CN103756448A - 一种特氟龙防火油漆配方 - Google Patents
一种特氟龙防火油漆配方 Download PDFInfo
- Publication number
- CN103756448A CN103756448A CN201410029183.XA CN201410029183A CN103756448A CN 103756448 A CN103756448 A CN 103756448A CN 201410029183 A CN201410029183 A CN 201410029183A CN 103756448 A CN103756448 A CN 103756448A
- Authority
- CN
- China
- Prior art keywords
- teflon
- paint
- mica powder
- pigment
- fireproof
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种特氟龙防火油漆配方,包含以下成分:油料、树脂、颜料、稀释剂、固化剂、云母粉和特氟龙,其中各成分按质量百分比计算所占比例为:油料40%~50%、树脂10%~20%、颜料5%~10%、稀释剂3%~5%、固化剂3%~5%、云母粉1%~5%和特氟龙1%~5%。通过上述方式,本发明能够对日常用的油漆进行改良,提供一种防火特氟龙油漆,能够利用特氟龙的耐热性和耐腐蚀性提高油漆的性能,同时添加云母粉的防火功能,使油漆的适用范围大大增加。
Description
技术领域
本发明涉及一种特氟龙制品的配方,特别是涉及一种特氟龙防火油漆配方。
背景技术
特氟龙具有耐热性、抗湿性和耐腐蚀性,表面不沾水和油质,在生活中被广泛应用。防火油漆也在市场上占据有重要位置,但是防火的效果却不是很明显,常常达不到预期的效果。
发明内容
本发明主要解决的技术问题是提供一种特氟龙防火油漆配方,能够对日常用的油漆进行改良,提供一种防火特氟龙油漆,能够利用特氟龙的耐热性和耐腐蚀性提高油漆的性能,同时添加云母粉的防火功能,使油漆的适用范围大大增加。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种特氟龙防火油漆配方,包含以下成分:油料、树脂、颜料、稀释剂、固化剂、云母粉和特氟龙,其中各成分按质量百分比计算所占比例为:油料40%~50%、树脂10%~20%、颜料5%~10%、稀释剂3%~5%、固化剂3%~5%、云母粉1%~5%和特氟龙1%~5%。
在本发明一个较佳实施例中,所述配方中颜料中进一步包含有防锈颜料。
在本发明一个较佳实施例中,所述油料为半干性油。
在本发明一个较佳实施例中,所述云母粉为白云母粉。
在本发明一个较佳实施例中,所述特氟龙为氟化乙烯丙烯共聚物。
本发明的有益效果是:本发明能够对日常用的油漆进行改良,提供一种防火特氟龙油漆,能够利用特氟龙的耐热性和耐腐蚀性提高油漆的性能,同时添加云母粉的防火功能,使油漆的适用范围大大增加。
具体实施方式
下面将对本发明实施例中的技术方案进行清楚、完整地描述,显然,所描述的实施例仅是本发明的一部分实施例,而不是全部的实施例。基于本发明中的实施例,本领域普通技术人员在没有做出创造性劳动前提下所获得的所有其它实施例,都属于本发明保护的范围。
本发明实施例提供如下技术方案。
在一个实施例中,一种特氟龙防火油漆配方,包含以下成分:油料、树脂、颜料、稀释剂、固化剂、云母粉和特氟龙,其中各成分按质量百分比计算所占比例为:油料40%~50%、树脂10%~20%、颜料5%~10%、稀释剂3%~5%、固化剂3%~5%、云母粉1%~5%和特氟龙1%~5%。
区别于现有技术,在一个实施例中,为了能够控制各个组分的成分,以至于能够提高油漆的质量,优选地,所述配方中颜料中进一步包含有防锈颜料,能够有效地提高油漆的质量。
优选地,所述油料为半干性油。
优选地,所述云母粉为白云母粉,可提高其机械强度,增强韧性、附着力、抗老化及耐腐蚀性。
优选地,所述特氟龙为氟化乙烯丙烯共聚物。
本发明能够对日常用的油漆进行改良,提供一种防火特氟龙油漆,能够利用特氟龙的耐热性和耐腐蚀性提高油漆的性能,同时添加云母粉的防火功能,使油漆的适用范围大大增加。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其它相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (5)
1.一种特氟龙防火油漆配方,其特征在于:包含以下成分:油料、树脂、颜料、稀释剂、固化剂、云母粉和特氟龙,其中各成分按质量百分比计算所占比例为:油料40%~50%、树脂10%~20%、颜料5%~10%、稀释剂3%~5%、固化剂3%~5%、云母粉1%~5%和特氟龙1%~5%。
2.根据权利要求1所述的一种特氟龙防火油漆配方,其特征在于:所述配方中颜料中进一步包含有防锈颜料。
3.根据权利要求1所述的一种特氟龙防火油漆配方,其特征在于:所述油料为半干性油。
4.根据权利要求1所述的一种特氟龙防火油漆配方,其特征在于:所述特氟龙为氟化乙烯丙烯共聚物。
5.根据权利要求1所述的一种特氟龙防火油漆配方,其特征在于:所述云母粉为白云母粉。