CN104479477A - Anti-aging water-proof building coating - Google Patents
Anti-aging water-proof building coating Download PDFInfo
- Publication number
- CN104479477A CN104479477A CN201410694590.2A CN201410694590A CN104479477A CN 104479477 A CN104479477 A CN 104479477A CN 201410694590 A CN201410694590 A CN 201410694590A CN 104479477 A CN104479477 A CN 104479477A
- Authority
- CN
- China
- Prior art keywords
- parts
- aging
- water
- proof
- architectural coating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses an anti-aging water-proof building coating which comprises the following raw materials in parts by weight: 35-50 parts of acrylate emulsion, 15-20 parts of oligoester polyol, 5-10 parts of methyl guaiacol, 5-15 parts of ethanediol, 3-8 parts of white latex, 5-10 parts of titanium dioxide, 1-3 parts of dispersing agents, 0.1-1 part of a wetting agent, 0.1-0.5 part of a softening agent and 0.1-2 parts of an antioxidant. The anti-aging water-proof building coating disclosed by the invention has the advantages of high aging resistance, excellent water-proof property and good leakage appearance protection, can be used for prolonging the service life of a building, can be used for enabling a roof to be water-proof, is high in tensile strength, and can not be deteriorated or softened at high temperature.
Description
Technical field
This has and relates to building material field, is specially a kind of anti-aging waterproof architectural coating.
Background technology
Paint finishing can bond very well with body material in body surface and form the material of complete and tough and tensile protective membrane, is called coating.Coating and paint are identical concepts.Paint is people's custom titles used for a long time, after introducing China, just utilizes in building trade always.The effect of coating may be summarized to be three aspects: provide protection, decoration function, specific function effect.The general composition of coating: comprise filmogen, solvent, auxiliary agent.China's decorative craft of building will enter new developing period, and the demand of building coating can continue to increase, and industry market development potentiality is huge.
Building coating has decoration functions, defencive function and livability and improves function.Proportion shared by various function is not quite similar because application target is different.Decoration functions is the function of beautifying the appearance value improving it by buildings.Mainly comprise the design design of plane color, pattern and gloss aspect and the design design of three-dimensional pattern.But to match with the size and shape of the moulding of buildings itself and base material itself, just can fully play out.Defencive function refers to architecture protection thing not by the impact of environment and the function of destruction.The content that different types of protected body requires defencive function is also different.As just very large in the indoor index difference with reaching required by outdoor application.Some buildingss to mildew-resistant, fire prevention, heat insulating, corrosion-resistant etc. have particular requirement.Livability improves function mainly for indoor application, contributes to the function improving living environment exactly, as effect and classification, the antisweat etc. of sound-proofing, sound absorbing coating.Coating act as decoration and protection, protects by the surface being coated with jewelry, prevents the erosion of the light, oxygen, chemical substance, solvent etc. from the external world, improve the work-ing life of coated thing; Paint finishing material surface, changes its color, decorative pattern, gloss, texture etc., improves the aesthetic value of object.
Along with development and the refinement of domestic coating industry, market is also more and more outstanding to the requirement with special functional coating, wherein anti-aging, water-fast, acid-alkali-corrosive-resisting, the performance requriements such as fire-retardant are more increased, in order to meet the requirement of every profession and trade to anti-aging waterproof paint, production high-performance, widely used anti-aging waterproof paint is necessary.
Summary of the invention
The object of this invention is to provide that a kind of ageing-resistant performance is high, the anti-aging water-proof building material of good water-proof effect.
The present invention is achieved through the following technical solutions:
A kind of anti-aging waterproof architectural coating, comprise the raw material composition of following parts by weight: acrylic ester emulsion 35 ~ 50 parts, oligomeric ester polyol 15 ~ 20 parts, methyl guaiacol and 45 ~ 10 parts, ethylene glycol 5 ~ 15 parts, white glue with vinyl 3 ~ 8 parts, titanium dioxide 5 ~ 10 parts, dispersion agent 1 ~ 3 part, wetting agent 0.1 ~ 1 part, softening agent 0.1 ~ 0.5 part, 0.1 ~ 2 part, oxidation inhibitor.
