CN103934092A CN201410140546.7A CN201410140546A CN103934092A CN 103934092 A CN103934092 A CN 103934092A CN 201410140546 A CN201410140546 A CN 201410140546A CN 103934092 A CN103934092 A CN 103934092A
Authority
CN
China
Prior art keywords
chute
zinc oxide
concentrate
mine tailing
beneficiation method
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201410140546.7A
Other languages
English (en)
Inventor
祁忠旭
于正华
李小健
李锦源
董艳红
胡波
肖骏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
LANPING JINLIDA MINING Co Ltd
Hunan Research Institute of Non Ferrous Metals
Original Assignee
LANPING JINLIDA MINING Co Ltd
Hunan Research Institute of Non Ferrous Metals
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by LANPING JINLIDA MINING Co Ltd, Hunan Research Institute of Non Ferrous Metals filed Critical LANPING JINLIDA MINING Co Ltd
Priority to CN201410140546.7A priority Critical patent/CN103934092A/zh
Publication of CN103934092A publication Critical patent/CN103934092A/zh
Pending legal-status Critical Current

Links

Abstract

本发明提供了一种从含氧化锌细泥中回收氧化锌矿物的方法,包括制浆,向矿浆中添加分散剂分散矿浆;然后进行两段溜槽选别获得溜槽精矿,之后对溜槽精矿进行离心选别获得最终的氧化锌精矿。本发明具有流程结构简单、易于操作、成本低、无污染等特点,可有效提高氧化锌资源利用率。

Description

一种从含氧化锌细泥中回收氧化锌的选矿方法
技术领域
本发明涉及一种矿物的选矿回收方法,特别是一种从含氧化锌细泥中回收氧化锌的选矿方法。
背景技术
我国氧化锌矿石储量巨大,随着经济的发展,易选硫化锌矿石日益枯竭,氧化锌矿石的开发利用必将成为日后锌资源开发的重点。
氧化锌矿石中常存在大量的泥质矿物,泥化现象严重。泥质主要来源于矿床中的粘土类矿物或被粘土所胶结成团的、风化成细粒的矿石。由于矿泥具有质量小、比表面积大等特点,容易附着在粗粒矿物表面形成矿泥覆盖;同时矿泥具有较大的表面能具有较强的药剂吸附能力,致使浮选过程中浮选捕收剂的吸附选择性变差,细泥与泡沫接触及粘附效率降低,进而对浮选过程产生一系列不利的影响。
对于泥质中的氧化锌矿石采用浮选法回收难度大,较高的细泥含量使浮选效果迅速恶化,药剂选择性变差,浮选过程往往消耗大量的选矿药剂也难以保证锌的回收率和富集比。研究发现采取降低浮选浓度和添加矿浆分散剂等方法,能够产生一定效果,但仍难以有效回收泥质中的锌矿物。由于常规选矿方法难以回收泥质中的氧化锌矿物,使含泥氧化锌的长期堆放,不仅造成资源的巨大浪费,而且长久的风吹、日晒、雨淋等,会造成环境尤其是水的重金属污染。
因此,开发可以有效回收泥质中氧化锌选矿方法迫在眉睫。
发明内容
本发明的目的在于提供一种从含氧化锌细泥中回收氧化锌矿物的方法,它能有效回收氧化锌矿物,同时可以有效降低在泥质中损失的氧化锌矿物。
本发明采用以下技术方案达到上述目的:一种从含氧化锌细泥中回收氧化锌矿物的方法,其特征在于,包括以下步骤:
1.将含有氧化锌的泥质,调节泥浆浓度至20-35%,添加分散剂,搅拌20-35min;
2.将上述泥浆进行溜槽试验,分别获得溜槽精矿和溜槽尾矿;
3.将上述获得的溜槽精矿进行离心选矿,分别获得精矿和尾矿,精矿即为最终氧化锌精矿;
其中,步骤1所述的泥质的细度为:-400目含量为50%至85%;所述分散剂为水玻璃、碳酸钠、六偏磷酸钠、焦磷酸中的两种或者三种。
步骤2所述的溜槽试验进行一到两段选别:一段溜槽试验分别获得溜槽精矿1、溜槽中矿、溜槽尾矿1;将获得的溜槽中矿再进行一次溜槽选别分别获得溜槽精矿2和溜槽尾矿2,将溜槽精矿1和溜槽精矿2合并得到溜槽精矿,溜槽尾矿1和溜槽尾矿2合并得到溜槽尾矿;
本发明的技术原理
本发明针对含泥矿物泥化后难以分选的特点,加入分散剂,使矿浆有效分散;根据分散矿浆的密度差别,采用多重重选联合的方法,有效分离出泥化的氧化锌矿物。
本发明的优点在于:
1.    本发明的方法可有效回收泥化的氧化锌,锌回收率高,同时避免了在传统工艺中需加入大量的浮选药剂的难题。
2.    本发明流程结构简单、易于操作、成本低、无污染,可有效提高氧化锌资源利用率,为含泥矿物的回收提供了一种可能。
具体实施方式
实施例一
某含氧化锌矿泥,粒度为-400目占61.4%,锌品位6.83%左右,主要锌矿物为菱锌矿。
将含有氧化锌的泥质,调节泥浆浓度至25%,添加分散剂六偏磷酸钠和水玻璃,搅拌30min;
将上述泥浆进行两段溜槽试验,分别获得溜槽精矿和溜槽尾矿:一段溜槽试验分别获得溜槽精矿1、溜槽中矿、溜槽尾矿1;将获得的溜槽中矿再进行一次溜槽选别分别获得溜槽精矿2和溜槽尾矿2,将溜槽精矿1和溜槽精矿2合并得到溜槽精矿,溜槽尾矿1和溜槽尾矿2合并得到溜槽尾矿;
将上述获得的溜槽精矿进行离心选矿,分别获得离心精矿和离心尾矿,精矿即为最终氧化锌精矿,离心尾矿与溜槽尾矿合并即为最终尾矿。实施例一试验结果见表1。
表1 实施例1试验指标(%)
 
