CN104681792A - 一种铅蓄电池负极板添加剂 - Google Patents

一种铅蓄电池负极板添加剂 Download PDF

Info

Publication number
CN104681792A
CN104681792A CN201310634955.8A CN201310634955A CN104681792A CN 104681792 A CN104681792 A CN 104681792A CN 201310634955 A CN201310634955 A CN 201310634955A CN 104681792 A CN104681792 A CN 104681792A
Authority
CN
China
Prior art keywords
carbon
additive
lead storage
negative plate
storage battery
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310634955.8A
Other languages
English (en)
Inventor
张�浩
张文峰
曹高萍
杨裕生
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
63971 Troops of PLA
Original Assignee
63971 Troops of PLA
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 63971 Troops of PLA filed Critical 63971 Troops of PLA
Priority to CN201310634955.8A priority Critical patent/CN104681792A/zh
Publication of CN104681792A publication Critical patent/CN104681792A/zh
Pending legal-status Critical Current

Abstract

本发明为一种铅蓄电池负极板添加剂,该该添加剂为活性炭、炭黑、石墨烯、碳纳米管、炭纤维、炭气凝胶、模板炭、介孔炭、碳化物衍生炭、聚苯胺、聚吡咯、聚噻吩、聚烷基噻吩、聚对氟苯基噻吩或抑制析氢添加剂,该添加剂可使得铅蓄电池具有优良的脉冲循环寿命,能提高铅蓄电池的充电接受能力,用于电动车、储能、电动工具、脉冲发射等领域的铅蓄电池。

