CN104043807B - Storage battery polar group cast welding straight column type manpower-free passes a bridge mould - Google Patents

Storage battery polar group cast welding straight column type manpower-free passes a bridge mould Download PDF

Info

Publication number
CN104043807B
CN104043807B CN201410317390.5A CN201410317390A CN104043807B CN 104043807 B CN104043807 B CN 104043807B CN 201410317390 A CN201410317390 A CN 201410317390A CN 104043807 B CN104043807 B CN 104043807B
Authority
CN
China
Prior art keywords
groove
manifold groove
manifold
row
mould
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201410317390.5A
Other languages
Chinese (zh)
Other versions
CN104043807A (en
Inventor
陈隐嵩
陈国刚
张小瑞
吴杰明
李岳云
游立强
叶宁
陈翔
陈华毅
张磊
周友盛
沈祎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Fujian Yaheng Mechanical Ltd By Share Ltd
Original Assignee
Fujian Jianyang Yaheng Machinery Manufacturing Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Fujian Jianyang Yaheng Machinery Manufacturing Co Ltd filed Critical Fujian Jianyang Yaheng Machinery Manufacturing Co Ltd
Priority to CN201410317390.5A priority Critical patent/CN104043807B/en
Publication of CN104043807A publication Critical patent/CN104043807A/en
Application granted granted Critical
Publication of CN104043807B publication Critical patent/CN104043807B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of storage battery polar group cast welding straight column type manpower-free to pass a bridge mould.The object of the present invention is to provide that a kind of demoulding is easy, die cost is low, leady raw materials consumption is little, easy to use and can directly cast and there is storage battery polar group cast welding straight column type manpower-free that vertical shape passes a bridge to pass a bridge mould, be provided with some groups of lug collecting tray groups in the front of mould, described lug collecting tray group comprises two rows the first manifold groove row arranged in parallel and the second manifold groove row; Described manifold groove unit comprises two transverse concave grooves and " U " font groove for connecting these two transverse concave grooves, and the middle part of described " U " font groove is provided with one in vertical block, and " U " font groove is divided into " U " shape tube passage by block; In lug collecting tray group, being provided with can the core rod movable block of lateral sliding, and described block is separately fixed on its corresponding core rod movable block with core rod movable block lateral sliding.

