CN105255317A - 一种环氧地坪面涂料 - Google Patents
一种环氧地坪面涂料 Download PDFInfo
- Publication number
- CN105255317A CN105255317A CN201510743647.8A CN201510743647A CN105255317A CN 105255317 A CN105255317 A CN 105255317A CN 201510743647 A CN201510743647 A CN 201510743647A CN 105255317 A CN105255317 A CN 105255317A
- Authority
- CN
- China
- Prior art keywords
- parts
- top coating
- floor top
- epoxy
- epoxy floor
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种环氧地坪面涂料,包括如下含量比例的成分:液体环氧树脂30-40份;环氧树脂28-35份;二甲苯6-12份;正丁醇4-8份;醋酸丁酯1-3份;分散剂5-10份;消泡剂0.5-1份;流平剂0.2-0.6份;氧化铁红3-8份;沉淀硫酸钡7-21份;滑石粉8-12份;石英砂18-26份;有机膨润土20-30份;水40-60份;本发明的有益效果是:提供一种环氧地坪面涂料,涂料环保无污染,耐磨性能好、能够用于多种不同场合,实用性好。
Description
技术领域
本发明涉及一种环氧地坪面涂料,属于涂料技术领域。
背景技术
环氧涂料一般分为油性环氧涂料和水性环氧涂料2种,按照使用性能划分,一般有耐磨环氧涂料和环氧防腐涂料,严格的划分还应该有防静电环氧涂料和建筑环氧装饰涂料,细分应该是4大种类比较确切,中国项目可行性研究中心可行性报告分析,就环氧(树脂地坪)涂料行业而言,客户价值主要有两个层次。首先,产品性能的价值,即是产品的环保性能、耐磨性能。产品的基本性能,如耐磨性得到了满足后,环保性、实用性就最为重要。其次,细分性能价值,针对不同客户对环氧涂料性能的需求,满足客户的产品性能要求,来研发生产环氧涂料产品。满足不同的客户需求,产品自然就有了差异化,所以这一价值层次最容易独立市场成为创新品类。明确并满足客户向上的价值,就能找到创新和升级的发力点,源于客户价值,高于顾客价值的产品,才能牢牢吸引消费者。
发明内容
本发明主要解决的技术问题是提供一种环保耐磨、实用性好的环氧地坪面涂料。
为解决上述技术问题,本发明采用的一个技术方案是:一种环氧地坪面涂料,包括如下含量比例的成分:液体环氧树脂30-40份;环氧树脂28-35份;二甲苯6-12份;正丁醇4-8份;醋酸丁酯1-3份;分散剂5-10份;消泡剂0.5-1份;流平剂0.2-0.6份;氧化铁红3-8份;沉淀硫酸钡7-21份;滑石粉8-12份;石英砂18-26份;有机膨润土20-30份;水40-60份。
本发明的有益效果是:提供一种环氧地坪面涂料,涂料环保无污染,耐磨性能好、能够用于多种不同场合,实用性好。
具体实施方式
下面对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
本发明实施例1包括:一种环氧地坪面涂料,包括如下含量比例的成分:液体环氧树脂30份;环氧树脂28份;二甲苯6份;正丁醇4份;醋酸丁酯1份;分散剂5份;消泡剂0.5份;流平剂0.2份;氧化铁红3份;沉淀硫酸钡7份;滑石粉8份;石英砂18份;有机膨润土20份;水40份。
本发明实施例2包括:一种环氧地坪面涂料,包括如下含量比例的成分:液体环氧树脂35份;环氧树脂32份;二甲苯9份;正丁醇5份;醋酸丁酯2份;分散剂7份;消泡剂0.7份;流平剂0.4份;氧化铁红5份;沉淀硫酸钡14份;滑石粉10份;石英砂22份;有机膨润土25份;水50份。
本发明实施例3包括:一种环氧地坪面涂料,包括如下含量比例的成分:液体环氧树脂40份;环氧树脂35份;二甲苯12份;正丁醇8份;醋酸丁酯3份;分散剂10份;消泡剂1份;流平剂0.6份;氧化铁红8份;沉淀硫酸钡21份;滑石粉12份;石英砂26份;有机膨润土30份;水60份。
上述实施例只为说明本发明的技术构思及特点,其目的在于让熟悉此项技术的人士能够了解本发明的内容并加以实施,并不能以此限制本发明的保护范围,凡根据本发明精神实质所作的等效变化或修饰,都应涵盖在本发明的保护范围内。
Claims (1)
1.一种环氧地坪面涂料,其特征在于:包括如下含量比例的成分:液体环氧树脂30-40份;环氧树脂28-35份;二甲苯6-12份;正丁醇4-8份;醋酸丁酯1-3份;分散剂5-10份;消泡剂0.5-1份;流平剂0.2-0.6份;氧化铁红3-8份;沉淀硫酸钡7-21份;滑石粉8-12份;石英砂18-26份;有机膨润土20-30份;水40-60份。