CN1054561A - The method for making of lacquer painting - Google Patents

The method for making of lacquer painting Download PDF

Info

Publication number
CN1054561A
CN1054561A CN 90101185 CN90101185A CN1054561A CN 1054561 A CN1054561 A CN 1054561A CN 90101185 CN90101185 CN 90101185 CN 90101185 A CN90101185 A CN 90101185A CN 1054561 A CN1054561 A CN 1054561A
Authority
CN
China
Prior art keywords
lacquer
pigment
picture
varnish
treat
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN 90101185
Other languages
Chinese (zh)
Other versions
CN1039108C (en
Inventor
董得福
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN90101185A priority Critical patent/CN1039108C/en
Publication of CN1054561A publication Critical patent/CN1054561A/en
Application granted granted Critical
Publication of CN1039108C publication Critical patent/CN1039108C/en
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

The present invention relates to a kind of method for making of lacquer painting, step comprises upper plate lacquer, modulation drawing pigment and drawing, and it is characterized in that: it is base-material that drawing pigment is selected phyteral and mineral powders for use, mixes well after adding a little glue; The step of drawing is: adopt above-mentioned pigment water transfer to draw a picture → treat to coat layer of transparent after picture is done coat with lacquer → treat the clear lacquer and do after, polish surface → repeat above-mentioned steps → so repeat, with sand paper until improving works at imperfect picture place.The present invention not only helps the artist and fully, freely expresses its creation artistic conception, and technology is simple.Its works have enjoying value and use value.

