CN104016586A - 一种含硒粉的暖瓶瓶坯材料 - Google Patents

一种含硒粉的暖瓶瓶坯材料 Download PDF

Info

Publication number
CN104016586A
CN104016586A CN201410190441.2A CN201410190441A CN104016586A CN 104016586 A CN104016586 A CN 104016586A CN 201410190441 A CN201410190441 A CN 201410190441A CN 104016586 A CN104016586 A CN 104016586A
Authority
CN
China
Prior art keywords
parts
oxide
selenium powder
coal gangue
flyash
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410190441.2A
Other languages
English (en)
Other versions
CN104016586B (zh
Inventor
薛宗洪
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Chuanlin Agricultural Technology Co.,Ltd.
Original Assignee
薛宗洪
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 薛宗洪 filed Critical 薛宗洪
Priority to CN201410190441.2A priority Critical patent/CN104016586B/zh
Publication of CN104016586A publication Critical patent/CN104016586A/zh
Application granted granted Critical
Publication of CN104016586B publication Critical patent/CN104016586B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种含硒粉的暖瓶瓶坯材料,它是由下述重量份的原料组成的:石英石60-65、低铁煤矸石20-35、方解石10-15、二氧化硅6-10、氧化钠3-4、氧化锌1-3、石膏1-2、氧化钾2-4、氧化镁3-4、硼酸2-3、五氧化二钒1-2、明矾粉1-2、硒粉0.08-0.1、复合澄清助剂2-5。本发明的材料中加入的硒粉可以有效的改善成品的抗弯折、硬度、强度等物理性能,煤矸石来源丰富,使用煤矸石不仅可以降低成产成本,还可以节约土地资源,降低环境污染。

Description

一种含硒粉的暖瓶瓶坯材料
技术领域
    本发明主要涉及一种含硒粉的暖瓶瓶坯材料,属于玻璃材料领域。
背景技术
    传统的暖瓶瓶坯是以二氧化硅为主料,加入几种氧化物混合制成,机械强度不高,导致在使用、运输的过程中比较容易破裂、造成资源的浪费,有的热稳定性不强,无法长期适应沸水环境,不仅容易破裂,还有可能会损害到人身安全。
发明内容
本发明目的就是提供一种含硒粉的暖瓶瓶坯材料。
本发明是通过以下技术方案实现的:
一种含硒粉的暖瓶瓶坯材料,它是由下述重量份的原料组成的:
石英石60-65、低铁煤矸石20-35、方解石10-15、二氧化硅6-10、氧化钠3-4、氧化锌1-3、石膏1-2、氧化钾2-4、氧化镁3-4、硼酸2-3、五氧化二钒1-2、明矾粉1-2、硒粉0.08-0.1、复合澄清助剂2-5;
所述的低铁煤矸石的制备包括以下步骤:
将煤矸石加入到2-3倍的硫酸溶液中,所述硫酸的浓度为15-20%,在80-90℃下加热搅拌1-2小时,过滤,记滤渣为料a,在滤液中加入氢氧化钠,至溶液ph为8-9,过滤,烘干,将非白色的沉淀去除,得到的白色沉淀与上述料a混合,即得所述低铁煤矸石;
所述的复合澄清助剂是由下述重量份的原料组成的:
粉煤灰25-30、碳酸钠8-14、骨炭1-2、硝酸钡4-7、50-60%的硫酸100、三氧化二砷0.8-1;
(1)将粉煤灰经过高温煅烧后除铁,使得所选粉煤灰中的成分含量为
50%≤SiO2≤70%、30%≤AL2O3≤40%,余量为氧化钙、氧化镁、氧化钠、氧化钾等;
(2)将上述粉煤灰与碳酸钠混合研磨,放入马弗炉内800-850℃煅烧1-2小时,取出后与骨炭混合研磨,加入上述硫酸,搅拌混合,置于90-100℃水浴中加热1-2小时,出料冷却,放入烘箱内120-130℃下烘干,研磨至细度为1-2μm;
(3)将上述硝酸钡、三氧化二砷混合,球磨,过筛,得粒径0.5-1.5mm;
(4)将上述处理后的各原料混合,球磨充分,即得所述复合澄清助剂。
本发明的优点是:
本发明的材料中加入的硒粉具有很好的澄清和脱色效果,可以增强瓶坯的透明性,有效的改善成品的抗弯折、硬度、强度等物理性能,煤矸石来源丰富,使用煤矸石不仅可以降低成产成本,还可以节约土地资源,降低环境污染。
本发明使用的复合澄清助剂,通过粉煤灰与碳酸钠和硫酸的反应处理,使得烘干后的物料中含有硫酸铝、硅酸铝等,其中硅酸铝可以增强玻璃的热稳定性,满足暖瓶的热需求,硫酸铝在770℃下加热可分解出三氧化硫,未反应完全的粉煤灰中的各成分可以作为玻璃的基料,三氧化二砷与硝酸钡混合使用,放氧能力强,且在1300℃的时候依然具有很好的放氧效果,各气体可以在不同的时期进入熔融玻璃液的气泡中,使气泡体积不断增大上浮排出液面,加速气泡的排除,从而起到澄清作用。
具体实施方式
实施例1
一种含硒粉的暖瓶瓶坯材料,它是由下述重量份(公斤)的原料组成的:
石英石65、低铁煤矸石35、方解石15、二氧化硅10、氧化钠4、氧化锌1、石膏2、氧化钾2、氧化镁4、硼酸2、五氧化二钒1、明矾粉1、硒粉0.08、复合澄清助剂5;
所述的低铁煤矸石的制备包括以下步骤:
将煤矸石加入到3倍的硫酸溶液中,所述硫酸的浓度为20%,在80℃下加热搅拌1小时,过滤,记滤渣为料a,在滤液中加入氢氧化钠,至溶液ph为8,过滤,烘干,将非白色的沉淀去除,得到的白色沉淀与上述料a混合,即得所述低铁煤矸石;
所述的复合澄清助剂是由下述重量份的原料组成的:
粉煤灰30、碳酸钠14、骨炭2、硝酸钡7、60%的硫酸100、三氧化二砷0.8;
(1)将粉煤灰经过高温煅烧后除铁,使得所选粉煤灰中的成分含量为
50%≤SiO2≤70%、30%≤AL2O3≤40%,余量为氧化钙、氧化镁、氧化钠、氧化钾等;
(2)将上述粉煤灰与碳酸钠混合研磨,放入马弗炉内850℃煅烧2小时,取出后与骨炭混合研磨,加入上述硫酸,搅拌混合,置于100℃水浴中加热1小时,出料冷却,放入烘箱内130℃下烘干,研磨至细度为1μm;
(3)将上述硝酸钡、三氧化二砷混合,球磨,过筛,得粒径0.5-1.5mm;
(4)将上述处理后的各原料混合,球磨充分,即得所述复合澄清助剂。
耐热急变性能测试:
将用本发明的瓶坯材料制得的暖瓶启口在环境温度下保持30min以上,灌沸水至满溢,维持1min,在不多于10s的时间倒去热水,立刻灌入5℃的冷水,至满溢,放置30s,倒出冷水,检查瓶胆有无开裂:
结果,无开裂。

