CN105170874A - 一种高强度型砂 - Google Patents

一种高强度型砂 Download PDF

Info

Publication number
CN105170874A
CN105170874A CN201510522419.8A CN201510522419A CN105170874A CN 105170874 A CN105170874 A CN 105170874A CN 201510522419 A CN201510522419 A CN 201510522419A CN 105170874 A CN105170874 A CN 105170874A
Authority
CN
China
Prior art keywords
parts
molding sand
hour
sand
yellow soil
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201510522419.8A
Other languages
English (en)
Inventor
孙爱琴
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hefei Tenver Precision Casting Co Ltd
Original Assignee
Hefei Tenver Precision Casting Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hefei Tenver Precision Casting Co Ltd filed Critical Hefei Tenver Precision Casting Co Ltd
Priority to CN201510522419.8A priority Critical patent/CN105170874A/zh
Publication of CN105170874A publication Critical patent/CN105170874A/zh
Pending legal-status Critical Current

Abstract

发明公开了一种高强度型砂,由以下成分制成,黄壤土、石英砂、高岭土、蛭石、铝酸钙粉、丙烯酸、膨润土、松脂岩、丙烯酸钠、顺丁烯二酸、氨基苯甲酸、氨己酸;本发明型砂通过对黄壤土与石英砂的煅烧处理,使型砂具有良好的透气性、流动性和韧性,同时结合使用铝酸钙粉一起煅烧,使型砂具有较高的强度和热稳定性,通过添加改性高岭土能够提高型砂的其可塑性、分散性、光滑度、粘结强度,本发明制作的型砂,不仅强度增加,易成型,型砂与铸件界面能够产生一层致密的烧结层,使得铸件剥离更加便捷,铸件表面光洁度极高。

Description

一种高强度型砂
技术领域
本发明涉及型砂制作领域,特别是涉及一种高强度型砂。
背景技术
型砂是在铸造中用来造型的材料。型砂一般由铸造用原砂、型砂粘结剂和辅加物等造型材料按一定的比例混合而成,也可用天然含粘土的硅砂,然而现有的型砂透气性差,容易粘接,导致铸件不易剥离,使得铸件表面粗糙,目前对于铸钢件和铸铁件的性能要求更高,从而要求进一步提升型砂的性能。
发明内容
本发明的目的是提供一种高强度型砂。
本发明通过以下技术方案实现:
一种高强度型砂,按重量份计由以下成分制成,黄壤土35份、石英砂210份、高岭土15份、蛭石5份、铝酸钙粉5份、丙烯酸2份、膨润土10份、松脂岩5份、丙烯酸钠3份、顺丁烯二酸1份、氨基苯甲酸0.7份、氨己酸0.5份;其由以下制作步骤制成:
1)将黄土壤粉碎至0.25-0.4毫米粒径,将黄土壤与丙烯酸钠、顺丁烯二酸均匀混合,放入300-350℃煅烧炉中煅烧1.5-2小时,将石英砂粉碎至0.15-0.3毫米粒径,将石英砂、黄土壤和铝酸钙粉混合均匀后放入450-500℃煅烧炉中煅烧4-5小时,然后取出;
2)将高岭土放入800℃煅烧炉中煅烧1.5-2小时后,然后放入3.5mol/L的盐酸中浸泡1-1.5小时,取出,干燥,磨成粉末,待用;
3)将膨润土研磨成粉末,搅拌到其2倍重量份的清水中,混合均匀后,添加对氨基苯甲酸与氨己酸,将温度调节到60-65℃,反应2-3小时后,干燥,待用;
4)将蛭石加热到300℃后,直接高温下研磨成粉末,再冷却至室温;
5)将松脂岩与1)、2)、3)、4)中物料均匀混合到一起,再添加0.5倍重量份的水,搅拌分散,送入250-300℃煅烧炉中煅烧4-5小时;
6)向5)中物料添加丙烯酸混合,研磨分散25-30分钟;
7)向6)中添加混合料重量1-1.5%的水均匀搅拌8-10分钟,即可。
本发明的有益效果是,与现有技术相比:
通过对黄壤土与石英砂的煅烧处理,使型砂具有良好的透气性、流动性和韧性,结合使用丙烯酸钠与顺丁烯二酸,同时结合使用铝酸钙粉一起煅烧,使型砂具有较高的强度和热稳定性,通过添加改性高岭土能够提高型砂的其可塑性、分散性、光滑度、粘结强度,通过配合蛭石粉,能够进一步提高型砂的强度,提高可塑性,通过添加改性膨润土能够提高型砂的热湿拉强度、湿粘结力,通过采用松脂岩粉末的煅烧调和使得型砂具有优异的防粘砂能力,因此能够适应多种硬化方式,并且能够提高旧型砂的回收利用率。本发明制作的型砂,不仅强度增加,易成型,型砂与铸件界面能够产生一层致密的烧结层,使得铸件剥离更加便捷,铸件表面光洁度极高。
具体实施方式
一种高强度型砂,按重量份计由以下成分制成,黄壤土35份、石英砂210份、高岭土15份、蛭石5份、铝酸钙粉5份、丙烯酸2份、膨润土10份、松脂岩5份、丙烯酸钠3份、顺丁烯二酸1份、氨基苯甲酸0.7份、氨己酸0.5份;其由以下制作步骤制成:
1)将黄土壤粉碎至0.25-0.4毫米粒径,将黄土壤与丙烯酸钠、顺丁烯二酸均匀混合,放入300-350℃煅烧炉中煅烧1.5-2小时,将石英砂粉碎至0.15-0.3毫米粒径,将石英砂、黄土壤和铝酸钙粉混合均匀后放入450-500℃煅烧炉中煅烧4-5小时,然后取出;
2)将高岭土放入800℃煅烧炉中煅烧1.5-2小时后,然后放入3.5mol/L的盐酸中浸泡1-1.5小时,取出,干燥,磨成粉末,待用;
3)将膨润土研磨成粉末,搅拌到其2倍重量份的清水中,混合均匀后,添加对氨基苯甲酸与氨己酸,将温度调节到60-65℃,反应2-3小时后,干燥,待用;
4)将蛭石加热到300℃后,直接高温下研磨成粉末,再冷却至室温;
5)将松脂岩与1)、2)、3)、4)中物料均匀混合到一起,再添加0.5倍重量份的水,搅拌分散,送入250-300℃煅烧炉中煅烧4-5小时;
6)向5)中物料添加丙烯酸混合,研磨分散25-30分钟;
7)向6)中添加混合料重量1-1.5%的水均匀搅拌8-10分钟,即可。
通过测试对比本发明型砂与一般型砂:
湿压强度/MPa 紧实率/% 热湿拉强度/KPa 透气性 破碎指数/%
本发明型砂 0.131 40 448 90
一般型砂 0.114 37 386 67
表1
通过表1可以看出本发明型砂比现有型砂在湿压轻度、紧实率、热湿拉强度、韧性上具有明显的优势。

