CN104264797A - 建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法 - Google Patents

建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法 Download PDF

Info

Publication number
CN104264797A
CN104264797A CN201410436639.4A CN201410436639A CN104264797A CN 104264797 A CN104264797 A CN 104264797A CN 201410436639 A CN201410436639 A CN 201410436639A CN 104264797 A CN104264797 A CN 104264797A
Authority
CN
China
Prior art keywords
bolt hole
hole
aperture
polymer cement
cleaning
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410436639.4A
Other languages
English (en)
Other versions
CN104264797B (zh
Inventor
陈超
李兆龙
贾杨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhongqing Jianan Construction Group Co Ltd
Qingdao Zhongjia Construction Group Co Ltd
Original Assignee
Qingdao Jianan Construction Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Qingdao Jianan Construction Group Co Ltd filed Critical Qingdao Jianan Construction Group Co Ltd
Priority to CN201410436639.4A priority Critical patent/CN104264797B/zh
Publication of CN104264797A publication Critical patent/CN104264797A/zh
Application granted granted Critical
Publication of CN104264797B publication Critical patent/CN104264797B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开一种建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法,包括如下步骤;(1)对剪力墙螺栓孔的内、外侧孔口进行剔凿,使之形成“V”型口,清理后冲水润湿,孔内表面无明水时,用聚合物水泥防水砂浆对外侧孔口进行封堵,压实抹平;(2)外侧孔口的聚合物水泥防水砂浆达到三天强度后,对螺栓孔进行精细清理;(3)螺栓孔植筋完成48小时后,检查封堵螺栓孔外侧孔口的聚合物水泥防水砂浆是否有松动,完成后将内侧孔口用聚合物水泥防水砂浆封堵、抹平;(4)采用热熔铺贴法,使SBS卷材底面的沥青熔化,与基层处理剂粘结牢固。本发明所公开的防渗施工方法,操作简单,通过四层防水阻断处理措施,有效避免建筑外墙螺栓孔渗水。

Description

建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法
技术领域
本发明涉及一种建筑孔洞防渗漏施工方法,尤其涉及建筑外墙剪力墙模板螺栓孔防水封堵施工技术。
背景技术
在框剪结构建筑施工中,在剪力墙模板支设过程中为保证模板强度和刚度,防止浇筑混凝土过程中出现涨模、漏浆、模板变形等质量事故的发生,采用对拉螺栓加固是必须的手段和措施。同时为了加快施工进度和施工便捷,目前施工单位普遍采用加套管可重复使用的对拉螺栓。从而造成剪力墙对拉螺栓部位产生人为孔洞。若采用常规砂浆封堵方法,极易发生外墙渗漏现象,影响使用功能和美观。
发明内容
本发明所要解决的技术问题就是提供一种有效防止建筑外墙螺栓孔渗水的施工方法
本发明采用如下技术方案:
一种建筑外墙螺栓孔防渗施工方法,包括如下步骤:
(1)对剪力墙螺栓孔的内、外侧孔口进行剔凿,使之形成“V”型口,清理后冲水润湿,孔口表面无明水时,用聚合物水泥防水砂浆对外侧孔口进行封堵,压实抹平;
(2)外侧孔口的聚合物水泥防水砂浆达到三天强度后,对螺栓孔进行精细清理,清除孔内垃圾及浮灰;清洗后将微膨胀型化学胶粘剂注入孔内,然后将预先制作的直段钢筋植入孔内,使孔内饱满;
(3)螺栓孔植筋完成48小时后,检查封堵螺栓孔外侧孔口的聚合物水泥防水砂浆是否有松动,如有松动及时修补,完成后将螺栓孔内侧孔口外溢的胶粘剂清理干净,并用清水湿润内侧孔口,完成后将内侧孔口用聚合物水泥防水砂浆封堵、抹平;
(4)将螺栓孔外侧孔口周围的基层浮浆、杂物清理干净,并且外侧孔口周围200mm范围内剪力墙表面平整无凸凹、干燥、含水量不大于9%,完成后在外侧孔口均匀涂刷基层处理剂,待基层处理剂干燥后,将SBS卷材进行定位,采用热熔铺贴法,使SBS卷材底面的沥青熔化,与基层处理剂粘结牢固。
进一步的,在步骤(1)中,利用外脚手架作为施工操作平台。
进一步的,在步骤(1)中,用棕毛刷清理“V”型口。
进一步的,在步骤(2)中,对螺栓孔进行精细清理包括采用压缩空气进行反复3—5次清理,清除孔内垃圾;然后用棉布或毛刷将孔壁浮灰擦净。
进一步的,在步骤(2)中,采用手动注浆机将微膨胀型化学胶粘剂注入孔内。
进一步的,在步骤(2)中,注胶量为孔体积的50%。
进一步的,在步骤(2)中,植入钢筋长度等于剪力墙厚度减60mm,钢筋表面浮锈应清理干净,露出金属光泽。
进一步的,在步骤(4)中,SBS卷材为150mm×150mm的小块。
进一步的,在步骤(4)中,点燃火焰喷枪或喷灯烘烤SBS卷材底面与基层处理剂的交接处,使SBS卷材底面的沥青熔化。
进一步的,在步骤(4)中,块型SBS卷材周边应采取碾压措施。
本发明的有益效果是:
本发明所公开的建筑外墙螺栓孔防渗施工方法,操作简单,通过四层防水阻断处理措施,有效避免建筑外墙螺栓孔渗水。
附图说明
图1是使用本发明实施例1所公开的施工方法处理后的建筑外墙螺栓孔的剖面图。
具体实施方式
为了使本发明的目的、技术方案及优点更加清楚明白,以下结合附图和实施例,对本发明进行进一步详细说明。应当理解,此处所描述的具体实施例仅仅用以解释本发明,并不用于限定本发明。
实施例1,请参照图1,本实施例公开了一种建筑外墙螺栓孔防渗施工方法,包括如下步骤:
(1)对剪力墙1螺栓孔的内、外侧孔口进行剔凿,使之形成“V”型口,清理后冲水润湿,孔口表面无明水时,用聚合物水泥防水砂浆2对外侧孔口进行封堵,压实抹平;
在步骤(1)中,利用外脚手架作为施工操作平台。
在步骤(1)中,用棕毛刷清理“V”型口。
在步骤(1)中,“V”型口可以加大聚合物水泥防水砂浆与剪力墙的接触面积,提高封堵强度及效果。
(2)外侧孔口的聚合物水泥防水砂浆达到三天强度后,对螺栓孔进行精细清理,清除孔内垃圾及浮灰;清洗后将微膨胀型化学胶粘剂3注入孔内,然后将预先制作的直段钢筋4植入孔内,使孔内饱满;
在步骤(2)中,对螺栓孔进行精细清理包括采用压缩空气进行反复3—5次清理,清除孔内垃圾;然后用棉布或毛刷将孔壁浮灰擦净。
在步骤(2)中,采用手动注浆机将微膨胀型化学胶粘剂注入孔内。
在步骤(2)中,注胶量为孔体积的50%。
在步骤(2)中,植入钢筋长度等于剪力墙厚度减60mm,钢筋表面浮锈应清理干净,露出金属光泽。
(3)螺栓孔植筋完成48小时后,检查封堵螺栓孔外侧孔口的聚合物水泥防水砂浆是否有松动,如有松动及时修补,完成后将螺栓孔内侧孔口外溢的胶粘剂清理干净,并用清水湿润内侧孔口,完成后将内侧孔口用聚合物水泥防水砂浆2封堵、抹平;
(4)将螺栓孔外侧孔口周围的基层浮浆、杂物清理干净,并且外侧孔口周围200mm范围内剪力墙表面平整无凸凹、干燥、含水量不大于9%,完成后在外侧孔口均匀涂刷基层处理剂,待基层处理剂干燥后,将SBS卷材5进行定位,采用热熔铺贴法,使SBS卷材底面的沥青熔化,与基层处理剂粘结牢固。
在步骤(4)中,SBS卷材为150mm×150mm的小块。
在步骤(4)中,点燃火焰喷枪或喷灯烘烤SBS卷材底面与基层处理剂的交接处,使SBS卷材底面的沥青熔化。
在步骤(4)中,块型SBS卷材周边应采取碾压措施。

