CN105199609A - Leather care agent and preparation method thereof - Google Patents

Leather care agent and preparation method thereof Download PDF

Info

Publication number
CN105199609A
CN105199609A CN201510648837.1A CN201510648837A CN105199609A CN 105199609 A CN105199609 A CN 105199609A CN 201510648837 A CN201510648837 A CN 201510648837A CN 105199609 A CN105199609 A CN 105199609A
Authority
CN
China
Prior art keywords
tank body
parts
care products
leather
agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510648837.1A
Other languages
Chinese (zh)
Inventor
夏穆兰
宋铜山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hubei Mulan Tongda Technology Co Ltd
Original Assignee
Hubei Mulan Tongda Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hubei Mulan Tongda Technology Co Ltd filed Critical Hubei Mulan Tongda Technology Co Ltd
Priority to CN201510648837.1A priority Critical patent/CN105199609A/en
Publication of CN105199609A publication Critical patent/CN105199609A/en
Pending legal-status Critical Current

Abstract

The invention provides a leather care agent which is prepared from the following raw materials in parts by weight: 100 parts of deionized water, 0.1-2 parts of brightening agent, 1-10 parts of glazing agent, 5-20 parts of lustering agent, 0.1-0.5 part of Germall, 0.1-0.5 part of rose essence and 1-5 parts of ethanol. The invention also provides a preparation method of the leather care agent. The leather care agent provided by the invention can soften the leather and enhance the luster and aesthetic feeling of the leather. Abundant grease is supplemented to the leather, thereby reducing the care frequency.

Description

Leather care products and preparation method thereof
Technical field
The present invention relates to leather care products field.More particularly, the present invention relates to leather care products and preparation method thereof.
Background technology
Along with people's living standard is more and more higher, leatherware enters in daily life gradually, and the leathercrafts such as leather shoes, fur clothing, suitcase become popular consumer goods.But along with the increase of duration of service, the grease of leather inside volatilizees or is destroyed, and leatherware can be hardening, and feel is deteriorated, and tarnishes, thus affects attractive in appearance.But more existing leather care products are too pursued and allowed leather brighten and glazing, have ignored and supplement grease to leather, thus make some leather products bright and new beautiful on the surface, in fact poor air permeability, has a strong impact on Consumer's Experience.Therefore, the leather care products that design is a kind of novelly, fully can supplement grease to leather is needed badly.
Summary of the invention
A further object of the invention is to provide a kind of leather care products, and it can soften leather, make leather again become glossy and aesthetic feeling, and owing to supplementing a large amount of grease to leather, decreases nursing frequency.
A further object of the invention is the preparation method by leather care products, improves the utilization ratio of raw material, improves solid particulate and organic dissolution degree, enables leather care products reach preferably result of use, and long quality-guarantee period, not easily layering.
In order to realize, according to these objects of the present invention and other advantage, providing a kind of leather care products, comprise the raw material of following parts by weight:
Deionized water 100 parts, brightener 0.1-2 part, lustering agent 1-10 part, light agent 5-20 part, outstanding horse 0.1-0.5 part, rose compound 0.1-0.5 part and ethanol 1-5 part.
Preferably, described leather care products, is characterized in that, described brightener is Q70 brightener, and described lustering agent is EH lustering agent, and described light agent is the agent of E3982 light.
Preferably, described leather care products, is characterized in that, described brightener is mixed to get with the mass ratio of 4:1 by triglyceride oleate and stearyl single ethanol amide;
Described lustering agent is mixed to get with the mass ratio of 1:1 by white oil and palm wax;
Described light agent is dimethyl silicone oil.
