CN103756404B - 一种用于导光油墨的扩散粒子的制备方法 - Google Patents

一种用于导光油墨的扩散粒子的制备方法 Download PDF

Info

Publication number
CN103756404B
CN103756404B CN201310236496.8A CN201310236496A CN103756404B CN 103756404 B CN103756404 B CN 103756404B CN 201310236496 A CN201310236496 A CN 201310236496A CN 103756404 B CN103756404 B CN 103756404B
Authority
CN
China
Prior art keywords
diffusion particle
carbamate
light guide
guide ink
preparation
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310236496.8A
Other languages
English (en)
Other versions
CN103756404A (zh
Inventor
朱梦白
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Zhejiang Yinlu Chemical Co ltd
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201310236496.8A priority Critical patent/CN103756404B/zh
Publication of CN103756404A publication Critical patent/CN103756404A/zh
Application granted granted Critical
Publication of CN103756404B publication Critical patent/CN103756404B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明属于导光油墨制备技术领域,具体涉及一种用于导光油墨的扩散粒子的制备方法。首先将甲基丙烯酸树脂、氨基甲酸酯溶入丁酮和醋酸丁酯的混合溶剂中,再加入多元醇树脂,搅拌均匀;然后在所得的混合液中,加入光引发剂二烷氧基苯乙酮,继续搅拌均匀;最后将所得的混合液放入UV光固化机进行固化,制得扩散粒子。本方法制得的扩散粒子具有消光效果,并有独特的舒滑手感,特别是不会吸收UV,不影响光引发剂的吸收能量,同时保持透明、优良的质感、抗刮和耐磨的效果。该扩散粒子具有良的耐热性与分散性,可提供优异的光学扩散效果和良好的亮度表现。

