CN103541099B - Semi-worsted warm fancy suiting and production method thereof - Google Patents

Semi-worsted warm fancy suiting and production method thereof Download PDF

Info

Publication number
CN103541099B
CN103541099B CN201310488617.8A CN201310488617A CN103541099B CN 103541099 B CN103541099 B CN 103541099B CN 201310488617 A CN201310488617 A CN 201310488617A CN 103541099 B CN103541099 B CN 103541099B
Authority
CN
China
Prior art keywords
hair
yarn
worsted
spinning
warm
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310488617.8A
Other languages
Chinese (zh)
Other versions
CN103541099A (en
Inventor
杨丽萍
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Jiangyin Huanju Textile Co.,Ltd.
Original Assignee
Jiangsu Nijiaxiang Group Worsted Textile Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangsu Nijiaxiang Group Worsted Textile Co Ltd filed Critical Jiangsu Nijiaxiang Group Worsted Textile Co Ltd
Priority to CN201310488617.8A priority Critical patent/CN103541099B/en
Publication of CN103541099A publication Critical patent/CN103541099A/en
Application granted granted Critical
Publication of CN103541099B publication Critical patent/CN103541099B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses semi-worsted warm fancy suiting. Warps of the suiting are made by stranding and twisting raw semi-worsted yarns of 66s Australasian wool and polyamide fiber and 75D polyester warm fiber. Wefts of the suiting are made by stranding and twisting raw semi-worsted yarns of 66s Australasian wool and polyamide fiber, 75D polyester warm fiber and 30D Lycra. The finished suiting comprises, by weight, 77% of 66s Australasian wool, 9% of polyamide fiber, 13% of 75D polyester warm fiber, and 1% of 30D Lycra. The invention further discloses a production method of the semi-worsted warm fancy suiting. The semi-worsted warm fancy suiting has the effects of permanent warmth retention in polyester warm fiber, excellent sweat transfer function, lightweight, warmness, provision of ease of action, softness and comfort; the semi-worsted warm fancy suiting is as styled as the semi-worsted product; compared to worsted fabric, the semi-worsted warm fancy suiting is bulky and soft; compared to worsted fabric of same material, the semi-worsted warm fancy suiting has the cost reduced by 30%; good economic benefit can be created for enterprises.