Description

Storage battery polar group cast welding straight column type manpower-free passes a bridge mould
Technical field
The present invention relates to a kind of storage battery polar group cast welding straight column type manpower-free to pass a bridge mould.
Background technology
Existing lead-acid accumulator has the pole group be made up of some positive plates and some negative plates usually, and the anode ear in the group of pole is connected respectively by cylinder manifold with negative electrode lug.The manual bus-bar of the main employing of weldering that helps of current lead acid accumulator pole group welds; The operation of manual bus-bar welding is: manual combo, mounted box, pole group are inverted in and help on welding mould, then help weldering cylinder manifold.Help the cylinder manifold that welds so not only the demoulding is difficult but also both positive and negative polarity column cap on bus-bar after the demoulding also needs to carry out welding by artificial mode and forms gap bridge.The method is both time-consuming, and effect is low, and causes quality unreliable due to artificial factor, and operating environment is polluted large, is both unfavorable for environmental protection, and is harmful to again the healthy of operative employee.
Applicant devised more early and a kind ofly helps welding mould patent (patent No.: 201120522378X) for the manufacture of lead-acid accumulator, and this mould is also the storage cell electrode group cast welding mould that manpower-free passes a bridge.But this technology is before the demoulding, column cap and gap bridge are not board erected state (relative to accumulator pole groups), need in knockout course, gap bridge groove part need in the effect bottom knockout of certain knockout press, to realize passing a bridge and vertically the erecting of column cap.This technology is in knockout course, and need to hold very good to the temperature spot of column cap during the demoulding, too high or too low temperature all cannot deviate from qualified gap bridge, easily produces waste product.
Summary of the invention
The object of the present invention is to provide that a kind of demoulding is easy, die cost is low, leady raw materials consumption is little, easy to use and can directly cast and there is storage battery polar group cast welding straight column type manpower-free that vertical shape passes a bridge to pass a bridge mould.
Object of the present invention is achieved through the following technical solutions: a kind of storage battery polar group cast welding straight column type manpower-free passes a bridge mould, be provided with some groups of lug collecting tray groups in the front of mould, described lug collecting tray group comprises two rows the first manifold groove row arranged in parallel and the second manifold groove row;
Described first manifold groove row and the second manifold groove row include several manifold groove unit of spaced setting;
Described manifold groove unit comprises two transverse concave grooves and " U " font groove for connecting these two transverse concave grooves, and the middle part of described " U " font groove is provided with one in vertical block, and " U " font groove is divided into " U " shape tube passage by block;
Described first manifold groove row is also separately positioned on anode ear manifold groove unit and the negative electrode lug manifold groove unit at its two ends, described anode ear manifold groove unit comprises a transverse concave groove and anode ear groove, and described negative electrode lug manifold groove unit comprises a transverse concave groove and negative electrode lug groove;
In lug collecting tray group, the outside that described first manifold groove row and the second manifold groove are arranged is equipped with one piece can the core rod movable block of lateral sliding, two pieces of core rod movable blocks are respectively as the groove outer webs of the manifold groove unit of the first manifold groove row and the second manifold groove row, and the block that described first manifold groove row and the second manifold groove are arranged is separately fixed on its corresponding core rod movable block with core rod movable block lateral sliding.
Further, become to misplace between the manifold groove unit that manifold groove unit and second manifold groove of described first manifold groove row are arranged, symmetrical.
Further, described mould is also provided with several condensation water channels.
Described condensation water channel is arranged between the first manifold groove row and the second manifold groove row.
During use, core rod movable block is compressed and is attached on manifold groove unit, make manifold groove unit become a closed cell body; Then in manifold groove unit, anode ear manifold groove unit and negative electrode lug manifold groove unit, cast welding liquation is injected, " U " shape tube passage that liquation injects each transverse concave groove, anode ear groove, negative electrode lug groove and is divided into by block; Again the lug correspondence of pole group is imbedded respectively in manifold groove unit, anode ear manifold groove unit or negative electrode lug manifold groove unit, and then the cast welding liquation led in condensed water to each groove at condensation water channel solidifies, finally core rod movable block is gone out to side slip, pole group is taken out.
Compared to prior art, the invention has the advantages that: owing to decreasing the program that manual welding is passed a bridge, thus can avoid workman human weld process be subject to lead fume to the infringement of human body, reduce environmental pollution.Owing to adopting mould once to help the type of being welded into, overcome the unstability of the quality that human weld produces, therefore improve product quality; And mould also can become thinner, die cost also becomes and more saves, and welding fabrication, directly by condensed water condensation, can realize cooling fast and fast demoulding.
Accompanying drawing explanation
Fig. 1 is the structural representation of an embodiment of the present invention.
Fig. 2 is the top view of Fig. 1.
Fig. 3 be in Fig. 2 A to structure sectional view.
Label declaration: 651 first manifold groove rows, 652 second manifold groove rows, 653 manifold groove unit, 654 transverse concave grooves, 655 " U " font groove, 656 blocks, 657 anode ear manifold groove unit, 658 negative electrode lug manifold groove unit, 659 anode ear grooves, 660 negative electrode lug grooves, 661 core rod movable blocks, 662 condensation water channels.
Detailed description of the invention
It should be noted that, the outside described in the present embodiment, inner side be in lug collecting tray group first manifold groove row 651 and second manifold groove row 652 center line centered by carry out stating.
Below in conjunction with Figure of description and embodiment, content of the present invention is described in detail:
As Fig. 1,2 and Figure 3 shows that a kind of storage battery polar group cast welding straight column type manpower-free provided by the invention passes a bridge the embodiment schematic diagram of mould.As shown in Figure 1, be provided with some groups of lug collecting tray groups in the front of mould, described lug collecting tray group comprises two rows the first manifold groove row 651 arranged in parallel and the second manifold groove row 652;
Described first manifold groove row 651 and the second manifold groove row 652 include several manifold groove unit 653 of spaced setting;
Described manifold groove unit 653 comprises two transverse concave grooves 654 and " U " font groove 655 for connecting these two transverse concave grooves 654, the middle part of described " U " font groove 655 is provided with one in vertical block 656, and " U " font groove 655 is divided into " U " shape tube passage by block 656;
Described first manifold groove row 651 is also separately positioned on anode ear manifold groove unit 657 and the negative electrode lug manifold groove unit 658 at its two ends, described anode ear manifold groove unit 657 comprises a transverse concave groove 654 and anode ear groove 659, and described negative electrode lug manifold groove unit 658 comprises a transverse concave groove 654 and negative electrode lug groove 660;
In lug collecting tray group, the outside of described first manifold groove row 651 and the second manifold groove row 652 is equipped with one piece can the core rod movable block 661 of lateral sliding, two pieces of core rod movable blocks 661 are respectively as the groove outer webs of the manifold groove unit 653 of the first manifold groove row 651 and the second manifold groove row 652, and the block 656 of described first manifold groove row 651 and the second manifold groove row 652 is separately fixed on its corresponding core rod movable block 661 with core rod movable block 661 lateral sliding.
When core rod movable block 661 be pressed in the first/bis-manifold groove row manifold groove unit 653 on time, core rod movable block 661 is pressed on the side of manifold groove unit 653, each manifold groove unit 653 to be closed into a complete groove, be convenient to manifold groove unit 653 and hold cast welding liquation.So after cast welding liquation solidifies, the pole group that " U " font groove 655 be positioned on block 656 can be frozen into " U " shape tubular type passes a bridge, for the ease of this gap bridge not stopped by block 656 from during mould separating with pole group, block 656 is fixed on core rod movable block 661, with core rod movable block 661 to being displaced sideways, block 656 can be allowed from U " the pole group of shape tubular type passes a bridge and separates.
Further, in order to accelerate the cooled and solidified speed of cast welding liquation, described mould is also provided with several condensation water channels 662; Described condensation water channel 662 is arranged between the first manifold groove row 651 and the second manifold groove row 652.
As shown in Figure 1, become to misplace between the manifold groove unit 653 that manifold groove unit 653 and second manifold groove of described first manifold groove row 651 arrange 652, symmetrical.Described dislocation is symmetrical to be referred to: in first row manifold groove row, " U " font groove 655 of a manifold groove unit 653 is just to the pars intermedia bit line of two adjacent manifold groove unit in second row manifold groove row 653 (or positive/negative lug manifold groove unit 658 be adjacent a manifold groove unit 653); Same, in second row manifold groove, " U " font groove 655 of manifold groove unit 653 is just to the pars intermedia bit line of two adjacent manifold groove unit 653 in first row manifold groove row, and the manifold groove row forming first row thus arranges with the manifold groove of second row and is dislocatedly distributed.

