CN104262877A - 一种耐老化亚克力树脂及其制备方法 - Google Patents

一种耐老化亚克力树脂及其制备方法 Download PDF

Info

Publication number
CN104262877A
CN104262877A CN201410457590.0A CN201410457590A CN104262877A CN 104262877 A CN104262877 A CN 104262877A CN 201410457590 A CN201410457590 A CN 201410457590A CN 104262877 A CN104262877 A CN 104262877A
Authority
CN
China
Prior art keywords
parts
powder
acryl resin
ageing
butadiene
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410457590.0A
Other languages
English (en)
Other versions
CN104262877B (zh
Inventor
戴晓宸
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Zhu new materials Co., Ltd.
Original Assignee
Suzhou Yunshu New Material Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Yunshu New Material Technology Co Ltd filed Critical Suzhou Yunshu New Material Technology Co Ltd
Priority to CN201410457590.0A priority Critical patent/CN104262877B/zh
Publication of CN104262877A publication Critical patent/CN104262877A/zh
Application granted granted Critical
Publication of CN104262877B publication Critical patent/CN104262877B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种耐老化亚克力树脂及其制备方法,耐老化亚克力树脂包括按照质量份数计的如下原料:亚克力树脂粉80-89份、有机硅树脂18-22份、甲基丙烯酸-丁二烯-苯乙烯共聚物10-13份、柠檬酸三甲酯10-15份、滑石粉8-10份、硅微粉8-10份、马来酸酐1-5份。本发明将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉、硅微粉和马来酸酐合理复配,所得耐老化亚克力树脂具有优良的耐老化性和耐磨性。

Description

一种耐老化亚克力树脂及其制备方法
技术领域
 本发明属于高分子材料领域,具体涉及一种耐老化亚克力树脂及其制备方法。
背景技术
亚克力,化学名称为聚甲基丙烯酸甲酯,其透明度如同玻璃一般。亚克力具有较好的化学稳定性、易染色、易加工及优美的外观而广受人们喜爱。现有的亚克力虽具有上述优点,但是其耐老化和耐磨性能不佳,在一定程度上影响了亚克力树脂的使用。
综上所述,如何克服现有技术的不足已成为现有领域亟待解决的问题。
发明内容
本发明的目的是克服现有技术的不足而提出一种耐老化亚克力树脂及其制备方法,本发明耐老化亚克力树脂具有优良的耐老化性和耐磨性。
本发明的技术方案如下:
一种耐老化亚克力树脂,包括按照质量份数计的如下原料:亚克力树脂粉80-89份、有机硅树脂18-22份、甲基丙烯酸-丁二烯-苯乙烯共聚物10-13份、柠檬酸三甲酯10-15份、滑石粉8-10份、硅微粉8-10份、马来酸酐1-5份。
作为优选,所述的耐老化亚克力树脂,包括按照质量份数计的如下原料:亚克力树脂粉86份、有机硅树脂20份、甲基丙烯酸-丁二烯-苯乙烯共聚物12份、柠檬酸三甲酯13份、滑石粉9份、硅微粉9份、马来酸酐3份。
一种耐老化亚克力树脂的制备方法,包括以下步骤:按照质量配比称取各原料,将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉硅微粉和马来酸酐加入高速搅拌机中搅拌混合均匀,送至挤出机挤出,挤出机温度控制在150-165℃,即得耐老化亚克力树脂。
有益效果:本发明将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉、硅微粉和马来酸酐合理复配,所得耐老化亚克力树脂具有优良的耐老化性和耐磨性。
具体实施方式
本发明中的亚克力树脂粉为Extec 14562。
下面结合具体实施方式对本发明作进一步详细说明。
实施例1
一种耐老化亚克力树脂,包括按照质量份数计的如下原料:亚克力树脂粉80份、有机硅树脂18份、甲基丙烯酸-丁二烯-苯乙烯共聚物10份、柠檬酸三甲酯10份、滑石粉8份、硅微粉8份、马来酸酐1-5份。
本实施例的制备方法,包括以下步骤:按照质量配比称取各原料,将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉硅微粉和马来酸酐加入高速搅拌机中搅拌混合均匀,送至挤出机挤出,挤出机温度控制在150℃,即得耐老化亚克力树脂。
将该实施例所得成品进行性能检测,检测结果见表1。
实施例2
一种耐老化亚克力树脂,包括按照质量份数计的如下原料:亚克力树脂粉89份、有机硅树脂22份、甲基丙烯酸-丁二烯-苯乙烯共聚物13份、柠檬酸三甲酯15份、滑石粉10份、硅微粉10份、马来酸酐5份。
本实施例的制备方法,包括以下步骤:按照质量配比称取各原料,将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉硅微粉和马来酸酐加入高速搅拌机中搅拌混合均匀,送至挤出机挤出,挤出机温度控制在165℃,即得耐老化亚克力树脂。
将该实施例所得成品进行性能检测,检测结果见表1。
实施例3
一种耐老化亚克力树脂,包括按照质量份数计的如下原料:亚克力树脂粉86份、有机硅树脂20份、甲基丙烯酸-丁二烯-苯乙烯共聚物12份、柠檬酸三甲酯13份、滑石粉9份、硅微粉9份、马来酸酐3份。
本实施例的制备方法,包括以下步骤:按照质量配比称取各原料,将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉硅微粉和马来酸酐加入高速搅拌机中搅拌混合均匀,送至挤出机挤出,挤出机温度控制在160℃,即得耐老化亚克力树脂。
 
将实施例1-3所得成品进行性能测试,耐候性测试:GB/T 16422.1,氙灯老化;结果如下表1:
表1 性能测试数据
性能 实施例1 实施例2 实施例3
耐候性 800h无变化 800h无变化 800h无变化
由上表可见,本发明所得成品具有良好的耐老化性能。
上述实施例仅是对本发明产品的说明,并非对本发明做出任何形式上的限制,在不脱离本发明的技术方案范围之内,任何利用上述揭示的技术内容作出简单变换的等同方案,均属本发明的保护范围。

Claims (3)

1.一种耐老化亚克力树脂,其特征在于,包括按照质量份数计的如下原料:亚克力树脂粉80-89份、有机硅树脂18-22份、甲基丙烯酸-丁二烯-苯乙烯共聚物10-13份、柠檬酸三甲酯10-15份、滑石粉8-10份、硅微粉8-10份、马来酸酐1-5份。
2.根据权利要求1所述的耐老化亚克力树脂,其特征在于,包括按照质量份数计的如下原料:亚克力树脂粉86份、有机硅树脂20份、甲基丙烯酸-丁二烯-苯乙烯共聚物12份、柠檬酸三甲酯13份、滑石粉9份、硅微粉9份、马来酸酐3份。
3.一种耐老化亚克力树脂的制备方法,其特征在于,包括以下步骤:按照质量配比称取各原料,将亚克力树脂粉、有机硅树脂、甲基丙烯酸-丁二烯-苯乙烯共聚物、柠檬酸三甲酯、滑石粉硅微粉和马来酸酐加入高速搅拌机中搅拌混合均匀,送至挤出机挤出,挤出机温度控制在150-165℃,即得耐老化亚克力树脂。
CN201410457590.0A 2014-09-10 2014-09-10 一种耐老化亚克力树脂及其制备方法 Expired - Fee Related CN104262877B (zh)