CN103864350B - 一种卫生间用防水材料及其制备方法 - Google Patents

一种卫生间用防水材料及其制备方法 Download PDF

Info

Publication number
CN103864350B
CN103864350B CN201210540599.9A CN201210540599A CN103864350B CN 103864350 B CN103864350 B CN 103864350B CN 201210540599 A CN201210540599 A CN 201210540599A CN 103864350 B CN103864350 B CN 103864350B
Authority
CN
China
Prior art keywords
parts
water
proof material
toilet
sewer line
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210540599.9A
Other languages
English (en)
Other versions
CN103864350A (zh
Inventor
陆明军
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Foshan Zhuo Shi high tech Material Co., Ltd.
Original Assignee
陆明军
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 陆明军 filed Critical 陆明军
Priority to CN201210540599.9A priority Critical patent/CN103864350B/zh
Publication of CN103864350A publication Critical patent/CN103864350A/zh
Application granted granted Critical
Publication of CN103864350B publication Critical patent/CN103864350B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种卫生间用防水材料,其是由下述重量份配比的原料组成:水40~50份、甲基丙烯酸甲酯20~25份、三聚氰胺甲醛树脂8~10份、酚醛树脂5~6份、木质素纤维2~6份、氢氧化铝15~20份、滑石粉25~35份、膨润土15~20份、可再分散乳胶粉2~5份、聚丙烯酸钠1~2份、石英砂3~5份。本发明防水材料涂刷后,可在24~48小时内形成防水膜层,该防水膜层与马桶下水管道及主下水管道等结合紧密,可有效防止下水管道周边的渗漏;而且本发明防水材料涂刷后所形成的防水膜层延展性好,可避免因建筑物产生的微小沉降和错位等而产生裂纹,进而可有效防止卫生间漏水,且不易老化,防水有效期长达20年以上。

Description

一种卫生间用防水材料及其制备方法
技术领域
本发明涉及一种适合在卫生间使用的防水材料,同时涉及该防水材料的制备方法。
背景技术
目前,卫生间常用的防水材料为防水灰浆,其主要存在以下缺陷:一是防水灰浆凝固后与管道周边结合不好,容易造成管道周边渗漏;二是防水灰浆凝固后延展性不好,随着建筑物产生的微小沉降和错位,防水灰浆形成的防水层会被扯裂,从而导致漏水。
发明内容
为了解决上述技术问题,本发明提供一种卫生间用防水材料。
其技术解决方案是:
一种卫生间用防水材料,其是由下述重量份配比的原料组成:水40~50份、甲基丙烯酸甲酯20~25份、三聚氰胺甲醛树脂8~10份、酚醛树脂5~6份、木质素纤维2~6份、氢氧化铝15~20份、滑石粉25~35份、膨润土15~20份、可再分散乳胶粉2~5份、聚丙烯酸钠1~2份、石英砂3~5份。
优选的,各原料的重量份配比为:水45份、甲基丙烯酸甲酯28份、三聚氰胺甲醛树脂9、酚醛树脂6份、木质素纤维4份、氢氧化铝18份、滑石粉30份、膨润土18份、可再分散乳胶粉4份、聚丙烯酸钠2份、石英砂4份。
上述卫生间用防水材料的制备方法包括以下步骤:
(1)将甲基丙烯酸甲酯、三聚氰胺甲醛树脂、酚醛树脂和部分水混合,搅拌,升温至65~70℃,保温30~45分钟,制成乳液;
(2)将氢氧化铝、滑石粉、膨润土与石英砂溶于余量水中,制成浆料;
(3)将步骤(1)中制得的乳液与步骤(2)中制得的浆料混合,然后向混合液中加入木质素纤维、聚丙烯酸钠与可再分散乳胶粉,搅拌均匀,制得防水材料。
本发明的有益技术效果是:
本发明防水材料涂刷后,可在24~48小时内形成防水膜层,该防水膜层与马桶下水管道及主下水管道等结合紧密,可有效防止下水管道周边的渗漏;而且本发明防水材料涂刷后所形成的防水膜层延展性好,可避免因建筑物产生的微小沉降和错位等而产生裂纹,进而可有效防止卫生间漏水,且不易老化,防水有效期长达20年以上。
具体实施方式
实施例1
称取水500g、甲基丙烯酸甲酯200g、三聚氰胺甲醛树脂80g、酚醛树脂60g、木质素纤维20g、氢氧化铝15g、滑石粉25g、膨润土20g、可再分散乳胶粉2g、聚丙烯酸钠2g、石英砂3g。
将称量好的甲基丙烯酸甲酯、三聚氰胺甲醛树脂、酚醛树脂和300g水混合,搅拌,升温至70℃,保温45分钟,制成乳液。将氢氧化铝、滑石粉、膨润土与石英砂溶于200g水中,制成浆料。将乳液与浆料混合制得混合液,然后向混合液中加入木质素纤维、聚丙烯酸钠与可再分散乳胶粉,搅拌均匀,制得防水材料。
实施例2
称取水500、甲基丙烯酸甲酯250g、三聚氰胺甲醛树脂100g、酚醛树脂50g、木质素纤维60g、氢氧化铝20g、滑石粉35g、膨润土15g、可再分散乳胶粉5g、聚丙烯酸钠1g、石英砂5g。
将称取的甲基丙烯酸甲酯、三聚氰胺甲醛树脂、酚醛树脂和300g水混合,搅拌,升温至65℃,保温30分钟,制成乳液。将氢氧化铝、滑石粉、膨润土与石英砂溶于200g水中,制成浆料。将乳液与浆料混合制得混合液,然后向混合液中加入木质素纤维、聚丙烯酸钠与可再分散乳胶粉,搅拌均匀,制得防水材料。
实施例3
称取水500g、甲基丙烯酸甲酯220g、三聚氰胺甲醛树脂90g、酚醛树脂55g、木质素纤维30g、氢氧化铝18g、滑石粉30g、膨润土18g、可再分散乳胶粉3g、聚丙烯酸钠2g、石英砂4g。
将称取的甲基丙烯酸甲酯、三聚氰胺甲醛树脂、酚醛树脂和300g水混合,搅拌,升温至68℃,保温40分钟,制成乳液。将氢氧化铝、滑石粉、膨润土与石英砂溶于200g水中,制成浆料。将乳液与浆料混合制得混合液,然后向混合液中加入木质素纤维、聚丙烯酸钠与可再分散乳胶粉,搅拌均匀,制得防水材料。
将实施例1、2、3制得的防水材料的拉伸强度、绍尔硬度及与高密度聚乙烯下水管道之间的剥离强度等进行性能测试,结果如下表1所示。
表1

Claims (2)

1.一种卫生间用防水材料,其特征在于是由下述重量份配比的原料组成:水40~50份、甲基丙烯酸甲酯20~25份、三聚氰胺甲醛树脂8~10份、酚醛树脂5~6份、木质素纤维2~6份、氢氧化铝15~20份、滑石粉25~35份、膨润土15~20份、可再分散乳胶粉2~5份、聚丙烯酸钠1~2份、石英砂3~5份。
2.根据权利要求1所述的一种卫生间用防水材料,其特征在于各原料的重量份配比为:水45份、甲基丙烯酸甲酯28份、三聚氰胺甲醛树脂9、酚醛树脂6份、木质素纤维4份、氢氧化铝18份、滑石粉30份、膨润土18份、可再分散乳胶粉4份、聚丙烯酸钠2份、石英砂4份。
CN201210540599.9A 2012-12-14 2012-12-14 一种卫生间用防水材料及其制备方法 Active CN103864350B (zh)