CN106351459A - 一种水泥预制构件裂缝高强度修补方法 - Google Patents

一种水泥预制构件裂缝高强度修补方法 Download PDF

Info

Publication number
CN106351459A
CN106351459A CN201610732105.5A CN201610732105A CN106351459A CN 106351459 A CN106351459 A CN 106351459A CN 201610732105 A CN201610732105 A CN 201610732105A CN 106351459 A CN106351459 A CN 106351459A
Authority
CN
China
Prior art keywords
mortar
slot
crack
chlorine
cement
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201610732105.5A
Other languages
English (en)
Inventor
刘兴汉
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Beihai Jinjiang Cement Products Co Ltd
Original Assignee
Beihai Jinjiang Cement Products Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beihai Jinjiang Cement Products Co Ltd filed Critical Beihai Jinjiang Cement Products Co Ltd
Priority to CN201610732105.5A priority Critical patent/CN106351459A/zh
Publication of CN106351459A publication Critical patent/CN106351459A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种水泥预制构件裂缝高强度修补方法,包括以下步骤:沿裂缝凿出一条深度不小于缝深,底宽3cm‑4cm、边坡小于1:0.3的梯形断面缝槽;然后用钢丝刷磨至新鲜混凝土面,并利用浓度5%的稀草酸溶液清洗刷磨面去除杂质与油污,待清洗区域晾干后,在缝槽内填补环氧砂浆、氯偏砂浆或苯丙乳液聚合物水泥砂浆;将缝槽完全填充后养护阴干。该修补方法,工艺简单,成本低,能够完成宽度>0.2 mm的裂缝的高强度修补,有效提高水泥预制构件裂缝处的强度,延长水泥预制构件的使用寿命。

