CN103709851B - 一种铜雕塑用含沥青的氟碳树脂漆 - Google Patents

一种铜雕塑用含沥青的氟碳树脂漆 Download PDF

Info

Publication number
CN103709851B
CN103709851B CN201310676109.2A CN201310676109A CN103709851B CN 103709851 B CN103709851 B CN 103709851B CN 201310676109 A CN201310676109 A CN 201310676109A CN 103709851 B CN103709851 B CN 103709851B
Authority
CN
China
Prior art keywords
paint
fluorocarbon resin
bitumeniferous
hour
auxiliary agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310676109.2A
Other languages
English (en)
Other versions
CN103709851A (zh
Inventor
郑东平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
TONGLING XINJIUDING COPPER CULTURE INDUSTRY Co Ltd
Original Assignee
TONGLING XINJIUDING COPPER CULTURE INDUSTRY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by TONGLING XINJIUDING COPPER CULTURE INDUSTRY Co Ltd filed Critical TONGLING XINJIUDING COPPER CULTURE INDUSTRY Co Ltd
Priority to CN201310676109.2A priority Critical patent/CN103709851B/zh
Publication of CN103709851A publication Critical patent/CN103709851A/zh
Application granted granted Critical
Publication of CN103709851B publication Critical patent/CN103709851B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种油漆,具体涉及一种铜雕塑用含沥青的氟碳树脂漆,本发明油漆由以下重量份的原料制成:氟碳树脂20-24、长油度醇酸树脂20-24、白炭黑10-12、2-苯并咪唑氨基甲酸甲酯4-7、沥青5-8、1,6-己二醇二丙烯酸酯20-30、醋酸丁酸纤维素1-2、六偏磷酸钠1-2、聚氨酯丙烯酸酯20-30、异佛尔酮二异氰酸酯9-12、硬脂酸钡2-5、四丙基溴化铵1-2、环烷酸钴2-3、助剂5-6、二甲苯10-12、乙酸丁酯10-12;本发明油漆涂层柔韧附着牢固,漆膜光亮饱满,耐候耐紫外辐照老化性能优良,耐热耐寒,综合性能突出,能广泛用于防护各种环境中的铜雕工艺品。

Description

一种铜雕塑用含沥青的氟碳树脂漆
技术领域
本发明涉及一种油漆,具体涉及一种铜雕塑用含沥青的氟碳树脂漆及其制备工艺。
背景技术
铜雕塑是日常生活中常见的一类工艺品,具有较高的艺术价值和欣赏价值,然而,铜雕塑艺术品由于其本身材质性质及摆放环境的特点,容易出现氧化腐蚀等问题,影响美观和使用寿命,为了保护铜器,往往需要在雕塑外面涂上油漆,并且对铜雕塑用漆有一定的要求,比如附着力、耐候老化、耐日光暴晒、耐温等等,因此,需要改进油漆配方,配制出适合不同使用场合的油漆,增加其艺术价值。
发明内容
本发明的目的在于,提供一种铜雕塑用含沥青的氟碳树脂漆,以保护雕塑品,为了实现上述目的,本发明采用的技术方案如下:
一种铜雕塑用含沥青的氟碳树脂漆,其特征在于,本发明材料由以下重量份的原料制成:氟碳树脂20-24、长油度醇酸树脂20-24、白炭黑10-12、2-苯并咪唑氨基甲酸甲酯4-7、沥青5-8、1,6-己二醇二丙烯酸酯20-30、醋酸丁酸纤维素1-2、六偏磷酸钠1-2、聚氨酯丙烯酸酯20-30、异佛尔酮二异氰酸酯9-12、硬脂酸钡2-5、四丙基溴化铵1-2、环烷酸钴2-3、助剂5-6、二甲苯10-12、乙酸丁酯10-12。
所述的助剂由以下重量份的原料制成:粘土10-14、纳米铁矿渣粉1-2、促进剂M3-4、苯基三乙氧基硅烷2-3、钼酸钠1-2、磁石2-3、苯甲酸钠1-2、柠檬酸三丁酯35-40、没食子酸丙酯2-3、薏仁油3-4、二硼化钒1-2、表儿茶素2-3;制备方法是将粘土、磁石送入煅烧炉中在720-740℃下煅烧2-3小时,然后取出,送入10-15%的盐酸溶液中浸泡2-3小时,过滤,得滤渣,用清水洗净,烘干、研磨成400-600目粉体;所得粉体与其它剩余成分混合,加热至60-70℃,搅拌反应40-50分钟,冷却,研磨成浆料,即得。
所述的一种铜雕塑用含沥青的氟碳树脂漆,其制备工艺为:
(1)将白炭黑、2-苯并咪唑氨基甲酸甲酯、沥青、助剂混合,加入到二甲苯、乙酸丁酯溶剂中,加热至120-130℃,反应3-4小时;
(2)将步骤(1)的物料冷却至70-85℃,加入醋酸丁酸纤维素、异佛尔酮二异氰酸酯、硬脂酸钡,搅拌反应3-4小时;
(3)将步骤(2)的物料降温至50-65℃,加入其它剩余物料,搅拌反应40-60分钟后,冷却至室温,研磨成20-60μm浆料,即得。
与现有技术相比,本发明提供的铜雕塑用油漆具备以下优点:添加的白炭黑、沥青等原料,增进了油漆的机械性能,使其坚固耐磨,再结合其它原料,制备的油漆涂层柔韧附着牢固,漆膜光亮饱满,耐候耐紫外辐照老化性能优良,耐热耐寒,综合性能突出,可以广泛用于防护各种环境中的铜雕工艺品。
具体实施方式
实施例
本实施例油漆由以下重量份原料制成:氟碳树脂22、长油度醇酸树脂22、白炭黑12、2-苯并咪唑氨基甲酸甲酯6、沥青8、1,6-己二醇二丙烯酸酯28、醋酸丁酸纤维素2、六偏磷酸钠2、聚氨酯丙烯酸酯26、异佛尔酮二异氰酸酯10、硬脂酸钡4、四丙基溴化铵2、环烷酸钴3、助剂6、二甲苯12、乙酸丁酯12。
所述的助剂由以下重量份的原料制成:粘土14、纳米铁矿渣粉2、促进剂M4、苯基三乙氧基硅烷3、钼酸钠2、磁石3、苯甲酸钠2、柠檬酸三丁酯40、没食子酸丙酯3、薏仁油4、二硼化钒2、表儿茶素3;制备方法是将粘土、磁石送入煅烧炉中在720-740℃下煅烧3小时,然后取出,送入15%的盐酸溶液中浸泡3小时,过滤,得滤渣,用清水洗净,烘干、研磨成600目粉体;所得粉体与其它剩余成分混合,加热至60-70℃,搅拌反应50分钟,冷却,研磨成浆料,即得。
所述的一种铜雕塑用含沥青的氟碳树脂漆,其制备工艺为:
(1)将白炭黑、2-苯并咪唑氨基甲酸甲酯、沥青、助剂混合,加入到二甲苯、乙酸丁酯溶剂中,加热至120-130℃,反应4小时;
(2)将步骤(1)的物料冷却至70-85℃,加入醋酸丁酸纤维素、异佛尔酮二异氰酸酯、硬脂酸钡,搅拌反应4小时;
(3)将步骤(2)的物料降温至50-65℃,加入其它剩余物料,搅拌反应60分钟后,冷却至室温,研磨成60μm浆料,即得。
本发明油漆的性能测试结果为:
上述测试均遵循相关标准进行。

