CN105153876A - 一种家用防盗门外层耐磨涂料及其制备方法 - Google Patents
一种家用防盗门外层耐磨涂料及其制备方法 Download PDFInfo
- Publication number
- CN105153876A CN105153876A CN201510582721.2A CN201510582721A CN105153876A CN 105153876 A CN105153876 A CN 105153876A CN 201510582721 A CN201510582721 A CN 201510582721A CN 105153876 A CN105153876 A CN 105153876A
- Authority
- CN
- China
- Prior art keywords
- parts
- epoxy resin
- preparation
- wear
- hours
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种家用防盗门外层耐磨涂料及其制备方法,涉及家庭装修材料生产技术领域,其特征在于:由以下重量份的材料制成,双酚S型环氧树脂20份、聚乙烯蜡10份、环氧化聚丁二烯树脂5份、高色素炭黑3份、对羟基苯甲酸对苯二酚二缩水甘油5份、二亚乙基三胺7份、二茂铁4份、环氧大豆油5份、纳米二氧化硅12份。本发明方法合理、配比合理、操作方便、耐磨损。
Description
技术领域:
本发明涉及家庭装修材料生产技术领域,具体涉及一种家用防盗门外层耐磨涂料及其制备方法。
背景技术:
防盗门的全称为“防盗安全门”。它兼备防盗和安全的性能。按照《防盗安全门通用技术条件》规定,合格的防盗门在15分钟内利用凿子、螺丝刀、撬棍等普通手工具和手电钻等便携式电动工具无法撬开或在门扇上开起一个615平方毫米的开口,或在锁定点150平方毫米的半圆内打开一个38平方毫米的开口。并且防盗门上使用的锁具必须是经过公安部检测中心检测合格的带有防钻功能的防盗门专用锁。防盗门可以用不同的材料制作,但只有达到标准检测合格,领取安全防范产品准产证的门才能称为防盗门。
在现今的生活中,防盗门不仅要性能优良,而且它的外观和便于清洁度都是非常重要的,有许多的防盗门时间长久容易掉漆,或者擦碰后就有非常严重的刮痕,这样对于消费者来说也是不能接受的。
发明内容:
本发明所要解决的技术问题在于克服现有的技术缺陷提供一种方法合理、配比合理、操作方便、耐磨损的一种家用防盗门外层耐磨涂料及其制备方法。
本发明所要解决的技术问题采用以下的技术方案来实现:
一种家用防盗门外层耐磨涂料及其制备方法,其特征在于:由以下重量份的材料制成,
双酚S型环氧树脂20份、聚乙烯蜡10份、环氧化聚丁二烯树脂5份、高色素炭黑3份、对羟基苯甲酸对苯二酚二缩水甘油5份、二亚乙基三胺7份、二茂铁4份、环氧大豆油5份、纳米二氧化硅12份;
其制备方法包括,
Ⅰ将双酚S型环氧树脂、环氧化聚丁二烯树脂、对羟基苯甲酸对苯二酚、二茂铁、二缩水甘油放入不锈钢反应釜内升温至240℃,开始搅拌反应,一共反应4个小时;
Ⅱ将聚乙烯蜡、高色素炭黑、二亚乙基三胺、环氧大豆油放入不锈钢反应釜,升温至200℃,开始搅拌反应,一共反应3个小时;
Ⅲ将Ⅱ在Ⅰ工作1个小时之后开始工作,然后在同时完成之后,将Ⅰ与Ⅱ内的材料放入一个新的反应釜中,以45℃/小时的升温搅拌反应4个小时,反应一个小时后加入纳米二氧化硅;
Ⅳ在Ⅲ步骤完成之后,将材料取出,并且震荡混合20分钟,然后通过双螺杆挤出机挤出,温度控制在100℃,然后挤出完成后材料静置10分钟,然后放入粉碎机中研磨粉碎成190-225目的粉末,包装入库。
本发明的有益效果为:涂料有很多种,有悬浊液状态的,有液态的也有颗粒或粉末状态的,颗粒或粉末状态的加工更加的方便并且使用效果更加的良好,而将不同的材料通过反应、震荡、混合等各种步骤来加工,使得产品的性能更加的优良,而材料的使用效率也会提高,这样就使得产品更加的优秀。本发明方法合理、配比合理、操作方便、耐磨损。
具体实施方式:
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面进一步阐述本发明。
一种家用防盗门外层耐磨涂料及其制备方法,其特征在于:由以下重量份的材料制成,
双酚S型环氧树脂20份、聚乙烯蜡10份、环氧化聚丁二烯树脂5份、高色素炭黑3份、对羟基苯甲酸对苯二酚二缩水甘油5份、二亚乙基三胺7份、二茂铁4份、环氧大豆油5份、纳米二氧化硅12份;
其制备方法包括,
Ⅰ将双酚S型环氧树脂、环氧化聚丁二烯树脂、对羟基苯甲酸对苯二酚、二茂铁、二缩水甘油放入不锈钢反应釜内升温至240℃,开始搅拌反应,一共反应4个小时;
Ⅱ将聚乙烯蜡、高色素炭黑、二亚乙基三胺、环氧大豆油放入不锈钢反应釜,升温至200℃,开始搅拌反应,一共反应3个小时;
Ⅲ将Ⅱ在Ⅰ工作1个小时之后开始工作,然后在同时完成之后,将Ⅰ与Ⅱ内的材料放入一个新的反应釜中,以45℃/小时的升温搅拌反应4个小时,反应一个小时后加入纳米二氧化硅;
Ⅳ在Ⅲ步骤完成之后,将材料取出,并且震荡混合20分钟,然后通过双螺杆挤出机挤出,温度控制在100℃,然后挤出完成后材料静置10分钟,然后放入粉碎机中研磨粉碎成190-225目的粉末,包装入库。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (1)
1.一种家用防盗门外层耐磨涂料及其制备方法,其特征在于:由以下重量份的材料制成,
双酚S型环氧树脂20份、聚乙烯蜡10份、环氧化聚丁二烯树脂5份、高色素炭黑3份、对羟基苯甲酸对苯二酚二缩水甘油5份、二亚乙基三胺7份、二茂铁4份、环氧大豆油5份、纳米二氧化硅12份;
其制备方法包括,
Ⅰ将双酚S型环氧树脂、环氧化聚丁二烯树脂、对羟基苯甲酸对苯二酚、二茂铁、二缩水甘油放入不锈钢反应釜内升温至240℃,开始搅拌反应,一共反应4个小时;
Ⅱ将聚乙烯蜡、高色素炭黑、二亚乙基三胺、环氧大豆油放入不锈钢反应釜,升温至200℃,开始搅拌反应,一共反应3个小时;
Ⅲ将Ⅱ在Ⅰ工作1个小时之后开始工作,然后在同时完成之后,将Ⅰ与Ⅱ内的材料放入一个新的反应釜中,以45℃/小时的升温搅拌反应4个小时,反应一个小时后加入纳米二氧化硅;
Ⅳ在Ⅲ步骤完成之后,将材料取出,并且震荡混合20分钟,然后通过双螺杆挤出机挤出,温度控制在100℃,然后挤出完成后材料静置10分钟,然后放入粉碎机中研磨粉碎成190-225目的粉末,包装入库。