China
Prior art keywords
parts
wicker
root
anticorrosion
corrosion agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410616354.9A
Other languages
Chinese (zh)
Inventor
徐治合
徐艳云
蔡建军
王培龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ANHUI FUNAN COUNTY WANJIAHE CRAFTS Co Ltd
Original Assignee
ANHUI FUNAN COUNTY WANJIAHE CRAFTS Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ANHUI FUNAN COUNTY WANJIAHE CRAFTS Co Ltd filed Critical ANHUI FUNAN COUNTY WANJIAHE CRAFTS Co Ltd
Priority to CN201410616354.9A priority Critical patent/CN104488991A/en
Publication of CN104488991A publication Critical patent/CN104488991A/en
Pending legal-status Critical Current

Links

Landscapes

  • Chemical And Physical Treatments For Wood And The Like (AREA)
  • Agricultural Chemicals And Associated Chemicals (AREA)

Abstract

The invention provides an anticorrosion reagent for processing wicker, and relates to the technical field of production of wicker products. The anticorrosion reagent for processing wicker is prepared from the following raw material compositions in parts by weight: 4-8 parts of herb of rosemary, 5-9 parts of spica prunellae, 1-3 parts of radix salviae miltiorrhizae, 2-4 parts of flos chrysanthemi indici, 3-7 parts of herba taraxaci, 2-4 parts of spica prunellae, 2-6 parts of lignum santali albi, 3-7 parts of herba asari, 5-9 parts of gleditsia sinensis, 3-5 parts of bark of Chinese redbud, 4-8 parts of fructus gardeniae, 5-9 parts of fructus perillae, 2-4 parts of prepared common monkshood daughter root, 2-4 parts of radix gentianae, 3-7 parts of root of fischer euphorbia, 2-4 parts of common threewingnut root, 4-8 parts of fructus evodiae, 1-3 parts of radix ophiopogonis, 2-6 parts of fructus phyllanthi, 3-7 parts of herba portulacae, 4-8 parts of gypsum fibrosum, 1-3 parts of rhizoma chuanxiong, 2-4 parts of radix angelicae dahuricae, and 3-7 parts of cortex moutan. The anticorrosion processing technology on live trees is simple, and a conventional anticorrosion method is broken through. After live willow is subjected to anticorrosion processing, the economic added value of wicker is improved, wicker can be directly used to knit wicker products, a step of performing anticorrosion processing on wicker in a conventional wicker-product technology is thoroughly changed, the anticorrosion effect is substantially improved, and the reagent utilization rate is relatively substantially improved compared with a conventional method.