Description

一种水泥预制构件裂缝高强度修补方法
技术领域
本发明涉及建筑施工技术领域,特别地,涉及一种水泥预制构件裂缝高强度修补方法。
背景技术
混凝土结构是我国建筑工程的主要形式,而水泥预制构件则是其中的一个组成部分。目前大多数中小型构件均采用预制方式进行制作,因为这样不仅能够提高劳动效率,而且还能够降低成本。然而水泥预制构件在制作及养护时常出现某些外观缺陷,如何对其进行防治,是保证生产合格预制构件重要因素。水泥预制构件养护不力,预制构件的拆模强度不合格,预制构件在安装过程中,坐浆不均,水泥砂浆的水灰比过大,构件在外力作用下整体性能破坏,产生弯曲现象等状况都会使水泥预制构件产生裂缝,为保证水泥预制构件的使用寿命,水泥预制构件裂缝的修补尤为重要。
发明内容
本发明目的在于提供一种水泥预制构件裂缝高强度修补方法,以解决水泥预制构件开裂的问题。
为实现上述目的,本发明提供一种水泥预制构件裂缝高强度修补方法,包括以下步骤:
沿裂缝凿出一条深度不小于缝深,底宽3cm-4cm、边坡小于1:0.3的梯形断面缝槽;然后用钢丝刷磨至新鲜混凝土面,并利用浓度5%的稀草酸溶液清洗刷磨面去除杂质与油污,待清洗区域晾干后,在缝槽内填补环氧砂浆、氯偏砂浆或苯丙乳液聚合物水泥砂浆;将缝槽完全填充后养护阴干。
进一步地:所述缝槽内填补物为氯偏砂浆时,填充氯偏砂浆前在缝槽内壁涂刷一层氯偏基液,氯偏砂浆初凝后以湿草袋或洒水进行表面湿养护,时间不应少于10天。
进一步地:所述缝槽内填补物为苯丙乳液聚合物水泥砂浆时,填充苯丙乳液聚合物水泥砂浆前在缝槽内壁涂刷一层二道苯丙基液;所述苯丙乳液聚合物水泥砂浆由重量百分比:10%-18%的水泥、82%-90%的苯乙烯一丙烯酸酯共聚乳液混合组成。
本发明具有以下有益效果:
该修补方法,工艺简单,成本低,能够完成宽度>0.2 mm的裂缝的高强度修补,有效提高水泥预制构件裂缝处的强度,延长水泥预制构件的使用寿命。
具体实施方式
以下对本发明的实施例进行详细说明。
本发明的优选实施例提供了一种水泥预制构件裂缝高强度修补方法,包括以下步骤:沿裂缝凿出一条深度不小于缝深,底宽3cm-4cm、边坡小于1:0.3的梯形断面缝槽;然后用钢丝刷磨至新鲜混凝土面,并利用浓度5%的稀草酸溶液清洗刷磨面去除杂质与油污,待清洗区域晾干后,在缝槽内填补环氧砂浆、氯偏砂浆或苯丙乳液聚合物水泥砂浆;将缝槽完全填充后养护阴干。该修补方法,工艺简单,成本低,能够完成宽度>0.2 mm的裂缝的高强度修补,有效提高水泥预制构件裂缝处的强度,延长水泥预制构件的使用寿命。
优选地:所述缝槽内填补物为氯偏砂浆时,填充氯偏砂浆前在缝槽内壁涂刷一层氯偏基液,氯偏砂浆是一种性能类似环氧砂浆的高强砂浆,缝槽内壁涂刷一层氯偏基液以提高氯偏砂浆的结合强度。氯偏砂浆初凝后以湿草袋或洒水进行表面湿养护,时间不应少于10天。
优选地:所述缝槽内填补物为苯丙乳液聚合物水泥砂浆时,填充苯丙乳液聚合物水泥砂浆前在缝槽内壁涂刷一层二道苯丙基液;苯丙乳液水泥砂浆是在以水泥作为胶凝材料的基础上,加入适量苯乙烯一丙烯酸酯共聚乳液所拌制而成的聚合物水泥砂浆,具有较高的抗压、抗裂、抗折强度,缝槽内壁涂刷一层二道苯丙基液以提高苯丙乳液聚合物水泥砂浆的结合强度。所述苯丙乳液聚合物水泥砂浆由重量百分比:10%-18%的水泥、82%-90%的苯乙烯一丙烯酸酯共聚乳液混合组成。
以上所述仅为本发明的优选实施例而已,并不用于限制本发明;对于本领域的技术人员来说,本发明可以有各种更改和变化。凡在本发明的精神和原则之内,所作的任何修改、等同替换、改进等,均应包含在本发明的保护范围之内。

Claims (3)

1.一种水泥预制构件裂缝高强度修补方法,其特征在于,包括以下步骤:
沿裂缝凿出一条深度不小于缝深,底宽3cm-4cm、边坡小于1:0.3的梯形断面缝槽;然后用钢丝刷磨至新鲜混凝土面,并利用浓度5%的稀草酸溶液清洗刷磨面去除杂质与油污,待清洗区域晾干后,在缝槽内填补环氧砂浆、氯偏砂浆或苯丙乳液聚合物水泥砂浆;将缝槽完全填充后养护阴干。
2.根据权利要求1所述的一种水泥预制构件裂缝高强度修补方法,其特征在于:
所述缝槽内填补物为氯偏砂浆时,填充氯偏砂浆前在缝槽内壁涂刷一层氯偏基液,氯偏砂浆初凝后以湿草袋或洒水进行表面湿养护,时间不应少于10天。
3.根据权利要求1所述的一种水泥预制构件裂缝高强度修补方法,其特征在于:
所述缝槽内填补物为苯丙乳液聚合物水泥砂浆时,填充苯丙乳液聚合物水泥砂浆前在缝槽内壁涂刷一层二道苯丙基液;所述苯丙乳液聚合物水泥砂浆由重量百分比:10%-18%的水泥、82%-90%的苯乙烯一丙烯酸酯共聚乳液混合组成。
CN201610732105.5A 2016-08-26 2016-08-26 一种水泥预制构件裂缝高强度修补方法 Pending CN106351459A (zh)