CN104695491A - 一种不合格预制柱基础杯口的加固方法及结构 - Google Patents

一种不合格预制柱基础杯口的加固方法及结构 Download PDF

Info

Publication number
CN104695491A
CN104695491A CN201310640431.XA CN201310640431A CN104695491A CN 104695491 A CN104695491 A CN 104695491A CN 201310640431 A CN201310640431 A CN 201310640431A CN 104695491 A CN104695491 A CN 104695491A
Authority
CN
China
Prior art keywords
bar planting
column foundation
unqualified
precast column
defective
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310640431.XA
Other languages
English (en)
Inventor
涂远
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Original Assignee
Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Guiyang Aluminum Magnesium Design and Research Institute Co Ltd filed Critical Guiyang Aluminum Magnesium Design and Research Institute Co Ltd
Priority to CN201310640431.XA priority Critical patent/CN104695491A/zh
Publication of CN104695491A publication Critical patent/CN104695491A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种不合格预制柱基础杯口的加固方法及结构。该方法是先将不合格预制柱基础台阶顶凿毛,后采用植筋的方式沿不合格预制柱基础台阶顶部在已浇注的杯口周边将植筋按一定间距植入不合格预制柱基础台阶顶部,植筋的植入深度一般不小于20倍植筋直径,植筋的外露长度为不合格预制柱基础杯口高度h减去植筋保护层。在h范围内加设箍筋,箍筋间距采用50~100mm。箍筋绑扎完毕后,采用高于不合格预制柱基础混凝土标号一级的细石混凝土将加固混凝土浇筑完毕即可。本发明通过在预制柱基础台阶顶部植入钢筋,同时在预制柱基础加厚范围内加设箍筋的方式,使得预制柱基础杯口加厚部分满足规范及设计要求。这对于预制柱的安全稳定有重要意义。

Description

一种不合格预制柱基础杯口的加固方法及结构
技术领域
本发明涉及一种不合格预制柱基础杯口的加固方法及结构,属于不合格预制柱基础杯口的修正技术领域。
背景技术
在建筑施工过程中,有时会因施工失误将不合格预制柱基础杯口浇偏,从而导致杯口某一边厚度达不到设计要求。如果不及时对这些不合格的不合格预制柱基础杯口进行修正,继续使用这些不合格预制柱基础杯口将会影响整个建筑工程的稳定性及安全性。因此必须要对这些不合格的须不合格预制柱基础杯口进行修正加固,以确保整体结构的稳定性及安全性。
发明内容
本发明的目的在于,提供一种不合格预制柱基础杯口的加固方法及结构,以确保整体结构的稳定性及安全性。。
本发明的技术方案:
一种不合格预制柱基础杯口的加固方法,其特征在于:该方法是先将不合格预制柱基础台阶顶凿毛,后采用植筋的方式沿不合格预制柱基础台阶顶部在已浇注的杯口周边将植筋按一定间距植入不合格预制柱基础台阶顶部,植筋的植入深度一般不小于20倍植筋直径d,植筋的外露长度为不合格预制柱基础杯口高度h减去植筋保护层。在h范围内加设箍筋,箍筋间距采用50~100mm。箍筋绑扎完毕后,采用高于不合格预制柱基础混凝土标号一级的细石混凝土将加固混凝土浇筑完毕即可。
根据前述方法构成的预制柱基础杯口加固结构,包括现有的不合格预制柱基础;其特征在于:在不合格预制柱基础顶部边缘设有一圈植筋,植筋外设有一组箍筋,植筋和箍筋外浇筑有加固混凝土。
前述加固结构中,所述植筋植入不合格预制柱基础内20倍植筋直径d。
前述加固结构中,所述一组箍筋沿着植筋外露部分按50~100mm间距均布。
前述加固结构中,所述加固混凝土为不合格预制柱基础所用混凝土标号高一级的细石混凝土。
与现有技术相比,本发明通过在预制柱基础台阶顶部植入钢筋,同时在预制柱基础加厚范围内加设箍筋的方式,使得预制柱基础杯口加厚部分满足规范及设计要求。这对于预制柱的安全稳定有重要意义。
附图说明
图1是本发明的结构示意图;
图2是图1的俯视图。
附图中的标记为:1-不合格预制柱基础,2-植筋,3-箍筋,4-加固混凝土。
具体实施方式
下面结合附图对本发明作进一步的详细说明,但不作为对本发明的任何限制。
一种不合格预制柱基础杯口的加固方法,如图1和图2所示。该方法是先将不合格预制柱基础1台阶顶凿毛,后采用植筋的方式沿不合格预制柱基础台阶顶部在已浇注的杯口周边将植筋2按一定间距植入不合格预制柱基础台阶1顶部,植筋2的植入深度一般不小于20倍植筋直径d,植筋2的外露长度为不合格预制柱基础杯口高度h减去植筋保护层。在h范围内加设箍筋3,箍筋3间距采用50~100mm。箍筋3绑扎完毕后,采用高于不合格预制柱基础1混凝土标号一级的细石混凝土将加固混凝土4浇筑完毕即可。
根据前述方法构成的不合格预制柱基础杯口加固结构,如图1和图2所示。包括现有的不合格预制柱基础1;在不合格预制柱基础1顶部边缘设有一圈植筋2,植筋2外设有一组箍筋3,植筋2和箍筋3外浇筑有加固混凝土4。植筋2植入不合格预制柱基础1内20倍植筋直径d。一组箍筋3沿着植筋2外露部分按50~100mm间距均布。加固混凝土4为不合格预制柱基础1所用混凝土标号高一级的细石混凝土。

Claims (5)

1. 一种不合格预制柱基础杯口的加固方法,其特征在于:该方法是先将不合格预制柱基础台阶顶凿毛,后采用植筋的方式沿不合格预制柱基础台阶顶部在已浇注的杯口周边将植筋按一定间距植入不合格预制柱基础台阶顶部,植筋的植入深度一般不小于20倍植筋直径d,植筋的外露长度为不合格预制柱基础杯口高度h减去植筋保护层;
在h范围内加设箍筋,箍筋间距采用50~100mm;
箍筋绑扎完毕后,采用高于不合格预制柱基础混凝土标号一级的细石混凝土将加厚部分浇筑完毕即可。
2.一种根据权利要求1所述方法构成的不合格预制柱基础杯口加固结构,包括现有的不合格预制柱基础(1);其特征在于:在不合格预制柱基础(1)顶部边缘设有一圈植筋(2),植筋(2)外设有一组箍筋(3),植筋(2)和箍筋(3)外浇筑有加固混凝土(4)。
3.根据权利要求2所述加固结构,其特征在于:所述植筋(2)植入不合格预制柱基础(1)内20倍植筋直径d。
4.根据权利要求2所述加固结构,其特征在于:所述一组箍筋(3)沿着植筋(2)外露部分按50~100mm间距均布。
5.根据权利要求2所述加固结构,其特征在于:所述加固混凝土(4)为不合格预制柱基础(1)所用混凝土标号高一级的细石混凝土。
CN201310640431.XA 2013-12-04 2013-12-04 一种不合格预制柱基础杯口的加固方法及结构 Pending CN104695491A (zh)