Description

A kind of anti-corrosion agent for the treatment of wicker
Technical field
The present invention relates to the production technical field of wicker products, be specifically related to a kind of anti-corrosion agent for the treatment of wicker.
Background technology
Wicker products is the artifacts of China's widespread among the people, " compile basket, compile basket, every household has ".This is because the raw material sources of this technique are very extensive.Basket is compiled in north primary raw material for compiling basket has withy, Chinese tamarisk branch, mulberry shoot, the twigs of the chaste tree, false indigo stem etc. multiple, produces in saline land and marshland.Wicker products of a great variety, has the polytypes such as seat, basket, basket, dustpan, round-bottomed basket, crate, shallow basket made of wicker or thin bamboo strips, the gaily decorated basket, bamboo strainer, food dish in domestic.Export trade aspect, has formed buck basket, flower pot coat, picnic tableware basket, hanging basket, lampshade, kennel, cat nest, Bird's Nest etc. through developing and design multiple, has formed the appreciation effect that low-grade goods become high-grade, very by the attention of foreign trade department in foreign trade.
The main skill and technique of willow-plaited process has flat sennit, line to compile, strangles volume, builds volume, wrapped edge five kinds.
Wicker products take wicker as primary raw material, but the wicker in use easily infested and mould corruption of generation, cause knitting shortening in service life.Therefore, wicker needs to process before use, uses immersion treatment now more, present inorganic agent many employings chemical agent, and often toxicity is comparatively strong, residual comparatively serious, often causes toxic residue to leak, affect user healthy in knitting use procedure.And prior art is all process felling the wicker got off, the liquid of process is also all adopt the mode of soaking mostly, and the efficiency that liquid enters wicker inside is slow, and also portion is desirable for the effect of mildew-resistant corruption.
Summary of the invention
Technical problem to be solved by this invention is the defect overcoming prior art, proposes further a kind of method for anticorrosion treatment of wicker, and for the treatment of the anticorrosion liquid of wicker.
Technical problem to be solved by this invention realizes by the following technical solutions:
A method for anticorrosion treatment for wicker, is characterized in that, this processing procedure is carried out for the live body wicker on willow, and concrete steps are:
1) below willow trunk crotch, adopt transfusion, in willow trunk, inject anticorrosion liquid;
2) initial time that the anticorrosion liquid of willow injects is determined:
A. the measurement of standing tree leaf flow velocity:
Adopt thermal pulse instrument or observe the flow velocity of trees resin in diel 24 hours with whole tree potometer, within 20 minutes, measure once, analyze the rule of trees flow velocity in 24 hours;
B. according to leaf rule in willow diel, the initial time that anti-corrosion agent injects is determined; When selecting flow velocity the slowest, to living, tree injects anti-corrosion agent, guarantees that anti-corrosion agent has the sufficient time to permeate to radial direction;
C. the duration of anti-corrosion agent injection:
It is 3-4 hour that 1 bottle of 500ml injects the duration, reaches 3-4kg/m to the injection rate to willow live body 3till;
3) wicker fells the determination of time:
After medicament injects timber, the negative pressure produced by tree transpiration effect makes liquid move up with resin, and meanwhile liquid also can carry out horizontal infiltration along the radial direction of trunk; Check whether treetop position exists anticorrosion liquid, when treetop location detection goes out anticorrosion liquid, can fell wicker, stand-by;
Described anti-corrosion agent is the water extraction liquid of Chinese medicine composition, and every kilogram of Chinese medicine composition prepares water extraction liquid 6 kilograms, and described Chinese medicine composition comprises the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 4-8 part, selfheal 5-9 part, red sage root 1-3 part, mother chrysanthemum 2-4 part, dandelion 3-7 part, selfheal 2-4 part, santal 2-6 part, root of Chinese wild ginger 3-7 part, Chinese honey locust 5-9 part, Kadsura Root-bark 3-5 part, cape jasmine 4-8 part, perillaseed 5-9 part, monkshood 2-4 part, felwort 2-4 part, root of langdu 3-7 part, thunder godvine 2-4 part, evodia rutaecarpa 4-8 part, the tuber of dwarf lilyturf 1-3 part, emblic 2-6 part, kitchen garden 3-7 part, gypsum 4-8 part, Ligusticum wallichii 1-3 part, root of Dahurain angelica 2-4 part, moutan bark 3-7 part.
