CN103508534A - 一种改性活性炭废水凝絮剂及其制备方法 - Google Patents

一种改性活性炭废水凝絮剂及其制备方法 Download PDF

Info

Publication number
CN103508534A
CN103508534A CN201310387326.XA CN201310387326A CN103508534A CN 103508534 A CN103508534 A CN 103508534A CN 201310387326 A CN201310387326 A CN 201310387326A CN 103508534 A CN103508534 A CN 103508534A
Authority
CN
China
Prior art keywords
parts
water
flocculant
attapulgite
modified
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310387326.XA
Other languages
English (en)
Inventor
孙夕雨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Original Assignee
BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd filed Critical BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Priority to CN201310387326.XA priority Critical patent/CN103508534A/zh
Publication of CN103508534A publication Critical patent/CN103508534A/zh
Pending legal-status Critical Current

Abstract

一种改性活性炭废水凝絮剂,由下列重量份的原料制成:活性炭100-120、丙烯酸10-12、丙烯酰胺3-4、甲基丙烯酰氧乙基三甲基氯化铵10-12、煅石膏10-12、枯矾5-6、改性凹凸棒土8-10、硅烷偶联剂KH-5501-2、水适量。本发明使用了丙烯酸、丙烯酰胺、甲基丙烯酰氧乙基三甲基氯化铵对活性炭进行改性,可以对水中污染物起到更好的凝絮作用,通过加入煅石膏、枯矾可以起到抗菌的作用,通过加入硅烷偶联剂KH-550,加强了该凝絮剂的强度,不易崩解。

Description

一种改性活性炭废水凝絮剂及其制备方法
技术领域
本发明涉及一种非金属矿的改性方法,尤其涉及一种改性活性炭废水凝絮剂及其制备方法。
背景技术
随着科技的发展,现代化工业的逐步建设,各种化学品被开发利用,给人们生活带来了便利,同时由于化学品产生了对环境和人体有害的物质,也成了人们不得不面对的问题。
目前空气中的污染物主要是工业燃料燃烧产生的气体、汽车尾气、生产中产生的有毒有害气体。水污染主要是工业生产排放的污水里含有大量有毒物质,还有人们生活中的污水产生很多有害物质。人们生活中也有很多时候需要脱除毒素,比如空调过滤网上有很多细菌、毒素,新装修的间有甲醛等有害物质,都需要脱除毒素。目前都脱除毒素经常用到吸附剂,主要有硅胶、活性氧化铝、活性炭、分子筛等,另外还有针对某种组分选择性吸附而研制的吸附材料。但是这些吸附剂大多吸附能力有限,需要针对不同的要求研究不同的吸附剂,发挥最好的作用。同时,寻找新的原料,以增强吸附效果,节约成本。
发明内容
本发明的目的在于提供一种改性活性炭废水凝絮剂及其制备方法。
本发明的技术方案如下:
一种改性活性炭废水凝絮剂,其特征在于由下列重量份的原料制成:活性炭100-120、丙烯酸10-12、丙烯酰胺3-4、甲基丙烯酰氧乙基三甲基氯化铵10-12、煅石膏10-12、枯矾5-6、改性凹凸棒土8-10、硅烷偶联剂KH-550 1-2、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、硝酸银1-2、明矾5-6、铁矿渣粉1-2、聚四氟乙烯4-5、硫酸钛14-18、玉石粉12-14、硫酸锌1-2、氧化铬3-4、吗啉1-2、N-2-(氨乙基)-3-氨丙基三甲氧基硅烷2-3、水适量;将凹凸棒土、铁矿渣粉送入煅烧炉中,在950-990℃下煅烧3-4小时,取出,洒上N-2-(氨乙基)-3-氨丙基三甲氧基硅烷再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
所述改性活性炭废水凝絮剂的制备方法,其特征在于包括以下步骤:将丙烯酸、丙烯酰胺、甲基丙烯酰氧乙基三甲基氯化铵、煅石膏、枯矾、硅烷偶联剂KH-550混合后,加适量水,加热至80-90℃,研磨至200-300目浆料,然后,加入活性炭、改性凹凸棒土继续研磨1-2小时,喷雾干燥后,送入320-350℃热处理炉中,处理2-3小时,取出,冷却即得。
分发明的有益效果
本发明使用了丙烯酸、丙烯酰胺、甲基丙烯酰氧乙基三甲基氯化铵对活性炭进行改性,可以对水中污染物起到更好的凝絮作用,通过加入煅石膏、枯矾可以起到抗菌的作用,通过加入硅烷偶联剂KH-550,加强了该凝絮剂的强度,不易崩解。
具体实施方式
一种改性活性炭废水凝絮剂,由下列重量份(公斤)的原料制成:活性炭110、丙烯酸11、丙烯酰胺3、甲基丙烯酰氧乙基三甲基氯化铵11、煅石膏11、枯矾5-6、改性凹凸棒土9、硅烷偶联剂KH-550 1.5、水适量;
所述改性凹凸棒土由以下重量份(公斤)的原料制成:凹凸棒土110、硝酸银1.5、明矾5、铁矿渣粉1、聚四氟乙烯4、硫酸钛16、玉石粉13、硫酸锌1、氧化铬3、吗啉1、N-2-(氨乙基)-3-氨丙基三甲氧基硅烷2、水适量;将凹凸棒土、铁矿渣粉送入煅烧炉中,在970℃下煅烧3小时,取出,洒上N-2-(氨乙基)-3-氨丙基三甲氧基硅烷再放入适量水中研磨,调节研磨液PH值为4,研磨1小时,得到100目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200目浆料,喷雾干燥,即得。
所述改性活性炭废水凝絮剂的制备方法,包括以下步骤:将丙烯酸、丙烯酰胺、甲基丙烯酰氧乙基三甲基氯化铵、煅石膏、枯矾、硅烷偶联剂KH-550混合后,加适量水,加热至85℃,研磨至200目浆料,然后,加入活性炭、改性凹凸棒土继续研磨1小时,喷雾干燥后,送入340℃热处理炉中,处理2小时,取出,冷却即得。
经测定,其碘值1574mg/g,亚甲基蓝吸附值27.9mL/0.1g。