Preferably, described leather care products, is characterized in that, also comprises the raw material of following parts by weight:
Tallow amine Soxylat A 25-7 5-6 part, rapeseed oil 3-7 part, sapn 5-6 part, polyoxyethylene octadecanol base trimethyl ammonium chloride 1-4 part, polyoxyethylene glycerol fatty acid esters 2-5 part, palmityl alcohol 1-2 part, lard 0.5-1 part, calcium carbonate 0.4-0.5 part, tripoly phosphate sodium STPP 2-5 part and Xylo-Mucine 3-5 part.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 35-45 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 25-35 minute;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, join in reactor by the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid, stir 10-20 minute, the mixed solution obtained, with 240-500 object strainer filtering, obtains leather care products.
Preferably, the preparation method of described leather care products, in described step 3, also comprise: stirring in the process of 10-20 minute, add the tallow amine Soxylat A 25-7 of above-mentioned weight part, rapeseed oil, sapn, polyoxyethylene octadecanol base trimethyl ammonium chloride, polyoxyethylene glycerol fatty acid esters, palmityl alcohol, lard, calcium carbonate, tripoly phosphate sodium STPP and Xylo-Mucine.
Preferably, the preparation method of described leather care products, in described step 3, before 240-500 object strainer filtering, also comprises:
Mixed solution is divided into equiponderant two parts, and with special device process 30-45 minute;
Described special device comprises the first tank body and the second tank body, described first tank body is used for a mixed solution of splendid attire, described second tank body is used for splendid attire another portion of mixed solution, described first tank body is cylindrical-shaped structure, the outer wall of described first tank body is arranged with multiple annular permanent magnnet, described second tank body is also cylindrical-shaped structure, described second tank wall is provided with a ultrasonic generator, described first tank body is communicated with by the first tubing with described second tank body, described first tubing is provided with the first recycle pump, for the mixed solution in described first tank body is pumped into described second tank body, described first tank body is also communicated with by the second tubing with described second tank body, described second tubing is provided with the second recycle pump, for the mixed solution in described second tank body is pumped into described first tank body,
Wherein, in the process with special device process mixed solution, described first recycle pump, described second recycle pump and described ultrasonic generator are all opened, the amount of infusion of described first recycle pump is 1:2 with the ratio of the amount of infusion of described second recycle pump, and described ultrasonic generator is 20MHz to the ultrasonic frequency of the second tank body internal irradiation.
The present invention at least comprises following beneficial effect:
(1) leather care products of the present invention can soften leather, make leather again become glossy and aesthetic feeling, and owing to supplementing a large amount of grease to leather, also shortens care cycle.
(2) add in raw material of the present invention and have calcium carbonate powders, utilize calcium carbonate powders to rub on the one hand and open the space of leather surface, the permeability of very big increase leather, and allow rapeseed oil and lard molecule can fully enter leather inside, for leather supplements sufficient grease, thus raising nursing efficacy, leather can be allowed close to the state before use; Calcium carbonate powders remains in the irregularity degree that leather surface can increase leather surface on the other hand, thus makes liquid nursing agent fully can be attached to leather surface, increases nursing agent to the action time of leather, improves nursing efficacy further.In addition, because nursing can supplement sufficient grease each time, after nursing, grease can keep for a long time so each time, which reduces nursing frequency.Wherein, the amount of the calcium carbonate added in every 100 parts of water is 0.4-0.5 part, and under this content, calcium carbonate is to the action time of leather care products and nursing efficacy the best, and when the amount of calcium carbonate is more than 0.5 part, calcium carbonate powders free settling, causes leather care products to lose efficacy.
