CN105484719A - 一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法 - Google Patents
一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法 Download PDFInfo
- Publication number
- CN105484719A CN105484719A CN201511001174.0A CN201511001174A CN105484719A CN 105484719 A CN105484719 A CN 105484719A CN 201511001174 A CN201511001174 A CN 201511001174A CN 105484719 A CN105484719 A CN 105484719A
- Authority
- CN
- China
- Prior art keywords
- well
- fracturing
- crack
- fluid
- solvable ball
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供了一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,包括以下步骤:1)使用通井规通井;2)对水平井第一段进行多簇射孔;3)压裂施工;4)泵注前置液和携砂液;5)通过压裂液泵多尺度可溶球;6)可溶球在压裂施工完后自行溶解;7)重复步骤2)至步骤6),压裂作业井全部层段;8)放喷、求产和完井。本发明提供的方法解决了现有水平井每段各簇开启率均较低的问题,通过多尺度可溶球,对已起裂和延伸的裂缝缝口进行多级暂堵,使流体在射孔簇间发生转向迫使未起裂的射孔簇起裂并造出新缝,可达到各射孔簇均能有效起裂并延伸的目的,且不会堵塞孔眼,影响油井产量。
Description
技术领域
本发明属于采油工程技术领域,具体涉及一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法。
背景技术
近年来,“水平井+分段多簇体积压裂”方法已经成为开发非常规油气藏的有效手段,该方法是对套管进行分段多簇射孔,多簇同时压裂,区别于常规的单段射孔、单段压裂。
目前,国外主要采用水力桥塞分段多簇压裂工艺,即通过水力泵送或连续油管将速钻桥塞与射孔枪联作钻具下至预订位置,座封并释放桥塞后,与射孔枪脱离,上提射孔枪至射孔位置,按设计进行多簇射孔,采用低粘清水或混合水进行大排量、大液量压裂施工,实现多簇开启,形成裂缝,下入新的速钻桥塞与射孔枪联作钻具;重复上述步骤,依次自下而上完成多个层段作业,最后采用连续油管或常规油管钻磨桥塞,投产。国内主要采用水力喷砂分段多簇压裂工艺,即通过下水平井水力喷射分段多簇压裂管柱至设计位置;进行第一段的多簇射孔和大排量、大液量压裂作业;重复上述步骤,直至该井所有层段改造完毕。
上述方法主要存在以下问题:由于受储层非均质性的影响,使用原有的“多簇射孔同时压裂”方法,水平井每段各簇裂缝开启并有效延伸的几率只有30-40%。
发明内容
本发明的目的在于提供一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,以解决现有水平井每段各簇开启几率均过低的问题。
为此,本发明提供了一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,包括以下步骤:
步骤1)使用通井规通井:通井至作业井的人工井底,确保井筒干净,检查作业井的内径是否有变形或堵塞,若作业井有变形或者堵塞,则修井;
步骤2)对水平井第一段进行多簇射孔;
步骤3)采用多簇压裂工艺进行压裂施工;
步骤4)泵注前置液和携砂液;
步骤5)通过压裂液泵送粒径组合为0.1mm、1mm、3mm、5mm的可溶球1,比例为2:1.8:3:0.8,可溶球在压裂液中的体积分数为0.17;
步骤6)可溶球在压裂施工完后自行溶解;
步骤7)重复步骤2)至步骤6),压裂作业井全部层段;
