CN103835135A - Production technique of ironing-free crease-resistant fabric - Google Patents

Production technique of ironing-free crease-resistant fabric Download PDF

Info

Publication number
CN103835135A
CN103835135A CN201210496802.7A CN201210496802A CN103835135A CN 103835135 A CN103835135 A CN 103835135A CN 201210496802 A CN201210496802 A CN 201210496802A CN 103835135 A CN103835135 A CN 103835135A
Authority
CN
China
Prior art keywords
ironing
production technique
textile production
wrinkle resistant
kept
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201210496802.7A
Other languages
Chinese (zh)
Inventor
缪建新
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
WUXI YINTAI TEXTILE Co Ltd
Original Assignee
WUXI YINTAI TEXTILE Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by WUXI YINTAI TEXTILE Co Ltd filed Critical WUXI YINTAI TEXTILE Co Ltd
Priority to CN201210496802.7A priority Critical patent/CN103835135A/en
Publication of CN103835135A publication Critical patent/CN103835135A/en
Pending legal-status Critical Current

Abstract

The invention relates to a production technique of an ironing-free crease-resistant fabric, which comprises the following steps: impregnating a cotton fabric in a NaOH solution, impregnating in a finishing solution and rolling twice, drying, baking, making clothes, and ironing. The finishing solution comprises 80-150 g/L resin JLSUN M2D, 20-25 g/L softener S960, 35-55 g/L catalyst, 0.5-1 g/L penetrant and 40-50 g/L fiber protective agent. In the roasting step, the temperature is kept at 80-90 DEG C, and the humidity is kept at 6-8%. The temperature is kept at 120-130 DEG C for 3-5 minutes in the baking step. The fabric produced by the technique feels soft and has favorable crease-resistant effect.

Description

A kind of non-ironing wrinkle resistant textile production technique
Technical field
The present invention relates to a kind of textile production technique, especially relate to a kind of non-ironing wrinkle resistant textile production technique.
Background technology
Cotton fiber is desirable clothes raw material, but elasticity is poor.COTTON FABRIC is easily wrinkled after washing, needs flatiron.
Summary of the invention
The applicant, for above-mentioned market demand, is studied improvement, and a kind of non-ironing wrinkle resistant textile production technique is provided.
In order to solve the problems of the technologies described above, the present invention adopts following technical scheme:
A kind of non-ironing wrinkle resistant textile production technique; step is as follows: COTTON FABRIC-> dipping NaOH solution-> bis-soaks two and rolls cure-> of dressing liquid-> oven dry-> clothing-> flatiron; described dressing liquid comprises the M2D of the resin JLSUN board of 80~150g/L; 20~25g/L softener S960; 35~55g/L catalyst; 0.5~1g/L bleeding agent, 40~50g/L fiber protective agent.
Further: described in dry step temperature and remain on 80~90 DEG C, moisturizing rate 6%~8%.
Described baking step temperature remains on 120 DEG C~130 DEG C, continues 3~5 minutes.
Technique effect of the present invention is:
The textile touch of producing through processing step of the present invention is submissive, and wrinkle-proof effect is good.
Below the specific embodiment of the present invention is described in further detail.
A kind of non-ironing wrinkle resistant textile production technique; step is as follows: COTTON FABRIC-> dipping NaOH solution-> bis-soaks two and rolls cure-> of dressing liquid-> oven dry-> clothing-> flatiron; described dressing liquid comprises the M2D of the resin JLSUN board of 80g/L; 20g/L softener S960; 55g/L catalyst; 1g/L bleeding agent, 40g/L fiber protective agent.The described step temperature of drying remains on 90 DEG C, moisturizing rate 6%.Described baking step temperature remains on 130 DEG C, continues 3 minutes.

Claims (3)

1. a non-ironing wrinkle resistant textile production technique; step is as follows: COTTON FABRIC-> dipping NaOH solution-> bis-soaks two and rolls cure-> of dressing liquid-> oven dry-> clothing-> flatiron; described dressing liquid comprises the M2D of the resin JLSUN board of 80~150g/L; 20~25g/L softener S960; 35~55g/L catalyst; 0.5~1g/L bleeding agent, 40~50g/L fiber protective agent.
2. according to the non-ironing wrinkle resistant textile production technique of one claimed in claim 1, it is characterized in that: described in dry step temperature and remain on 80~90 DEG C, moisturizing rate 6%~8%.
3. according to the non-ironing wrinkle resistant textile production technique of one claimed in claim 1, it is characterized in that: described baking step temperature remains on 120 DEG C~130 DEG C, continue 3~5 minutes.
CN201210496802.7A 2012-11-24 2012-11-24 Production technique of ironing-free crease-resistant fabric Pending CN103835135A (en)