(3) in the preparation method of leather care products of the present invention, employ a kind of special device and process mixed solution, this special device comprises the equal tank body of two size shape, the mixed solution of two tank body splendid attire equivalent.The outside surface of the first tank body is arranged with multiple annular permanent magnnet, can magnetize water, magnetized glassware for drinking water has higher solubleness, the dissolution degree to all the other compositions in raw material can be strengthened, second tank body outside surface is provided with ultrasonic generator, can carry out ultrasonic to mixed solution, ultrasonic wave can cause the particle violent oscillatory motion in mixed solution can strengthen the movement degree of each raw particles, increases the dissolution degree of raw material in water further.In the present invention, allow mixed solution in the first tank body flow to the second tank body, also allow the mixed solution in the second tank body flow into the first tank body simultaneously, magnetization and ultrasonication fully can be combined like this, greatly add the dissolution degree of raw particles in water.Wherein, first tank body is 1:2 to the flow of the second tank body and the second tank body to the preferred ratio of flow of the first tank body, treatment effect is best, the nursing efficacy of the leather care products obtained is best, when ratio is greater than 1:2, the time of ultrasonication increases, and ultrasonic wave can destroy the structure of raw molecule, thus reduces the quality of leather care products.
Part is embodied by explanation below by other advantage of the present invention, target and feature, part also will by research and practice of the present invention by those skilled in the art is understood.
Accompanying drawing explanation
Fig. 1 is the structural representation of special device of the present invention.
Embodiment
Below in conjunction with accompanying drawing, the present invention is described in further detail, can implement according to this with reference to specification sheets word to make those skilled in the art.
Should be appreciated that used hereinly such as " to have ", other element one or more do not allotted in " comprising " and " comprising " term or the existence of its combination or interpolation.
< example 1>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, Q70 brightener 0.1 part, EH lustering agent 1 part, E3982 light agent 5 parts, outstanding horse 0.1 part, rose compound 0.1 part and ethanol 1 part.
Q70 brightener
Brand: EVONIK-DEGUSSA/ Germany wins wound Degussa-Gao Shi meter Te
Product grade: TEGOPolishAdditivQ70
Name of product: remarkable oven dry/clean and modified form brightener
Product performance: TEGOPolishAdditivQ70 is the oven dry, clean that can be used for automobile, not containing petroleum distillate, and high enrichment, easy to operate, there is after process modified form ripple line marginal zone and have hydrophobic interaction, good antistatic and antiredeposition.TEGOPolishAdditvQ70 is that one comprises the organosilyl mixture of long chain active.TEGOPolishAdditivQ70 is highly enriched, and be highly susceptible to dilution, viscosity is low, easy to operate, has modified form ripple line marginal zone and have hydrophobic interaction, good antistatic and antiredeposition after process.
EH lustering agent
Brand: EVONIK-DEGUSSA/ Germany wins wound Degussa-Gao Shi meter Te
Product grade: TEGOPolishAdditivEH
Name of product: oil-in-water type emulsion silicone oil
Product performance: polishAdditivEH is silicone oil glazing emulsion, easy to use, has good compatibility in nonionic, positively charged ion, anion systems, soluble in water, improves wiping effect, excellent glossiness, waterproof. polishAdditivEH is non-ionic type silicone oil emulsion, almost can with all kinds of additives and emulsion mutually composite.The silicone oil emulsion of this type of oil-in-water-type is highly stable, and used water is diluted with arbitrary proportion substantially. polishAdditivEH contains the very high silicone oil of viscosity, therefore can be considered as " wax component " in shoe polish, substitute solid wax.Two or more silicone oil emulsion mixture can be used to make lustering agent produce the color of glossy, different levels in various degree and water resistance not of uniform size.
The agent of E3982 light
Brand: EVONIK-DEGUSSA/ Germany wins wound Degussa-Gao Shi meter Te
Product grade: TEGOPolishAdditivE3982
Name of product: oil-in-water type emulsion silicone oil
Product performance: TEGOPolishAdditivE3982 is that wind erosion prevention exposes the light agent emulsion with sanitising agent to the open air, concentrated type plastics light agent emulsion, dilutable water, good rigid surface avidity. the active substance of PolishAdditivE3982 emulsion is crosslinked silicone oil. polishAdditivE3982 is the agent of efficient plastics light, and the surface luster after process is splendid, and color as newly, and waterproofly to wash with the several of scavenging solution. still have enough effect after PolishAdditivE3982 dilution, the chance that the surface that processed is again dirty can be greatly reduced.Be added into after in light agent, the upper optical property of light agent, anti-sanitising agent performance and color renovation performance can be improved. polishAdditivE3982 is applicable to various frosting: all plastic components comprising automobile, as collision bumper, dashboard and plastics ceiling etc.Also be specially adapted to through exposing to wind and rain, the renovation of the plastic article (as camping items) of burnt hair and the garden furniture that becomes with the blocking of good fortune rice etc. and maintenance etc.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 35 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 25 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 10 minutes, the mixed solution obtained, with 240 object strainer filterings, obtain leather care products.
