CN1055503A - 塑料挤注成型新工艺 - Google Patents
塑料挤注成型新工艺 Download PDFInfo
- Publication number
- CN1055503A CN1055503A CN90101850A CN90101850A CN1055503A CN 1055503 A CN1055503 A CN 1055503A CN 90101850 A CN90101850 A CN 90101850A CN 90101850 A CN90101850 A CN 90101850A CN 1055503 A CN1055503 A CN 1055503A
- Authority
- CN
- China
- Prior art keywords
- plastics
- basal body
- cooling
- exterior sheathing
- body pipe
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种塑料挤注成型新工艺,它由塑
料挤注、内芯加热与冷却、基体管(外管)或外模板退
出等过程组成。主要特征是利用挤注塑料的推力,逐
渐将基体管或外模板从加热芯推到冷却芯,从而在基
体管或外模板的内壁注上一层塑料。本发明可用于
为化工、造纸、电力等工业中贮存与输送强腐蚀材料
的槽与管道等挤注塑料防腐内衬,也可用于一次注成
大型塑料罐、塔、槽等产品。
Description
本发明属于塑料挤注成型技术领域。
在化工、电力、造纸、制药等工业中,经常需要大量存贮或输送酸、碱、盐等强腐蚀液体、气体或固体。用普通管道或容器输送、存贮这些强腐蚀材料,因抗不住腐蚀而易发生跑、冒、滴、漏现象。严重污染环境,造成设备停产,甚至导致人员伤亡。目前,国内外各企业在解决这个问题上,均采用不锈钢方法,或在基体材料(如碳钢)上附加橡胶防腐内衬方法。这几种方法主要有价格昂贵、耐腐寿命短等缺点。另外,目前工业中,还无法解决大型塑料产品(如贮槽、球罐、塔器等)的一次注射成型问题。现在,发电、化工等工业中所用的塑料设备,如大罐、球罐、贮槽等,都是用塑料板压形拼焊组装的。这种拼焊组装的塑料容器容易出现泄漏事故,就好象补过的车胎比没补过的车胎容易漏气一样,而且这种拼焊工艺要求工序繁多、技术复杂、难度大,因而造成成本较高。
本发明的目的在于提出一种新的技术方案-塑料挤注成型新工艺。用此技术方案,可以满意地解决大型塑料容器等产品的一次注成问题,并能解决化工、造纸等工业中管道、贮槽等的塑料防腐内衬挤注成型问题。
本发明的内容及工艺实现方法如下:见图1,(1)是塑料挤注管;(2)是基体管(外管)或外模板;(3)是加热内芯;(4)是定心套;(5)是接机头;(6)是端头模具;(7)是水嘴;(8)是冷却芯。当需要给管道或贮槽挤注塑料防腐内衬时,将管道或贮槽作为基体管(2),它与冷却芯(8)之间的间隙等于注射的防腐塑料厚度。挤注时,塑料从挤注机中射出,通过接机头(5)并沿着挤注管(2)注入到端头(6),在行进过程中,由于受加热内芯(3)加热,塑料不会冷却成型。到端头后,由于受封装无处可去,则挤注推力将推动端头模具(6)和基体管(2)向冷却芯(8)方向退出。退出时,塑料受到冷却芯(8)的冷却,立即成型。由于受到定心套(4)的固定,基体管(2)退出时,其内壁与冷却芯(8)之间的间隙始终保持为塑料防腐内衬的厚度。冷却芯中的循环冷却水由水嘴(7)控制。最后,基体管全部退出,管的防腐塑料内衬全部挤注完成,本发明的整个工艺过程也就实现了。当需要挤注大型塑料产品时,只需将基体管(2)换成相应的外模板即可。在上述工艺中,接机头(5)与挤注机联接。端头模具(6)是挡在基体管一端的模具,除能防止塑料泣出外,还能使塑料在基体管端部注成各种外沿。加热内芯(3)可用电加热管、棒或其它加热体。冷却芯(8)可用中空体,中间用循环凉水冷却,也可用其它冷却体。
本发明的优点在于:1、可为普通的碳钢管道、管件、容器或其它产品注上一层防腐塑料内衬,这些带有防腐塑料内衬的管道、管件和容器可用于化工、造纸等工业有强腐蚀的条件下,耐腐寿命长、工艺简单。2、利用本发明,可以一次注成目前其它方法无法一次注成的大型塑料罐、塔、槽等产品。
Claims (2)
1、一种塑料挤注成型新工艺,由挤注机,挤注管(1)、基体管或外模板(2)、加热内芯(3)、定心套(4)、端头模具(6)、冷却芯(8)等组成,其特征在于用挤注机将塑料从基体管或外模板(2)的一端通过挤注管(1)挤注到另一端,塑料在挤注管(1)中流动时,受到加热内芯(3)的加热而不会冷却,塑料挤注到另一端后,推动端头模具(6)和基体管或外模板(2)向冷却芯(8)方向退出,退出时注到基体管或外模板(2)内壁的塑料受冷却而成型,基体管或外模板(2)的内壁与冷却芯(8)之间的间隙靠定心套(4)控制。
2、如权利要求1所述的塑料挤注成型新工艺,基体管或外模板(2)可采用碳钢或其它材料,加热内芯(3)可用电加热方法或其它加热方法,冷却芯(8)可用中空体内循环冷却水方法或其它冷却方法。