The preferred weight ratio of each raw material of described Chinese medicine composition is: rosemary, Xue MingRosma rinus officinalis 6 parts, selfheal 7 parts, the red sage root 2 parts, mother chrysanthemum 3 parts, dandelion 5 parts, selfheal 3 parts, 4 parts, santal, the root of Chinese wild ginger 5 parts, Chinese honey locust 7 parts, Kadsura Root-bark 4 parts, cape jasmine 6 parts, perillaseed 7 parts, monkshood 3 parts, felwort 3 parts, the root of langdu 5 parts, thunder godvine 3 parts, evodia rutaecarpa 6 parts, the tuber of dwarf lilyturf 2 parts, emblic 4 parts, kitchen garden 5 parts, 6 parts, gypsum, Ligusticum wallichii 2 parts, the root of Dahurain angelica 3 parts, moutan bark 5 parts.
For the treatment of an anti-corrosion agent for wicker, be prepared from by the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 4-8 part, selfheal 5-9 part, red sage root 1-3 part, mother chrysanthemum 2-4 part, dandelion 3-7 part, selfheal 2-4 part, santal 2-6 part, root of Chinese wild ginger 3-7 part, Chinese honey locust 5-9 part, Kadsura Root-bark 3-5 part, cape jasmine 4-8 part, perillaseed 5-9 part, monkshood 2-4 part, felwort 2-4 part, root of langdu 3-7 part, thunder godvine 2-4 part, evodia rutaecarpa 4-8 part, the tuber of dwarf lilyturf 1-3 part, emblic 2-6 part, kitchen garden 3-7 part, gypsum 4-8 part, Ligusticum wallichii 1-3 part, root of Dahurain angelica 2-4 part, moutan bark 3-7 part.
The preferred weight ratio preparing each raw material of anti-corrosion agent is: rosemary, Xue MingRosma rinus officinalis 6 parts, selfheal 7 parts, the red sage root 2 parts, mother chrysanthemum 3 parts, dandelion 5 parts, selfheal 3 parts, 4 parts, santal, the root of Chinese wild ginger 5 parts, Chinese honey locust 7 parts, Kadsura Root-bark 4 parts, cape jasmine 6 parts, perillaseed 7 parts, monkshood 3 parts, felwort 3 parts, the root of langdu 5 parts, thunder godvine 3 parts, evodia rutaecarpa 6 parts, the tuber of dwarf lilyturf 2 parts, emblic 4 parts, kitchen garden 5 parts, 6 parts, gypsum, Ligusticum wallichii 2 parts, the root of Dahurain angelica 3 parts, moutan bark 5 parts.
A preparation method for wicker anti-corrosion agent, is characterized in that, concrete steps are:
(1) each material component preparing anti-corrosion agent is taken mixture together by weight;
(2) put into container to add water and decoct, first boiled by water with big fire, then young man simmers 20-30min, filter out the dregs of a decoction, taking liquid, amount of water is according to the liquid of the waste after every kilogram of mixture 6 kilograms;
(3) liquid adopts nanofiltration to remove macromolecular substances, i.e. obtained wicker anti-corrosion agent;
Each material component and weight proportion as follows:
Rosemary, Xue MingRosma rinus officinalis 4-8 part, selfheal 5-9 part, red sage root 1-3 part, mother chrysanthemum 2-4 part, dandelion 3-7 part, selfheal 2-4 part, santal 2-6 part, root of Chinese wild ginger 3-7 part, Chinese honey locust 5-9 part, Kadsura Root-bark 3-5 part, cape jasmine 4-8 part, perillaseed 5-9 part, monkshood 2-4 part, felwort 2-4 part, root of langdu 3-7 part, thunder godvine 2-4 part, evodia rutaecarpa 4-8 part, the tuber of dwarf lilyturf 1-3 part, emblic 2-6 part, kitchen garden 3-7 part, gypsum 4-8 part, Ligusticum wallichii 1-3 part, root of Dahurain angelica 2-4 part, moutan bark 3-7 part.
Each material component and preferred weight proportion as follows:
Rosemary, Xue MingRosma rinus officinalis 6 parts, selfheal 7 parts, the red sage root 2 parts, mother chrysanthemum 3 parts, dandelion 5 parts, selfheal 3 parts, 4 parts, santal, the root of Chinese wild ginger 5 parts, Chinese honey locust 7 parts, Kadsura Root-bark 4 parts, cape jasmine 6 parts, perillaseed 7 parts, monkshood 3 parts, felwort 3 parts, the root of langdu 5 parts, thunder godvine 3 parts, evodia rutaecarpa 6 parts, the tuber of dwarf lilyturf 2 parts, emblic 4 parts, kitchen garden 5 parts, 6 parts, gypsum, Ligusticum wallichii 2 parts, the root of Dahurain angelica 3 parts, moutan bark 5 parts.
Medicament moves and permeates the inspection of uniformity coefficient in trunk:
After wicker is felled, trunk gathers wicker after felling again, studies the infiltration uniformity coefficient of the liquid on different trunk height and radial direction; The wooden color of willow is generally yellow-white, and after ACQ preservative treatment, wooden color, often in light brown, by the change of wood color in trunk, differentiates the uniformity coefficient of medicinal liquid osmosis;
The inspection of wicker antiseptic property.
Beneficial effect of the present invention is:
The invention provides a kind of method for anticorrosion treatment and anti-corrosion agent of wicker, tree anticorrosion treatment technology of living is simple, breaches traditional method for anticorrosion treatment; After the preservative treatment of live body willow, log, plate square bar can directly in outdoor applications, also the economic value added of willow is improved, wicker can be directly used in establishment wicker products, revolutionize in traditional willow-plaited process and antiseptic step is carried out to wicker, and antiseptic effect has had large increase, utilization ratio of drug also comparatively conventional method had larger lifting.
Embodiment
The technological means realized to make the present invention, creation characteristic, reaching object and effect is easy to understand, below in conjunction with specific embodiment, set forth the present invention further, but following embodiment being only the preferred embodiments of the present invention, and not all.Based on the embodiment in embodiment, those skilled in the art under the prerequisite not making creative work obtain other embodiment, all belong to the protection domain of this patent.
Embodiment 1
For the treatment of an anti-corrosion agent for wicker, be prepared from by the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 4g, selfheal 5g, red sage root 1g, mother chrysanthemum 2g, dandelion 3g, selfheal 2g, santal 2g, root of Chinese wild ginger 3g, Chinese honey locust 5g, Kadsura Root-bark 3g, cape jasmine 4g, perillaseed 5g, monkshood 2g, felwort 2g, root of langdu 3g, thunder godvine 2g, evodia rutaecarpa 4g, the tuber of dwarf lilyturf 1g, emblic 2g, kitchen garden 3g, gypsum 4g, Ligusticum wallichii 1g, root of Dahurain angelica 2g, moutan bark 3g.
The preparation method of wicker anti-corrosion agent, is characterized in that, concrete steps are:
(1) each material component preparing anti-corrosion agent is taken mixture together by weight;
(2) put into container to add water and decoct, first boiled by water with big fire, then young man simmers 20-30min, filter out the dregs of a decoction, taking liquid, amount of water is according to the liquid of the waste after every kilogram of mixture 6 kilograms;
(3) liquid adopts nanofiltration to remove macromolecular substances, i.e. obtained wicker anti-corrosion agent.
The method for anticorrosion treatment of wicker, this processing procedure is carried out for the live body wicker on willow, and concrete steps are:
1) below willow trunk crotch, adopt transfusion, in willow trunk, inject anticorrosion liquid;
2) initial time that the anticorrosion liquid of willow injects is determined:
A. the measurement of standing tree leaf flow velocity:
Adopt thermal pulse instrument or observe the flow velocity of trees resin in diel 24 hours with whole tree potometer, within 20 minutes, measure once, analyze the rule of trees flow velocity in 24 hours;
B. according to leaf rule in willow diel, the initial time that anti-corrosion agent injects is determined; When selecting flow velocity the slowest, to living, tree injects anti-corrosion agent, guarantees that anti-corrosion agent has the sufficient time to permeate to radial direction;
C. the duration of anti-corrosion agent injection:
It is 3-4 hour that every bottle of 500ml injects the duration, reaches 3-4kg/m to the injection rate to willow live body 3till;
3) wicker fells the determination of time:
After medicament injects timber, the negative pressure produced by tree transpiration effect makes liquid move up with resin, and meanwhile liquid also can carry out horizontal infiltration along the radial direction of trunk; Check whether treetop position exists anticorrosion liquid, when treetop location detection goes out anticorrosion liquid, can fell wicker, stand-by.
Embodiment 2
For the treatment of an anti-corrosion agent for wicker, be prepared from by the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 8g, selfheal 9g, red sage root 3g, mother chrysanthemum 4g, dandelion 7g, selfheal 4g, santal 6g, root of Chinese wild ginger 7g, Chinese honey locust 9g, Kadsura Root-bark 5g, cape jasmine 8g, perillaseed 9g, monkshood 4g, felwort 4g, root of langdu 7g, thunder godvine 4g, evodia rutaecarpa 8g, the tuber of dwarf lilyturf 3g, emblic 6g, kitchen garden 7g, gypsum 8g, Ligusticum wallichii 3g, root of Dahurain angelica 4g, moutan bark 7g.
The preparation method of wicker anti-corrosion agent, is characterized in that, concrete steps are:
(1) each material component preparing anti-corrosion agent is taken mixture together by weight;
(2) put into container to add water and decoct, first boiled by water with big fire, then young man simmers 20-30min, filter out the dregs of a decoction, taking liquid, amount of water is according to the liquid of the waste after every kilogram of mixture 6 kilograms;
(3) liquid adopts nanofiltration to remove macromolecular substances, i.e. obtained wicker anti-corrosion agent.