Description

一种铅蓄电池负极板添加剂
技术领域
本发明涉及一种铅蓄电池负极板添加剂,属于化学工程领域。
背景技术
能源是人类社会生存发展的基础,从天然矿藏能源到电能的利用代表了科技发展的历程。近代,特别是上一世纪人类社会的飞速发展,使得人类资源消耗量急剧增加,致使以石油为主的传统化石能源日趋紧张,且造成大气污染越发严重,寻求可持续发展的途径、保护自然资源和自然环境成为21世纪的严重挑战。电能已经成为人类社会不可或缺的一种洁净的能源,任何其它资源利用一般都必须使用电能,电能的储存、转化、输送都用到电池/电容技术。
电动汽车(包括纯电动车和混合电动车HEV)无污染、使用成本低且有望调谐电网系统夜间的谷电,成为目前的研究热点和未来交通工具的发展趋势。铅蓄电池因其原料资源丰富、价格低廉、制备、维护工艺成熟和安全性好等特点,在电动车上有较好的应用前景,但目前其比功率低、循环寿命短的缺点制约了其在电动车上的应用。超级电容器(Supercapacitors)是性能介于传统电容器和电池之间的一种新型储能装置,其比能量是传统电容器的20~200倍,比功率一般大于1000W/kg,高于一般二次电池,循环寿命(>105次)也优于电池,还具有能瞬间大电流充放电、工作温度范围宽、安全、无污染等优点,因而具有在电动汽车上的潜在应用前景。但是,迄今为止,电化学电容器的比能量还是低于二次电池,制约了其在电动车上的应用。
铅蓄电池的比功率较低以及大功率放电下寿命差,主要是受限于负极:在高密度电流放电情况下,负极产生大量铅离子进入电解液,与之相对的情况是电解液中硫酸根离子扩散受限,致使铅离子过饱和,容易在负极表面形成一层致密的硫酸铅沉淀层,造成负极表面钝化。硫酸铅导电性差,溶解度小,会降低负极内部铅的反应活性,增加反应过电位,致使充电时析氢较为严重,充电效率下降,并形成恶性循环。若继续大功率充放电,以上情况会进一步恶化,硫酸铅沉淀颗粒增大且过程不可逆,最终负极丧失反应活性,电池失效(参见J.PowerSources133(2004)126)。若能通过外电路的控制,避免铅蓄电池大功率充放电,能有效提高其寿命。中国专利200620097371.7公开了一种电池,其在传统的电池外并联了一个耐高功率充放电的电容器,通过一个外壳将电池和电容固定,构成一种电池-电容组合。该类电池-电容组合虽然将铅蓄电池和超级电容器进行了结合,但属于外组合式,两个电源均需要各自的电解液、隔膜等,不但器件总体积较大,还需要外电路和相应的管理系统进行实时测试、控制,成本较高。
若将超级电容器与铅蓄电池的“外并”改成“内并”,则能省去复杂的外电路与控制系统,有效的降低成本。中国专利200810136333.1公开了一种铅蓄电池,其部分负级铅板为碳板所代替,可以提高铅蓄电池比功率,延长电池寿命。中国专利200910002836.4公开了将超级电容器活性炭电极和铅负极“内并”的电池,近期也有人称之为“超级电池”(Ultrabattery,参见J.Power Source174(2007)16)。该电池将超级电容器的高比功率、长寿命的优势融合到铅蓄电池中,在保持提高功率、延长电池寿命优点的同时,又能简化电路、提高比容量,并降低总费用(参见《科学时报》2009年8月14日的《科学时评》专栏)。但是,由于减少了负极片,这种电池的比能量将有所下降。
将超级活性炭直接加入到铅蓄电池负极板中,也能很好的起到提升电池脉冲功率的作用。如中国专利200810136333.1,中国专利200880009193.X和中国专利200910098917.9均公开了活性炭直接加入铅蓄电池电极板,能有效提高器件性能。但是这些专利只是笼统的将炭材料类添加剂的添加量控制在1%以上。
本课题组通过实验证明,用高比表面的活性炭或高分散性的碳纳米管、石墨烯材料做添加剂,添加量在0.1%时便能取得很好的效果,添加到0.2~0.5%则能够有效提高铅蓄电池的脉冲循环寿命和充电接受能力。
发明内容
本发明的目的是提供一种铅蓄电池负极板添加剂,能提高铅蓄电池的功率密度和循环使用寿命。
本发明的技术方案如下:铅蓄电池负极板添加剂为活性炭、炭黑、石墨烯、碳纳米管、炭纤维、炭气凝胶、模板炭、介孔炭、碳化物衍生炭、聚苯胺、聚吡咯、聚噻吩、聚烷基噻吩、聚对氟苯基噻吩或抑制析氢添加剂,该添加剂添加量为铅蓄电池负极板活性物质质量的0.05~5%。活性炭比表面积为1200~3300m2/g、孔容0.5~2.0cm3/g;石墨烯的平均石墨层为1~50层;碳纳米管为单壁、双壁和多壁碳纳米管,管长0.1~100微米;抑制析氢添加剂为含铅、钛、锌、钡、锑、镉、银、汞或铋的氧化物、氢氧化物、硫酸盐或其混合物。
本发明提供的负极板优点在于:该添加剂使得铅蓄电池具有了长脉冲循环寿命(5万次以上)和较强的充电接受能力的优点。
具体实施方式
实例1
在一个铅蓄电池负极板中,添加0.25%质量比的石墨烯添加剂,石墨烯平均壁数为3层。使用该添加剂极板制备出的铅蓄电池脉冲循环寿命4万次,充电时间缩短27%。
实例2
在一个铅蓄电池负极板中,添加0.12%质量比的多壁碳纳米管,碳纳米管平均长度为5微米。使用该添加剂极板制备出的铅蓄电池脉冲循环寿命4.8万次,充电时间缩短35%。

Claims (1)

1.一种铅蓄电池负极板添加剂,其特征在于:该添加剂为活性炭、炭黑、石墨烯、碳纳米管、炭纤维、炭气凝胶、模板炭、介孔炭、碳化物衍生炭、聚苯胺、聚吡咯、聚噻吩、聚烷基噻吩、聚对氟苯基噻吩或抑制析氢添加剂,该添加剂添加量为铅蓄电池负极板活性物质质量的0.05~5%;活性炭比表面积为1200~3300m2/g、为孔容0.5~2.0cm3/g;抑制析氢添加剂为含铅、钛、锌、钡、锑、镉、银、汞或铋的氧化物、氢氧化物、硫酸盐或其混合物;石墨烯的平均石墨层为1~50层;碳纳米管为单壁、双壁和多壁碳纳米管,管长0.1~100微米。
CN201310634955.8A 2013-12-03 2013-12-03 一种铅蓄电池负极板添加剂 Pending CN104681792A (zh)