CN105153593A - 配电箱用高强度彩色塑料外壳 - Google Patents
配电箱用高强度彩色塑料外壳 Download PDFInfo
- Publication number
- CN105153593A CN105153593A CN201510618014.4A CN201510618014A CN105153593A CN 105153593 A CN105153593 A CN 105153593A CN 201510618014 A CN201510618014 A CN 201510618014A CN 105153593 A CN105153593 A CN 105153593A
- Authority
- CN
- China
- Prior art keywords
- plastic shell
- silicon carbide
- strength
- shell
- obtains
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种配电箱用高强度彩色塑料外壳,其特征在于,该外壳是由以下质量百分比的组分制成:PVC废料58%、聚氯乙烯糊树脂5%、玻璃粉5%、石墨1%、硅烷偶联剂2%、环氧固化剂1%、抗氧剂2%、环氧树脂5%、增强剂3%、纳米碳化硅2%、表面活性剂1%、蓝晶石粉1%、元明粉0.5%、氧化铁0.5%、纳米钴粉0.5%、碳化硅晶须0.5%、氟硅酸钠2%、钛白粉5%、耐晒大红5%。本发明制备的外壳色彩美观,颜色搭配和谐,整体强度好,质量轻,非常适合现代家庭装修使用。
Description
技术领域
本发明涉及新材料技术领域,具体涉及一种配电箱用高强度彩色塑料外壳。
背景技术
建筑工地、工厂、马路边等场合,配电箱是电力动力环节中不可或缺的设备。家庭、工作室、办公室装修的时候,也经常会使用配电箱。但是,市场上现有的配电箱产品外形单一、不够美观。家庭装修的时候,不得不考虑把配电箱做小、然后放置到隐蔽的地方,由此一来,需要使用的时候极为不便。而且不管多隐蔽,总是或多或少影响到了家庭装修的美观。
发明内容
本发明所要解决的技术问题在于提高一种成型方便,使用寿命长的配电箱用高强度彩色塑料外壳。
本发明所要解决的技术问题采用以下技术方案来实现:
一种配电箱用高强度彩色塑料外壳,该外壳是由以下质量百分比的组分制成:PVC废料58%、聚氯乙烯糊树脂5%、玻璃粉5%、石墨1%、硅烷偶联剂2%、环氧固化剂1%、抗氧剂2%、环氧树脂5%、增强剂3%、纳米碳化硅2%、表面活性剂1%、蓝晶石粉1%、元明粉0.5%、氧化铁0.5%、纳米钴粉0.5%、碳化硅晶须0.5%、氟硅酸钠2%、钛白粉5%、耐晒大红5%。
上述彩色塑料外壳的制备方法如下:
1)按比例称取上述原料,将PVC废料晾晒后粉碎成颗粒,与其它物料一同送入反应釜,混合均匀后将混合原料升温热处理,处理结束后得到混合物;热处理的温度为160-180℃,热处理时间为2-3小时;
2)将步骤1)制备的混合物在送入捏合机中混炼均匀,得到胶料;
3)将步骤2)制备的胶料送入挤出机,通过挤出机将胶料挤入到成型模具中,得到彩色塑料外壳半成品;
4)将步骤3)中的彩色塑料外壳半成品送入硫化设备进行硫化处理,在200℃条件下的烘箱中连续硫化两次,每次2小时,中间间隔6小时,取出得到成品。
本发明的有益效果是:本发明制备的外壳色彩美观,颜色搭配和谐,整体强度好,质量轻,非常适合现代家庭装修使用。
具体实施方式
为了使本发明实现的技术手段、创作特征、达成目的与功效易于明白了解,下面结合具体实施例,进一步阐述本发明。
实施例1