Preferably, described dispersant polycarboxylate type dispersion agent.
Preferably, described lubricant is methyl-silicone oil.
Preferably, described softening agent is ester based quaternary ammonium salt.
Preferably, described oxidation inhibitor is antioxidant 1076.
The invention has the beneficial effects as follows: the coating resistance to deterioration that the present invention proposes is strong, can extend the work-ing life of buildings, water resistance is excellent simultaneously, protection is manifested well to seepage, can be used for roof waterproof, and tensile strength is high, at high temperature undergoes no deterioration softening.
Embodiment
Below in conjunction with embodiment, the present invention is described further.
Embodiment 1
A kind of anti-aging waterproof architectural coating, comprise the raw material composition of following parts by weight: acrylic ester emulsion 35 parts, oligomeric ester polyol 15 parts, methyl guaiacol and 45 parts, ethylene glycol 5 parts, white glue with vinyl 3 parts, titanium dioxide 5 parts, poly carboxylic acid salt form dispersion agent 1 part, methyl-silicone oil 0.1 part, ester based quaternary ammonium salt 0.1 part, antioxidant 1076 0.1 part.
Embodiment 1
A kind of anti-aging waterproof architectural coating, comprise the raw material composition of following parts by weight: acrylic ester emulsion 40 parts, oligomeric ester polyol 18 parts, methyl guaiacol and 48 parts, ethylene glycol 10 parts, white glue with vinyl 5 parts, titanium dioxide 6 parts, poly carboxylic acid salt form dispersion agent 2 parts, methyl-silicone oil 0.5 part, ester based quaternary ammonium salt 0.3 part, antioxidant 1076 0.5 part.
Embodiment 1
A kind of anti-aging waterproof architectural coating, comprise the raw material composition of following parts by weight: acrylic ester emulsion 50 parts, oligomeric ester polyol 20 parts, methyl guaiacol and 4 10 parts, ethylene glycol 15 parts, white glue with vinyl 8 parts, titanium dioxide 10 parts, poly carboxylic acid salt form dispersion agent 3 parts, methyl-silicone oil 1 part, ester based quaternary ammonium salt 0.5 part, antioxidant 1076 2 parts.
The coating resistance to deterioration that the present invention proposes is strong, can extend the work-ing life of buildings, and water resistance is excellent simultaneously, manifests protection well to seepage, can be used for roof waterproof, and tensile strength is high, at high temperature undergoes no deterioration softening.
The above is only embodiments of the invention, is not restriction the present invention being made to any other form, and any amendment done according to technical spirit of the present invention or equivalent variations, still belong to the present invention's scope required for protection.
Claims (5)
1. an anti-aging waterproof architectural coating, it is characterized in that: the raw material composition comprising following parts by weight: acrylic ester emulsion 35 ~ 50 parts, oligomeric ester polyol 15 ~ 20 parts, methyl guaiacol and 45 ~ 10 parts, ethylene glycol 5 ~ 15 parts, white glue with vinyl 3 ~ 8 parts, titanium dioxide 5 ~ 10 parts, dispersion agent 1 ~ 3 part, wetting agent 0.1 ~ 1 part, softening agent 0.1 ~ 0.5 part, 0.1 ~ 2 part, oxidation inhibitor.
2. a kind of anti-aging waterproof architectural coating according to claim 1, is characterized in that: described dispersant polycarboxylate type dispersion agent.
3. a kind of anti-aging waterproof architectural coating according to claim 1, is characterized in that: described lubricant is methyl-silicone oil.
4. a kind of anti-aging waterproof architectural coating according to claim 1, is characterized in that: described softening agent is ester based quaternary ammonium salt.
5. a kind of anti-aging waterproof architectural coating according to claim 1, is characterized in that: described oxidation inhibitor is antioxidant 1076.