CN105273487A - Preparation method of rosin environment-friendly desiccant - Google Patents

Preparation method of rosin environment-friendly desiccant Download PDF

Info

Publication number
CN105273487A
CN105273487A CN201410319397.0A CN201410319397A CN105273487A CN 105273487 A CN105273487 A CN 105273487A CN 201410319397 A CN201410319397 A CN 201410319397A CN 105273487 A CN105273487 A CN 105273487A
Authority
CN
China
Prior art keywords
rosin
desiccant
preparation
environment
friendly
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410319397.0A
Other languages
Chinese (zh)
Inventor
侯霞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410319397.0A priority Critical patent/CN105273487A/en
Publication of CN105273487A publication Critical patent/CN105273487A/en
Pending legal-status Critical Current

Abstract

The invention relates to a preparation method of a rosin environment-friendly desiccant, and relates to the technical field of desiccant preparation. The method is characterized in that the rosin environment-friendly desiccant is composed of the components of, by weight: 30-35% of rosin, 10-18% of linseed oil, 30-40% of cobalt, 10-15% of soybean oil, and 10-20% of S-1 mineral oil. According to the invention, prepared rosin, linseed oil, soybean oil and S-1 mineral oil are added first; the temperature is increased to 120+/-5 DEG C; the temperature is maintained for 1h, and cobalt is added; the materials are well mixed by stirring, and a product can be fetched. The desiccant provided by the invention is green, environment-friendly, nontoxic, and odorless. The desiccant causes no damage to human body. Under room temperature and normal humidity, the desiccant has good adsorption activity, static dehumidification function, odor-removing function, and the like.

Description

The preparation method of rosin environmental protection siccative
Technical field
The present invention relates to siccative preparing technical field, be specifically related to a kind of preparation method of rosin environmental protection siccative.
Background technology
Ink is the important materials for wrapping material printing, and it is by printing by pattern, literal table now on the substrate, and ink comprises main component and ancillary component, and they mix equably and form the gluey fluid of a kind of viscosity through repeat-rolling.Be made up of pigment, low-melting ink vehicle and auxiliary agent etc.For various printings such as books and periodicals, packing and decorating, building decorations.Along with social demand increases, ink kind and output is respective extension and growth also.Along with the stable development in China's offset printing market, flexographic ink have also been obtained very fast development, and its quality level is substantially close or reach international most advanced level.According to incompletely statistics, the ratio occupied in China's ink market of flexographic ink rises to 50% ~ 60%, still occupies an leading position, and this ratio can not great changes have taken place within significant period of time from now on.In recent years, along with expanding economy, environmental protection cry is more and more high, and printing bound pair flexographic ink proposes new requirement in nontoxic, pollution-free, and environment-friendlyadhesive adhesive printing ink is subject to the extensive concern of user and starts to be applied to packaging, newspaper, commercial printing etc.Environment-friendlyadhesive adhesive printing ink has obtained large-scale application in the U.S., Japan and other countries, but application is at home also quite few, and this wherein has the factor of technical elements, but more chief reason is that understanding is not enough.Environment-friendlyadhesive adhesive printing ink is mainly without aromatic hydrocarbons soya-bean ink.The PAH (polycyclic aromatic hydrocarbons) contained in tradition ink composition is a kind of volatile solvent printing film, harmful; The volatile organic compounds wherein contained not only increases topsoil, also can damage human body.Offset printing soya-bean ink adopts soybean ep-type material to replace part petroleum solvent, can reduce the injury of pollution to environment and human body.Siccative is also absorbent, is to be used in protection against the tide, mildew-resistant aspect, plays desiccation, is not all point physical adsorption siccative and chemisorption siccative by suction type and reaction product.Traditional is heavier for the siccative taste in ink, and drying effect is bad.
Summary of the invention
It is good that technical problem to be solved by this invention is to provide a kind of drying effect, the preparation method of free of contamination rosin environmental protection siccative.
Technical problem to be solved by this invention realizes by the following technical solutions:
The preparation method of described rosin environmental protection siccative is made up of the combination of following weight percent, it is characterized in that: first drop into the rosin, oleum lini, soya-bean oil and the S-1 Dormant oils that configure, be warmed up to 120 ± 5 DEG C, be incubated after one hour, start to drop into cobalt, after stirring, take the dish out of the pot.
The invention has the beneficial effects as follows: environmental protection of the present invention, nonpoisonous and tasteless, harmless to human body, under room temperature and general humidity, there is good adsorption activity, the effects such as static dehumidification and peculiar smell removal.
Embodiment
The technique means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, below in conjunction with specific examples, setting forth the present invention further.
The preparation method of rosin environmental protection siccative is, first drops into the rosin, oleum lini, soya-bean oil and the S-1 Dormant oils that configure, is warmed up to 120 DEG C, is incubated after one hour, starts to drop into cobalt, after stirring, take the dish out of the pot.
More than show and describe ultimate principle of the present invention and principal character and advantage of the present invention.The technician of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and specification sheets just illustrates principle of the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (1)

1. the preparation method of rosin environmental protection siccative, it is characterized in that: the preparation method of described rosin environmental protection siccative is made up of the combination of following weight percent, the preparation method of the preparation method of rosin environmental protection siccative, it is characterized in that: first drop into the rosin, oleum lini, soya-bean oil and the S-1 Dormant oils that configure, be warmed up to 120 ± 5 DEG C, be incubated after one hour, start to drop into cobalt, after stirring, take the dish out of the pot.
CN201410319397.0A 2014-07-07 2014-07-07 Preparation method of rosin environment-friendly desiccant Pending CN105273487A (en)