CN104404730A - Method for improving dazzling effect of knitting fabric through spray drying and shaping - Google Patents
Method for improving dazzling effect of knitting fabric through spray drying and shaping Download PDFInfo
- Publication number
- CN104404730A CN104404730A CN201410664376.2A CN201410664376A CN104404730A CN 104404730 A CN104404730 A CN 104404730A CN 201410664376 A CN201410664376 A CN 201410664376A CN 104404730 A CN104404730 A CN 104404730A
- Authority
- CN
- China
- Prior art keywords
- grey cloth
- machine speed
- humidification
- spraying
- dazzling
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention discloses a method for improving a dazzling effect of a knitting fabric through spray drying and shaping. The method comprises the following steps that dyed blank cloth enters an annular baking tube to be subjected to annular baking, wherein the annular baking temperature is 75 to 90 DEG C, and the machine speed is 15 to 20 m/min; then, the blank cloth subjected to the annular baking enters a spray humidification machine to be subjected to spray humidification, wherein the machine speed is 25 to 30 m/min; next, the blank cloth subjected to the humidification enters a shaping machine to be shaped, wherein shaping temperature is 110 to 180 DEG C, and the machine speed is 30 to 40 m/min. Through adopting the mode, the method provided by the invention has the advantages that the dazzling effect occurring probability of the dyed and shaped knitting fabric can be reduced, the cloth surface quality is improved, and the reworking and rejection cost is reduced.
Description
Technical field
The present invention relates to fabric process field, particularly relate to a kind of spraying and dry surely improve the dazzling method of knit fabric.
Background technology
Knit fabric, in dyeing or type-approval process, because temperature is too high or overlong time, easily causes fibrous fracture, occurs dazzling.
At present, also do not have the systems approach that pre-prevention fabric is dazzling, when dazzling phenomenon appears in fabric, the method that ordinary stain factory often adopts is: do over again to there being dazzling fabric, be sprayed on dazzling fabric after being watered by softener, deposit after 1 day and again carry out washing and drying technique.This kind of method is loaded down with trivial details, deals with relatively hard, and easily causes time and cost waste, instead contaminates for serious then needs or scraps.
summary of the invention
The technical problem that the present invention mainly solves is to provide a kind of spraying and dry surely improves the dazzling method of knit fabric, can reduce knit fabric and occur dazzling probability after dyeing sizing, improve fabric quality, reduce the cost returning something for repairs and scrap.
For solving the problems of the technologies described above, the technical scheme that the present invention adopts is: provide a kind of spraying dry surely to improve the dazzling method of knit fabric, comprising:
Grey cloth after dyeing is entered ring drying cylinder ring dry, it is 75-90 DEG C that ring dries temperature, and machine speed is 15-20 m/min; Then the grey cloth after being dried by ring enters spraying humidifier, and carry out spraying humidification, machine speed is 25-30 m/min; Then the grey cloth after humidification is entered setting machine sizing, setting temperature is 110-180 DEG C, and machine speed is 30-40 m/min.
In a preferred embodiment of the present invention, temperature when described ring drying cylinder is dried is 80 DEG C, and machine speed is 20 ms/min.
In a preferred embodiment of the present invention, machine speed during described spraying humidification is 30 ms/min.
In a preferred embodiment of the present invention, the grey cloth moisture after described humidification is 25%-30%.
In a preferred embodiment of the present invention, described grey cloth is terylen cotton knitting grey cloth, and temperature during described sizing is 135 DEG C, and machine speed is 35 ms/min.
In a preferred embodiment of the present invention, described grey cloth is pure cotton knitting grey cloth, and temperature during described sizing is 120 DEG C, and machine speed is 35 ms/min.
In a preferred embodiment of the present invention, described grey cloth is purely wash knitted fabric, and temperature during described sizing is 175 DEG C, and machine speed is 30 ms/min.
The invention has the beneficial effects as follows: after the grey cloth after dyeing is dried, then shape again after carrying out spraying humidification, knit fabric can be reduced after dyeing sizing, occur dazzling probability, improve fabric quality, reduce the cost returning something for repairs and scrap.
Detailed description of the invention
Below preferred embodiment of the present invention is described in detail, can be easier to make advantages and features of the invention be readily appreciated by one skilled in the art, thus more explicit defining is made to protection scope of the present invention.