< example 2>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, Q70 brightener 1 part, EH lustering agent 5 parts, E3982 light agent 10 parts, outstanding horse 0.3 part, rose compound 0.3 part and ethanol 3 parts.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 40 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 30 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 15 minutes, the mixed solution obtained, with 300 object strainer filterings, obtain leather care products.
< example 3>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, Q70 brightener 2 parts, EH lustering agent 10 parts, E3982 light agent 20 parts, outstanding horse 0.5 part, rose compound 0.5 part and ethanol 5 parts.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 45 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 35 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 20 minutes, the mixed solution obtained, with 500 object strainer filterings, obtain leather care products.
< example 4>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, brightener 0.1 part, lustering agent 1 part, light agent 5 parts, outstanding horse 0.1 part, rose compound 0.1 part and ethanol 1 part.
Described brightener is mixed to get with the mass ratio of 4:1 by triglyceride oleate and stearyl single ethanol amide;
Described lustering agent is mixed to get with the mass ratio of 1:1 by white oil and palm wax;
Described light agent is dimethyl silicone oil.
Described leather care products, is characterized in that, also comprises the raw material of following parts by weight:
Tallow amine Soxylat A 25-7 5 parts, rapeseed oil 3 parts, sapn 5 parts, polyoxyethylene octadecanol base trimethyl ammonium chloride 1 part, polyoxyethylene glycerol fatty acid esters 2 parts, palmityl alcohol 1 part, lard 0.5 part, 0.4 part, calcium carbonate, tripoly phosphate sodium STPP 2 parts and Xylo-Mucine 3 parts.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 35 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 25 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 10 minutes, the mixed solution obtained, with 240 object strainer filterings, obtain leather care products.
The preparation method of described leather care products, in described step 3, also comprise: in the stirring process of 10 minutes, add the tallow amine Soxylat A 25-7 of above-mentioned weight part, rapeseed oil, sapn, polyoxyethylene octadecanol base trimethyl ammonium chloride, polyoxyethylene glycerol fatty acid esters, palmityl alcohol, lard, calcium carbonate, tripoly phosphate sodium STPP and Xylo-Mucine.
The preparation method of described leather care products, in described step 3, before 240 object strainer filterings, also comprises:
Mixed solution is divided into equiponderant two parts, and with special device process 30 minutes;
As shown in Figure 1, described special device comprises the first tank body 1 and the second tank body 2, described first tank body 1 is for a mixed solution of splendid attire, described second tank body 2 is for splendid attire another portion of mixed solution, described first tank body 1 is cylindrical-shaped structure, the outer wall of described first tank body 1 is arranged with multiple annular permanent magnnet, described second tank body 2 is also cylindrical-shaped structure, described second tank body 2 outer wall is provided with a ultrasonic generator, described first tank body 1 is communicated with by the first tubing 3 with described second tank body 2, described first tubing 3 is provided with the first recycle pump, for the mixed solution in described first tank body 1 is pumped into described second tank body 2, described first tank body 1 is also communicated with by the second tubing 4 with described second tank body 2, described second tubing 4 is provided with the second recycle pump, for the mixed solution in described second tank body 2 is pumped into described first tank body 1,
Wherein, in the process with special device process mixed solution, described first recycle pump, described second recycle pump and described ultrasonic generator are all opened, the amount of infusion of described first recycle pump is 1:2 with the ratio of the amount of infusion of described second recycle pump, and described ultrasonic generator is 20MHz to the ultrasonic frequency of the second tank body 2 internal irradiation.