Claims (2)

1.一种铜雕塑用含沥青的氟碳树脂漆,其特征在于,该油漆由以下重量份的原料制成:氟碳树脂20-24、长油度醇酸树脂20-24、白炭黑10-12、2-苯并咪唑氨基甲酸甲酯4-7、沥青5-8、1,6-己二醇二丙烯酸酯20-30、醋酸丁酸纤维素1-2、六偏磷酸钠1-2、聚氨酯丙烯酸酯20-30、异佛尔酮二异氰酸酯9-12、硬脂酸钡2-5、四丙基溴化铵1-2、环烷酸钴2-3、助剂5-6、二甲苯10-12、乙酸丁酯10-12;
所述的助剂由以下重量份的原料制成:粘土10-14、纳米铁矿渣粉1-2、促进剂M3-4、苯基三乙氧基硅烷2-3、钼酸钠1-2、磁石2-3、苯甲酸钠1-2、柠檬酸三丁酯35-40、没食子酸丙酯2-3、薏仁油3-4、二硼化钒1-2、表儿茶素2-3;制备方法是将粘土、磁石送入煅烧炉中在720-740℃下煅烧2-3小时,然后取出,送入10-15%的盐酸溶液中浸泡2-3小时,过滤,得滤渣,用清水洗净,烘干、研磨成400-600目粉体;所得粉体与其它剩余成分混合,加热至60-70℃,搅拌反应40-50分钟,冷却,研磨成浆料,即得。
2.如权利要求1所述的一种铜雕塑用含沥青的氟碳树脂漆,其制作工艺为:
(1)将白炭黑、2-苯并咪唑氨基甲酸甲酯、沥青、助剂混合,加入到二甲苯、乙酸丁酯溶剂中,加热至120-130℃,反应3-4小时;
(2)将步骤(1)的物料冷却至70-85℃,加入醋酸丁酸纤维素、异佛尔酮二异氰酸酯、硬脂酸钡,搅拌反应3-4小时;
(3)将步骤(2)的物料降温至50-65℃,加入其它剩余物料,搅拌反应40-60分钟后,冷却至室温,研磨成20-60μm浆料,即得。
CN201310676109.2A 2013-12-07 2013-12-07 一种铜雕塑用含沥青的氟碳树脂漆 Active CN103709851B (zh)