The embodiment of the present invention comprises:
Embodiment one
Spray to do and surely improve the dazzling method of knit fabric, specifically comprise:
Grey cloth after dyeing is entered ring drying cylinder ring dry, it is 75-90 DEG C that ring dries temperature, and be preferably 80 DEG C, machine speed is 15-20 m/min, is preferably 20 ms/min; Then the grey cloth after being dried by ring enters spraying humidifier, and carry out spraying humidification, machine speed is 25-30 m/min, is preferably 30 ms/min; Then the grey cloth after humidification is entered setting machine sizing, setting temperature is 135 DEG C, and machine speed is 35 ms/min.
Wherein, described grey cloth is terylen cotton knitting grey cloth.
Grey cloth moisture after described humidification is 25%-30%, by controlling the grey cloth moisture after humidification, the fabric after sizing is not easily occurred dazzling.
Embodiment two
Spray to do and surely improve the dazzling method of knit fabric, specifically comprise:
Grey cloth after dyeing is entered ring drying cylinder ring dry, it is 75-90 DEG C that ring dries temperature, and be preferably 80 DEG C, machine speed is 15-20 m/min, is preferably 20 ms/min; Then the grey cloth after being dried by ring enters spraying humidifier, and carry out spraying humidification, machine speed is 25-30 m/min, is preferably 30 ms/min; Then the grey cloth after humidification is entered setting machine sizing, setting temperature is 120 DEG C, and machine speed is 35 ms/min.
Wherein, described grey cloth is pure cotton knitting grey cloth.
Grey cloth moisture after described humidification is 25%-30%, by controlling the grey cloth moisture after humidification, the fabric after sizing is not easily occurred dazzling.
Embodiment three
Spray to do and surely improve the dazzling method of knit fabric, specifically comprise:
Grey cloth after dyeing is entered ring drying cylinder ring dry, it is 75-90 DEG C that ring dries temperature, and be preferably 80 DEG C, machine speed is 15-20 m/min, is preferably 20 ms/min; Then the grey cloth after being dried by ring enters spraying humidifier, and carry out spraying humidification, machine speed is 25-30 m/min, is preferably 30 ms/min; Then the grey cloth after humidification is entered setting machine sizing, setting temperature is 175 DEG C, and machine speed is 30 ms/min.
Wherein, described grey cloth is purely wash knitted fabric.
Grey cloth moisture after described humidification is 25%-30%, by controlling the grey cloth moisture after humidification, the fabric after sizing is not easily occurred dazzling.
A kind of spraying of the present invention dry improves the dazzling method of knit fabric surely, after the grey cloth after dyeing is dried, then shape again after carrying out spraying humidification, knit fabric can be reduced after dyeing sizing, occur dazzling probability, improve fabric quality, reduce the cost returning something for repairs and scrap.
The foregoing is only embodiments of the invention; not thereby the scope of the claims of the present invention is limited; every utilize description of the present invention to do equivalent structure or equivalent flow process conversion; or be directly or indirectly used in other relevant technical fields, be all in like manner included in scope of patent protection of the present invention.
Claims (7)
1. spraying is dry improves the dazzling method of knit fabric surely, it is characterized in that, comprising:
Grey cloth after dyeing is entered ring drying cylinder ring dry, it is 75-90 DEG C that ring dries temperature, and machine speed is 15-20 m/min; Then the grey cloth after being dried by ring enters spraying humidifier, and carry out spraying humidification, machine speed is 25-30 m/min; Then the grey cloth after humidification is entered setting machine sizing, setting temperature is 110-180 DEG C, and machine speed is 30-40 m/min.
2. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, and it is characterized in that, temperature when described ring drying cylinder is dried is 80 DEG C, and machine speed is 20 ms/min.
3. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, and it is characterized in that, machine speed during described spraying humidification is 30 ms/min.
4. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, and it is characterized in that, the grey cloth moisture after described humidification is 25%-30%.
5. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, and it is characterized in that, described grey cloth is terylen cotton knitting grey cloth, and temperature during described sizing is 135 DEG C, and machine speed is 35 ms/min.
6. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, and it is characterized in that, described grey cloth is pure cotton knitting grey cloth, and temperature during described sizing is 120 DEG C, and machine speed is 35 ms/min.
7. a kind of spraying according to claim 1 dry improves the dazzling method of knit fabric surely, it is characterized in that, described grey cloth is purely wash knitted fabric, and temperature during described sizing is 175 DEG C, and machine speed is 30 ms/min.