resin in component b and starch ensure that component b can be with molding it is ensured that medicament
The integrity of granule.When setting off, component b of outer layer is first seted off, and sends a kind of smog of color;After intervals, internal layer
Component a just burn, and send the smog of another kind of color.The difference that the firecracker that the present invention prepares is sent when setting off
The smog of color discharges successively, thus increased the stereovision of smog color, forms more gorgeous visual effect.
Preferably, in order to improve the color of smog, in described multicolored firecracker manufacture method, described component a is by by weight
The following components composition of amount number meter: 45 parts of potassium hyperchlorate, 10 parts of aluminium powder, 10 parts of barium nitrate, 2.5 parts of antimony oxide, chlorination
3 parts of rubber.
Preferably, in order to improve the color of smog, in described multicolored firecracker manufacture method, described component b is by by weight
The following components composition of amount number meter: 40 parts of potassium hyperchlorate, 7 parts of aluminium powder, 7 parts of potassium nitrate, 1 part of chlorinated rubber, 7 parts of starch, phenol
8 parts of urea formaldehyde.
Preferably, in order that the color of final smog is more rich in level, in described multicolored firecracker manufacture method, by group
B is divided to be divided into several pieces, every part of 4g;Component a is divided into several pieces, every part of 1g.
Preferably, in order to promote pharmacy particle fully to set off, in described multicolored firecracker manufacture method, described medicament
The particle diameter of grain is 0.8~1mm.
Embodiment one
Step (1) prepares medicament using component a and component b;Described component a is by the following components group of meter by weight
Become: 40 parts of potassium hyperchlorate, 7 parts of aluminium powder, 7 parts of barium nitrate, 2 parts of antimony oxide, 0.8 part of chlorinated rubber;Described component b is by by weight
The following components composition of amount number meter: 45 parts of potassium hyperchlorate, 10 parts of aluminium powder, 10 parts of potassium nitrate, 4 parts of chlorinated rubber, 9 parts of starch,
9 parts of phenolic resin;Component b is divided into several pieces, every part of 3g, and every part of component b kneading is become cake skin shape;Component a is divided equally
For several pieces, every part of 0.5g;Every part of component a is placed in every part of component b, makes with every part of component a as core, with every part of component b
Pharmacy particle for skin;
Step (2) loads described medicament in paper web.
Embodiment two
Step (1) prepares medicament using component a and component b;Described component a is by the following components group of meter by weight
Become: 45 parts of potassium hyperchlorate, 10 parts of aluminium powder, 10 parts of barium nitrate, 2.5 parts of antimony oxide, 3 parts of chlorinated rubber;Described component b is by pressing
The following components composition of parts by weight meter: 40 parts of potassium hyperchlorate, 7 parts of aluminium powder, 7 parts of potassium nitrate, 1 part of chlorinated rubber, 7 parts of starch,
8 parts of phenolic resin;Component b is divided into several pieces, every part of 4g, and every part of component b kneading is become cake skin shape;Component a is divided equally
For several pieces, every part of 1g;Every part of component a is placed in every part of component b, makes with every part of component a as core, with every part of component b be
The pharmacy particle of skin;
Step (2) loads described medicament in paper web.
Although embodiment of the present invention is disclosed as above, it is not restricted to listed in description and embodiment
With, it can be applied to various suitable the field of the invention completely, for those skilled in the art, can be easily
Realize other modification, therefore under the general concept being limited without departing substantially from claim and equivalency range, the present invention does not limit
In specific details.
Claims (5)
1. a kind of five colours firecracker manufacture method is it is characterised in that include:
Step (1) prepares medicament using component a and component b;Described component a is made up of the following components of meter by weight: high
40~45 parts of potassium chlorate, 7~10 parts of aluminium powder, 7~10 parts of barium nitrate, 2~2.5 parts of antimony oxide, 0.8~3 part of chlorinated rubber;
Described component b is made up of the following components of meter by weight: 40~45 parts of potassium hyperchlorate, 7~10 parts of aluminium powder, and potassium nitrate 7~
10 parts, 1~4 part of chlorinated rubber, 7~9 parts of starch, 8~9 parts of phenolic resin;Component b is divided into several pieces, every part of 3~4g,
And every part of component b kneading is become cake skin shape;Component a is divided into several pieces, every part of 0.5~1g;Every part of component a is placed in every part
In component b, make with every part of component a as core, the pharmacy particle with every part of component b as skin;
Step (2) loads described medicament in paper web.
2. five colours firecracker manufacture method as claimed in claim 1 is it is characterised in that described component a is by meter by weight
Following components forms: 45 parts of potassium hyperchlorate, 10 parts of aluminium powder, 10 parts of barium nitrate, 2.5 parts of antimony oxide, 3 parts of chlorinated rubber.
3. five colours firecracker manufacture method as claimed in claim 2 is it is characterised in that described component b is by meter by weight
Following components forms: 40 parts of potassium hyperchlorate, 7 parts of aluminium powder, 7 parts of potassium nitrate, 1 part of chlorinated rubber, 7 parts of starch, 8 parts of phenolic resin.
4. five colours firecracker manufacture method as claimed in claim 3 is it is characterised in that be divided into several pieces by component b, every part
4g;Component a is divided into several pieces, every part of 1g.
5. as claimed in claim 1 the five colours firecracker manufacture method it is characterised in that described pharmacy particle particle diameter be 0.8~
1mm.