CN103881149A - 一种环保塑料地膜 - Google Patents
一种环保塑料地膜 Download PDFInfo
- Publication number
- CN103881149A CN103881149A CN201410065936.2A CN201410065936A CN103881149A CN 103881149 A CN103881149 A CN 103881149A CN 201410065936 A CN201410065936 A CN 201410065936A CN 103881149 A CN103881149 A CN 103881149A
- Authority
- CN
- China
- Prior art keywords
- parts
- mulch film
- friendly plastic
- raw material
- lubricant
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明提供了一种环保塑料地膜,由下列重量份数的原料组成:热塑性淀粉70-80份,线性低密度聚乙烯15-30份,复合增塑剂15-20份,减雾剂0.5-3份,抗氧化剂0.5-1.5份,降解促进剂5-8份,润滑剂2-10份。本发明的优点是:该地膜能有效解决因高温、湿度等因素造成的雾化问题,促进植物的光合作用,对土壤无污染,透气性好;制备简单,成本低;还可被生物降解,便于推广使用。
Description
技术领域
本发明属于塑料膜生产领域,具体涉及一种环保塑料地膜。
背景技术
为促进植物的生长,人们通常会在植物初期的生长时覆盖一层地膜,以提高土壤湿度,保持土壤水分,维持土壤结构,防止害虫侵袭和某些微生物引起的病害等。但是,在高温或者湿度较大的天气情况下,地膜表面容易聚集水雾,大大降低了光对植物的光合作用;再者,塑料制品带来的白色污染正在不断地破坏自然环境,而绝大部分的地膜都是由不可降解的塑料制得的,其在一次使用后即被丢弃于地面,我国是农业大国,一直在向机械化农业的方向发展,这就势必导致地膜的规模化使用,为缓解甚至杜绝白色污染的严重化,急需提供一种对环境友好的新型地膜。
发明内容
本发明所要解决的技术问题是提供一种对土壤无危害,不妨碍植物光合作用,生产工艺简单、成本低,使用性能优越的可降解环保塑料地膜。
为解决上述技术问题,本发明采用的技术方案是:
一种环保塑料地膜,由下列重量份数的原料组成:热塑性淀粉70-80份,线性低密度聚乙烯15-30份,复合增塑剂15-20份,减雾剂0.5-3份,抗氧化剂0.5-1.5份,降解促进剂5-8份,润滑剂2-10份。
制备上述环保塑料地膜的方法,包括如下步骤:
1)将原料加入高速混合机内充分搅拌均匀,其中的润滑剂分至少两次加入;
2)将上述混合后的原料在造粒机中进行混炼、熔融、挤出、冷却后切粒得到可生物降解的塑料颗粒;
3)将步骤2)中得到的塑料颗粒加入吹膜机中制作地膜。
其中,上述热塑性淀粉为玉米淀粉、小麦淀粉或土豆淀粉中的至少一种;上述复合增塑剂为甘油、乙二醇、乙酸山梨醇酯中的至少一种;上述减雾剂为改性聚硅氧烷或十四烷基二甲基氧化胺;上述抗氧化剂为二丁基羟基甲苯或硫辛酸;上述降解促进剂为聚乳酸或聚羟基烷酸酯;上述润滑剂为脂肪酸酰胺、单硬脂酸甘油脂、滑石粉中的至少一种。
本发明的优点是:该地膜能有效解决因高温、湿度等因素造成的雾化问题,促进植物的光合作用,对土壤无污染,透气性好;制备简单,成本低;还可被生物降解,便于推广使用。
具体实施方式:
下面结合各实施例对本发明作进一步的阐述,但不是对本发明的限制:
实施例1
一种环保塑料地膜,由下列重量份数的原料组成:玉米淀粉70份,线性低密度聚乙烯15份,甘油15份,改性聚硅氧烷0.5份,二丁基羟基甲苯0.5份,聚乳酸5份,脂肪酸酰胺2份。
制备上述环保塑料地膜的方法,包括如下步骤:
1)将原料加入高速混合机内充分搅拌均匀,其中的润滑剂分至少两次加入;
2)将上述混合后的原料在造粒机中进行混炼、熔融、挤出、冷却后切粒得到可生物降解的塑料颗粒;
3)将步骤2)中得到的塑料颗粒加入吹膜机中制作地膜。
实施例2
一种环保塑料地膜,由下列重量份数的原料组成:小麦淀粉75份,线性低密度聚乙烯25份,乙二醇18份,十四烷基二甲基氧化胺1.5份,硫辛酸1份,聚羟基烷酸酯7份,滑石粉6份。
制备上述环保塑料地膜的方法,包括如下步骤:
1)将原料加入高速混合机内充分搅拌均匀,其中的润滑剂分至少两次加入;
2)将上述混合后的原料在造粒机中进行混炼、熔融、挤出、冷却后切粒得到可生物降解的塑料颗粒;
3)将步骤2)中得到的塑料颗粒加入吹膜机中制作地膜。
实施例3
一种环保塑料地膜,由下列重量份数的原料组成:土豆淀粉80份,线性低密度聚乙烯30份,乙酸三梨醇酯20份,改性聚硅氧烷3份,硫辛酸1.5份,聚羟基烷酸酯8份,单硬脂酸甘油脂10份。
制备上述环保塑料地膜的方法,包括如下步骤:
1)将原料加入高速混合机内充分搅拌均匀,其中的润滑剂分至少两次加入;
2)将上述混合后的原料在造粒机中进行混炼、熔融、挤出、冷却后切粒得到可生物降解的塑料颗粒;
3)将步骤2)中得到的塑料颗粒加入吹膜机中制作地膜。
Claims (3)
1.一种环保塑料地膜,其特征在于,由下列重量份数的原料组成:热塑性淀粉70-80份,线性低密度聚乙烯15-30份,复合增塑剂15-20份,减雾剂0.5-3份,抗氧化剂0.5-1.5份,降解促进剂5-8份,润滑剂2-10份。
2.一种制备根据权利要求1所述的环保塑料地膜的方法,其特征在于,该制备方法包括如下步骤:
1)将原料加入高速混合机内充分搅拌均匀,其中的润滑剂分至少两次加入;
2)将上述混合后的原料在造粒机中进行混炼、熔融、挤出、冷却后切粒得到可生物降解的塑料颗粒;
3)将步骤2)中得到的塑料颗粒加入吹膜机中制作地膜。
3.根据权利要求1所述的一种环保塑料地膜,其特征在于,所述热塑性淀粉为玉米淀粉、小麦淀粉或土豆淀粉中的至少一种;所述复合增塑剂为甘油、乙二醇、乙酸山梨醇酯中的至少一种;所述减雾剂为改性聚硅氧烷或十四烷基二甲基氧化胺;所述抗氧化剂为二丁基羟基甲苯或硫辛酸;所述降解促进剂为聚乳酸或聚羟基烷酸酯;所述润滑剂为脂肪酸酰胺、单硬脂酸甘油脂、滑石粉中的至少一种。