CN104342931A - 一种适用于贴身织物的环保型柔软剂及其制备方法 - Google Patents

一种适用于贴身织物的环保型柔软剂及其制备方法 Download PDF

Info

Publication number
CN104342931A
CN104342931A CN201410580376.4A CN201410580376A CN104342931A CN 104342931 A CN104342931 A CN 104342931A CN 201410580376 A CN201410580376 A CN 201410580376A CN 104342931 A CN104342931 A CN 104342931A
Authority
CN
China
Prior art keywords
environment
applicable
span80
emulsifying agent
sucrose polyester
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410580376.4A
Other languages
English (en)
Inventor
张玲玲
王际平
刘今强
段鹏真
张军燚
张爱萍
杨云飞
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Sci Tech University ZSTU
Zhejiang University of Science and Technology ZUST
Original Assignee
Zhejiang Sci Tech University ZSTU
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhejiang Sci Tech University ZSTU filed Critical Zhejiang Sci Tech University ZSTU
Priority to CN201410580376.4A priority Critical patent/CN104342931A/zh
Publication of CN104342931A publication Critical patent/CN104342931A/zh
Priority to PCT/CN2015/078858 priority patent/WO2016065888A1/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种纺织品柔软剂,尤其是涉及一种适用于贴身织物的环保型柔软剂 , 属于纺织品技术领域,是由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n=6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水=30:4.45~5.65:2.55~3.28:61~63。该环保型柔软剂适用于各种织物的柔软处理,尤其适用于贴身衣物或婴儿服装面料加工时的软化,且不会在布料中残留有毒物质,使用时更加安全。

Description

一种适用于贴身织物的环保型柔软剂及其制备方法
技术领域
本发明涉及一种纺织品柔软剂,具体是涉及一种适用于婴儿服装或贴身织物的环保型柔软剂,属于纺织品技术领域。
背景技术
柔软剂是印染加工行业后整理工序中经常用到的常规助剂,是一种能赋予衣物和织物平滑手感、柔软感觉的日用化工产品。随着人们环保意识的提高,很多有高毒害和低降解性的柔软剂已经被停止使用,如含有单烷基季铵盐和二烷基季铵盐的柔软剂,由于生物降解性差,易污染环境,在上世纪90年代初已被停止使用。
目前,应市场对生态纺织品和环境要求的提高,国内外纺织助剂厂商竞相开发新型表面活性剂作为柔软剂活性物,选择以低毒性、低刺激性,易生物降解的产品作为开发方向,如烷基咪唑啉型、脂肪酸三乙醇季铵盐、双酯基季铵盐、卵磷脂型季铵盐都属于新一代的柔软剂产品。但是,作为贴身内衣用或者婴儿服饰用面料,除了要具备柔软平滑手感更需兼顾完全健康零刺激的理念,上述柔软剂虽然有良好软化功能也兼具生物可降解性,但是都会有少量毒害物质的残留,对人体健康会产生极大影响。
发明内容
为了解决现有技术中存在的上述技术问题,本发明的目的在于提供一种环保型柔软剂,该环保型柔软剂采用可食无毒性原料加工而成,适用于各种织物的柔软处理,尤其适用于贴身衣物或婴儿服装面料加工时的软化,且该环保型柔软剂不会在布料中残留有毒物质,使用时更加安全。
本发明的目的是通过以下技术方案实现的:适用于贴身织物的环保型柔软剂,由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30: 4.45~5.72: 2.55~3.28:61~63。
进一步的,蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.09:2.91:62。
进一步的,蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:4.45:2.55:63。
进一步的,蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.72:3.28:61。
本发明还公开了一种适用于贴身织物的环保型柔软剂的制备方法,包括以下步骤:
a、将所取乳化剂1309和span80进行混合,充分搅拌至均匀;
b、在搅拌条件下,将所取蔗糖聚酯缓慢加到步骤a中所得混合液中,充分搅拌混合均匀;
c、在恒定乳化温度(80℃)下,在高速(10000r/min)剪切的同时,将所取去离子水在1min中内缓慢加入到步骤b所得的混合液中,共高速剪切3分钟后即可制得所述产品。
本发明柔软剂处理织物的方法可以采用浸轧法:
浸轧工艺:在室温下,将漂染后的织物,经浸轧(10-30g/L,二浸二轧,带液率80%~100%)后取出,然后脱水处理,最后80~100℃烘干即可。
本发明的有益效果在于:该环保柔软剂可以对化纤、棉纺等各类布料进行较好的软化,该环保柔软剂使用时无毒害、无不良刺激、绿色环保,可以作为贴身内衣面料或婴儿服饰的软化剂使用,而且该环保柔软剂可以对生活中多种原因造成的布料硬化,进行柔软,完全无毒害。
具体实施方式
实施例1
适用于贴身面料织物的环保型柔软剂,是由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.09:2.91:62。
制备的所述适用于贴身织物的环保型柔软剂的方法,包括以下步骤:
a、将所取1309乳化剂和span80乳化剂进行混合,充分搅拌至均匀;
b、在搅拌条件下,将所取蔗糖聚酯缓慢加到步骤a中所得混合液中,充分搅拌混合均匀;
c、在恒定乳化温度(80℃)下,在高速(10000r/min)剪切的同时,将所取去离子水在1min中内缓慢加入到步骤b所得的混合液中,共高速剪切3分钟后即可制得所述产品。
实施例2
适用于贴身面料织物的环保型柔软剂,是由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:4.45:2.55:63。其它同实施例1。
实施例3
适用于贴身面料织物的环保型柔软剂,是由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.72:3.28:61。其它同实施例1。
本发明柔软剂处理织物的方法可以采用浸轧法:在室温下,将漂染后的织物,经浸轧(10-30g/L,二浸二轧,带液率80%~100%)后取出,然后脱水处理,最后80~100℃烘干即可。

Claims (5)

1.适用于贴身织物的环保型柔软剂,其特征在于:由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30: 4.45~5.72: 2.55~3.28:61~63。
2.如权利要求1所述的适用于贴身织物的环保型柔软剂,其特征在于:由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.09:2.91:62。
3.如权利要求1所述的适用于贴身织物的环保型柔软剂,其特征在于:由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:4.45:2.55:63。
4.如权利要求1所述的适用于贴身织物的环保型柔软剂,其特征在于:由下述原料按重量份数比制备而成:蔗糖聚酯(酯化度n = 6-8):乳化剂1309(异构十三醇与环氧乙烷缩合物):span80(失水山梨糖醇单油酸酯):去离子水 = 30:5.72:3.28:61。
5.如权利要求1-4之一的适用于贴身织物的环保型柔软剂的制备方法,包括以下步骤:
a、将所取乳化剂1309和span80进行混合,充分搅拌至均匀;
b、在搅拌条件下,将所取蔗糖聚酯缓慢加到步骤a中所得混合液中,充分搅拌混合均匀;
c、在恒定乳化温度(80℃)下,在高速(10000r/min)剪切的同时,将所取去离子水在1min中内缓慢加入到步骤b所得的混合液中,共高速剪切3分钟后即可制得所述产品。
CN201410580376.4A 2014-10-27 2014-10-27 一种适用于贴身织物的环保型柔软剂及其制备方法 Pending CN104342931A (zh)