Description

Half spinning warming fancy suiting and production method thereof
Technical field
The present invention relates to a kind of half worsted fabric, particularly relate to a kind of half spinning warming fancy suiting and production method thereof.
Background technology
Along with the development of society, people more and more pay attention to natural environmental protection, wear healthy, comfortable, lie fallow that oneself becomes the topic of a fashion of people.In this year, the simple theory that people act on " life is exactly life ", makes every effort to the normal state keeping life, and seek new hope wherein, fabric mainly with " life perpetuity, decorative art; be suitable for as upper, usually spirit " four themes, towards environmental protection, health, the future development that gets close to nature.The parent that quality fabric that is good, that have again specific function more and more obtains people looks at.At present, in this area, du pont company is proposed a kind of terylene thermal fiber by studying the fur of polar bear, and this thermal fiber has forever warming usefulness, the function of remarkable perspire, merrily and lightheartedly warmly makes activity freely, and soft comfortable.
Summary of the invention
For the demand, the object of the present invention is to provide a kind of feel sliding glutinous, soft comfortable, good springiness, has half spinning warming fancy suiting of permanent thermal property and remarkable perspiration discharging performance simultaneously.
Another object of the present invention is to provide the production method of this half spinning warming fancy suiting.
The object of the invention is to be achieved through the following technical solutions:
A kind of half spinning warming fancy suiting, this fabric is with 66 saustralia's hair, nylon fibre, 75D terylene thermal fiber and 30D Lycra are raw material, and the warp thread of this fabric is by 66 saustralia's hair and nylon fibre are that the spinning obtained yarn of raw material half and 75D terylene thermal fiber doubling twisting are made, and the weft yarn of this fabric is by 66 saustralia's hair and nylon fibre are that the spinning obtained yarn of raw material half and 75D terylene thermal fiber and 30D Lycra doubling twisting are made; In this article, the weight ratio of each raw material is 66 saustralia's hair 77%, nylon fibre 9%, 75D terylene thermal fiber 13%, 30D Lycra 1%
The production method of above-mentioned half spinning warming fancy suiting, its step is as follows:
(1), first by 66 saustralia's hair, nylon fibre adopt loose stock dyeing to dye respectively, adopt loose stock dyeing can overcome the unmanageable problem of homochromatism of the different fibers caused when wool fibre and these two kinds of different materials of nylon fibre carry out blending, ensure dyeing quality;
(2), by 66 after above-mentioned dyeing saustralia's hair and nylon fibre carry out and hair, cotton spinning spinning process is adopted again namely through opening picking → comb and parallel cotton fibers prior to spinning → drafting → silver lap → combing → drafting (three roads) → rove → spun yarn → obtain spun yarn from winder on cotton spinning apparatus, adopt wool yarn spinning process to obtain warp thread through double twisting → yarn steaming by after spun yarn and the doubling of 75D terylene thermal fiber, adopt wool yarn spinning process to obtain weft yarn through double twisting → yarn steaming by after spun yarn and 75D terylene thermal fiber and the doubling of 30D Lycra, wherein, with add wool lubricant water and antistatic additive during hair, frictionally damage when making fiber surface smoothly reduce combing, with hair more than 2 times, to ensure to mix, the raw material after becoming reconciled need store 24 hours in hair storehouse, allows wool lubricant water and the abundant osmotic absorption of antistatic additive, reach balanced required regain, for the combing slivering of lower road creates conditions, adopt and prepare spun yarn with cotton spinning spinning process on cotton spinning apparatus, that plurality of raw materials blending can be avoided to adopt run into during smart wool spinning equipment is larger in the fibre loss of front yarn grilling operation, higher in spinning process end breakage rate, serious around roller, bar is done poor, the problem that cost of material waste is larger, the method can make up the difference in wool fibre and polyamide fibre length simultaneously, cohesive force between fiber is provided, improve the brute force of yarn, save cost-effectively simultaneously, and yarn texture is different from common smart wool spinning, though technical requirement is higher, trial-production difficulty, but wastage of material is less, obtained yarn texture is tight, soft and smooth, fabric good hand touch, and cotton spinning apparatus processing cost is lower, effectively save production cost, improve added value of product.