< example 5>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, brightener 2 parts, lustering agent 10 parts, light agent 20 parts, outstanding horse 0.5 part, rose compound 0.5 part and ethanol 5 parts.
Described brightener is mixed to get with the mass ratio of 4:1 by triglyceride oleate and stearyl single ethanol amide;
Described lustering agent is mixed to get with the mass ratio of 1:1 by white oil and palm wax;
Described light agent is dimethyl silicone oil.
Described leather care products, is characterized in that, also comprises the raw material of following parts by weight:
Tallow amine Soxylat A 25-7 6 parts, rapeseed oil 7 parts, sapn 6 parts, polyoxyethylene octadecanol base trimethyl ammonium chloride 4 parts, polyoxyethylene glycerol fatty acid esters 5 parts, palmityl alcohol 2 parts, lard 1 part, 0.5 part, calcium carbonate, tripoly phosphate sodium STPP 5 parts and Xylo-Mucine 5 parts.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 45 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 35 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 20 minutes, the mixed solution obtained, with 500 object strainer filterings, obtain leather care products.
The preparation method of described leather care products, in described step 3, also comprise: in the stirring process of 20 minutes, add the tallow amine Soxylat A 25-7 of above-mentioned weight part, rapeseed oil, sapn, polyoxyethylene octadecanol base trimethyl ammonium chloride, polyoxyethylene glycerol fatty acid esters, palmityl alcohol, lard, calcium carbonate, tripoly phosphate sodium STPP and Xylo-Mucine.
The preparation method of described leather care products, in described step 3, before 500 object strainer filterings, also comprises:
Mixed solution is divided into equiponderant two parts, and with special device process 45 minutes;
Described special device comprises the first tank body and the second tank body, described first tank body is used for a mixed solution of splendid attire, described second tank body is used for splendid attire another portion of mixed solution, described first tank body is cylindrical-shaped structure, the outer wall of described first tank body is arranged with multiple annular permanent magnnet, described second tank body is also cylindrical-shaped structure, described second tank wall is provided with a ultrasonic generator, described first tank body is communicated with by the first tubing with described second tank body, described first tubing is provided with the first recycle pump, for the mixed solution in described first tank body is pumped into described second tank body, described first tank body is also communicated with by the second tubing with described second tank body, described second tubing is provided with the second recycle pump, for the mixed solution in described second tank body is pumped into described first tank body,
Wherein, in the process with special device process mixed solution, described first recycle pump, described second recycle pump and described ultrasonic generator are all opened, the amount of infusion of described first recycle pump is 1:2 with the ratio of the amount of infusion of described second recycle pump, and described ultrasonic generator is 20MHz to the ultrasonic frequency of the second tank body internal irradiation.
< example 6>
A kind of leather care products, comprises the raw material of following parts by weight:
Deionized water 100 parts, brightener 1 part, lustering agent 5 parts, light agent 10 parts, outstanding horse 0.3 part, rose compound 0.3 part and ethanol 3 parts.
Described brightener is mixed to get with the mass ratio of 4:1 by triglyceride oleate and stearyl single ethanol amide;
Described lustering agent is mixed to get with the mass ratio of 1:1 by white oil and palm wax;
Described light agent is dimethyl silicone oil.
Described leather care products, is characterized in that, also comprises the raw material of following parts by weight:
Tallow amine Soxylat A 25-7 5 parts, rapeseed oil 5 parts, sapn 5 parts, polyoxyethylene octadecanol base trimethyl ammonium chloride 3 parts, polyoxyethylene glycerol fatty acid esters 4 parts, palmityl alcohol 1 part, lard 0.8 part, 0.4 part, calcium carbonate, tripoly phosphate sodium STPP 3 parts and Xylo-Mucine 4 parts.