The method for anticorrosion treatment of wicker, this processing procedure is carried out for the live body wicker on willow, and concrete steps are:
1) below willow trunk crotch, adopt transfusion, in willow trunk, inject anticorrosion liquid;
2) initial time that the anticorrosion liquid of willow injects is determined:
A. the measurement of standing tree leaf flow velocity:
Adopt thermal pulse instrument or observe the flow velocity of trees resin in diel 24 hours with whole tree potometer, within 20 minutes, measure once, analyze the rule of trees flow velocity in 24 hours;
B. according to leaf rule in willow diel, the initial time that anti-corrosion agent injects is determined; When selecting flow velocity the slowest, to living, tree injects anti-corrosion agent, guarantees that anti-corrosion agent has the sufficient time to permeate to radial direction;
C. the duration of anti-corrosion agent injection:
It is 3-4 hour that every bottle of 500ml injects the duration, reaches 3-4kg/m to the injection rate to willow live body 3till;
3) wicker fells the determination of time:
After medicament injects timber, the negative pressure produced by tree transpiration effect makes liquid move up with resin, and meanwhile liquid also can carry out horizontal infiltration along the radial direction of trunk; Check whether treetop position exists anticorrosion liquid, when treetop location detection goes out anticorrosion liquid, can fell wicker, stand-by.
Embodiment 3
For the treatment of an anti-corrosion agent for wicker, be prepared from by the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 6g, selfheal 7g, red sage root 2g, mother chrysanthemum 3g, dandelion 5g, selfheal 3g, santal 4g, root of Chinese wild ginger 5g, Chinese honey locust 7g, Kadsura Root-bark 4g, cape jasmine 6g, perillaseed 7g, monkshood 3g, felwort 3g, root of langdu 5g, thunder godvine 3g, evodia rutaecarpa 6g, the tuber of dwarf lilyturf 2g, emblic 4g, kitchen garden 5g, gypsum 6g, Ligusticum wallichii 2g, root of Dahurain angelica 3g, moutan bark 5g.
The preparation method of wicker anti-corrosion agent, is characterized in that, concrete steps are:
(1) each material component preparing anti-corrosion agent is taken mixture together by weight;
(2) put into container to add water and decoct, first boiled by water with big fire, then young man simmers 20-30min, filter out the dregs of a decoction, taking liquid, amount of water is according to the liquid of the waste after every kilogram of mixture 6 kilograms;
(3) liquid adopts nanofiltration to remove macromolecular substances, i.e. obtained wicker anti-corrosion agent.
The method for anticorrosion treatment of wicker, this processing procedure is carried out for the live body wicker on willow, and concrete steps are:
1) below willow trunk crotch, adopt transfusion, in willow trunk, inject anticorrosion liquid;
2) initial time that the anticorrosion liquid of willow injects is determined:
A. the measurement of standing tree leaf flow velocity:
Adopt thermal pulse instrument or observe the flow velocity of trees resin in diel 24 hours with whole tree potometer, within 20 minutes, measure once, analyze the rule of trees flow velocity in 24 hours;
B. according to leaf rule in willow diel, the initial time that anti-corrosion agent injects is determined; When selecting flow velocity the slowest, to living, tree injects anti-corrosion agent, guarantees that anti-corrosion agent has the sufficient time to permeate to radial direction;
C. the duration of anti-corrosion agent injection:
It is 3-4 hour that every bottle of 500ml injects the duration, reaches 3-4kg/m to the injection rate to willow live body 3till;
3) wicker fells the determination of time:
After medicament injects timber, the negative pressure produced by tree transpiration effect makes liquid move up with resin, and meanwhile liquid also can carry out horizontal infiltration along the radial direction of trunk; Check whether treetop position exists anticorrosion liquid, when treetop location detection goes out anticorrosion liquid, can fell wicker, stand-by.
More than show and describe general principle of the present invention, principal character and advantage of the present invention.The technical staff of the industry should understand; the present invention is not restricted to the described embodiments; what describe in above-described embodiment and specification is only preference of the present invention; be not used for limiting the present invention; without departing from the spirit and scope of the present invention; the present invention also has various changes and modifications, and these changes and improvements all fall in the claimed scope of the invention.Application claims protection domain is defined by appending claims and equivalent thereof.