(3), by above-mentioned obtained warp thread and weft yarn undertaken weaving obtained fancy suiting grey cloth, fancy suiting grey cloth is carried out Final finishing and gets product, weaving process is: warping → gait, draw reed → weave → base inspection → raw to repair, wherein, warping technology parameter is: linear velocity 300m/min, the reduction of this place's Negotiation speed, thus avoids broken end serious, weaving efficiency is improved, beaming speed 50m/min, yarn tension 3.5 degree, beaming tension force 1kg, adjustment Warp line is back rest front and back position 105cm, highly-1cm, menelipsis height-2cm, front and back position 56cm, tension force 200kg, the adjustment of this Warp line can solve fault such as latitude bow yarn, skips etc., because half spinning warming fancy suiting is multiple fiber blend, Final finishing will take into full account the characteristic of various fiber, as inappropriate technology, can have an impact to certain fiber, and change product style, can produce a desired effect to make finished product, hindlimb unload is the key guaranteeing final finished quality, for this reason in Final finishing process, we carry out test of many times to main technique, final technique is: middle inspection (base inspection) → singe → put down boil → wash contracting → flat boiling → drying → shaping → middle inspection → ripely to repair → bristle → cropping → hydrophilic processing → brush cuts → high pressure steaming → tank steaming → preshrunk → one-tenth examines, wherein, singe: strong flame, positive and negative respectively once, braying: first adopt low speed to wash, 150 ms/min, 40 minutes, fabric preliminarily stabilised is shunk, then by washing at a high speed, 250 ms/min, 20 minutes, strengthen feel, bristle: 2 is positive 1 anti-, cropping: 3 is positive 1 anti-, preshrunk: setting moisture regain 11%, speed 10 ms/min, overfeeding 10%, in this article, the weight ratio of each raw material is Australia's hair 77%, nylon fibre 9%, 75D terylene thermal fiber 13%, 30D Lycra 1%.
In half spinning warming fancy suiting of the present invention, by Australia's hair, polyamide fibre, terylene thermal fiber and Lycra organically merge, and formulated a series of rational bar dye, spinning, weave, postfinishing process is to ensure that each raw material plays respective effect and makes finished product produce a desired effect, 66s Australia hair, nylon fibre and 30D Lycra can make fabric feeling sliding glutinous, soft comfortable, good springiness, especially 66s Australia hair and nylon fibre adopt half spinning technique to combine, make fabric can have the style of the novel fashion of half spun yarn product, 75D terylene thermal fiber can make fabric have forever warming usefulness, remarkable perspiration functions, merrily and lightheartedly warmly make activity freely and the usefulness of soft comfortable.
The present invention compared with prior art beneficial effect be:
Fabric of the present invention not only has the forever warming usefulness of terylene thermal fiber, remarkable perspiration functions, merrily and lightheartedly warmly makes activity freely and the usefulness of soft comfortable, and there is the style of the novel fashion of half spun yarn product, fabric feel, property of hanging down, body bone have new meaning very much, find everything fresh and new to the sensation of people, have higher social benefit; Meanwhile, it is fluffy, soft that fabric compares smart wool spinning, reduces costs 30% compared with spinning homogeneity fabric, can be enterprise and create good economic benefit.
concrete enforcement formula
Embodiment 1
First by 66 saustralia's hair, nylon fibre adopt loose stock dyeing to dye respectively;
By 66 after above-mentioned dyeing saustralia's hair and nylon fibre carry out and hair, cotton spinning spinning process is adopted again namely through opening picking → comb and parallel cotton fibers prior to spinning → drafting → silver lap → combing → drafting (three roads) → rove → spun yarn → obtain spun yarn from winder on cotton spinning apparatus, adopt wool yarn spinning process to obtain warp thread through double twisting → yarn steaming by after spun yarn and the doubling of 75D terylene thermal fiber, adopt wool yarn spinning process to obtain weft yarn through double twisting → yarn steaming by after spun yarn and 75D terylene thermal fiber and the doubling of 30D Lycra; Wherein, and during hair, add wool lubricant water and antistatic additive, and hair more than 2 times, the raw material after becoming reconciled need store 24 hours in hair storehouse;
Above-mentioned obtained warp thread and weft yarn are carried out weaving obtained fancy suiting grey cloth, fancy suiting grey cloth is carried out Final finishing and gets product; Weaving process is: warping → gait, draw reed → weave → base inspection → raw to repair; Wherein, warping technology parameter is: linear velocity 300m/min, beaming speed 50m/min, yarn tension 3.5 degree, beaming tension force 1kg; Adjustment Warp line is back rest front and back position 105cm, highly-1cm, menelipsis height-2cm, front and back position 56cm, tension force 200kg; Postfinishing process is: middle inspection (base inspection) → singe → put down boil → wash contracting → flat boiling → drying → shaping → middle inspection → ripely to repair → bristle → cropping → hydrophilic processing → brush cuts → high pressure steaming → tank steaming → preshrunk → one-tenth examines; Wherein, singe: strong flame, positive and negative respectively once; Braying: first adopt low speed to wash, 150 ms/min, 40 minutes, then by washing at a high speed, 250 ms/min, 20 minutes; Bristle: 2 is positive 1 anti-; Cropping: 3 is positive 1 anti-; Preshrunk: setting moisture regain 11%, speed 10 ms/min, overfeeding 10%.
In this article, the weight ratio of each raw material is Australia's hair 77%, nylon fibre 9%, 75D terylene thermal fiber 13%, 30D Lycra 1%; Finished product warp count: 158/10 centimetres, weft count: 135/10 centimetres, fabric width: 154 centimetres, meter Chong: 340 grams/meter.
The above, be only the specific embodiment of the present invention, but protection scope of the present invention is not limited thereto, and any change of expecting without creative work or replacement, all should be encompassed within protection scope of the present invention.Therefore, the protection domain that protection scope of the present invention should limit with claims is as the criterion.