A preparation method for leather care products, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 40 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 30 minutes;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid are joined in reactor, stir 15 minutes, the mixed solution obtained, with 300 object strainer filterings, obtain leather care products.
The preparation method of described leather care products, in described step 3, also comprise: in the stirring process of 15 minutes, add the tallow amine Soxylat A 25-7 of above-mentioned weight part, rapeseed oil, sapn, polyoxyethylene octadecanol base trimethyl ammonium chloride, polyoxyethylene glycerol fatty acid esters, palmityl alcohol, lard, calcium carbonate, tripoly phosphate sodium STPP and Xylo-Mucine.
The preparation method of described leather care products, in described step 3, before 300 object strainer filterings, also comprises:
Mixed solution is divided into equiponderant two parts, and with special device process 40 minutes;
Described special device comprises the first tank body and the second tank body, described first tank body is used for a mixed solution of splendid attire, described second tank body is used for splendid attire another portion of mixed solution, described first tank body is cylindrical-shaped structure, the outer wall of described first tank body is arranged with multiple annular permanent magnnet, described second tank body is also cylindrical-shaped structure, described second tank wall is provided with a ultrasonic generator, described first tank body is communicated with by the first tubing with described second tank body, described first tubing is provided with the first recycle pump, for the mixed solution in described first tank body is pumped into described second tank body, described first tank body is also communicated with by the second tubing with described second tank body, described second tubing is provided with the second recycle pump, for the mixed solution in described second tank body is pumped into described first tank body,
Wherein, in the process with special device process mixed solution, described first recycle pump, described second recycle pump and described ultrasonic generator are all opened, the amount of infusion of described first recycle pump is 1:2 with the ratio of the amount of infusion of described second recycle pump, and described ultrasonic generator is 20MHz to the ultrasonic frequency of the second tank body internal irradiation.
In order to effect of the present invention is described, contriver provides comparative experiments as follows:
< comparative example 1>
When choosing raw material, not containing calcium carbonate raw material, identical with example 6 of all the other parameters, technological process is also identical.
< comparative example 2>
When preparing leather care products, process without special device.Identical with example 6 of all the other parameters, technological process is also identical.
The leather having started one piece to harden is divided into 24 pieces, every three pieces of compositions one group, totally eight groups of pieces of leather.Apply to eight groups of pieces of leather the leather care products that example 1, example 2, example 3, example 4, example 5, example 6, comparative example 1 and comparative example 2 obtain respectively, coated weight is identical, process same time.Adopt the flexibility of softness instrument to leather to measure, and estimate permeability.Result is as shown in table 1.
[pliability of the leather of the leather care products process that table 1 obtains through each example and each comparative example and permeability]
Pliability Permeability
Example 1 Soft Good
Example 2 Soft Good
Example 3 Soft Good
Example 4 Very soft Very well
Example 5 Very soft Very well
Example 6 Very soft Very well
Comparative example 1 Firmly Good
Comparative example 2 Harder Good
Can find out from upper table 1, due to containing calcium carbonate in example 6, after the leather care products process leather that it obtains, the pliability of leather and permeability are higher than comparative example 1.And owing to adopting special device process mixed solution in example 6, after the leather care products process leather that it obtains, the pliability of leather and permeability are significantly higher than the situation in comparative example 2.Visible, increase calcium carbonate of the present invention is as raw material and adopt special device process mixed solution, greatly can improve the nursing efficacy of leather care products.
Although embodiment of the present invention are open as above, it is not restricted to listed in specification sheets and embodiment utilization.It can be applied to various applicable the field of the invention completely.For those skilled in the art, can easily realize other amendment.Therefore do not deviating under the universal that claim and equivalency range limit, the present invention is not limited to specific details and illustrates here and the example described.