Claims (4)

1. a storage battery polar group cast welding straight column type manpower-free passes a bridge mould, it is characterized in that: be provided with some groups of lug collecting tray groups in the front of mould, described lug collecting tray group comprises two rows the first manifold groove row (651) arranged in parallel and the second manifold groove row (652);
Described first manifold groove row (651) and the second manifold groove row (652) include several manifold groove unit (653) of spaced setting;
Described manifold groove unit (653) comprises two transverse concave grooves (654) and " U " font groove (655) for connecting these two transverse concave grooves (654), the middle part of described " U " font groove (655) is provided with one in vertical block (656), and " U " font groove (655) is divided into " U " shape tube passage by block (656);
Described first manifold groove row (651) is also separately positioned on anode ear manifold groove unit (657) and the negative electrode lug manifold groove unit (658) at its two ends, described anode ear manifold groove unit (657) comprises a transverse concave groove (654) and anode ear groove (659), and described negative electrode lug manifold groove unit (658) comprises a transverse concave groove (654) and negative electrode lug groove (660);
In lug collecting tray group, described first manifold groove row (651) and the second manifold groove arrange the outside of (652) be equipped with one piece can the core rod movable block (661) of lateral sliding, two pieces of core rod movable blocks (661) arrange the groove outer webs of the manifold groove unit (653) of (651) and the second manifold groove row (652) respectively as the first manifold groove, described first manifold groove row (651) and the second manifold groove are arranged the block (656) of (652) and are separately fixed on its corresponding core rod movable block (661) with core rod movable block (661) lateral sliding.
2. storage battery polar group cast welding straight column type manpower-free according to claim 1 passes a bridge mould, it is characterized in that: described mould is also provided with several condensation water channels (662).
3. storage battery polar group cast welding straight column type manpower-free according to claim 2 passes a bridge mould, it is characterized in that: described condensation water channel (662) is arranged on the first manifold groove row (651) and the second manifold groove is arranged between (652).
4. storage battery polar group cast welding straight column type manpower-free according to claim 1 passes a bridge mould, it is characterized in that: become to misplace between the manifold groove unit (653) of described first manifold groove row (651) arranges (652) manifold groove unit (653) with the second manifold groove, symmetrical.
CN201410317390.5A 2014-07-05 2014-07-05 Storage battery polar group cast welding straight column type manpower-free passes a bridge mould Expired - Fee Related CN104043807B (en)