CN105252123A - 环缝焊接工艺 - Google Patents

环缝焊接工艺 Download PDF

Info

Publication number
CN105252123A
CN105252123A CN201410330853.1A CN201410330853A CN105252123A CN 105252123 A CN105252123 A CN 105252123A CN 201410330853 A CN201410330853 A CN 201410330853A CN 105252123 A CN105252123 A CN 105252123A
Authority
CN
China
Prior art keywords
circle
ring
plane
sealing cap
capping
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410330853.1A
Other languages
English (en)
Inventor
丁春燕
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201410330853.1A priority Critical patent/CN105252123A/zh
Publication of CN105252123A publication Critical patent/CN105252123A/zh
Pending legal-status Critical Current

Abstract

本发明涉及焊接领域,具体公开了一种环缝焊接工艺。该环缝焊接方法,其特征在于:首先将封盖与筒体插接接触部位加工刺挠过程在封盖上与筒体插接接触环面上的止口部位外圈是一圈和垂直径行面呈32.5度的斜坡环面,在32.5度的径向斜坡环面和轴向圆柱面详解的轴向圆柱面根部是一圈宽1.5毫米,深0.5毫米的凹环,筒体与插入的封盖的下沿最底部是一圈厚0.3毫米,款0.5毫米的底环边,紧靠底环边封盖的下沿是一圈和垂直径向面呈32.5度的斜坡环面,再在梯形部位进行焊接。本发明的有益效果是:与封盖熔焊在一起,使筒体横向部位融化焊牢,达到焊接部位的厚度要求,达到密封要求。

Description

环缝焊接工艺
技术领域
本发明涉及焊接领域,具体为一种环缝焊接工艺。
背景技术
目前,带压的铝合金筒体焊接部分要求达到一定的密封强度要求,但是原有的铝合金筒体和封盖在焊接时,封盖上和筒体接触环面加工成止口,止口根部加工成坡面,再将封盖止口根部插入筒体口,径行氩弧焊焊接,由于焊接部位的封盖会吸收一些热量,焊剂和焊材不能深入环缝额内部,焊缝环面不能完全融化,焊接部位较浅,焊接达不到密封强度要求。
发明内容
本发明所要解决的技术问题是:提供一种环缝焊接方法。焊剂和焊料能深入环缝内部,焊接环面达到完全融化,焊接部位后,达到密封强度压球。
本发明的技术方案是:
一种环缝焊接方法,其特征在于:首先将封盖与筒体插接接触部位加工刺挠过程在封盖上与筒体插接接触环面上的止口部位外圈是一圈和垂直径行面呈32.5度的斜坡环面,在32.5度的径向斜坡环面和轴向圆柱面详解的轴向圆柱面根部是一圈宽1.5毫米,深0.5毫米的凹环,筒体与插入的封盖的下沿最底部是一圈厚0.3毫米,款0.5毫米的底环边,紧靠底环边封盖的下沿是一圈和垂直径向面呈32.5度的斜坡环面,再在梯形部位进行焊接。
本发明的有益效果是:焊剂和焊料能够深入焊缝内部的环槽中,筒体上的焊接底环面由于有一个悬空的面,焊枪打火时与梯形槽底部形成小熔池,焊接热量不会传到出去,集中在筒体上底环面的这个悬空的换面上,热量不流失,使得这个悬空的环面能达到完全融化,与封盖熔焊在一起,使筒体横向部位融化焊牢,达到焊接部位的厚度要求,达到密封要求。
具体实施方式
带压的铝合金筒体焊接部分要求达到一定的密封强度要求,但是原有的铝合金筒体和封盖在焊接时,封盖上和筒体接触环面加工成止口,止口根部加工成坡面,再将封盖止口根部插入筒体口,径行氩弧焊焊接,由于焊接部位的封盖会吸收一些热量,焊剂和焊材不能深入环缝额内部,焊缝环面不能完全融化,焊接部位较浅,焊接达不到密封强度要求。
本发明所要解决的技术问题是:提供一种环缝焊接方法。焊剂和焊料能深入环缝内部,焊接环面达到完全融化,焊接部位后,达到密封强度压球。
一种环缝焊接方法,其特征在于:首先将封盖与筒体插接接触部位加工刺挠过程在封盖上与筒体插接接触环面上的止口部位外圈是一圈和垂直径行面呈32.5度的斜坡环面,在32.5度的径向斜坡环面和轴向圆柱面详解的轴向圆柱面根部是一圈宽1.5毫米,深0.5毫米的凹环,筒体与插入的封盖的下沿最底部是一圈厚0.3毫米,款0.5毫米的底环边,紧靠底环边封盖的下沿是一圈和垂直径向面呈32.5度的斜坡环面,再在梯形部位进行焊接。
本发明的有益效果是:焊剂和焊料能够深入焊缝内部的环槽中,筒体上的焊接底环面由于有一个悬空的面,焊枪打火时与梯形槽底部形成小熔池,焊接热量不会传到出去,集中在筒体上底环面的这个悬空的换面上,热量不流失,使得这个悬空的环面能达到完全融化,与封盖熔焊在一起,使筒体横向部位融化焊牢,达到焊接部位的厚度要求,达到密封要求。
当然,上述说明并非是对本发明的限制,本发明也并不限于上述举例,本技术领域的普通技术人员,在本发明的实质范围内,作出的变化、改型、添加或替换,都应属于本发明本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。

Claims (1)

1.一种环缝焊接方法,其特征在于:首先将封盖与筒体插接接触部位加工刺挠过程在封盖上与筒体插接接触环面上的止口部位外圈是一圈和垂直径行面呈32.5度的斜坡环面,在32.5度的径向斜坡环面和轴向圆柱面详解的轴向圆柱面根部是一圈宽1.5毫米,深0.5毫米的凹环,筒体与插入的封盖的下沿最底部是一圈厚0.3毫米,款0.5毫米的底环边,紧靠底环边封盖的下沿是一圈和垂直径向面呈32.5度的斜坡环面,再在梯形部位进行焊接。
CN201410330853.1A 2014-07-14 2014-07-14 环缝焊接工艺 Pending CN105252123A (zh)