Claims (1)

1.一种高强度型砂,其特征在于,按重量份计由以下成分制成,黄壤土35份、石英砂210份、高岭土15份、蛭石5份、铝酸钙粉5份、丙烯酸2份、膨润土10份、松脂岩5份、丙烯酸钠3份、顺丁烯二酸1份、氨基苯甲酸0.7份、氨己酸0.5份;其由以下制作步骤制成:
1)将黄土壤粉碎至0.25-0.4毫米粒径,将黄土壤与丙烯酸钠、顺丁烯二酸均匀混合,放入300-350℃煅烧炉中煅烧1.5-2小时,将石英砂粉碎至0.15-0.3毫米粒径,将石英砂、黄土壤和铝酸钙粉混合均匀后放入450-500℃煅烧炉中煅烧4-5小时,然后取出;
2)将高岭土放入800℃煅烧炉中煅烧1.5-2小时后,然后放入3.5mol/L的盐酸中浸泡1-1.5小时,取出,干燥,磨成粉末,待用;
3)将膨润土研磨成粉末,搅拌到其2倍重量份的清水中,混合均匀后,添加对氨基苯甲酸与氨己酸,将温度调节到60-65℃,反应2-3小时后,干燥,待用;
4)将蛭石加热到300℃后,直接高温下研磨成粉末,再冷却至室温;
5)将松脂岩与1)、2)、3)、4)中物料均匀混合到一起,再添加0.5倍重量份的水,搅拌分散,送入250-300℃煅烧炉中煅烧4-5小时;
6)向5)中物料添加丙烯酸混合,研磨分散25-30分钟;
7)向6)中添加混合料重量1-1.5%的水均匀搅拌8-10分钟,即可。
CN201510522419.8A 2015-08-21 2015-08-21 一种高强度型砂 Pending CN105170874A (zh)