Claims (2)

1.一种改性活性炭废水凝絮剂,其特征在于由下列重量份的原料制成:活性炭100-120、丙烯酸10-12、丙烯酰胺3-4、甲基丙烯酰氧乙基三甲基氯化铵10-12、煅石膏10-12、枯矾5-6、改性凹凸棒土8-10、硅烷偶联剂KH-550 1-2、水适量;所述改性凹凸棒土由以下重量份的原料制成:凹凸棒土120-130、硝酸银1-2、明矾5-6、铁矿渣粉1-2、聚四氟乙烯4-5、硫酸钛14-18、玉石粉12-14、硫酸锌1-2、氧化铬3-4、吗啉1-2、N-2-(氨乙基)-3-氨丙基三甲氧基硅烷2-3、水适量;将凹凸棒土、铁矿渣粉送入煅烧炉中,在950-990℃下煅烧3-4小时,取出,洒上N-2-(氨乙基)-3-氨丙基三甲氧基硅烷再放入适量水中研磨,调节研磨液PH值为4-5,研磨1-2小时,得到100-150目浆料,再调节研磨液PH值为中性,加入其它剩余成分,继续研磨,得到200-300目浆料,喷雾干燥,即得。
2.根据权利要求1所述改性活性炭废水凝絮剂的制备方法,其特征在于包括以下步骤:将丙烯酸、丙烯酰胺、甲基丙烯酰氧乙基三甲基氯化铵、煅石膏、枯矾、硅烷偶联剂KH-550混合后,加适量水,加热至80-90℃,研磨至200-300目浆料,然后,加入活性炭、改性凹凸棒土继续研磨1-2小时,喷雾干燥后,送入320-350℃热处理炉中,处理2-3小时,取出,冷却即得。
CN201310387326.XA 2013-08-30 2013-08-30 一种改性活性炭废水凝絮剂及其制备方法 Pending CN103508534A (zh)