CN105398258A - Paintbrush used for oil paintings and manufacturing method of paintbrush - Google Patents
Paintbrush used for oil paintings and manufacturing method of paintbrush Download PDFInfo
- Publication number
- CN105398258A CN105398258A CN201510795963.XA CN201510795963A CN105398258A CN 105398258 A CN105398258 A CN 105398258A CN 201510795963 A CN201510795963 A CN 201510795963A CN 105398258 A CN105398258 A CN 105398258A
- Authority
- CN
- China
- Prior art keywords
- bristles
- hair
- minute
- paintbrush
- stalk
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to the technical field of paintbrushes, in particular to a paintbrush used for oil paintings and a manufacturing method of the paintbrush. A paintbrush point is composed of, by weight, 60-70% of bristles, 0-20% of ox hair and 20-30% of modified straw. The paintbrush is good in elasticity, not prone to deformation, and good in pigment absorption performance and is not affected by cold and heat, the softness is achieved based on thickness, and a sense of uniform textures is achieved.
Description
Technical field:
The present invention relates to paintbrush technical field, be specifically related to a kind of oil painting paintbrush and preparation method thereof.
Background technology:
Oil painting paintbrush: be the special draw tool of a kind of oil painting, general penholder mostly is wooden, pen hair is bristles, also has minority writing brush and chemical fibre.Divide round end pen, tack pen, fan pen, spread pen etc. to be divided into 12 kinds of models by size by written shape, be respectively 1#-12# from small to large, also have some large models in addition.Oil painting brush plays the most basic function in oil painting drawing process.Handy paintbrush, brings temperament and interest can to artistical work.Gimmick of drawing a picture is depended in selecting of oil painting brush.The paintbrush of differing texture, shape, model, its effect is also different, and existing bristle paintbrush mostly is bristles, is used for the abundant technique of painting having style of writing skin texture, but time painted, uneven fusion, pigments absorbalight is not fine.
Summary of the invention:
Technical problem to be solved by this invention is that overcoming existing technological deficiency provides a kind of oil painting paintbrush and preparation method thereof.
Technical problem to be solved by this invention adopts following technical scheme to realize:
A kind of oil painting paintbrush, comprise penholder and nib, it is characterized in that: described nib is made up of bristles, ox hair and modified straw, described bristles percentage by weight is 60-70%, described ox hair percentage by weight is 0-20%, and described modified straw percentage by weight is 20-30%.
A preparation method for oil painting paintbrush, is characterized in that comprising the following steps:
(1) modified straw processing method: after being tiled by stalk, stalk thickness is 8-10 centimetre, then sprinkles one deck lime above, and lime thickness is 1-2 centimetre, finally sprinkles water, is as the criterion to lime half is wet, moisturizing 2-3 days; Stalk is taken out and cleans, after drying, put into sealing acidification pool, in acidification pool, evenly put into 10% hydrochloric acid solution, the temperature of acidification pool is elevated to 130-140 DEG C, pressure is elevated to 7-8MPa, after 20 minutes, then add 15% acetum, pressure is elevated to 10-11MPa, time is 30 minutes, period stirring frequency be 50 revs/min; Stalk is taken out and spends deionized water, then carry out drying at 30-40 DEG C of temperature; By dried Straw decomposing, fineness is 35-80 micron;
(2) bristles processing method: by bristles root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the soda ash solution of 110-120 DEG C is used to rinse bristles 15-20 minute, the diethyl ether solution containing 20% acetic acid re-using 50-60 DEG C rinses 10-13 minute, finally make to spend 90-100 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(3) ox hair processing method: by ox hair root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the limewash of 60-70 DEG C is used to rinse ox hair 9-13 minute, 15% ammonium sulfate that contains re-using 40-50 DEG C rinses 10-15 minute, finally make to spend 80-90 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(4) by after the modified straw, ox hair and the bristles precentagewise Homogeneous phase mixing that processed, make nib, then use metal skin nib and penholder to be linked together.
