CN103525388A - 一种消除井筒内硫化氢的化学配方 - Google Patents

一种消除井筒内硫化氢的化学配方 Download PDF

Info

Publication number
CN103525388A
CN103525388A CN201310422460.9A CN201310422460A CN103525388A CN 103525388 A CN103525388 A CN 103525388A CN 201310422460 A CN201310422460 A CN 201310422460A CN 103525388 A CN103525388 A CN 103525388A
Authority
CN
China
Prior art keywords
hydrogen sulfide
water
pit shaft
alkaline agent
agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310422460.9A
Other languages
English (en)
Inventor
蒋生健
王家暖
廉清勤
韩海龙
李胜文
刘喜成
杨雄
赵德宝
闫大雨
汤琦
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liaohe Petroleum Exploration Bureau
Original Assignee
Liaohe Petroleum Exploration Bureau
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Liaohe Petroleum Exploration Bureau filed Critical Liaohe Petroleum Exploration Bureau
Priority to CN201310422460.9A priority Critical patent/CN103525388A/zh
Publication of CN103525388A publication Critical patent/CN103525388A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种油田汽驱作业井筒硫化氢防治技术领域,特别涉及一种消除井筒内硫化氢的化学配方。该该化学配方由氟碳表面活性剂FC-4430、主剂、碱剂和水组成,其中主剂采用三氯化铁,碱剂采用三乙醇胺或碳酸氢钠;主剂与碱剂溶解在水中,主剂和碱剂的质量之和占水的质量百分比为5%~9.4%,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.05%~0.8%。本发明实现了较少消除剂即可完全消除井筒内硫化氢的目的,使用有效率高,成本低,有效时间长,地层污染少。克服了现有硫化氢消除剂使用有效率低和过量压井污染地层的不足。

Description

一种消除井筒内硫化氢的化学配方
技术领域:
本发明涉及一种油田汽驱作业井筒硫化氢防治技术领域,特别涉及一种消除井筒内硫化氢的化学配方。
背景技术:
消除井筒内硫化氢的方法主要有两种,常规方法为添加碱中和法,钻井时采用的硫化氢消除剂主要成分为碱式碳酸铜,即属于碱中和法。油水井作业时添加碳酸钠,磷酸钠等也属于碱中和法。使用碱中和法时,由于硫化氢酸性较弱,所以往往碱需要先中和掉其他酸才能与硫化氢反应,造成消除剂使用有效率低。另一类办法即过量压井,采用大量压井液,将硫化氢顶入地层,该方法造成地层污染严重。
发明内容:
本发明要解决的技术问题是提供一种消除井筒内硫化氢的化学配方,该配方实现了较少消除剂即可完全消除井筒内硫化氢的目的,使用有效率高,成本低,有效时间长,地层污染少。克服了现有硫化氢消除剂使用有效率低和过量压井污染地层的不足。
本发明所采取的技术方案是:一种消除井筒内硫化氢的化学配方,该化学配方由氟碳表面活性剂FC-4430、主剂、碱剂和水组成,其中主剂采用三氯化铁,碱剂采用三乙醇胺或碳酸氢钠;主剂与碱剂溶解在水中,主剂和碱剂的质量之和占水的质量百分比为5%~9.4%,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.05%~0.8%。
本发明的有益效果是:本发明实现了较少消除剂即可完全消除井筒内硫化氢的目的,使用有效率高,成本低,有效时间长,地层污染少。
具体实施方式:
一种消除井筒内硫化氢的化学配方,该化学配方由氟碳表面活性剂FC-4430、主剂、碱剂和水组成,其中主剂采用三氯化铁,碱剂采用三乙醇胺或碳酸氢钠;主剂与碱剂溶解在水中,主剂和碱剂的质量之和占水的质量百分比为5%~9.4%,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.05%~0.8%。在该配方中,主剂与碱剂的量根据地层进入井筒的硫化氢的量来决定。其中主剂的量应该为理论值的1.8倍以上,碱剂为理论值的2倍以上。
实施例1:
将17kg三氯化铁和18kg碳酸氢钠溶解在600kg的水中,主剂和碱剂的质量之和占水的质量百分比为5.8%,再向水中加入0.48kg氟碳表面活性剂,并搅匀,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.08%。从井口向套管内灌注该消除剂,10分钟后进行作业。同时在井口采用硫化氢检测仪进行井口硫化氢含量测定。直至施工结束,作业时间约60小时,监控硫化氢浓度时间75小时,期间硫化氢含量最高时出现在第49小时,为5ppm,其余时间均低于该值,满足现场施工需求。
实施例2:
将13kg三氯化铁和14kg碳酸氢钠溶解在500kg的水中,主剂和碱剂的质量之和占水的质量百分比为5.4%,再向水中加入4kg氟碳表面活性剂,并搅匀,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.8%。从井口向套管内灌注该消除剂,10分钟后进行作业。同时在井口采用硫化氢检测仪进行井口硫化氢含量测定。直至施工结束,作业时间约72小时,监控硫化氢浓度时间80小时,期间硫化氢含量最高时出现在第60小时,为3ppm,其余时间均低于该值,满足现场施工需求。
实施例3:
将162kg三氯化铁和167kg碳酸氢钠溶解在3500kg的水中,主剂和碱剂的质量之和占水的质量百分比为9.4%,再向水中加入1.75kg氟碳表面活性剂,并搅匀,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.05%。从井口向套管内灌注该消除剂,10分钟后进行作业。同时在井口采用硫化氢检测仪进行井口硫化氢含量测定。直至施工结束,作业时间约64小时,监控硫化氢浓度时间71小时,期间硫化氢含量最高时出现在第59小时,为7ppm,其余时间均低于该值,满足现场施工需求。
实施例4:
将14kg三氯化铁和26kg三乙醇胺溶解在800kg的水中,主剂和碱剂的质量之和占水的质量百分比为5%,再向水中加入0.5kg氟碳表面活性剂,并搅匀,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.06%。从井口向套管内灌注该消除剂,10分钟后进行作业。同时在井口采用硫化氢检测仪进行井口硫化氢含量测定。直至施工结束,作业时间约66小时,监控硫化氢浓度时间72小时,期间硫化氢含量最高时为7ppm,其余时间均低于该值,满足现场施工需求。
可以理解的是,以上关于本发明的具体描述,仅用于说明本发明而并非受限于本发明实施例所描述的技术方案,本领域的普通技术人员应当理解,仍然可以对本发明进行修改或等同替换,以达到相同的技术效果;只要满足使用需要,都在本发明的保护范围之内。

Claims (1)

1.一种消除井筒内硫化氢的化学配方,其特征在于:该化学配方由氟碳表面活性剂FC-4430、主剂、碱剂和水组成,其中主剂采用三氯化铁,碱剂采用三乙醇胺或碳酸氢钠;主剂与碱剂溶解在水中,主剂和碱剂的质量之和占水的质量百分比为5%~9.4%,氟碳表面活性剂FC-4430的质量占水的质量百分比为0.05%~0.8%。
CN201310422460.9A 2013-09-17 2013-09-17 一种消除井筒内硫化氢的化学配方 Pending CN103525388A (zh)