一种配电箱用高强度彩色塑料外壳,该外壳是由以下质量百分比的组分制成:PVC废料58%、聚氯乙烯糊树脂5%、玻璃粉5%、石墨1%、硅烷偶联剂2%、环氧固化剂1%、抗氧剂2%、环氧树脂5%、增强剂3%、纳米碳化硅2%、表面活性剂1%、蓝晶石粉1%、元明粉0.5%、氧化铁0.5%、纳米钴粉0.5%、碳化硅晶须0.5%、氟硅酸钠2%、钛白粉5%、耐晒大红5%。
上述彩色塑料外壳的制备方法如下:
1)按比例称取上述原料,将PVC废料晾晒后粉碎成颗粒,与其它物料一同送入反应釜,混合均匀后将混合原料升温热处理,处理结束后得到混合物;热处理的温度为160-180℃,热处理时间为2-3小时;
2)将步骤1)制备的混合物在送入捏合机中混炼均匀,得到胶料;
3)将步骤2)制备的胶料送入挤出机,通过挤出机将胶料挤入到成型模具中,得到彩色塑料外壳半成品;
4)将步骤3)中的彩色塑料外壳半成品送入硫化设备进行硫化处理,在200℃条件下的烘箱中连续硫化两次,每次2小时,中间间隔6小时,取出得到成品。
实施例2
一种配电箱用高强度彩色塑料外壳,该外壳是由以下质量百分比的组分制成:PVC废料58%、聚氯乙烯糊树脂5%、玻璃粉5%、石墨1%、硅烷偶联剂2%、环氧固化剂1%、抗氧剂2%、环氧树脂5%、增强剂3%、纳米碳化硅2%、表面活性剂1%、蓝晶石粉1%、元明粉0.5%、氧化铁0.5%、纳米钴粉0.5%、碳化硅晶须0.5%、氟硅酸钠2%、钛白粉5%、耐晒大红5%。
上述彩色塑料外壳的制备方法如下:
1)按比例称取上述原料,将PVC废料晾晒后粉碎成颗粒,与其它物料一同送入反应釜,混合均匀后将混合原料升温热处理,处理结束后得到混合物;热处理的温度为160-180℃,热处理时间为2-3小时;
2)将步骤1)制备的混合物在送入捏合机中混炼均匀,得到胶料;
3)将步骤2)制备的胶料送入挤出机,通过挤出机将胶料挤入到成型模具中,得到彩色塑料外壳半成品;
4)将步骤3)中的彩色塑料外壳半成品送入硫化设备进行硫化处理,在200℃条件下的烘箱中连续硫化两次,每次2小时,中间间隔6小时,取出得到成品。
上述抗氧剂是由以下重量的组分制成:抗氧剂101010kg、木糖醇溶液5kg、酵母粉2kg、辣椒素2kg、橄榄油1.5kg、壬二酸2kg、乙酸异戊酯1.5kg、二苯基硅二醇0.5kg。
以上显示和描述了本发明的基本原理和主要特征和本发明的优点。本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明书中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内。本发明要求保护范围由所附的权利要求书及其等效物界定。
Claims (2)
1.一种配电箱用高强度彩色塑料外壳,其特征在于,该外壳是由以下质量百分比的组分制成:PVC废料58%、聚氯乙烯糊树脂5%、玻璃粉5%、石墨1%、硅烷偶联剂2%、环氧固化剂1%、抗氧剂2%、环氧树脂5%、增强剂3%、纳米碳化硅2%、表面活性剂1%、蓝晶石粉1%、元明粉0.5%、氧化铁0.5%、纳米钴粉0.5%、碳化硅晶须0.5%、氟硅酸钠2%、钛白粉5%、耐晒大红5%。
2.一种制备权利要求1所述彩色塑料外壳的方法,其特征在于,步骤如下:
1)按比例称取上述原料,将PVC废料晾晒后粉碎成颗粒,与其它物料一同送入反应釜,混合均匀后将混合原料升温热处理,处理结束后得到混合物;热处理的温度为160-180℃,热处理时间为2-3小时;
2)将步骤1)制备的混合物在送入捏合机中混炼均匀,得到胶料;
3)将步骤2)制备的胶料送入挤出机,通过挤出机将胶料挤入到成型模具中,得到彩色塑料外壳半成品;
4)将步骤3)中的彩色塑料外壳半成品送入硫化设备进行硫化处理,在200℃条件下的烘箱中连续硫化两次,每次2小时,中间间隔6小时,取出得到成品。