CN103614039A - 一种硅丙乳液防水涂料 - Google Patents

一种硅丙乳液防水涂料 Download PDF

Info

Publication number
CN103614039A
CN103614039A CN201310517163.2A CN201310517163A CN103614039A CN 103614039 A CN103614039 A CN 103614039A CN 201310517163 A CN201310517163 A CN 201310517163A CN 103614039 A CN103614039 A CN 103614039A
Authority
CN
China
Prior art keywords
parts
raw material
organosilicon crylic
adds
crylic acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN201310517163.2A
Other languages
English (en)
Other versions
CN103614039B (zh
Inventor
肖宪书
文庆华
张俊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BENGBU GAOHUA ELECTRONIC Co.,Ltd.
Original Assignee
BENGBU CITY GAOHUA ELECTRONIC Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU CITY GAOHUA ELECTRONIC Co Ltd filed Critical BENGBU CITY GAOHUA ELECTRONIC Co Ltd
Priority to CN201310517163.2A priority Critical patent/CN103614039B/zh
Publication of CN103614039A publication Critical patent/CN103614039A/zh
Application granted granted Critical
Publication of CN103614039B publication Critical patent/CN103614039B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种硅丙乳液防水涂料,它是由下述重量份的原料组成的:SD528硅丙乳液75-80、10,10’-氧代双吩恶砒1-2、山梨醇2-3、聚丙烯酰胺1-2、硼酸1-2、硅酸钾钠2-3、苯酚1-2、大理石粉10-14、硬脂酸镉0.5-2、松香酸聚氧乙烯酯1-2、氯化石蜡0.5-1、粘结助剂6-10、去离子水7-20,本发明的防水涂料涂层柔韧性好,手感好,能遮蔽基层细小裂纹,有一定的装饰效果,防水性强,对基材的保护性好。

Description

一种硅丙乳液防水涂料
技术领域
    本发明主要涉及一种涂料,尤其涉及一种硅丙乳液防水涂料。
背景技术
    随着国内涂料行业的不断发展和细化,市场对具有特种功能性涂料的要求亦越来越突出,其中对于抗老化、耐水、耐酸碱腐蚀、阻燃等性能要求更加高,为了满足各行业对防水涂料的要求,生产高性能,应用广泛的防水涂料很有必要。
发明内容
本发明目的就是提供一种硅丙乳液防水涂料。
本发明是通过以下技术方案实现的:
一种硅丙乳液防水涂料,它是由下述重量份的原料组成的:
SD528硅丙乳液75-80、10,10’-氧代双吩恶砒1-2、山梨醇2-3、聚丙烯酰胺1-2、硼酸1-2、硅酸钾钠2-3、苯酚1-2、大理石粉10-14、硬脂酸镉0.5-2、松香酸聚氧乙烯酯1-2、氯化石蜡0.5-1、粘结助剂6-10、去离子水7-20;
所述的粘结助剂是由下述重量份的原料组成的:
白乳胶32-40、硅烷偶联剂KH-5504-6、聚乙烯吡咯烷酮1-2、泡花碱2-3、聚乳酸3-5、偏硅酸钠1-2、纳米碳1-2;
将上述聚乳酸加热到180-185℃,加入硅烷偶联剂KH-550,搅拌混合3-5分钟,降低温度为55-60℃,加入纳米碳,300-500转/分搅拌分散6-10分钟,降低至常温,加入偏硅酸钠、聚乙烯吡咯烷酮、泡花碱,球磨1-2小时,加入剩余各原料,在70-90℃下保温静置1-2小时,冷却,充分球磨,即得所述粘结助剂。
一种硅丙乳液防水涂料的制备方法,包括以下步骤:
将上述除了SD528硅丙乳液以外的各原料混合,1000-1400转/分搅拌分散17-20分钟,加入剩余各原料,高速搅拌至混合均匀,即得所述硅丙乳液防水涂料。
本发明的优点是:
本发明的防水涂料涂层柔韧性好,手感好,能遮蔽基层细小裂纹,有一定的装饰效果,防水性强,对基材的保护性好。
具体实施方式
实施例1
一种硅丙乳液防水涂料,它是由下述重量份(公斤)的原料组成的:
SD528硅丙乳液80、10,10’-氧代双吩恶砒2、山梨醇3、聚丙烯酰胺2、硼酸1、硅酸钾钠2、苯酚1-2、大理石粉14、硬脂酸镉0.5、松香酸聚氧乙烯酯2、氯化石蜡0.5、粘结助剂10、去离子水10;
所述的粘结助剂是由下述重量份的原料组成的:
白乳胶40、硅烷偶联剂KH-5506、聚乙烯吡咯烷酮2、泡花碱3、聚乳酸3、偏硅酸钠1、纳米碳2;
将上述聚乳酸加热到185℃,加入硅烷偶联剂KH-550,搅拌混合3分钟,降低温度为60℃,加入纳米碳,500转/分搅拌分散6分钟,降低至常温,加入偏硅酸钠、聚乙烯吡咯烷酮、泡花碱,球磨2小时,加入剩余各原料,在90℃下保温静置1小时,冷却,充分球磨,即得所述粘结助剂。
一种硅丙乳液防水涂料的制备方法,包括以下步骤:
将上述除了SD528硅丙乳液以外的各原料混合,1400转/分搅拌分散20分钟,加入剩余各原料,高速搅拌至混合均匀,即得所述硅丙乳液防水涂料。
性能测试:
延伸率:≥300% ;
不透水性:0.3MPa( 一个小时不透水)。

Claims (2)

1.一种硅丙乳液防水涂料,其特征在于它是由下述重量份的原料组成的:
SD528硅丙乳液75-80、10,10’-氧代双吩恶砒1-2、山梨醇2-3、聚丙烯酰胺1-2、硼酸1-2、硅酸钾钠2-3、苯酚1-2、大理石粉10-14、硬脂酸镉0.5-2、松香酸聚氧乙烯酯1-2、氯化石蜡0.5-1、粘结助剂6-10、去离子水7-20;
所述的粘结助剂是由下述重量份的原料组成的:
白乳胶32-40、硅烷偶联剂KH-5504-6、聚乙烯吡咯烷酮1-2、泡花碱2-3、聚乳酸3-5、偏硅酸钠1-2、纳米碳1-2;
将上述聚乳酸加热到180-185℃,加入硅烷偶联剂KH-550,搅拌混合3-5分钟,降低温度为55-60℃,加入纳米碳,300-500转/分搅拌分散6-10分钟,降低至常温,加入偏硅酸钠、聚乙烯吡咯烷酮、泡花碱,球磨1-2小时,加入剩余各原料,在70-90℃下保温静置1-2小时,冷却,充分球磨,即得所述粘结助剂。
2.一种如权利要求1所述的硅丙乳液防水涂料的制备方法,其特征在于包括以下步骤:
将上述除了SD528硅丙乳液以外的各原料混合,1000-1400转/分搅拌分散17-20分钟,加入剩余各原料,高速搅拌至混合均匀,即得所述硅丙乳液防水涂料。
CN201310517163.2A 2013-10-28 2013-10-28 一种硅丙乳液防水涂料 Active CN103614039B (zh)