Claims (7)

1. a leather care products, is characterized in that, comprises the raw material of following parts by weight:
Deionized water 100 parts, brightener 0.1-2 part, lustering agent 1-10 part, light agent 5-20 part, outstanding horse 0.1-0.5 part, rose compound 0.1-0.5 part and ethanol 1-5 part.
2. leather care products as claimed in claim 1, it is characterized in that, described brightener is Q70 brightener, and described lustering agent is EH lustering agent, and described light agent is the agent of E3982 light.
3. leather care products as claimed in claim 1, it is characterized in that, described brightener is mixed to get with the mass ratio of 4:1 by triglyceride oleate and stearyl single ethanol amide;
Described lustering agent is mixed to get with the mass ratio of 1:1 by white oil and palm wax;
Described light agent is dimethyl silicone oil.
4. leather care products as claimed in claim 1, is characterized in that, also comprise the raw material of following parts by weight:
Tallow amine Soxylat A 25-7 5-6 part, rapeseed oil 3-7 part, sapn 5-6 part, polyoxyethylene octadecanol base trimethyl ammonium chloride 1-4 part, polyoxyethylene glycerol fatty acid esters 2-5 part, palmityl alcohol 1-2 part, lard 0.5-1 part, calcium carbonate 0.4-0.5 part, tripoly phosphate sodium STPP 2-5 part and Xylo-Mucine 3-5 part.
5. a preparation method for the leather care products as described in as arbitrary in claim 1-4, is characterized in that, comprising:
Step one, the deionized water of 90 weight parts is put into reactor, be heated to 35-45 DEG C, open and stir, then add the brightener of above-mentioned weight part, lustering agent and light agent, stir 25-35 minute;
Step 2, by the remaining 10 parts of deionized water dissolvings of the outstanding horse of above-mentioned weight part, get Jie Ma solution, and the rose compound of above-mentioned weight part and ethanol being mixed, obtains Muscat Hamburg seminal fluid;
Step 3, join in reactor by the outstanding horse solution in step 2 and Muscat Hamburg seminal fluid, stir 10-20 minute, the mixed solution obtained, with 240-500 object strainer filtering, obtains leather care products.
6. the preparation method of leather care products as claimed in claim 5, it is characterized in that, in described step 3, also comprise: stirring in the process of 10-20 minute, add the tallow amine Soxylat A 25-7 of above-mentioned weight part, rapeseed oil, sapn, polyoxyethylene octadecanol base trimethyl ammonium chloride, polyoxyethylene glycerol fatty acid esters, palmityl alcohol, lard, calcium carbonate, tripoly phosphate sodium STPP and Xylo-Mucine.
7. the preparation method of leather care products as claimed in claim 6, is characterized in that, in described step 3, before 240-500 object strainer filtering, also comprise:
Mixed solution is divided into equiponderant two parts, and with special device process 30-45 minute;
Described special device comprises the first tank body and the second tank body, described first tank body is used for a mixed solution of splendid attire, described second tank body is used for splendid attire another portion of mixed solution, described first tank body is cylindrical-shaped structure, the outer wall of described first tank body is arranged with multiple annular permanent magnnet, described second tank body is also cylindrical-shaped structure, described second tank wall is provided with a ultrasonic generator, described first tank body is communicated with by the first tubing with described second tank body, described first tubing is provided with the first recycle pump, for the mixed solution in described first tank body is pumped into described second tank body, described first tank body is also communicated with by the second tubing with described second tank body, described second tubing is provided with the second recycle pump, for the mixed solution in described second tank body is pumped into described first tank body,
Wherein, in the process with special device process mixed solution, described first recycle pump, described second recycle pump and described ultrasonic generator are all opened, the amount of infusion of described first recycle pump is 1:2 with the ratio of the amount of infusion of described second recycle pump, and described ultrasonic generator is 20MHz to the ultrasonic frequency of the second tank body internal irradiation.
CN201510648837.1A 2015-10-09 2015-10-09 Leather care agent and preparation method thereof Pending CN105199609A (en)