CN103660328A - 能锯钻孔打不烂耐用性提高几倍的泡沫塑玻板 - Google Patents
能锯钻孔打不烂耐用性提高几倍的泡沫塑玻板 Download PDFInfo
- Publication number
- CN103660328A CN103660328A CN201210352171.1A CN201210352171A CN103660328A CN 103660328 A CN103660328 A CN 103660328A CN 201210352171 A CN201210352171 A CN 201210352171A CN 103660328 A CN103660328 A CN 103660328A
- Authority
- CN
- China
- Prior art keywords
- glass
- glass plate
- foam plastic
- plate
- plastic
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
泡沫塑玻板由塑料粘合玻璃布组成。玻璃纤维的拉力是金属纤维拉力的几倍,玻璃布由多条玻璃纤维组成的玻璃线编织成,所以玻璃布拉力强,富有弹性;由多层玻璃布组成的塑玻板抗紫外线;塑玻板内的泡沫,令泡沫塑玻板的浮力比竹伐大几倍;玻璃布1元/m2,回收塑料约二千元/吨;竹伐使用几年,泡沫塑玻板寿命百年;泡沫塑玻板的浮力比竹伐大几倍,所以泡沫塑玻板取代竹伐,广泛使用于水面养殖,以及山区的浅水河面运输;在做车厢,船舱,家具,铺盖大型厂房,装修等占有优势。
Description
玻璃,不怕酸碱虫蚁,但怕撞击,一碰即碎;若无撞击,寿命过千年,令金属板自感不如。
目前,竹伐广泛使用于水面养殖,以及山区的浅水河面运输,但竹伐是竹子制作,寿命短。本技术提出的《取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板》,简称泡沫塑玻板,能解决上述问题。
《取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板》,其有益效果是,取代竹伐,延长使用时间,减轻重量,降低成本。
取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板,其解决技术问题所采用的技术方案是,由塑料(1)粘合玻璃布(2)组成,其工艺是,将塑料加热成熔液作为粘合剂,用机具使多块玻璃布通过塑料熔液,令塑料熔液包裹玻璃布,刮除多余的塑料熔浆,令多块玻璃布重叠制成塑玻板(3);取塑玻板制成板条,在板条一边相隔同等距离开窄缝(4),窄缝宽等于板条厚度,窄缝长大于板条宽度一半,获得扦板条(5);将扦板条的窄缝对扦,获得格板(6);取格板放在塑玻板上,再取塑玻板放在格板上,塑玻板格板相间重叠至要求厚度,然后送入炉膛加热,令塑玻板格板的接触处熔粘紧密,冷却后获得泡沫塑玻板(7);从而使取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板得以运行。如图1
现结合原理介绍泡沫塑玻板:
据报道,玻璃纤维的拉力是金属纤维拉力的几倍。
本技术将玻璃纤维和塑料两种材料有机地结合起来。令产品富有全新的优点。
玻璃布由多条玻璃纤维组成的玻璃线编织成,所以玻璃布富有弹性。当塑玻板受到冲击时,塑料将冲击力传给玻璃布,富有弹性的玻璃布就将冲击力吸收。而且随着玻璃布层数增多,塑玻板承受的冲击力不断增强,直至可和钢板较量。
由于玻璃纤维的拉力是金属纤维拉力的几倍,所以,塑玻板的抗拉性能,也可和钢板较量,使塑料板不能相比。
塑玻板的抗紫外线性能比塑料板提高数倍,因为,塑玻板由多层玻璃布组成。当面层的塑料受损老化。老化的塑料会将紫外线阻隔,令第二层塑料免受紫外线侵害。同时,面层玻璃布也会拦截紫外线,令第二层塑料免受紫外线侵害。
塑玻板内含多层富有弹性的玻璃布,令它稍有弹性。这种特性是塑料板,钢板所没有的,令它在特殊的场合占有优势。
塑玻板格板相间重叠,板壁之间构成泡沫,经炉膛加热,令各板壁熔粘紧密,使板内泡沫保持不变,水不能进入泡沫内,令泡沫塑玻板的浮力比竹伐大几倍。
玻璃布是用硅砂制作。塑料是用石油制作。塑玻板含玻璃布的比例远大于塑料,使我们节省大量石油,因此,塑玻板是环保产品。
经济效益,玻璃布市场价每平方米小于一元,回收塑料约二千元一吨;竹伐使用几年,泡沫塑玻板寿命百年;泡沫塑玻板的浮力比竹伐大几倍。
说明书附图说明
图1:取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板
1塑料,2玻璃布,3塑玻板,4窄缝,5扦板条,6格板,7泡沫塑玻板
Claims (1)
1.取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板,其特征是,由塑料粘合玻璃布组成,其工艺是,将塑料加热成熔液作为粘合剂,用机具使多块玻璃布通过塑料熔液,令塑料熔液包裹玻璃布,刮除多余的塑料熔浆,令多块玻璃布重叠制成塑玻板;取塑玻板制成板条,在板条一边相隔同等距离开窄缝,窄缝宽等于板条厚度,窄缝长大于板条宽度一半,获得扦板条;将扦板条的窄缝对扦,获得格板;取格板放在塑玻板上,再取塑玻板放在格板上,塑玻板格板相间重叠至要求厚度,然后送入炉膛加热,令塑玻板格板的接触处熔粘紧密,冷却后获得泡沫塑玻板;从而使取代竹伐寿命百年能锯钻孔打不烂的泡沫塑玻板得以运行。