CN103949456A - 一种防止露天堆放碱渣山扬尘的处理方法 - Google Patents

一种防止露天堆放碱渣山扬尘的处理方法 Download PDF

Info

Publication number
CN103949456A
CN103949456A CN201410139652.3A CN201410139652A CN103949456A CN 103949456 A CN103949456 A CN 103949456A CN 201410139652 A CN201410139652 A CN 201410139652A CN 103949456 A CN103949456 A CN 103949456A
Authority
CN
China
Prior art keywords
alkaline residue
mountain
residue mountain
airborne dust
processing method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201410139652.3A
Other languages
English (en)
Other versions
CN103949456B (zh
Inventor
严建华
庞保雪
谢尧生
张程浩
周朋
张东梅
柏晓强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Huzhou Nanxun Charm New Rural Construction Co.,Ltd.
Original Assignee
Beijing University of Technology
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Beijing University of Technology filed Critical Beijing University of Technology
Priority to CN201410139652.3A priority Critical patent/CN103949456B/zh
Publication of CN103949456A publication Critical patent/CN103949456A/zh
Application granted granted Critical
Publication of CN103949456B publication Critical patent/CN103949456B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种防止露天堆放碱渣山扬尘的处理方法,属于固体废弃物利用和环境保护领域。其技术特征是利用碱渣中的氯化物对活性硅酸盐粉体进行激发,使其表面形成水化硬壳层,从而起到防止扬尘的作用。其主要步骤是活性硅酸盐以一定比例和水混合,并在其中加入聚乙烯醇溶液,形成聚合物浆体,将该聚合物复合浆体喷于覆盖了防尘网的碱渣山表面。经过养护,使其在碱渣山表面形成一定厚度的水化硬壳层,起到防止碱渣山扬尘的作用。

