CN105199269A - 一种用于封隔器的橡胶制品 - Google Patents
一种用于封隔器的橡胶制品 Download PDFInfo
- Publication number
- CN105199269A CN105199269A CN201410264607.0A CN201410264607A CN105199269A CN 105199269 A CN105199269 A CN 105199269A CN 201410264607 A CN201410264607 A CN 201410264607A CN 105199269 A CN105199269 A CN 105199269A
- Authority
- CN
- China
- Prior art keywords
- parts
- rubber product
- packer
- pkr
- resistance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供一种用于石油钻采中封隔器的橡胶制品,属于橡胶制品领域。为了解决目前的封隔器耐油、耐高温、耐高压程度差,易老化,需要不断进行更换,增加了劳动量,降低了工作效率等问题,本发明提供一种用于封隔器的橡胶制品,其配方为:23型氟橡胶140~180份;白炭黑5~20份;云母粉40~50份;细粒子碳酸钙20~40份;氧化锌5~25份;氧化镁4份;脂肪酸甘油酯5~10份;促进剂DM5~10份;防老剂NBC1~5份;硫化剂BP5~20份;环氧类增塑剂5~10份。利用本发明提供的配方,制得的橡胶制品可耐250℃的高温,可耐60MPa的压力,并且具有优异的耐油、耐老化性能,可广泛用于石油钻采中连续油管的封隔器使用。
Description
技术领域
本发明属于橡胶制品领域,具体涉及一种用于石油钻采中封隔器的橡胶制品。
背景技术
连续油管是相对于常规单根螺纹连接油管而言的,又称为挠性油管、蛇形管或盘管,是一种缠绕在卷筒上、可以连续下入或起出的无螺纹连接的长油管口。近年来,连续油管以其高效、经济的特点广泛应用于各种井下作业,其中包括喷砂射孔压裂工艺。国外应用于连续油管喷砂射孔压裂作业的井下工具按封隔形式分为砂塞封隔、可钻桥塞封隔和封隔器封隔3种。完成喷砂射孔作业后砂塞封隔需要第2趟管柱完成冲砂作业,可钻桥塞需要第2趟管柱完成钻塞作业,而封隔器封隔只需解封封隔器便可,因此具有工艺简单、时间成本低、效率高等优点。
封隔器是分层采油及注水过程中必不可少的工具之一,其主要位于套管与油管之间。橡胶封隔器本身属于弹性密封元件,它的具体作用是能够将油井下不同的油层进行分隔,而实现这一作用的器件是封隔器中的密封胶筒。
在钻采过程中,经常会发生封隔器失效的现象,主要原因是胶筒在井下高温高压的作用下,橡胶本身发生老化和撕裂造成的,胶筒的质量好坏直接影响整体密封效果。胶筒是非线性弹性橡胶材料,其力学性能与橡胶材料的配方密切相关,即使相同硬度的橡胶,其压缩或剪切模量也各不相同。
目前的封隔器耐油、耐高温、耐高压程度差,易老化,需要不断进行更换,增加了劳动量,降低了工作效率。
发明内容
为解决上述问题,本发明提供一种耐高温高压、耐老化的封隔器用橡胶制品,采用如下技术方案:
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶140~180份;白炭黑5~20份;云母粉40~50份;细粒子碳酸钙20~40份;氧化锌5~25份;氧化镁4份;脂肪酸甘油酯5~10份;促进剂DM5~10份;防老剂NBC1~5份;硫化剂BP5~20份;环氧类增塑剂5~10份。
本发明的有益效果如下:
1.本发明提供的用于封隔器的橡胶制品,其配方中是以23型氟橡胶为主原料,此橡胶可耐200~250℃的高温,为封隔器的耐高温要求提供保障。
2.本发明提供的用于封隔器的橡胶制品,其配方中包括云母粉和细粒子碳酸钙。云母粉和细粒子碳酸钙可作为半补强填料及增量填料,以增大橡胶体积和质量,达到降低生产成本的目的,同时还可以提高橡胶硬度,改善其耐油性能和工艺性能。可改善混炼加工性能及延长胶料存放时间,使其不易结构化。
3.本发明提供的用于封隔器的橡胶制品,其配方中将氧化锌和氧化镁共用,作为硫化体系,可获得高的硫化程度,改善耐热性能,有利于弹性保持。
4.本发明提供的用于封隔器的橡胶制品,其配方中包括脂肪酸甘油酯,能起氧接受体作用,改善硫化胶耐热性,延长老化诱导期;此配方中还包括聚四氟乙烯,可以提高橡胶制品的抗撕裂性能。
5.本发明提供的用于封隔器的橡胶制品,对原料及其含量的选择,制得的橡胶制品可耐250℃的高温,可耐60MPa的压力,并且具有优异的耐油、耐老化性能,可广泛用于石油钻采中连续油管的封隔器使用。
具体实施方式
下面结合具体实施例对本发明进行详细说明。以下实施例将有助于本领域的技术人员进一步理解本发明,但不以任何形式限制本发明。应当指出的是,对本领域的普通技术人员来说,在不脱离本发明构思的前提下,还可以做出若干变形和改进。这些都属于本发明的保护范围。
实施例1
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶140份;白炭黑20份;云母粉40份;细粒子碳酸钙40份;氧化锌5份;氧化镁4份;脂肪酸甘油酯5份;促进剂DM10份;防老剂NBC1份;硫化剂BP20份;环氧类增塑剂5份。
实施例2
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶150份;白炭黑15份;云母粉42份;细粒子碳酸钙35份;氧化锌10份;氧化镁4份;脂肪酸甘油酯6份;促进剂DM9份;防老剂NBC2份;硫化剂BP18份;环氧类增塑剂6份。
实施例3
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶160份;白炭黑10份;云母粉46份;细粒子碳酸钙30份;氧化锌15份;氧化镁4份;脂肪酸甘油酯8份;促进剂DM8份;防老剂NBC3份;硫化剂BP15份;环氧类增塑剂8份。
实施例4
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶170份;白炭黑12份;云母粉48份;细粒子碳酸钙25份;氧化锌20份;氧化镁4份;脂肪酸甘油酯9份;促进剂DM7份;防老剂NBC4份;硫化剂BP10份;环氧类增塑剂9份。
实施例5
一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶180份;白炭黑5份;云母粉50份;细粒子碳酸钙20份;氧化锌25份;氧化镁4份;脂肪酸甘油酯10份;促进剂DM5份;防老剂NBC5份;硫化剂BP5份;环氧类增塑剂10份。
采用实施例1~5制备而成的橡胶制品,其耐温耐压结果见下表:
项目 | 实施例1 | 实施例2 | 实施例3 | 实施例4 | 实施例5 |
耐温性能(250℃下作用72h) | 未变形 | 未变形 | 未变形 | 未变形 | 未变形 |
耐压性能(60MPa下作用72h) | 未变形 | 未变形 | 未变形 | 未变形 | 未变形 |
Claims (1)
1.一种用于封隔器的橡胶制品,其特征在于,按重量份计,其配方为:23型氟橡胶140~180份;白炭黑5~20份;云母粉40~50份;细粒子碳酸钙20~40份;氧化锌5~25份;氧化镁4份;脂肪酸甘油酯5~10份;促进剂DM5~10份;防老剂NBC1~5份;硫化剂BP5~20份;环氧类增塑剂5~10份。