实施例二
某含氧化锌矿泥,粒度为-400目占61.4%,锌品位9.93%左右,主要锌矿物为菱锌矿。
将含有氧化锌的泥质,调节泥浆浓度至30%,添加分散剂碳酸钠和水玻璃,搅拌30min;
将上述泥浆进行溜槽试验,分别获得溜槽精矿和溜槽尾矿;
将上述获得的溜槽精矿进行离心选矿,分别获得离心精矿和离心尾矿,精矿即为最终氧化锌精矿,离心尾矿与溜槽尾矿合并即为最终尾矿。实施例二结果见表2。
表2 实施例2试验指标(%)

Claims (4)

1.一种从含氧化锌细泥中回收氧化锌的选矿方法,其特征在于,包括以下步骤:
(1)  将含有氧化锌的泥质,调节泥浆浓度至20-35%,添加分散剂,搅拌20-35min;
(2)  将上述泥浆进行溜槽试验,分别获得溜槽精矿和溜槽尾矿;
(3)  将上述获得的溜槽精矿进行离心选矿,分别获得精矿和尾矿,精矿即为最终氧化锌精矿。
2.根据权利要求1所述的一种从含氧化锌细泥中回收氧化锌的选矿方法,其特征在于,步骤(1)所述的泥质的细度为:-400目含量为50%至85%。
3.根据权利要求1所述的一种从含氧化锌细泥中回收氧化锌的选矿方法,其特征在于,所述分散剂为水玻璃、碳酸钠、六偏磷酸钠、焦磷酸钠中的两种或者三种。
4.根据权利要求1所述的一种从含氧化锌细泥中回收氧化锌的选矿方法,其特征在于,步骤(2)所述的溜槽试验进行两段选别:一段溜槽试验分别获得溜槽精矿1、溜槽尾矿1;将获得的溜槽中矿再进行一次溜槽选别分别获得溜槽精矿2和溜槽尾矿2,将溜槽精矿1和溜槽精矿2合并得到溜槽精矿,溜槽尾矿1和溜槽尾矿2合并得到溜槽尾矿。
CN201410140546.7A 2014-04-10 2014-04-10 一种从含氧化锌细泥中回收氧化锌的选矿方法 Pending CN103934092A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201410140546.7A CN103934092A (zh) 2014-04-10 2014-04-10 一种从含氧化锌细泥中回收氧化锌的选矿方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201410140546.7A CN103934092A (zh) 2014-04-10 2014-04-10 一种从含氧化锌细泥中回收氧化锌的选矿方法