Claims (2)

1. for the treatment of an anti-corrosion agent for wicker, it is characterized in that, be prepared from by the material component of following weight:
Rosemary, Xue MingRosma rinus officinalis 4-8 part, selfheal 5-9 part, red sage root 1-3 part, mother chrysanthemum 2-4 part, dandelion 3-7 part, selfheal 2-4 part, santal 2-6 part, root of Chinese wild ginger 3-7 part, Chinese honey locust 5-9 part, Kadsura Root-bark 3-5 part, cape jasmine 4-8 part, perillaseed 5-9 part, monkshood 2-4 part, felwort 2-4 part, root of langdu 3-7 part, thunder godvine 2-4 part, evodia rutaecarpa 4-8 part, the tuber of dwarf lilyturf 1-3 part, emblic 2-6 part, kitchen garden 3-7 part, gypsum 4-8 part, Ligusticum wallichii 1-3 part, root of Dahurain angelica 2-4 part, moutan bark 3-7 part.
2. the anti-corrosion agent for the treatment of wicker according to claim 1, is characterized in that: the preferred weight ratio preparing each raw material of anti-corrosion agent is: rosemary, Xue MingRosma rinus officinalis 6 parts, selfheal 7 parts, the red sage root 2 parts, mother chrysanthemum 3 parts, dandelion 5 parts, selfheal 3 parts, 4 parts, santal, the root of Chinese wild ginger 5 parts, Chinese honey locust 7 parts, Kadsura Root-bark 4 parts, cape jasmine 6 parts, perillaseed 7 parts, monkshood 3 parts, felwort 3 parts, the root of langdu 5 parts, thunder godvine 3 parts, evodia rutaecarpa 6 parts, the tuber of dwarf lilyturf 2 parts, emblic 4 parts, kitchen garden 5 parts, 6 parts, gypsum, Ligusticum wallichii 2 parts, the root of Dahurain angelica 3 parts, moutan bark 5 parts.
CN201410616354.9A 2014-11-04 2014-11-04 Anticorrosion reagent for processing wicker Pending CN104488991A (en)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410616354.9A CN104488991A (en) 2014-11-04 2014-11-04 Anticorrosion reagent for processing wicker