Description

一种防止露天堆放碱渣山扬尘的处理方法
技术领域
本发明涉及一种防止露天堆放碱渣山扬尘的处理方法,属于固体废弃物利用和环境保护领域,
技术背景
碱渣是一种工业废渣,是氨碱法生产纯碱过程中排放的主要废弃物。目前,我国是世界上最大的纯碱生产国。据中国纯碱工业协会统计,2012年的纯碱产量为2401万吨,其中,氨碱法产量为1032万吨,占43%。氨碱法成产1吨纯碱会排放0.3-0.35吨的碱渣,依此推算,我国每年新增的碱渣在310-360万吨。碱渣中由于含有大量氯化物(16%左右)而难以处理。目前,其回收利用途径主要有:生产建材、制造化肥等,但用量均不大,碱厂处理碱渣的方法主要还是露天堆放。
由于碱渣粉体颗粒较细,其堆放过程中扬尘是一个重大问题,碱厂的碱渣以湿态排放,高度达十米以上甚至几十米,表面一旦风干就会产生较为严重的扬尘现象。若没有合理有效的防尘措施,在不利气象条件下,将导致严重的扬尘。目前,碱渣山的防治扬尘的措施有表面喷水防尘,用覆盖剂控制扬尘和封闭储存等。其中应用较为广泛的是喷水防尘,堆场附近要设置喷水、排水装置,并设置绿化带。但每天要洒水3次或洒化学抑尘剂以防止风蚀发生,且停止抑尘操作的间隔时间不得超过4天,处理扬尘问题耗费巨大。
具有水化活性的固体废弃物如矿渣、粉煤灰、硅灰等因其可受碱等的激发产生强度而在水泥混凝土中得到了广泛的应用。研究表明,氯化物如氯化钙等可使活性粉体激发而产生强度。由于碱渣中含有大量的氯化物,因而,当湿态或浆体形态存在的活性粉体和碱渣接触时,碱渣中的氯化物可通过扩散将活性粉体胶结而形成硬块。因而,在碱渣山上喷涂粉煤灰等浆体时,可在碱渣上表面起到遮盖作用,该层浆体还可以和塑料纤维网形成复合结构,起到复合表面增强的作用。
发明内容
本发明的目的旨在解决露天堆放的碱渣风干扬尘等问题。
一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,利用具有水化活性效应的固体废弃物粉体形成浆液,喷洒在碱渣山表面,利用碱渣氯盐的激发作用使其水化,在碱渣山表面形成一个3-10mm厚的水化硬化层,以减少碱渣山扬尘问题。
进一步一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,包括以下步骤:
(1)利用搅拌装置,将具有水化活性效应的固体废弃物粉体以粉体:水的质量比=0.5:0.5~1的比例混合形成浆体,并在其中加入质量百分含量为3%的聚乙烯醇溶液,聚乙烯醇溶液占浆体体积的10~100%,最终得到聚合物浆体。
(2)在碱渣山上覆盖塑料纤维防尘网,在塑料纤维防尘网上直接喷涂一层厚度为3~10mm的上述聚合物浆体,静置3小时,每4小时喷水,喷水量为0.1-1kg/m2;
(3)48小时后,改为每天喷水一次,喷水量为0.05-0.3kg/m2,优选喷水7天,得到覆盖于碱渣山的水化硬壳层。
具有水化活性的固体废弃物选自具有水化活性的硅酸盐固体废弃物,进一步为:高钙粉煤灰、低钙粉煤灰、矿渣粉、废砖粉及其他具有水化活性的硅酸盐固体废弃物。
利用该法进行防护,由于浆体中含有一定量的聚乙烯醇,浆体在初期可形成由有机物和活性固体废弃物粉体形成的一个由塑料纤维网加强的壳层,通过上述过程的养护,该壳层的活性组分可在碱渣中氯化物的激发下,水化硬化,形成一定的强度,对碱渣表面的风干可起到抑制作用,从而,具有防止碱渣山扬尘的作用。
具体实施方式
下面结合实施例对本发明作进一步说明,但本发明并不限于以下实施例。
实施例1
1、利用搅拌装置,将高钙粉煤灰以粉体:水=0.5:0.5的比例混合形成浆体,并在其中以体积比加入3%的聚乙烯醇溶液,聚乙烯醇溶液占的加入量为浆体体积的10%,最终得到聚合物浆体。
2、在碱渣山覆盖塑料纤维防尘网,在其上直接喷涂一层厚度为10mm的上述聚合物浆体,静置3小时,每4小时喷水,喷水量为1kg/m2
3、48小时后,改为每天喷水一次,喷水量为0.05kg/m2,优选喷水7天。
4、得到覆盖于碱渣山的水化硬壳层,起到防止碱渣山扬尘的作用。
实施例2:
1、利用搅拌装置,将废弃砖粉以粉体:水=0.5:1的比例混合形成浆体,并在其中以体积比加入3%的聚乙烯醇溶液,聚乙烯醇溶液占的加入量为浆体体积的50%,最终得到聚合物浆体。
2、在碱渣山覆盖塑料纤维防尘网,在其上直接喷涂一层厚度为5mm的上述聚合物浆体,静置3小时,每4小时喷水,喷水量为0.1kg/m2
3、48小时后,改为每天喷水一次,喷水量为0.05kg/m2,优选喷水7天。
4、得到覆盖于碱渣山的水化硬壳层,起到防止碱渣山扬尘的作用。
实施例3:
1、利用搅拌装置,将矿渣粉以粉体:水=0.5:0.7的比例混合形成浆体,并在其中以体积比加入3%的聚乙烯醇溶液,聚乙烯醇溶液占的加入量为浆体体积的50%,最终得到聚合物浆体。
2、在碱渣山覆盖塑料纤维防尘网,在其上直接喷涂一层厚度为3mm的上述聚合物浆体,静置3小时,每4小时喷水,喷水量为0.5kg/m2
3、48小时后,改为每天喷水一次,喷水量为0.1kg/m2,优选喷水7天,。
4、得到覆盖于碱渣山的水化硬壳层,起到防止碱渣山扬尘的作用。

Claims (5)

1.一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,利用具有水化活性的固体废弃物粉体形成浆液,喷洒在碱渣山表面,利用碱渣氯盐的激发作用使其水化,在碱渣山表面形成一个3-10mm厚的水化硬化层,以减少碱渣山扬尘问题。
2.按照权利要求1的一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,包括以下步骤:
(1)利用搅拌装置,将具有水化活性效应的固体废弃物粉体以粉体:水的质量比=0.5:0.5~1的比例混合形成浆体,并在其中加入质量百分含量为3%的聚乙烯醇溶液,聚乙烯醇溶液占浆体体积的10~100%,最终得到聚合物浆体。
(2)在碱渣山上覆盖塑料纤维防尘网,在塑料纤维防尘网上直接喷涂一层厚度为3~10mm的上述聚合物浆体,静置3小时,每4小时喷水,喷水量为
0.1-1kg/m2;
(3)48小时后,改为每天喷水一次,喷水量为0.05-0.3kg/m2,得到覆盖于碱渣山的水化硬壳层。
3.按照权利要求1的一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,具有水化活性的固体废弃物选自具有水化活性的硅酸盐固体废弃物。
4.按照权利要求1的一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,具有水化活性的固体废弃物选自高钙粉煤灰、低钙粉煤灰、矿渣粉、废砖粉及其他具有水化活性的硅酸盐固体废弃物。
5.按照权利要求1的一种防止露天堆放碱渣山扬尘的处理方法,其特征在于,步骤(3)喷水7天。
CN201410139652.3A 2014-04-09 2014-04-09 一种防止露天堆放碱渣山扬尘的处理方法 Active CN103949456B (zh)