Claims (2)

1. a half spinning warming fancy suiting, it is characterized in that, this fabric is with 66 saustralia's hair, nylon fibre, 75D terylene thermal fiber and 30D Lycra are raw material, and the warp thread of this fabric is by 66 saustralia's hair and nylon fibre are that the spinning obtained yarn of raw material half and 75D terylene thermal fiber doubling twisting are made, and the weft yarn of this fabric is by 66 saustralia's hair and nylon fibre are that the spinning obtained yarn of raw material half and 75D terylene thermal fiber and 30D Lycra doubling twisting are made; In this article, the weight ratio of each raw material is 66 saustralia's hair 77%, nylon fibre 9%, 75D terylene thermal fiber 13%, 30D Lycra 1%.
2. the production method of half spinning warming fancy suiting according to claim 1, it is characterized in that, its step is as follows:
(1), first by 66 saustralia's hair, nylon fibre adopt loose stock dyeing to dye respectively;
(2), by 66 after above-mentioned dyeing saustralia's hair and nylon fibre carry out and hair, cotton spinning spinning process is adopted again namely through opening picking → comb and parallel cotton fibers prior to spinning → drafting → silver lap → combing → tri-road drafting → rove → spun yarn → obtain spun yarn from winder on cotton spinning apparatus, adopt wool yarn spinning process to obtain warp thread through double twisting → yarn steaming by after spun yarn and the doubling of 75D terylene thermal fiber, adopt wool yarn spinning process to obtain weft yarn through double twisting → yarn steaming by after spun yarn and 75D terylene thermal fiber and the doubling of 30D Lycra; Wherein, and during hair, add wool lubricant water and antistatic additive, and hair more than 2 times, the raw material after becoming reconciled need store 24 hours in hair storehouse;
(3), by above-mentioned obtained warp thread and weft yarn undertaken weaving obtained fancy suiting grey cloth, fancy suiting grey cloth is carried out Final finishing and gets product; Weaving process is: warping → gait, draw reed → weave → base inspection → raw to repair; Wherein, warping technology parameter is: linear velocity 300m/min, beaming speed 50m/min, yarn tension 3.5 degree, beaming tension force 1kg; Adjustment Warp line is back rest front and back position 105cm, highly-1cm, menelipsis height-2cm, front and back position 56cm, tension force 200kg; Postfinishing process is: base examines → singes → flat boil → wash contracting → flat boiling → drying → shaping → middle inspection → ripely to repair → bristle → cropping → hydrophilic processing → brush cuts → high pressure steaming → tank steaming → preshrunk → one-tenth examines; Wherein, singe: strong flame, positive and negative respectively once; Braying: first adopt low speed to wash, 150 ms/min, 40 minutes, then by washing at a high speed, 250 ms/min, 20 minutes; Bristle: 2 is positive 1 anti-; Cropping: 3 is positive 1 anti-; Preshrunk: setting moisture regain 11%, speed 10 ms/min, overfeeding 10%; In this article, the weight ratio of each raw material is Australia's hair 77%, nylon fibre 9%, 75D terylene thermal fiber 13%, 30D Lycra 1%.
CN201310488617.8A 2013-10-18 2013-10-18 Semi-worsted warm fancy suiting and production method thereof Active CN103541099B (en)