CN104594113A - Corrugated paper containing modified polyphenyl ether resin and preparation method of corrugated paper - Google Patents
Corrugated paper containing modified polyphenyl ether resin and preparation method of corrugated paper Download PDFInfo
- Publication number
- CN104594113A CN104594113A CN201410844417.6A CN201410844417A CN104594113A CN 104594113 A CN104594113 A CN 104594113A CN 201410844417 A CN201410844417 A CN 201410844417A CN 104594113 A CN104594113 A CN 104594113A
- Authority
- CN
- China
- Prior art keywords
- ether resin
- corrugated paper
- parts
- paper
- polyphenylene ether
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses corrugated paper containing modified polyphenyl ether resin and a preparation method of the corrugated paper. The corrugated paper comprises the following raw materials in parts by weight: 60 parts of waste paper, 20 parts of corn starch, 10 parts of a modified polyphenyl ether resin, 5 parts of glass fibers, 4 parts of plastics, 2 parts of a thickening agent, 1.5 parts of an aluminate ester, 2 parts of zinc maleate and 1 part of aluminum sulfate. The modified polyphenyl ether resin is taken as a main ingredient, and the polyphenyl ether resin is modified, so that the product can achieve the maximum strength and water resistance and is high in stability in the using process, flat in surface and high in plane bearing pressure.
Description
Technical field
The present invention relates to a kind of corrugated paper, be specifically related to a kind of corrugated paper containing modified polyphenylene ether resin and preparation method thereof.
Background technology
Corrugated paper is the common materials of paper packaging box, and it has hardness again than wooden case light weight, and size is easily cut out, and is used for other packaged products of protection not to be compromised.Corrugated paper can print pattern and the word of different color or write letter symbol in outside, cost is also relatively cheap.But, corrugated paper avoid water logging, humidity, mouldy, enter water, hand hook etc.But existing corrugated paper is all weak in process of production, intensity and the water proofing property of corrugated paper can not be improved.
Summary of the invention
The object of the present invention is to provide a kind of corrugated paper containing modified polyphenylene ether resin and preparation method thereof.
The present invention adopts following technical scheme:
A corrugated paper containing modified polyphenylene ether resin, is characterized in that the weight portion of its constitutive material is: waste paper 60-70, cornstarch 20-25, modified polyphenylene ether resin 10-15, glass fibre 5-6, plastics 4-6, thickener 2-3, Aluminate 1.5-2, maleic acid zinc 2-2.5, aluminum sulfate 1-2.
Described a kind of corrugated paper preparation method containing modified polyphenylene ether resin, is characterized in that following steps:
(1) screen: waste paper is smashed screening;
(2) slurrying: add water and waste paper cornstarch in reactor, water and waste paper and cornstarch mass ratio are 5: 1: 1, and temperature remains on 80 DEG C ~ 85 DEG C, stir and add modified polyphenylene ether resin, glass fibre, plastics, thickener, mix, obtain paper pulp;
(3) adding material: stir in paper pulp and add Aluminate, maleic acid zinc, aluminum sulfate, mix, be warming up to 85 DEG C ~ 95 DEG C, keep this temperature 30 ~ 50 minutes;
(4) drying and processing: in reactor, temperature is adjusted to 75 DEG C ~ 85 DEG C, and wherein mixture remains on 10% ~ 15%, obtains corrugated paper finished product.
Beneficial effect of the present invention:
The present invention adopts modified polyphenylene ether resin as major ingredient, by the modification of polyphenylene ether resin, enables its product reach maximum intensity and resistance to water.In use good stability, surfacing, bears applanation high.
Detailed description of the invention
Embodiment 1: a kind of corrugated paper containing modified polyphenylene ether resin, the weight portion of its constitutive material is: waste paper 60, cornstarch 20, modified polyphenylene ether resin 10, glass fibre 5, plastics 4, thickener 2, Aluminate 1.5, maleic acid zinc 2, aluminum sulfate 1.
Described a kind of corrugated paper preparation method containing modified polyphenylene ether resin, has following steps:
(1) screen: waste paper is smashed screening;
(2) slurrying: add water and waste paper cornstarch in reactor, water and waste paper and cornstarch mass ratio are 5: 1: 1, and temperature remains on 80 DEG C, stir and add modified polyphenylene ether resin, glass fibre, plastics, thickener, mix, obtain paper pulp;
(3) adding material: stir in paper pulp and add Aluminate, maleic acid zinc, aluminum sulfate, mix, be warming up to 85 DEG C, keep this temperature 30 minutes;
(4) drying and processing: in reactor, temperature is adjusted to 75 DEG C, and wherein mixture remains on 10%, obtains corrugated paper finished product.
Claims (2)
1. the corrugated paper containing modified polyphenylene ether resin, is characterized in that the weight portion of its constitutive material is: waste paper 60-70, cornstarch 20-25, modified polyphenylene ether resin 10-15, glass fibre 5-6, plastics 4-6, thickener 2-3, Aluminate 1.5-2, maleic acid zinc 2-2.5, aluminum sulfate 1-2.
2. a kind of corrugated paper preparation method containing modified polyphenylene ether resin according to claim 1, is characterized in that following steps:
(1) screen: waste paper is smashed screening;
(2) slurrying: add water and waste paper cornstarch in reactor, water and waste paper and cornstarch mass ratio are 5: 1: 1, and temperature remains on 80 DEG C ~ 85 DEG C, stir and add modified polyphenylene ether resin, glass fibre, plastics, thickener, mix, obtain paper pulp;
(3) adding material: stir in paper pulp and add Aluminate, maleic acid zinc, aluminum sulfate, mix, be warming up to 85 DEG C ~ 95 DEG C, keep this temperature 30 ~ 50 minutes;
(4) drying and processing: in reactor, temperature is adjusted to 75 DEG C ~ 85 DEG C, and wherein mixture remains on 10% ~ 15%, obtains corrugated paper finished product.