CN105690814A - Conveyor belt damage repairing method - Google Patents
Conveyor belt damage repairing method Download PDFInfo
- Publication number
- CN105690814A CN105690814A CN201610231389.XA CN201610231389A CN105690814A CN 105690814 A CN105690814 A CN 105690814A CN 201610231389 A CN201610231389 A CN 201610231389A CN 105690814 A CN105690814 A CN 105690814A
- Authority
- CN
- China
- Prior art keywords
- repairing
- conveyor belt
- mixture
- described mixture
- coated
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a conveyor belt damage repairing method, and relates to the technical field of rubber products. The method includes the steps that a grinder is used for grinding a damage portion of a conveyor belt, and the ground surface is cleaned and roughened; the ground surface of the conveyor belt is coated with a mixture of a cold vulcanization binder and a curing agent, a damage opening is filled and leveled up, after complete drying, the mixture is applied to the repairing range in a coating mode, and the conveyor belt is air-dried until the conveyor belt is not adhesive to the back of the hand; a repairing strip coated with the mixture is pasted to the surface processed in the step B, a rolling wheel is used for rolling the repairing strip from the middle area to the periphery, and rolling is repeated for three or more times; and the edge of the repairing strip is ground and trimmed, the repairing strip is coated with the mixture along the edge of the repairing strip, the edge of the repairing strip is covered with the mixture, and then the conveyor belt is fully dried. By means of the method, the problems that an existing conveyor belt repairing method is not convenient to operate, complex in process and long in repairing time are solved.
Description
Technical field
The present invention relates to rubber technical field, especially a kind of damages of conveyor belt method for repairing and mending。
Background technology
Conveyer belt is mainly used in carrying and transports material; originally it is widely used in all trades and professions; in the more severe operating mode enterprise of production environment and cement production enterprise; conveyer belt can wear and tear often, degumming, scratch, the damaging problem such as tear; it is continuing with if damaged part not repaired; then can expand the scope of breakage, cause conveyer belt to be scrapped in advance。In order to save cost, extend the service life of conveyer belt, enterprise generally all can there occurs in controlled range damaged time will in time conveyer belt be repaired, conventional repairing adopts mechanical connection manner or heat cure gluing connected mode, there is the easy fatigue damage of connecting portion in mechanical connection manner, and joint is uneven, it is easy to damage carrying roller;Heat cure gluing connected mode relative mechanical mode, its joint is convinced, without impact, but, existing heat cure gluing connected mode needs large-scale vulcanizing equipment to reach the repair efficiency of sulfuration, and it operates inconvenience, complex process, the problem repairing time length。
Summary of the invention
It is an object of the invention to provide a kind of damages of conveyor belt method for repairing and mending, this method can solve the problem that existing conveyer belt method for repairing and mending exists operation inconvenience, complex process and repairing time length。
In order to solve the problems referred to above, the technical solution used in the present invention is: this damages of conveyor belt method for repairing and mending comprises the following steps: A, the damaged part of conveyer belt carries out with polisher grinding process, cleaning polishing surface, surface roughening of polishing;
B, the mixture of cold cure bonding agent and firming agent is coated in the polishing surface of conveyer belt, and fills and leads up damaged mouth, after being completely dried, then be coated with within the scope of repairing and brush one times described mixture, dry to the tack-free back of the body;
C, the bar of repairing having brushed described mixture is pasted the step B surface processed, roll from zone line to surrounding with roller and repair bar, such repeat rolling more than three times;
D, carry out polishing finishing to repairing bar edge, by described mixture along repairing bar edge brushing cover this edge, fully dry。
In the technical scheme of said conveyer belt damage revamping method, technical scheme is it may also is that the polishing of step A ranges for damaged mouth periphery 10-15mm more specifically。
Further, described mixture is the cold cure bonding agent SC2000 and firming agent UT-R40 in the mixing of 25:2 ratio。
Further, use in described mixture upon mixing 1 hour。
Owing to have employed technique scheme, the present invention compared with prior art has the advantages that easy to operate, technique is simple, the repairing time is short, can use behind 2 hours after having repaired, and tearing strength can reach 12N/mm。
Detailed description of the invention
Below in conjunction with embodiment, the invention will be further described:
The damages of conveyor belt method for repairing and mending of the present embodiment comprises the following steps:
A, the damaged part of conveyer belt carrying out with polisher grinding process, polishing ranges for damaged mouth periphery 10-15mm, cleaning polishing surface, surface roughening of polishing;
B, cold cure bonding agent SC2000 and firming agent UT-R40 is mixed in 25:2 ratio, mixture is coated in the polishing surface of conveyer belt, and fills and leads up damaged mouth, after being completely dried, then be coated with within the scope of repairing and brush one times described mixture, dry to the tack-free back of the body;
C, the bar of repairing having brushed described mixture is pasted the step B surface processed, roll from zone line to surrounding with roller and repair bar, such repeat rolling more than three times;
D, carry out polishing finishing to repairing bar edge, by described mixture along repairing bar edge brushing cover this edge, fully dry。
Preferably, use in mixture upon mixing 1 hour;In step C and step D, available rubber hammer blow repairs bar。
Claims (4)
1. a damages of conveyor belt method for repairing and mending, it is characterised in that comprise the following steps:
A, with polisher the damaged part of conveyer belt carried out grinding process, cleaning polishing surface, surface roughening of polishing;
B, the mixture of cold cure bonding agent and firming agent is coated in the polishing surface of conveyer belt, and fills and leads up damaged mouth, after being completely dried, then be coated with within the scope of repairing and brush one times described mixture, dry to the tack-free back of the body;
C, the bar of repairing having brushed described mixture is pasted the step B surface processed, roll from zone line to surrounding with roller and repair bar, such repeat rolling more than three times;
D, carry out polishing finishing to repairing bar edge, by described mixture along repairing bar edge brushing cover this edge, fully dry。
2. damages of conveyor belt method for repairing and mending according to claim 1, it is characterised in that: the polishing of step A ranges for damaged mouth periphery 10-15mm。
3. damages of conveyor belt method for repairing and mending according to claim 1, it is characterised in that: described mixture is the cold cure bonding agent SC2000 and firming agent UT-R40 in the mixing of 25:2 ratio。
4. damages of conveyor belt method for repairing and mending according to claim 3, it is characterised in that: use in described mixture upon mixing 1 hour。