The technology that the present invention uses modified straw, bristles and ox hair to combine, degreasing is more thorough, and do not hinder cutting edge of a knife or a sword person of outstanding talent, do not add any anticorrisive agent, holding time is long, adopts stalk also can reduce costs, and the present invention has good springiness, not yielding, heat affecting of not catching a cold, pigments absorbalight are good, abundant basis adds mildness, presents uniform skin texture sensation.
Detailed description of the invention:
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, setting forth the present invention further below.
In embodiment: a kind of oil painting paintbrush, comprise penholder and nib, it is characterized in that: described nib is made up of bristles, ox hair and modified straw, described bristles percentage by weight is 65%, described ox hair percentage by weight is 10%, and described modified straw percentage by weight is 25%.
A preparation method for oil painting paintbrush, is characterized in that comprising the following steps:
(1) modified straw processing method: after being tiled by stalk, stalk thickness is 8-10 centimetre, then sprinkles one deck lime above, and lime thickness is 1-2 centimetre, finally sprinkles water, is as the criterion to lime half is wet, moisturizing 2-3 days; Stalk is taken out and cleans, after drying, put into sealing acidification pool, in acidification pool, evenly put into 10% hydrochloric acid solution, the temperature of acidification pool is elevated to 130-140 DEG C, pressure is elevated to 7-8MPa, after 20 minutes, then add 15% acetum, pressure is elevated to 10-11MPa, time is 30 minutes, period stirring frequency be 50 revs/min; Stalk is taken out and spends deionized water, then carry out drying at 30-40 DEG C of temperature; By dried Straw decomposing, fineness is 35-80 micron;
(2) bristles processing method: by bristles root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the soda ash solution of 110-120 DEG C is used to rinse bristles 15-20 minute, the diethyl ether solution containing 20% acetic acid re-using 50-60 DEG C rinses 10-13 minute, finally make to spend 90-100 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(3) ox hair processing method: by ox hair root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the limewash of 60-70 DEG C is used to rinse ox hair 9-13 minute, 15% ammonium sulfate that contains re-using 40-50 DEG C rinses 10-15 minute, finally make to spend 80-90 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(4) by after the modified straw, ox hair and the bristles precentagewise Homogeneous phase mixing that processed, make nib, then use metal skin nib and penholder to be linked together.
More than show and describe general principle of the present invention and principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and description just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.
Claims (2)
1. an oil painting paintbrush, comprise penholder and nib, it is characterized in that: described nib is made up of bristles, ox hair and modified straw, described bristles percentage by weight is 60-70%, described ox hair percentage by weight is 0-20%, and described modified straw percentage by weight is 20-30%.
2. a preparation method for oil painting paintbrush, is characterized in that comprising the following steps:
(1) modified straw processing method: after being tiled by stalk, stalk thickness is 8-10 centimetre, then sprinkles one deck lime above, and lime thickness is 1-2 centimetre, finally sprinkles water, is as the criterion to lime half is wet, moisturizing 2-3 days; Stalk is taken out and cleans, after drying, put into sealing acidification pool, in acidification pool, evenly put into 10% hydrochloric acid solution, the temperature of acidification pool is elevated to 130-140 DEG C, pressure is elevated to 7-8MPa, after 20 minutes, then add 15% acetum, pressure is elevated to 10-11MPa, time is 30 minutes, period stirring frequency be 50 revs/min; Stalk is taken out and spends deionized water, then carry out drying at 30-40 DEG C of temperature; By dried Straw decomposing, fineness is 35-80 micron;
(2) bristles processing method: by bristles root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the soda ash solution of 110-120 DEG C is used to rinse bristles 15-20 minute, the diethyl ether solution containing 20% acetic acid re-using 50-60 DEG C rinses 10-13 minute, finally make to spend 90-100 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(3) ox hair processing method: by ox hair root upward, cutting edge of a knife or a sword person of outstanding talent place down, then the limewash of 60-70 DEG C is used to rinse ox hair 9-13 minute, 15% ammonium sulfate that contains re-using 40-50 DEG C rinses 10-15 minute, finally make to spend 80-90 DEG C of de-ionised water 10-15 minute, then carry out 20-30 DEG C of low temperature drying;
(4) by after the modified straw, ox hair and the bristles precentagewise Homogeneous phase mixing that processed, make nib, then use metal skin nib and penholder to be linked together.