CN106350033A - 耐热抗盐钻井泥浆处理剂 - Google Patents
耐热抗盐钻井泥浆处理剂 Download PDFInfo
- Publication number
- CN106350033A CN106350033A CN201610749899.6A CN201610749899A CN106350033A CN 106350033 A CN106350033 A CN 106350033A CN 201610749899 A CN201610749899 A CN 201610749899A CN 106350033 A CN106350033 A CN 106350033A
- Authority
- CN
- China
- Prior art keywords
- parts
- drilling mud
- product
- chloride
- heat
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明的耐热抗盐钻井泥浆处理剂,其特征在于:以重量计,由多缩硅醇钠溶液10‑30份,水玻璃50‑80份,硬脂酸铝5‑25份,粘土15‑30份,氯化钠30‑50份,氯化钙2‑10份,氯化镁2‑10份,淀粉2‑5份,羧甲基纤维素钠2‑10份,苯酚1‑5份,硫1‑5份,硼砂3‑9份,水50‑80份组成,将全部原料混合搅拌均匀,在180‑190℃下反应60‑120分钟,即得产品;具有原料易得,成本低,绿色环保,使用方便,效果好的优点。
Description
技术领域
本发明属于一种油田化学品。
背景技术
油田化学品,从广义上说,系指用于石油勘探、钻采、集输等所有工艺过程中的各灯化学品,主要包括矿物产品(如搬土等)、通用化学品(如各种酸和碱等)、天然产品(如淀粉)、无机产品(如碳酸锌)和专用(精细化工)产品(如聚合物和表面活性剂等)。
发明内容:
本发明的目的在于;提出一种耐热抗盐钻井泥浆处理剂。
本发明的耐热抗盐钻井泥浆处理剂,其特征在于:以重量计,由多缩硅醇钠溶液10-30份,水玻璃50-80份,硬脂酸铝5-25份,粘土15-30份,氯化钠30-50份,氯化钙2-10份,氯化镁2-10份,淀粉2-5份,羧甲基纤维素钠2-10份,苯酚1-5份,硫1-5份,硼砂3-9份,水50-80份组成,将全部原料混合搅拌均匀,在180-190℃下反应60-120分钟,即得产品。
本发明与现有技术相比其有益效果是:具有原料种类少,易得,成本低,绿色环保,使用方便,效果好的优点。
具体实施方式:
下面结合实施例对本发明作进一步说明,但本发明的实施方式不限于此。
本发明的耐热抗盐钻井泥浆处理剂制备方法,所用原料可购买获得。
实施例
本发明的耐热抗盐钻井泥浆处理剂,其特征在于:以重量计,由多缩硅醇钠溶液10-30份,水玻璃50-80份,硬脂酸铝5-25份,粘土15-30份,氯化钠30-50份,氯化钙2-10份,氯化镁2-10份,淀粉2-5份,羧甲基纤维素钠2-10份,苯酚1-5份,硫1-5份,硼砂3-9份,水50-80份组成,将全部原料混合搅拌均匀,在180-190℃下反应60-120分钟,即得产品。
本发明的产品质量指标:
1、外观 橙黄色液态胶
2、固体含量 ≥85%。
Claims (1)
1.一种耐热抗盐钻井泥浆处理剂,其特征在于:以重量计,由多缩硅醇钠溶液10-30份,水玻璃50-80份,硬脂酸铝5-25份,粘土15-30份,氯化钠30-50份,氯化钙2-10份,氯化镁2-10份,淀粉2-5份,羧甲基纤维素钠2-10份,苯酚1-5份,硫1-5份,硼砂3-9份,水50-80份组成,将全部原料混合搅拌均匀,在180-190℃下反应60-120分钟,即得产品。