Description

The method for making of lacquer painting
The present invention relates to is a kind of method for making of lacquer painting.
This novelty is drawn kind, and (common name: lacquer painting) similarity is arranged, promptly showing picture has the feature of " lacquer ", but basic difference is being arranged aspect painting material and the method for making with the contemporary Chinese lacquer painting.
The making processes of contemporary Chinese lacquer painting is: with natural raw lacquer is to draw raw material.Be modulated into color lacquer (traditional colour is as black, red, gold) with lacquer through special process, paint on special lacquer plate with coating with lacquer lacquer technology (being coated on the implements) then with lacquer, be particular about temperature, humidity, dry in the shade, after waiting to dry in the shade, grind or do not grind according to the needs on the drawing, cover lacquer or do not cover lacquer.Sometimes in order to reach certain certain effects, also need add many exotic materialss.
Because the lacquer painting complex process, synthetic color lacquer look kind color lacquer few and not homochromy kind is difficult for the existence of problems such as mixing, therefore is an impediment to the artist and fully, freely expresses its creation artistic conception.
The objective of the invention is to provide a kind of method for making of lacquer painting, this method for making not only helps the artist and fully, freely expresses its creation artistic conception, and manufacture craft is easy, and material is easy to get.Its method for making can provide the artist the wide art exploration world, and its works have higher artistic value and practical value, and easy to use and preservation.
Making processes of the present invention is: on the smooth smooth floor even be coated with base plate and coat with lacquer → treat polish base plate lacquer painting → modulation drawing pigment → drawing with sand paper again after lacquer is done.The method that is characterized in A, modulation drawing pigment is: selecting mineral substance and phyteral powder for use is to mix well after base-material adds a little glue, makes various pigment.The step of B, drawing is: adopt above-mentioned pigment water transfer to draw a picture, treat to coat the layer of transparent lacquer after picture is done; After treating that the clear lacquer is done, polish the surface with sand paper; Repeat above-mentioned steps at imperfect picture place, so repeat until improve works (last is all over after drawing a picture, and treats that picture dries should coat the layer of transparent lacquer, and omits the step that polishes lacquer painting with sand paper) comprehensively.
Pull at the above-mentioned end can be plank, three-ply-wood, five-ply board, paper, calcium-plastic board, cement plate, concrete floor, metope etc., and the plate face that all adaptation base plate lacquers adhere to all can.
Above-mentioned base plate lacquer is general chemistry paint, coats the back and easily does to well.
Above-mentioned drawing pigment can be modulated usually voluntarily, directly selects existing drawing pigments such as watercolor, pigment, traditional Chinese Painting and propylene for use.As satisfying the color needs, can modulate voluntarily by above-mentioned modulator approach.(add as powder such as gold and silver, copper, aluminium and can use after a little glue is mixed well.)
The above-mentioned clear lacquer can be selected alkyd varnish, phenolic varnish, first polyamine fat varnish, second polyamine fat varnish or first, second polyamine fat mixing varnish for use.
Than lacquer painting, method for making of the present invention has following several respects advantage:
1, drawing pigment look kind is abundant, good water solubility, and water transfer uses color change multifarious.
2, use the pigment and the clear lacquer and successively paint, not only help the artist to revise, improve picture, reach the creation artistic conception of its perfection, and can make works that transparent feel, spatial level sense, thick and heavy sense, reflecting feel and color mystique are arranged.Far, closely the artistic effect of appreciating is all good.
3, manufacture craft is easy, material is easy to get, cost is low, be convenient to popularization and application.
Be that example is specifically described the present invention with the marble image method for making of decorating the floor, room below:
One, get all the following articles for use ready: sand paper, chi, paintbrush, painting brush, base plate lacquer (chemistry paint), the clear lacquer (selecting alkyd varnish for use), drawing pigments such as drawing pigment-directly select for use or general watercolor, pigment, traditional Chinese Painting, propylene, water, kerosene is (in order to clean Brush or pen that alkyd varnish and chemistry paint are arranged).
Two, marble image drawing process (directly on the floor, drawing a picture)
(1) polishes concrete floor with sand paper, get final product to being smooth to the touch.
(2) the concrete floor wash clean is dried after, be coated with upper plate lacquer (with thin evenly for good), treat to polish with sand paper again after lacquer is done, being smooth to the touch gets final product.Japanning like this one, two times (purpose is to avoid the floor suction).
(3) line, the square grid bottom line that draws (every length of side value is 0.5 meter or 0.6 meter).
(4) in square grid, adopt above-mentioned drawing pigment to draw a picture: after coating required color, water injects or watering, with or hand make color and water molten.Because water can be with pigment to flow, and presents various unexpected and natural marble skin texture image, therefore the person of drawing a picture can be as required, make water mobile or mobile, till satisfaction (if image is not good, can be local or all fall heavily to come with scrub water, very free, make things convenient for).
(5) wait to dry after, with black (also available prepared Chinese ink) or coppery draw square line.This moment image is as the brocatel picture, and (this is that top layer pigment has hidden the pigment of bottom because after water did, pigment deposited but color is good-looking when wet; In addition, pigment itself is become dry by wet, also causes color change).Coat alkyd varnish again, image returns back to the effect when wetting again substantially.(this is because the clear lacquer has penetrant action, and the thickness that layer of transparent is arranged when dried, and therefore, under the effect of light, color shows effect when wet, makes image have transparent feel and mystique).
(6) treat that lacquer dries after, in unsatisfied place, draw a picture (before repeating drawing, application sand paper polishes the injustice place of picture, and being smooth to the touch gets final product) by above-mentioned steps (4), treat that picture dries after, brush alkyd varnish more comprehensively.
(7) dry at last, come into operation.Concrete floor is as layer overlay brocatel slabstone.
Three, effect
1, the skin texture of marble image is true to nature, and color is attractive in appearance, smooth surface.
2, durable in use.Through the uses in 5 years in the room, the marble image does not fade so far, weares and teares.
3, be convenient to clean, repair.
4, technology is simple, cost is low.Decorate 14 square metres concrete floor, used base plate lacquer, pigment and alkyd varnish only needs 30~50 yuan.
In addition, the method for making of single width lacquer painting and marble image drawing process are similar, and the key distinction is: 1, base plate adopts three-ply-wood, paper or monolithic cement plate, hangs with civilian dress.2, drawing method can be drawn kind of a general drawing technique of expression by above-mentioned steps (4) and in conjunction with each.
Making jumbo indoor mural painting, can above-mentioned single width lacquer painting be that the unit makes up.
The advantage and the pictorial skill of lacquer painting collection western drawing of the present invention, contemporary Chinese lacquer painting, and formation and development unique artistic language and the artistic effect of self.Both had graceful value of art appreciation, popular again practicality.Therefore be a kind of novelty picture kind that characteristic is full of vitality that has much.

Claims (2)

1, the method for making of lacquer painting, concrete steps comprise (1) even base plate lacquer that is coated with on smooth smooth floor; (2) treat that base plate lacquer is done after, polish with sand paper, being smooth to the touch gets final product; (3) modulation drawing pigment and (4) drawing is characterized in that:
The method of modulation drawing pigment is: (3.a) selecting mineral substance and phyteral powder for use is base-material, mixes well after (3.b) adding a little glue, makes pigment of all kinds.
The step of drawing is: (4.a) adopt above-mentioned pigment water transfer to draw a picture; (4.b) treat to coat the layer of transparent lacquer after picture is done; (4.c) treat that the clear lacquer is done after, polish the surface with sand paper and be smooth to the touch and get final product; (4.d) repeat above-mentioned steps (4.a), (4.b), (4.c), so repeat, until improving works (finally once omitting step 4.C) at imperfect picture place.
2, the method for making of lacquer painting according to claim 1 is characterized in that the described clear lacquer is alkyd varnish, phenolic varnish, first polyamine fat varnish, second polyamine fat varnish or first, second polyamine fat mixing varnish.
CN90101185A 1990-03-02 1990-03-02 Making method of lacquer painting Expired - Fee Related CN1039108C (en)