Description

一种用于导光油墨的扩散粒子的制备方法
技术领域
本发明属于导光油墨制备技术领域,具体涉及一种用于导光油墨的扩散粒子的制备方法。
背景技术
导光板是液晶面板中背光模组中重要组成部分,使用时利用导光油墨通过网版印刷技术,将油墨印刷成反光点,从而将点光源转化成面光源,达到使得整个导光板发光均匀的效果。
导光油墨的成分会直接影响到导光点的质量,而导光点的质量直接影响到导光板的亮度均匀性。
目前使用的导光油墨主要存在的问题是制得的导光板辉度低、发光均匀性较差,同时导光油墨中所含溶剂容易挥发,对环境造成污染,损害工人健康。
专利ZL200910241577.0公开了一种导光油墨及其制备方法和使用方法,其采用的散射粒子为二氧化钛、硫酸钡、氧化镁、氧化硅等无机粒子,这些无机粒子通常是坚硬的、不规则的,使得分散相的粒度很难达到均匀,而且无机粒子的加入会严重影响光透光率,这些都严重限制了无机粒子在导光板中的应用。
发明内容
针对背景技术中存在的问题,本发明的目的在于提供一种用于导光油墨的扩散粒子的制备方法。
实现本发明目的的技术方案为:一种用于导光油墨的扩散粒子的制备方法,其具体制备步骤如下:
步骤a、将甲基丙烯酸树脂、氨基甲酸酯溶入丁酮和醋酸丁酯的混合溶剂中,再加入多元醇树脂,搅拌均匀;
步骤b、在步骤1所得的混合液中,加入光引发剂二烷氧基苯乙酮,继续搅拌均匀;
步骤c、将步骤2所得的混合液放入UV光固化机进行固化。
步骤a中所述的甲基丙烯酸树脂和氨基甲酸酯的质量比为:(1~3):1,混合溶剂与氨基甲酸酯的质量比为:(2~4):1,其中丁酮与醋酸丁酯的质量比为:2:1,多元醇树脂与氨基甲酸酯的质量比为:(3~5):1。
步骤b中所述的光引发剂二烷氧基苯乙酮与氨基甲酸酯的质量比为:(0.2~0.4):1。
步骤c中所述的固化时间为20s~40s,紫外光照射强度为120w/cm2
本发明所述的扩散粒子,其直径在10微米~100微米之间。
本发明的优点在于:
1.本发明的的扩散粒子具有消光效果,并有独特的舒滑手感,特别是不会吸收UV,不影响光引发剂的吸收能量,同时保持透明、优良的质感、抗刮和耐磨的效果。
2.本发明采用的扩散粒子具有良的耐热性与分散性,适合用于光学应用产品,可提供优异的光学扩散效果和良好的亮度表现。
3.相对于无机粒子,本发明的扩散粒子与PC或PET基板之间相容性良好。
具体实施方式
下面将结合实施例对本发明作进一步地说明。
本发明一种用于导光油墨的扩散粒子的制备方法,所述的扩散粒子是由甲基丙烯酸树脂、氨基甲酸酯、多元醇树脂和光引发剂二烷氧基苯乙酮,经紫外光照射固化聚合而成的共聚物,使用时,由于扩散粒子与丙烯酸树脂、甲基丙烯酸甲酯具有相似结构,因此扩散粒子在UV固化油墨中的相容性和稳定性表现良好。
实施例1
取250毫升的锥形烧瓶,加入甲基丙烯酸树脂30克、氨基甲酸酯10克,丁酮20克、醋酸丁酯10克,再加入多元醇树脂30克,高速搅拌,搅拌速度1500rpm,搅拌时间10分钟,再慢慢加入光引发剂二烷氧基苯乙酮2克,继续搅拌10分钟,然后放入小型UV光固化机进行固化,固化时间20秒,紫外光照射强度为120w/cm2,该扩散粒子的直径为100微米。
实施例2
扩散粒子的制备:取250毫升的锥形烧瓶,加入甲基丙烯酸树脂10克、氨基甲酸酯10克,丁酮14克、醋酸丁酯6克,再加入多元醇树脂50克,高速搅拌,搅拌速度1500rpm,搅拌时间10分钟,再慢慢加入光引发剂二烷氧基苯乙酮4克,继续搅拌10分钟,然后放入小型UV光固化机进行固化,固化时间10秒,紫外光照射强度为120w/cm2,该扩散粒子的直径为10微米。
实施例3
扩散粒子的制备:取250毫升的锥形烧瓶,加入甲基丙烯酸树脂20克、氨基甲酸酯10克,丁酮27克、醋酸丁酯13克,再加入多元醇树脂40克,高速搅拌,搅拌速度1500rpm,搅拌时间10分钟,再慢慢加入光引发剂二烷氧基苯乙酮3克,继续搅拌10分钟,然后放入小型UV光固化机进行固化,固化时间15秒,紫外光照射强度为120w/cm2,该扩散粒子的直径为50微米。
以上述依据本发明的理想实施例为启示,通过上述的说明内容,相关技术人员完全可以在不偏离本项发明技术思想的范围内,进行多样的变更以及修改。本项发明的技术性范围并不局限于说明书上的内容,必须要根据权利要求范围来确定其技术性范围。

Claims (1)

1.一种用于导光油墨的扩散粒子的制备方法,其具体制备步骤如下:
步骤a、将甲基丙烯酸树脂、氨基甲酸酯溶入丁酮和醋酸丁酯的混合溶剂中,再加入多元醇树脂,搅拌均匀;
步骤b、在步骤a所得的混合液中,加入光引发剂二烷氧基苯乙酮,继续搅拌均匀;
步骤c、将步骤b所得的混合液放入UV光固化机进行固化,制得扩散粒子;
其中,步骤a中所述的甲基丙烯酸树脂和氨基甲酸酯的质量比为:(1~3):1,混合溶剂与氨基甲酸酯的质量比为:(2~4):1,其中丁酮与醋酸丁酯的质量比为:2:1,多元醇树脂与氨基甲酸酯的质量比为:(4~5):1;
其中,步骤b中所述的光引发剂二烷氧基苯乙酮与步骤a中所述的氨基甲酸酯的质量比为:(0.2~0.4):1;
其中,步骤c中所述的固化时间为10s或15s,紫外光照射强度为120w/cm2
其中,所述的扩散粒子,其直径在10微米~50微米之间。
CN201310236496.8A 2013-06-17 2013-06-17 一种用于导光油墨的扩散粒子的制备方法 Active CN103756404B (zh)