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410616354.9A CN104488991A (en) 2014-11-04 2014-11-04 Anticorrosion reagent for processing wicker

Publications (1)

Publication Number Publication Date
CN104488991A true CN104488991A (en) 2015-04-08

Family

ID=52930524

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410616354.9A Pending CN104488991A (en) 2014-11-04 2014-11-04 Anticorrosion reagent for processing wicker

Country Status (1)

Country Link
CN (1) CN104488991A (en)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104999531A (en) * 2015-07-16 2015-10-28 安徽华安达集团工艺品有限公司 Persistent mosquito-repelling lemon scent treatment agent for surface coating of wicker products and preparation method thereof
CN106182248A (en) * 2016-07-13 2016-12-07 阜南县猛发工艺品有限公司 A kind of method promoting wicker products decay resistance
CN107877644A (en) * 2017-11-09 2018-04-06 宾阳县东弘五金工艺品有限公司 A kind of straw plaited Feedstock treating liquid
CN111685131A (en) * 2020-06-15 2020-09-22 山东省农业科学院植物保护研究所 Pharmaceutical composition for preventing peanut rust by using purslane extract and preparation method thereof

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2005305988A (en) * 2004-04-19 2005-11-04 Hiromi Ida Injecting technique of chemical into standing tree and using method
CN102660138A (en) * 2012-04-25 2012-09-12 王吉云 Production and application method of bamboo wood mould-proof dyeing agent
CN103283516A (en) * 2013-05-30 2013-09-11 南京林业大学 Antiseptic treatment method for live poplar
CN104026172A (en) * 2014-05-26 2014-09-10 阜南腾强工艺品有限公司 Rattan treatment agent for wickerwork
CN104026161A (en) * 2014-05-26 2014-09-10 阜南腾强工艺品有限公司 Wicker treatment agent for wickerwork

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2005305988A (en) * 2004-04-19 2005-11-04 Hiromi Ida Injecting technique of chemical into standing tree and using method
CN102660138A (en) * 2012-04-25 2012-09-12 王吉云 Production and application method of bamboo wood mould-proof dyeing agent
CN103283516A (en) * 2013-05-30 2013-09-11 南京林业大学 Antiseptic treatment method for live poplar
CN104026172A (en) * 2014-05-26 2014-09-10 阜南腾强工艺品有限公司 Rattan treatment agent for wickerwork
CN104026161A (en) * 2014-05-26 2014-09-10 阜南腾强工艺品有限公司 Wicker treatment agent for wickerwork

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104999531A (en) * 2015-07-16 2015-10-28 安徽华安达集团工艺品有限公司 Persistent mosquito-repelling lemon scent treatment agent for surface coating of wicker products and preparation method thereof
CN106182248A (en) * 2016-07-13 2016-12-07 阜南县猛发工艺品有限公司 A kind of method promoting wicker products decay resistance
CN106182248B (en) * 2016-07-13 2018-01-23 阜南县猛发工艺品有限公司 A kind of method for lifting wicker products decay resistance
CN107877644A (en) * 2017-11-09 2018-04-06 宾阳县东弘五金工艺品有限公司 A kind of straw plaited Feedstock treating liquid
CN111685131A (en) * 2020-06-15 2020-09-22 山东省农业科学院植物保护研究所 Pharmaceutical composition for preventing peanut rust by using purslane extract and preparation method thereof

Similar Documents

Publication Publication Date Title
CN104476638B (en) A kind of wicker plaiting article material processing
CN104476636B (en) A kind of mildew-proof treatment method of rattan
CN104476639A (en) Sterilization processing method of rattan plaited article materials
CN105165536B (en) A kind of method and its agalloch eaglewood formation promotor of promotion suspension culture of Aquilaria sinensis tree production agalloch eaglewood
CN104397071A (en) Sterilizing processing liquid for processing rattans
CN104430646A (en) Method for preparing rattan mildew proofing medicament
CN104441157A (en) Softening steam for treating wicker
CN104488991A (en) Anticorrosion reagent for processing wicker
CN104441125A (en) Braiding method of wickerwork
CN104385401A (en) Insect prevention and mothproof conditioning fluid for wickerwork
CN104522091A (en) Mildew resistant treatment agent of wood
CN104441163B (en) A kind of preparation method of willow rattan anti-mould and anti-moth treatment fluid
CN106113195A (en) A kind of anti-mould and anti-moth processing method of wicker products
CN104354202B (en) A kind of anti-mould and anti-moth treatment fluid for the treatment of willow rattan
CN104441126A (en) Treatment liquid for treating wicker
CN104441123A (en) Rattan processing method for willow artworks
CN105666614A (en) Preparation method for anti-cracking color protecting drug liquid for living rattan
CN104488992A (en) Preparation method for wicker anticorrosion drug
CN104441141A (en) Mildew-proof and insect-proof wickerwork treating agent
CN104441131A (en) Method for anticorrosive treatment of willow twigs
CN103999886B (en) Botanical biological pesticide of preventing and treating FLOS CHRYSANTHEMI ALBA from Haizhou of China aphid and preparation method thereof
CN105643740A (en) Cracking prevention and color protection solution for treating rattans
CN104397065A (en) Preparation method of wicker insect-resistant moth-proofing treatment liquid
CN104430647A (en) Mildew proofing medicament for treating rattan
CN106182293A (en) A kind of coffee-like stain of wicker products

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
RJ01 Rejection of invention patent application after publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20150408