步骤8)放喷、求产和完井。
步骤2)中水平井采用火力多簇或水力喷砂多簇射孔。
步骤3)中采用水力桥塞分段多簇压裂工艺或水力喷砂分段多簇压裂工艺进行压裂施工。
本发明的有益效果是:本发明提供的方法解决了现有水平井每段各簇开启率均较低的问题,通过多尺度可溶球,对已起裂和延伸的裂缝缝口进行多级暂堵,使流体在射孔簇间发生转向迫使未起裂的射孔簇起裂并造出新缝,可达到各射孔簇均能有效起裂并延伸的目的,且不会堵塞孔眼,影响油井产量。
下面将结合附图做进一步详细说明。
附图说明
图1是为常规水平井部分射孔簇开启示意图;
图2为采用多尺度可溶球实现水平井多簇开启示意图;
图3为压裂施工中,加入多尺度可溶球前后的压裂施工特征曲线;
图4为多尺度可溶球自行溶解后的水平井多簇示意图。
附图说明:1、可溶球。
具体实施方式
实施例1:
本实施例提供了一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,包括以下步骤:
步骤1)使用通井规通井:通井至作业井的人工井底,确保井筒干净,检查作业井的内径是否有变形或堵塞,若作业井有变形或者堵塞,则修井;
步骤2)对水平井第一段进行多簇射孔;
步骤3)采用多簇压裂工艺进行压裂施工;
步骤4)泵注前置液和携砂液;
步骤5)通过压裂液泵送粒径组合为0.1mm、1mm、3mm、5mm的可溶球1,比例为2:1.8:3:0.8,可溶球1在压裂液中的体积分数为0.17;
步骤6)可溶球1在压裂施工完后自行溶解;
步骤7)重复步骤2)至步骤6),压裂作业井全部层段;
步骤8)放喷、求产和完井。
本发明原理:
采用多尺度可溶球1,大粒径的可溶球1到达射孔孔眼被截堵在裂缝端口,较小的可溶球1填充在大粒径可溶球1之间,有效快速提高封堵效果,使流体在射孔簇间发生转向,迫使未起裂的射孔簇起裂并造出新缝;施工结束后,多尺度可溶球1在井底温度的作用下完全降解,无残渣,不对地层产生二次污染。
实施例2:
在实施例1的基础上,水平井采用火力多簇或水力喷砂多簇射孔;压裂采用水力桥塞分段多簇压裂工艺或水力喷砂分段多簇压裂工艺进行压裂施工。
图1为常规水平井部分射孔簇开启示意图;图2为本发明采用多尺度可溶球1实现水平井多簇开启示意图;压裂施工中,支撑剂浓度、地面压力及携砂液排量见图3所示,图4为多尺度可溶球1自行溶解后的水平井多簇示意图。
本发明提供的方法解决了现有水平井每段各簇开启率均较低的问题,通过多尺度可溶球1,对已起裂和延伸的裂缝缝口进行多级暂堵,使流体在射孔簇间发生转向迫使未起裂的射孔簇起裂并造出新缝,可达到各射孔簇均能有效起裂并延伸的目的,且不会堵塞孔眼,影响油井产量。
本实施例没有详细叙述的方法或具体施工过程属本行业的公知常识,这里不一一叙述。
以上例举仅仅是对本发明的举例说明,并不构成对本发明的保护范围的限制,凡是与本发明相同或相似的设计均属于本发明的保护范围之内。
Claims (3)
1.一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,其特征在于,包括以下步骤:
步骤1)使用通井规通井:通井至作业井的人工井底,确保井筒干净,检查作业井的内径是否有变形或堵塞,若作业井有变形或者堵塞,则修井;
步骤2)对水平井第一段进行多簇射孔;
步骤3)采用多簇压裂工艺进行压裂施工;
步骤4)泵注前置液和携砂液;
步骤5)通过压裂液泵送粒径组合为0.1mm、1mm、3mm、5mm的可溶球(1),比例为2:1.8:3:0.8,可溶球(1)在压裂液中的体积分数为0.17;
步骤6)可溶球(1)在压裂施工完后自行溶解;
步骤7)重复步骤2)至步骤6),压裂作业井全部层段;
步骤8)放喷、求产和完井。
2.根据权利要求1所述的一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,其特征在于:步骤2)中水平井采用火力多簇或水力喷砂多簇射孔。
3.根据权利要求1所述的一种采用多尺度可溶球封堵缝口提高多簇起裂有效性的方法,其特征在于:步骤3)中采用水力桥塞分段多簇压裂工艺或水力喷砂分段多簇压裂工艺进行压裂施工。