Publications (1)

Publication Number Publication Date
CN103934092A true CN103934092A (zh) 2014-07-23

Family

ID=51182121

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201410140546.7A Pending CN103934092A (zh) 2014-04-10 2014-04-10 一种从含氧化锌细泥中回收氧化锌的选矿方法

Country Status (1)

Country Link
CN (1) CN103934092A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106622631A (zh) * 2016-11-03 2017-05-10 深圳清华大学研究院 一种高泥氧化锌矿脱泥装置及方法
CN113304874A (zh) * 2021-04-29 2021-08-27 中国恩菲工程技术有限公司 铌矿浮选预处理方法

Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1597128A (zh) * 2004-08-11 2005-03-23 昆明理工大学 旋转尖缩溜槽式离心选矿机
CN101468330A (zh) * 2007-12-24 2009-07-01 鞍钢集团矿业公司 处理混合型铁矿石的工艺
CN101708481A (zh) * 2008-10-31 2010-05-19 鞍钢集团矿业公司 螺旋溜槽粗选尾矿增设分级工艺
CN102688802A (zh) * 2012-06-11 2012-09-26 中国瑞林工程技术有限公司 调浆重选工艺

Patent Citations (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN1597128A (zh) * 2004-08-11 2005-03-23 昆明理工大学 旋转尖缩溜槽式离心选矿机
CN101468330A (zh) * 2007-12-24 2009-07-01 鞍钢集团矿业公司 处理混合型铁矿石的工艺
CN101708481A (zh) * 2008-10-31 2010-05-19 鞍钢集团矿业公司 螺旋溜槽粗选尾矿增设分级工艺
CN102688802A (zh) * 2012-06-11 2012-09-26 中国瑞林工程技术有限公司 调浆重选工艺

Cited By (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN106622631A (zh) * 2016-11-03 2017-05-10 深圳清华大学研究院 一种高泥氧化锌矿脱泥装置及方法
CN106622631B (zh) * 2016-11-03 2019-10-18 深圳清华大学研究院 一种高泥氧化锌矿脱泥装置及方法
CN113304874A (zh) * 2021-04-29 2021-08-27 中国恩菲工程技术有限公司 铌矿浮选预处理方法

Similar Documents

Publication Publication Date Title
CN100515576C (zh) 超细贫铅锑锌絮凝载体浮选的方法
CN102658236B (zh) 一种微细泥锡石的回收方法
CN102909136B (zh) 一种锂辉石矿的选矿方法
CN110170381B (zh) 一种从锡铜共生矿中回收锡石的选矿方法
CN104624389A (zh) 一种重选尾矿锡石浮选方法
CN102744160B (zh) 一种硅钙质胶磷矿等可浮分选工艺
CN107583764B (zh) 一种铜矿尾矿回收云母的选矿方法
CN104741245A (zh) 一种新型锂云母浮选方法和一种捕收剂及其应用
CN101879479A (zh) 一种榴辉岩型金红石矿的选矿方法
CN103990540B (zh) 一种长石矿物的差别化选矿提质方法
CN105268559A (zh) 低品位硫化铜矿的选矿方法
CN111346740A (zh) 一种钽铌尾矿中回收铁锂云母的工艺
CN105689150A (zh) 一种氧化铅锌矿浮选抑制剂及其应用
CN103386358A (zh) 一种低品位稀土矿的选矿方法
CN104226465A (zh) 一种油页岩重力分选富集油母质工艺
CN102728455A (zh) 高中间密度物含量的难选煤泥重选浮选联合分选工艺
CN103447146A (zh) 一种从选钼尾矿中回收长石的方法
CN102747228A (zh) 一种高炉瓦斯泥回收有价元素的方法
CN105750089B (zh) 一种镁质胶磷矿分选方法
CN103962244B (zh) 一种铜硫尾矿中金属铷资源回收的分选富集处理工艺
CN110813517A (zh) 一种从尾矿中回收黑钨矿的选矿方法
CN103878069A (zh) 一种辉钼矿的选矿方法
CN103934092A (zh) 一种从含氧化锌细泥中回收氧化锌的选矿方法
CN110523540B (zh) 一种新型表面活性剂在氧化锌矿浮选上的应用方法
CN102773151B (zh) 一种风化胶磷矿分质加工工艺

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20140723