Claims (1)

1.一种含硒粉的暖瓶瓶坯材料,其特征在于它是由下述重量份的原料组成的:
石英石60-65、低铁煤矸石20-35、方解石10-15、二氧化硅6-10、氧化钠3-4、氧化锌1-3、石膏1-2、氧化钾2-4、氧化镁3-4、硼酸2-3、五氧化二钒1-2、明矾粉1-2、硒粉0.08-0.1、复合澄清助剂2-5;
所述的低铁煤矸石的制备包括以下步骤:
将煤矸石加入到2-3倍的硫酸溶液中,所述硫酸的浓度为15-20%,在80-90℃下加热搅拌1-2小时,过滤,记滤渣为料a,在滤液中加入氢氧化钠,至溶液ph为8-9,过滤,烘干,将非白色的沉淀去除,得到的白色沉淀与上述料a混合,即得所述低铁煤矸石;
所述的复合澄清助剂是由下述重量份的原料组成的:
粉煤灰25-30、碳酸钠8-14、骨炭1-2、硝酸钡4-7、50-60%的硫酸100、三氧化二砷0.8-1;
(1)将粉煤灰经过高温煅烧后除铁,使得所选粉煤灰中的成分含量为
50%≤SiO2≤70%、30%≤AL2O3≤40%,余量为氧化钙、氧化镁、氧化钠、氧化钾等;
(2)将上述粉煤灰与碳酸钠混合研磨,放入马弗炉内800-850℃煅烧1-2小时,取出后与骨炭混合研磨,加入上述硫酸,搅拌混合,置于90-100℃水浴中加热1-2小时,出料冷却,放入烘箱内120-130℃下烘干,研磨至细度为1-2μm;
(3)将上述硝酸钡、三氧化二砷混合,球磨,过筛,得粒径0.5-1.5mm;
(4)将上述处理后的各原料混合,球磨充分,即得所述复合澄清助剂。
CN201410190441.2A 2014-05-07 2014-05-07 一种含硒粉的暖瓶瓶坯材料 Active CN104016586B (zh)