CN103964761A - 一种抗裂水泥砂浆 - Google Patents

一种抗裂水泥砂浆 Download PDF

Info

Publication number
CN103964761A
CN103964761A CN201410133903.7A CN201410133903A CN103964761A CN 103964761 A CN103964761 A CN 103964761A CN 201410133903 A CN201410133903 A CN 201410133903A CN 103964761 A CN103964761 A CN 103964761A
Authority
CN
China
Prior art keywords
parts
cement
cracking
cement mortar
powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410133903.7A
Other languages
English (en)
Other versions
CN103964761B (zh
Inventor
黄裕兵
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Haimen tidelead new building materials Co. Ltd.
Original Assignee
黄裕兵
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 黄裕兵 filed Critical 黄裕兵
Priority to CN201410133903.7A priority Critical patent/CN103964761B/zh
Publication of CN103964761A publication Critical patent/CN103964761A/zh
Application granted granted Critical
Publication of CN103964761B publication Critical patent/CN103964761B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种抗裂水泥砂浆,按质量份包括以下原料:水泥35-40份;珍珠岩15-17份;聚氨酯硬泡颗粒7-10份;水性环氧乳液8-10份;矿渣粉14-20份;水泥防水剂5-7份;塑化粉4-7份;硬化剂3-5份;水25-45份。珍珠岩重量轻、不腐蚀,聚氨酯硬泡颗粒是一种保温材料,水性环氧乳液的耐磨性好,矿渣粉的抗裂性好,再加上水泥防水剂,起补偿收缩和张拉钢筋产生预应力以及充分填充水泥间隙的作用,塑化粉加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度,硬化剂能大大提高水泥砂浆的硬度。

Description

一种抗裂水泥砂浆
技术领域
本发明涉及一种水泥砂浆,尤其涉及一种抗裂水泥砂浆。
背景技术
水泥砂浆用于建筑工程等场所,如建房等。普通的水泥砂浆主要成分就是水泥和砂子,传统的水泥砂浆作为抹灰材料存在着裂缝、空鼓、粘结性能差等缺点,其次凝固硬化速度慢。因此,需要提供一种新的技术方案来解决上述问题。
发明内容
为解决上述问题,本发明提供一种抗裂水泥砂浆。
本发明采用的技术方案:
一种抗裂水泥砂浆,按质量份包括以下原料:
水泥 35-40份;
珍珠岩 15-17份;
聚氨酯硬泡颗粒 7-10份;
水性环氧乳液 8-10份;
矿渣粉 14-20份;
水泥防水剂 5-7份;
塑化粉 4-7份;
硬化剂 3-5份;
水 25-45份。
所述塑化粉为高岭土和α-烯基磺酸钠的混合物。
所述硬化剂为硬脂酸、氢氧化钠和氧化钙的混合物。
将矿渣投入到粉碎机中充分粉碎后,再经磨粉机充分打磨,经80-100目网,过筛后,得矿渣粉待用。
本发明的优点是:珍珠岩重量轻、不腐蚀,聚氨酯硬泡颗粒是一种保温材料,水性环氧乳液的耐磨性好,矿渣粉的抗裂性好,再加上水泥防水剂,起补偿收缩和张拉钢筋产生预应力以及充分填充水泥间隙的作用,塑化粉加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度,硬化剂能大大提高水泥砂浆的硬度。
具体实施方式
下述实施例仅用于说明本发明,但并不能限定本发明的保护范围。
实施例1
一种抗裂水泥砂浆,按质量份包括以下原料:
水泥 35份;
珍珠岩 15份;
聚氨酯硬泡颗粒 7份;
水性环氧乳液 8份;
矿渣粉 14份;
水泥防水剂 5份;
塑化粉 4份;
硬化剂 3份;
水 25份。
塑化粉为高岭土和α-烯基磺酸钠的混合物;硬化剂为硬脂酸、氢氧化钠和氧化钙的混合物;将矿渣投入到粉碎机中充分粉碎后,再经磨粉机充分打磨,经80目网,过筛后,得矿渣粉待用。
实施例2
一种抗裂水泥砂浆,按质量份包括以下原料:
水泥 38份;
珍珠岩 16份;
聚氨酯硬泡颗粒 8份;
水性环氧乳液 9份;
矿渣粉 17份;
水泥防水剂 6份;
塑化粉 5份;
硬化剂 4份;
水 30份。
塑化粉为高岭土和α-烯基磺酸钠的混合物;硬化剂为硬脂酸、氢氧化钠和氧化钙的混合物;将矿渣投入到粉碎机中充分粉碎后,再经磨粉机充分打磨,经90目网,过筛后,得矿渣粉待用。
实施例3
一种抗裂水泥砂浆,按质量份包括以下原料:
水泥 40份;
珍珠岩 17份;
聚氨酯硬泡颗粒 10份;
水性环氧乳液 10份;
矿渣粉 20份;
水泥防水剂 7份;
塑化粉 7份;
硬化剂 5份;
水 45份。
塑化粉为高岭土和α-烯基磺酸钠的混合物;硬化剂为硬脂酸、氢氧化钠和氧化钙的混合物;将矿渣投入到粉碎机中充分粉碎后,再经磨粉机充分打磨,经100目网,过筛后,得矿渣粉待用。
珍珠岩重量轻、不腐蚀,聚氨酯硬泡颗粒是一种保温材料,水性环氧乳液的耐磨性好,矿渣粉的抗裂性好,再加上水泥防水剂,加在水泥中,当水泥凝结硬化时,随之体积膨胀,起补偿收缩和张拉钢筋产生预应力以及充分填充水泥间隙的作用,塑化粉具有减水、引气、增稠、保水、增塑功能,加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度,硬化剂能大大提高水泥砂浆的硬度,用于地下水管、水池、水塔等建筑工程。

Claims (4)

1.一种抗裂水泥砂浆,其特征在于,按质量份包括以下原料:
水泥 35-40份;
珍珠岩 15-17份;
聚氨酯硬泡颗粒 7-10份;
水性环氧乳液 8-10份;
矿渣粉 14-20份;
水泥防水剂 5-7份;
塑化粉 4-7份;
硬化剂 3-5份;
水 25-45份。
2.根据权利要求1所述的一种抗裂水泥砂浆,其特征在于:所述塑化粉为高岭土和α-烯基磺酸钠的混合物。
3.根据权利要求1所述的一种抗裂水泥砂浆,其特征在于:所述硬化剂为硬脂酸、氢氧化钠和氧化钙的混合物。
4.根据权利要求1所述的一种抗裂水泥砂浆,其特征在于:将矿渣投入到粉碎机中充分粉碎后,再经磨粉机充分打磨,经80-100目网,过筛后,得矿渣粉待用。
CN201410133903.7A 2014-04-04 2014-04-04 一种抗裂水泥砂浆 Expired - Fee Related CN103964761B (zh)