Claims (2)

1.一种建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法,其特征在于,包括如下步骤:
(1)对剪力墙螺栓孔的内、外侧孔口进行剔凿,使之形成“V”型口,清理后冲水润湿,孔内表面无明水时,用聚合物水泥防水砂浆对外侧孔口进行封堵,压实抹平;
(2)外侧孔口的聚合物水泥防水砂浆达到三天强度后,对螺栓孔进行精细清理,包括采用压缩空气进行反复3-5次清理,清除孔内垃圾;然后用棉布或毛刷将孔壁浮灰擦净,清除孔内垃圾及浮灰;清洗后将微膨胀型化学胶粘剂注入孔内,采用手动注浆机将微膨胀型化学胶粘剂注入孔内,注胶量为孔体积的50%,然后将预先制作的直段钢筋植入孔内,使孔内饱满;
(3)螺栓孔植筋完成48小时后,检查封堵螺栓孔外侧孔口的聚合物水泥防水砂浆是否有松动,如有松动及时修补,完成后将螺栓孔内侧孔口外溢的胶粘剂清理干净,并用清水湿润内侧孔口,完成后将内侧孔口用聚合物水泥防水砂浆封堵、抹平;
(4)将螺栓孔外侧孔口周围的基层浮浆、杂物清理干净,并且外侧孔口周围200mm范围内剪力墙表面平整无凸凹、干燥、含水量不大于9%,完成后在外侧孔口均匀涂刷基层处理剂,待基层处理剂干燥后,将SBS卷材进行定位,采用热熔铺贴法,使SBS卷材底面的沥青熔化,与基层处理剂粘结牢固。
2.根据权利要求1所述的建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法,其特征在于:在步骤(2)中,植入钢筋长度等于剪力墙厚度减60mm,钢筋表面浮锈应清理干净,露出金属光泽。
CN201410436639.4A 2013-06-26 2013-06-26 建筑外墙采用微膨胀型化学胶粘剂的螺栓孔防渗施工方法 Active CN104264797B (zh)